Engineering PapersSearch

SEARCH · Engineering Papers

Results for “Molten Salt System”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Na/beta-alumina/NaAlCl4, Cl2/C circulating cell

A study was made of a high specific energy battery based on a sodium negative electrode and a chlorine positive electrode with molten AlCl3-NaCl electrolyte and a solid beta alumina separator. The basic performance of a Na beta-alumina NaAlCl4, Cl2/C circulating cell at 200 C was demonstrated. This cell can be started at 150 C. The use of melting sodium chloroaluminate electrolyte overcomes some of the material problems associated with the high working temperatures of present molten salt systems, such as Na/S and LiAl/FeS, and retains the advantages of high energy density and relatively efficient electrode processes. Preliminary investigations were conducted on a sodium-chlorine static cell, material compability, electrode design, wetting, and theoretical calculations to assure a better chance of success before assembling a Na/Cl2 circulating cell. Mathematical models provide a theoretical explanation for the performance of the NaCl2 battery. The results of mathematical models match the experimental results very well. According to the result of the mathematical modeling, an output at 180 mA/sq cm and 3.2 V can be obtained with optimized cell design.

Cherng, Jing-Yih

High-temperature molten salt thermal energy storage systems

The results of comparative screening studies of candidate molten carbonate salts as phase change materials (PCM) for advanced solar thermal energy storage applications at 540 to 870 C (1004 to 1600 F) and steam Rankine electric generation at 400 to 540 C (752 to 1004 F) are presented. Alkali carbonates are attractive as latent heat storage materials because of their relatively high storage capacity and thermal conductivity, low corrosivity, moderate cost, and safe and simple handling requirements. Salts were tested in 0.1 kWhr lab scale modules and evaluated on the basis of discharge heat flux, solidification temperature range, thermal cycling stability, and compatibility with containment materials. The feasibility of using a distributed network of high conductivity material to increase the heat flux through the layer of solidified salt was evaluated. The thermal performance of an 8 kWhr thermal energy storage (TES) module containing LiKCO3 remained very stable throughout 5650 hours and 130 charge/discharge cycles at 480 to 535 C (896 to 995 F). A TES utilization concept of an electrical generation peaking subsystem composed of a multistage condensing steam turbine and a TES subsystem with a separate power conversion loop was defined. Conceptual designs for a 100 MW sub e TES peaking system providing steam at 316 C, 427 C, and 454 C (600 F, 800 F, and 850 F) at 3.79 million Pa (550 psia) were developed and evaluated. Areas requiring further investigation have also been identified.

Petri, R. J.

Multiphase Species Transport Modeling for Molten Salt Reactors in the System Analysis Module: Generation, Decay, Deposition, and Extraction of Insoluble Fission Products

With the increase of interests in the design and deployment of advanced reactor systems, a desire for simulation tools supporting system analysis of reactor operation and safety is rising. Molten salt reactors (MSRs), one of the advanced reactor systems, utilize liquid fused salt fuel as both coolant and fuel. During operation, MSR generates insoluble fission products, including noble metals and gases. The buildup of these species in fuel salt presents safety concerns as they may deposit on surfaces of critical components and produce excessive decay heat, causing the failure of system components. Timely removal of these noble metals and gases would ensure the safe operation of the reactor system. The dynamic nature of salt fuel system, involving the generation, decay, deposition, and extraction of noble metals and gases, calls for robust species transport models to facilitate system analysis and monitoring, and design of efficient species removal components. This paper concentrates on the development of a computational framework for species transport, consisting of multiphase transport model formulation, mass transfer between phases, numerical implementation in MOOSE environment, verification through Method of Manufacture Solutions (MMS) and validation against experimental data from the Molten Salt Reactor Experiment (MSRE). Integrating this framework into the System Analysis Module (SAM) code further enhances SAM’s capabilities for advanced reactor analysis in the future.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS

MSTL Re-Start Phase 1.5 Project Final Report

This document provides an overview of re-start efforts at Sandia National Laboratories (SNL), National Solar Thermal Test Facility (NSTTF), for the SNL Molten Salt Test Loop (MSTL). MSTL is one of the world’s only industrial-scale molten salt test systems, capable of testing commercial-scale thermal hydraulic equipment at an industrial scale, required for confident bankability of products. This work was facilitated as part of the Phase 1 re-start effort for facilitating forensics assessments to inform final refurbishments and upgrades costs and schedule information for revitalizing MSTL for use during a separate Phase 2 effort. This work was facilitated to further de-risk a Phase 2 effort pertaining to the tank and the pump, which were considered during Phase 1 to be high-risk items for a successful re-start. Impact from a successful re-start will allow SNL and other industrial molten salt systems companies, such as those in the Market Utilization Report provided in the Phase 1 submission package. An objective of this document is to also ensure longevity of utilization of MSTL after re start.

14 SOLAR ENERGY

Application of a Triple Bubbler Inside Molten Salt for Pyroprocessing Safeguards Purposes

The application of a triple bubbler system within molten salt environments, specifically a eutectic mixture of LiCl-KCl, is explored for nuclear safeguards purposes, focusing on nuclear material accountancy (NMA) and holdup accountancy in pyroprocessing techniques. Traditional holdup accountancy methods, which involve periodic sampling and lengthy lead times, are being supplemented by the development of actinide sensors using electrochemistry. However, these methods alone are insufficient to meet regulatory requirements set by agencies like NRC and IAEA. The triple bubbler device measures salt level, density, and surface tension simultaneously using three dip tubes of varying diameters and heights. This study investigates the accuracy and robustness of the triple bubbler in molten salt conditions at temperatures ranging from 450-550°C. The updated bubbler design, utilizing tantalum metal and larger tube geometry, demonstrated minimal plugging and maintained measurement accuracy within acceptable uncertainties: 0.611% for depth, 1.34% for density, and approximately 40% for surface tension. Results indicate that the triple bubbler system is effective for real-time, accurate measurements in pyroprocessing environments, making it a promising tool for ensuring compliance with nuclear safeguards and supporting nuclear non-proliferation efforts.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS

In Situ Spectroscopic Monitoring of MSR Molten Salt and Off-Gas Systems

A significant challenge that must be overcome before commercialization of molten salt reactors is tracking special nuclear material (SNM) through the reactor and subsystems such as fuel chemical processing and off-gas systems. In recent years, several approaches have been explored to track SNM, fission products, and corrosion products in these different subsystems. One such approach is to employ laser and optical spectroscopy to measure the atomic and molecular signals of MSR salts. The advantages of these approaches are that they typically are non-intrusive and offer the capability of process monitoring while still providing low uncertainties. At the Idaho National Laboratory, spectroscopy approaches such as laser-induced breakdown spectroscopy (LIBS) and ultraviolet-visible (UV-Vis) spectroscopy have been utilized to investigate molten salts in an aerosol (LiCl, KCl, RbCl2, NdCl3, and PrCl3) and vapor phases (MgCl5, NdCl5, and ZrCl4) with success. Testing to date has yielded qualitative information on all the above species and quantitative data and analytical figures of merit for species in the vapor phases. These findings, including results from ongoing testing, as well as the experimental conditions and potential applications will be presented.

98 - NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL

Assessment of RELAP5-3D Code with Molten Salt Heat Transfer Experiments

The accurate thermal-hydraulic assessment of thermal storage systems is crucial for addressing the integrity and performance of the storage system design. This is particularly important for thermal storage systems using molten salts as a heat transport and storage medium, as the chemical corrosion and erosion by the high-temperature molten salts can cause serious damage to the structural components of the storage system. To understand these effects for TerraPower’s Natrium® Demonstration Reactor design, the system thermal-hydraulic analysis code, RELAP5-3D, is utilized to analyze the thermal storage system. This study evaluates two heat transfer correlations implemented in the RELAP5-3D code—the Dittus-Boelter and Gnielinski correlations—using selected benchmark cases from two molten salt heat transfer experiments conducted at Xi’an Jiao Tong University and the German Aerospace Center. The Nusselt numbers calculated using the Gnielinski correlation agree with the experimental data within ±5% of the relative deviations at 300°C and 400°C. With the increasing Reynolds numbers, the Dittus-Boelter correlation underestimates the Nusselt numbers by up to 22% compared to the Gnielinski correlation. Comparison of the RELAP5-3D calculation results with experimental data at a high temperature of 550°C revealed that the thermo-chemical characteristics of solar salt at high temperatures surpassing the decomposition temperatures of nitrate salts reduce the accuracy of heat transfer model of the RELAP5-3D code. Specifically, it has been observed that the temperatures of the wall surface and liquid near the wall can surpass the decomposition temperatures, even though the bulk temperature of molten salts remains significantly lower than these decomposition temperatures. In summary, this study recommends the use of the Gnielinski correlation for the heat transfer analysis of molten salt, rather than the Dittus-Boelter correlation.

21 - SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLAN

Effect of Surrogate Fission Products on Thermal Conductivity and Viscosity of NaCl-UCl 3

Thermophysical properties of salt systems relevant to molten salt reactors (MSRs) are experimentally measured in support of the US Department of Energy Office of Nuclear Energy (DOE-NE) MSR campaign within the Advanced Reactor Technology (ART) Program. These property measurements also support the development of the thermophysical arm of the Molten Salt Database (MSD) within DOE-NE’s Nu clear Energy Advanced Modeling and Simulation (NEAMS) Program. Several US Department of Energy (DOE) laboratories, including Oak Ridge National Laboratory (ORNL), have been capitalizing on modern methodologies and sample characterization techniques to conduct thermophysical property measurements to support these programs and to provide MSR developers and modelers with more recent and higher-quality data.

22 GENERAL STUDIES OF NUCLEAR REACTORS

High-temperature molten salt thermal energy storage systems for solar applications

Experimental results of compatibility screening studies of 100 salt/containment/thermal conductivity enhancement (TCE) combinations for the high temperature solar thermal application range of 704 deg to 871 C (1300 to 1600 F) are presented. Nine candidate containment/HX alloy materials and two TCE materials were tested with six candidate solar thermal alkali and alkaline earth carbonate storage salts (both reagent and technical grade of each). Compatibility tests were conducted with salt encapsulated in approx. 6.0 inch x 1 inch welded containers of test material from 300 to 3000 hours. Compatibility evaluations were end application oriented, considering the potential 30 year lifetime requirement of solar thermal power plant components. Analyses were based on depth and nature of salt side corrosion of materials, containment alloy thermal aging effects, weld integrity in salt environment, air side containment oxidation, and chemical and physical analyses of the salt. A need for more reliable, and in some cases first time determined thermophysical and transport property data was also identified for molten carbonates in the 704 to 871 C temperature range. In particular, accurate melting point (mp) measurements were performed for Li2CO3 and Na2CO3 while melting point, heat of fusion, and specific heat determinations were conducted on 81.3 weight percent Na2CO3-18.7 weight percent K2CO3 and 52.2 weight percent BaCO3-47.8 weight percent Na2CO3 to support future TES system design and ultimate scale up of solar thermal energy storage (TES) subsystems.

Petri, R. J.

Molten Salt Thermal Energy Storage Systems

The feasibility of storing thermal energy at temperatures of 450 C to 535 C in the form of latent heat of fusion was examined for over 30 inorganic salts and salt mixtures. Alkali carbonate mixtures were chosen as phase-change storage materials in this temperature range because of their relatively high storage capacity and thermal conductivity, moderate cost, low volumetric expansion upon melting, low corrosivity, and good chemical stability. Means of improving heat conduction through the solid salt were explored.

Maru, H. C.

High-temperature molten salt thermal energy storage systems for solar applications

Alkali and alkaline earth carbonate latent-heat storage salts, metallic containment materials, and thermal conductivity enhancement materials were investigated to satisfy the high temperature (704 to 871 C) thermal energy storage requirements of advanced solar-thermal power generation concepts are described. Properties of the following six salts selected for compatibility studies are given: three pure carbonates, K2CO3, Li2CO3 and Na2CO3; two eutectic mixtures, BaCO3/Na2CO3 and K2CO3/NaCO3, and one off-eutectic mixture of Na2CO3/K2CO3.

Petri, R. J.

Impact of molten salt inflow on the temperature distribution in thermal energy storage tanks at startup for central receiver concentrating solar power plants

Concentrating Solar Power (CSP) systems with molten salt thermal energy storage (TES) tanks are one of the most promising, renewable-based energy conversion technologies for larger-scale power generation. The TES tank is one of the most critical components in CSP plants due to its high-temperature operation (up to 565 °C), daily thermal cycling, and intermittent solar radiation conditions. The plant startup is one of the most challenging operation conditions that could lead to damaging thermal gradients due to low salt inventory levels. In this study an analytical model for the sparger ring was developed and integrated with a detailed computational fluid dynamics model of a commercial-scaled molten salt tank. The integrated model allows an accurate representation of the tank operation to evaluate the effect of molten salt inflow on the mixing process. The tank filling process during plant startup was analyzed considering sparger rings with variations in design features, including inlet orifice configurations, number of orifices, direction of the inlets, and orifice diameter. The results demonstrated that higher temperature gradients are obtained in the tank floor during the plant startup. A sparger ring configuration with a predetermined orifice inlet inclination (30°, 45° and 60°) leads to significant temperature differences in the floor, between 57 °C and 62 °C, but better homogeneity in the temperature of the salt inventory. Lower salt inflow velocities result in a more homogeneous floor temperature, with maximum temperature differences under 38 °C. The sparger ring configuration with 52 orifices of 1-in. diameter and vertical flow showed better homogeneity in the temperature differences as a function of the salt level and lower temperature gradients in the tank floor. Because large temperature gradients in the tank's floor have been identified as one of the main factors contributing to tank failures, assessing various sparger ring design features is fundamental to determining proper inflow conditions that lead to low-temperature gradients and reducing failure susceptibility.

14 SOLAR ENERGY

Internally insulated thermal storage system development program

A cost effective thermal storage system for a solar central receiver power system using molten salt stored in internally insulated carbon steel tanks is described. Factors discussed include: testing of internal insulation materials in molten salt; preliminary design of storage tanks, including insulation and liner installation; optimization of the storage configuration; and definition of a subsystem research experiment to demonstrate the system. A thermal analytical model and analysis of a thermocline tank was performed. Data from a present thermocline test tank was compared to gain confidence in the analytical approach. A computer analysis of the various storage system parameters (insulation thickness, number of tanks, tank geometry, etc.,) showed that (1) the most cost-effective configuration was a small number of large cylindrical tanks, and (2) the optimum is set by the mechanical constraints of the system, such as soil bearing strength and tank hoop stress, not by the economics.

Scott, O. L.

Elucidating the corrosion mechanism of Ni-based superalloys in the presence of uranium-containing chloride molten salt

The United States Department of Energy (DOE) is committed to the advancement of nuclear reactor technology through initiatives such as the Advanced Reactor Development Program (ARDP), in an effort to diversify the United States energy portfolio towards more sustainable energy options. The ARDP includes demonstration by industry partners of molten chloride fast reactors (MCFRs). Construction of MCFRs requires qualified nuclear structural materials. Unfortunately, there are no current materials that are fully qualified by the Nuclear Regulatory Commission for the construction of molten salt reactors, including MCFRs. Adapting current structural material qualifications requires expansion of our current knowledgebase on the property-performance relationships regarding corrosion performance. In this investigation, we assess microstructural changes in a Ni-based superalloy after exposure to a UCl3¬-containing chloride salt eutectic mixture through a correlated multi-modal approach combining several advanced characterization techniques, including scanning electron microscopy/focused ion beam (SEM/FIB) and transmission electron microscopy (TEM). SEM/FIB analysis will illustrate changes in elemental composition, microstructure, and isotopic information acquired from energy x-ray dispersive spectroscopy (EDS), electron backscatter diffraction (EBSD), and secondary ion mass spectroscopy (SIMS), respectively. This information will then aid in identifying localized regions to elucidate the corrosion mechanism with TEM through a combination of electron diffraction, electron energy loss spectroscopy (EELS), and additional EDS. The findings from this investigation will further expand our assessment of the corrosion performance of structural materials in molten salt chloride systems, aiding to developing fully qualified materials for construction of MCFRs.

36 MATERIALS SCIENCE

CSP Systems Analysis 2022-2024 (Final Technical Report)

The CSP Systems Analysis project estimates the current market cost of CSP subsystems and technologies for use by the DOE Program and within NREL analysis tools. The project addresses upgrades to NREL's System Advisor Model (SAM) related to CSP, as well as development of new modules within SAM to expand the types of CSP systems that can be simulated and new tools for evaluating CSP subsystem performance or optimizing CSP system layouts, for example, SolarPILOT and SolTrace. The project evaluates the potential cost and performance of new CSP-relevant technologies and generally includes assessment of CSP technologies in support of the DOE subprogram. A primary goal of the CSP System Analysis project is to provide timely and accurate cost data to the DOE to assess the current state of CSP technologies as well as predict performance and cost for pre-commercial and emerging technologies that may impact the industry. Prior work in this task has produced technology cost reports and roadmaps for DOE and highlighted promising research paths that could reduce overall CSP cost, such as the supercritical CO2 power cycle and molten-salt trough systems. CSP Systems Analysis produces modeling tools to evaluate the performance of CSP systems, subsystems, or components, and journal articles, conference papers, technical reports and databases to disseminate information to the CSP industry. CSP technology costs are estimated and tracked using these tools as well as analysis of literature and industry sources. The CSP modeling tools and NREL analysis results are used by researchers; government, financial, and industry analysts; and other CSP stakeholders. The purpose of this final technical report is to summarize the key accomplishments of the past three years of this project. The project was divided into seven separate tasks, and in what follows, we describe the background, objectives, key accomplishments, and path forward for each task within the project, with one section of this report summarizing each task.

14 SOLAR ENERGY

Reciprocal Ternary Molten Salts Enable the Direct Upcycling of Spent Lithium‐Nickel‐Manganese‐Cobalt Oxide (NMC) Mixtures to Make NMC 622

Cathode active material is the most valuable component of spent lithium‐ion batteries, accounting for ≈30% of their overall value. Direct recycling of cathode materials involves recovering, regenerating, and reusing them without breaking down their chemical structure. This approach maximizes the added value of the cathode compound and reduces manufacturing costs by avoiding the need for virgin material production. However, one key challenge in scaling direct recycling from lab to industry is the requirement for highly purified cathode materials, contrasting with the low purity of black mass generated from battery shredding. No efficient separation process currently exists to isolate different lithium‐nickel‐manganese‐cobalt oxides (NMCs) from each other. Thus, direct recycling technologies that can operate with mixtures of multiple NMC stoichiometries will be best‐suited for industrial adoption. This study explores the direct recycling of NMC mixtures into NMC 622 using a “reciprocal ternary molten salts (RTMS)” system. Ionothermal relithiation and upcycling within the RTMS system successfully restore the layered structure, lithium content, and electrochemical performance of degraded NMCs, yielding results comparable to pristine NMC 622 (P‐NMC 622).

25 ENERGY STORAGE

Quantification of trace iodine using laser-induced breakdown spectroscopy for real-time monitoring of nuclear off-gas streams

This study evaluated the potential of laser-induced breakdown spectroscopy (LIBS) for real-time monitoring of trace gas-phase iodine, which is an element of high significance in nuclear applications due to its long radioactive half-life (as iodine-129), volatility, and biological impact. In anticipation of iodine evolving into off-gas systems in molten salt reactor and nuclear fuel recycling applications, this research aimed to assess LIBS performance in flowing argon and helium matrices; optimize measurement parameters using a multichannel spectrometer; and perform calibrations to assess predictive capabilities and limits of detection (LODs). Experimental results successfully measured gas-phase iodine in flowing argon and helium; however, trace iodine was not detected in air. Optimal delay times were determined to be 10 µs for argon and 1 µs for helium, which are consistent with the expected shorter plasma lifetime in helium relative to argon. An emission line survey was provided with the 206.16, 804.37, 902.24, and 905.83 nm peaks, which were identified as the strongest emission peaks. Calibration models were successfully built in both helium and argon, achieving LODs down to 3 ppm in helium and 5 ppm in argon. The iodine emission at 905.83 nm emerged as the most robust for calibration and was subsequently applied to a time series dataset in argon. The predictive trace confirmed the feasibility of employing LIBS for continuous, online quantification of trace iodine in flowing gas systems.

Andrews, Hunter B. [Oak Ridge National Laboratory

Measurement of partial vapor pressures of salt mixtures via combined horizontal transpiration and thermogravimetric analysis

A method combining thermogravimetric analysis (TGA) and horizontal transpiration with elemental analysis via inductively coupled plasma mass spectrometry or ion chromatography enabled calculation of partial pressures of individual salts in molten mixtures. TGA quantified total mass loss, while transpiration identified vapor-phase composition. Furthermore, two chloride (NaCl-MgCl 2 , NaCl-MgCl 2 + UCl 3 ) salts and one mixed halide (LiCl-LiF + Li 2 O) salt were analyzed at 750 °C and 550 °C, respectively. NaCl and MgCl 2 vapor pressures were 2.19–2.61 × 10 -4 atm and 2.47–2.48 × 10 -5 atm (dependent upon the identity of the invesitgated mixture); UCl 3 was 1.42 × 10 -7 atm. LiCl and LiF vapor pressures at 550 °C were 1.53 × 10 -6 and 6.32 × 10 -6 atm, respectively. Additionally, the TGA method was validated against values from the literature for unary LiCl and LiF.

36 MATERIALS SCIENCE