Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “METALLOGRAPHY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Non-destructive Quantitative Phase Analysis and Microstructural Characterization of Zirconium Coated U-10Mo Fuel Foils via Neutron Diffraction

This report uses neutron diffraction to investigate the crystal phase composition of uranium-molybdenum alloy foils (U-10Mo) for the CONVERT MP-1 Reactor Conversion Project, and determines the effect on alpha-uranium contamination following the deposition of a Zr metal diffusion layer by various methods: plasma spray deposition of Zr powders at LANL and hot co-rolling with Zr foils at BWXT. In summary, there is minimal decomposition of the gamma phase U-10Mo foil to alpha phase contamination following both plasma spraying and hot co-rolling. The average unit cell volume, i.e. lattice spacing, of the Zr layer can be mathematically extracted from the diffraction data; co-rolled Zr matches well with literature values of bulk Zr, while plasma sprayed Zr shows a slight increase in the lattice spacing, indicative of interstitial oxygen in the lattice. Neutron diffraction is a beneficial alternative to conventional methods of phase composition, i.e. x ray diffraction (XRD) and destructive metallography. XRD has minimal penetration depth in high atomic number materials, particularly uranium, and can only probe the first few microns of the fuel plate; neutrons pass completely through the foil, allowing for bulk analysis of the foil composition and no issues with addition of cladding layers, as in the final, aluminum-clad reactor fuel plates. Destructive metallography requires skilled technicians, cutting of the foil into small sections, hazardous etching conditions, long polishing and microscopy times, etc.; the neutron diffraction system has an automated sample loader and can fit larger foils, so there is minimal analysis preparation; the total spectrum acquisition time is ~ 1 hour per sample. The neutron diffraction results are limited by spectra refinement/calculation times and the availability of the neutron beam source. In the case of LANSCE at Los Alamos, the beam operates ~50% of the year. Following the lessons learned from these preliminary results, optimizations to the process and analysis can be made, and neutron diffraction can become a viable and efficient technique for gamma/alpha phase composition determination for nuclear fuels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Examination of Legacy Metallic Fuel Pins (U-10Zr) Tested in FFTF

The MFF series of metallic fuel (U-10wt%Zr) tests performed in the Fast Fuel Test Facility (FFTF) were the beginning tests to qualify the fuel as a driver fuel for FFTF. They all performed very well, to relatively high burnup and with no pin breaches. Tests MFF-3 and MFF-5 were chosen to be destructively examined because they were run at high peak cladding temperatures, 643 and 649°C respectively, and to modest to high burnup (138 and 101 MWd/kgM respectively). They were the only sodium fast reactor (SFR) metallic tests, with long (91.4 cm) fuel columns and clad in HT9, to be operated at these high temperatures. Extensive operating condition reconstruction was performed to accompany the examination, providing detailed operating conditions axially along the pins. In addition, detailed ORIGEN calculations provided fuel burnup along the pin length. These calculations and detailed cross-section metallography allowed a PhD dissertation to be performed where the fuel/cladding chemical interaction (FCCI) was modeled using Fickian and Soret Effect driven diffusion of rare earth fission products to the cladding surface and interact with the cladding. The examination of the MFF-3 and MFF-5 pins included neutron radiography, axial profilometry including pin bow and length measurements, precision gamma scanning, plenum gas puncturing to measure fission gas release, detailed chemical/isotopic analyses of fuel samples to confirm burnup calculations, and metallography of pin cross-sections, including micro-hardness measurements of fuel and cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An Investigation of Liquefaction in Irradiated TRIGA Fuel Exposed to Relatively High Temperatures

This report presents the findings of an investigation into high temperature fuel cladding chemical interactions (FCCI) in Training, Research, Isotopes, General Atomics (TRIGA) fuel rods. A TRIGA fuel-rod core or meat is principally composed of uranium (U) particles dispersed in a zirconium hydride (Zr H) matrix. The fuel is clad in sealed 304SS or Incoloy 800 tubes. At high temperatures, the fuel will interact with the cladding, resulting in FCCI. To investigate the FCCI (in this case, liquefaction), irradiated TRIGA fuel rods were exposed to relatively high temperatures in furnace tests. The tests were performed at different temperatures using segments from an irradiated TRIGA fuel rod at the Hot Fuel Examination Facility located at Idaho National Laboratory (INL). The data from this study is important for developing a better understanding of the performance of U-ZrH fuel type during transient events (e.g., a Loss of Coolant Accident (LOCA) event) that may result in high temperatures while operating a TRIGA reactor. Furnace tests were run for 6 hours at 730, 800, 900, 950, and 1,000°C. One test was run for 12 hours at 950°C. Post-test microstructural characterization was performed on the heat-treated samples using optical metallography to look for evidence of liquefaction. Additionally, microstructural characterization was performed using scanning electron microscopy to investigate the microstructure of the as-irradiated fuel before heat treatment and the microstructural changes that occurred after heat treating for the 730 and 950°C heat treatments for 6 hours. Results of the analysis were compared to those produced during diffusion studies performed using unirradiated TRIGA fuel meat and type 304 stainless steel. A gap is typically present in as-irradiated fuel that limits any possibility for chemical interaction between the fuel and cladding. Optical metallography (OM) was used to identify areas in the specimens heat treated at 950 and 1000°C where fuel and cladding contact was satisfactory for the FCCI to transpire. The bulk of the interaction zones that form due to FCCI developed in the fuel meat and not as much in the cladding. Even in the sample tested at 1,000°C, no evidence was found that gross fuel meat or cladding melting had occurred. Only limited porosity was found in the fuel meat that possibly could have been due to melting of a particular precipitate phase or phases that had formed during FCCI. These results agreed with those reported for the unirradiated diffusion couple studies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Investigation of high temperature fracture of T-111 and ASTAR-811C

The high temperature deformation and fracture behavior of T-111 and ASTAR-811C were studied over the temperature range 982 to 2205 C (1800 to 4000 F). As-cast and wrought-recrystallized material as well as GTA welds in sheet and plate were evaluated using conventional tensile and creep tests. Post test examinations were performed using optical metallography, scanning electron microscopy and transmission electron microscopy. A high temperature region of reduced ductility, in terms of tensile elongation, was identified for both alloys. The reduction in tensile elongation became more severe with increase in grain size, being near catastrophic for the as-cast specimens. Optical and electron metallography indicated that even for failures at very low total strain, considerable deformation of a very localized nature had occurred prior to fracture.

Gold, R. E.↗

Laser Brazing of High Temperature Braze Alloy

The Space Shuttle Main Engine (SSME) consists of 1080 conical tubes, which are furnace brazed themselves, manifolds, and surrounding structural jacket making almost four miles of braze joints. Subsequent furnace braze cycles are performed due to localized braze voids between the coolant tubes. SSME nozzle experiences extremely high heat flux (180 mW/sq m) during hot fire. Braze voids between coolant tubes may result in hot combustion gas escape causing jacket bulges. The nozzle can be disqualified for flight or result in mission failure if the braze voids exceed the limits. Localized braze processes were considered to eliminate braze voids, however, damage to the parent materials often prohibited use of such process. Being the only manned flight reusable rocket engine, it has stringent requirement on the braze process. Poor braze quality or damage to the parent materials limits the nozzle service life. The objective of this study was to develop a laser brazing process to provide quality, localized braze joints without adverse affect on the parent materials. Gold (Au-Cu-Ni-Pd-Mn) based high temperature braze alloys were used in both powder and wire form. Thin section iron base superalloy A286 tube was used as substrate materials. Different Laser Systems including CO2 (10.6 micrometers, 1kW), ND:YAG (1.06 micrometers, 4kW). and direct diode laser (808nm. 150W) were investigated for brazing process. The laser process variables including wavelength. laser power, travel speed and angle of inclination were optimized according to bead geometry and braze alloy wetting at minimum heat input level, The properties of laser brazing were compared to that of furnace brazing. Microhardness profiles were used for braze joint property comparison between laser and furnace brazing. The cooling rate of laser brazing was compared to furnace brazing based on secondary dendritic arm spacing, Both optical and Scanning Electron Microscope (SEM) were used to evaluate the microstructures of the braze materials and tube substrate. Metallography of the laser braze joint was compared to the furnace braze. SEM Energy Disperse X-Ray Spectra (EDX) and back scattered imaging were used to analyze braze alloy segregation. Although all of the laser systems, CO2, ND:YAG, and direct diode laser produced good braze joint, the direct diode laser was selected for its system simplicity, compactness and portability. Excellent laser and braze alloy coupling is observed with powder alloy compared to braze alloy wire. Good wetting is found with different gold based braze alloys. The laser brazing process can be optimized so that the adverse affect on the parent materials can be eliminated. Metallography of the laser braze joint has shown that quality braze joint was produced with laser brazing process. Penetration of the laser braze to the substrate is at neglectable level. Zero penetration is observed. Microstructure examinations shown that no observable changes of the microstructure (grain structure and precipitation) in the HAZ area between laser braze and furnace braze. Wide gaps can be laser brazed with single pass for up to 0.024 inches. Finer dendritic structure is observed in laser brazing compared with equiaxial and coarser grain of the furnace brazing microstructure. Greater segregation is also found in the furnace braze. Higher hardness of the laser braze joint comparing to furnace braze is observed due to the fast cooling rate and Finer microstructure in the laser brazing. Laser braze joint properties meet or exceed the furnace joint properties. Direct diode laser for thin section tube brazing with high temperature braze alloys have been successfully demonstrated. The laser's high energy density and precise control has shown significant advantages in reducing process heat input to the substrates and provide high quality braze joints comparing to other localized braze process such as torch, TIG, and MPTA processes. Significant cost savings can be realized particularly with localized braze comparing to a full furnace braze cycle.

Gao, Y. P.↗

Three-Dimensional Computed Tomography as a Method for Finding Die Attach Voids in Diodes

NASA analyzes electrical, electronic, and electromechanical (EEE) parts used in space vehicles to understand failure modes of these components. The diode is an EEE part critical to NASA missions that can fail due to excessive voiding in the die attach. Metallography, one established method for studying the die attach, is a time-intensive, destructive, and equivocal process whereby mechanical grinding of the diodes is performed to reveal voiding in the die attach. Problems such as die attach pull-out tend to complicate results and can lead to erroneous conclusions. The objective of this study is to determine if three-dimensional computed tomography (3DCT), a nondestructive technique, is a viable alternative to metallography for detecting die attach voiding. The die attach voiding in two- dimensional planes created from 3DCT scans was compared to several physical cross sections of the same diode to determine if the 3DCT scan accurately recreates die attach volumetric variability

Brahm, E. N.↗

Computational Process Modeling for Additive Manufacturing

Computational Process and Material Modeling of Powder Bed additive manufacturing of IN 718. Optimize material build parameters with reduced time and cost through modeling. Increase understanding of build properties. Increase reliability of builds. Decrease time to adoption of process for critical hardware. Potential to decrease post-build heat treatments. Conduct single-track and coupon builds at various build parameters. Record build parameter information and QM Meltpool data. Refine Applied Optimization powder bed AM process model using data. Report thermal modeling results. Conduct metallography of build samples. Calibrate STK models using metallography findings. Run STK models using AO thermal profiles and report STK modeling results. Validate modeling with additional build. Photodiode Intensity measurements highly linear with power input. Melt Pool Intensity highly correlated to Melt Pool Size. Melt Pool size and intensity increase with power. Applied Optimization will use data to develop powder bed additive manufacturing process model.

Bagg, Stacey↗

Inclusion Detection in Aluminum Alloys Via Laser-Induced Breakdown Spectroscopy

Laser-induced breakdown spectroscopy (LIBS) has shown promise as a technique to quickly determine molten metal chemistry in real time. Because of its characteristics, LIBS could also be used as a technique to sense for unwanted inclusions and impurities. Simulated Al{sub 2}O{sub 3} inclusions were added to molten aluminum via a metal-matrix composite. LIBS was performed in situ to determine whether particles could be detected. Outlier analysis on oxygen signal was performed on LIBS data and compared to oxide volume fraction measured through metallography. It was determined that LIBS could differentiate between melts with different amounts of inclusions by monitoring the fluctuations in signal for elements of interest. LIBS shows promise as an enabling tool for monitoring metal cleanliness.

36 MATERIALS SCIENCE↗

Archaeological Arsenical Bronzes and Equilibrium in the As-Cu System

Understanding the effects of impurities, segregation, undercooling, and solidification velocity is necessary to reconstruct prehistoric As-Cu alloy manufacturing processes and practices. Moreover, these alloys often contain a wide variety of minor and trace elements such that the binary As-Cu equilibrium phase diagram does not adequately represent arsenical bronze artifacts as-cast in ancient molds. Furthermore, the variable cooling rates present in as-cast alloys of predominantly arsenic and copper, due to the thermal properties of differing mold materials, would have had profound effects on the formation of inversely segregated arsenic. Alloys with 1 to 15 wt pct arsenic were prepared and studied using differential thermal analysis, metallography, and scanning electron microscopy with energy-dispersive X-ray spectroscopy. Equilibrium diagrams were established and the potential influence of trace elements discussed. A new liquidus curve for the equilibrium diagram in this compositional range, measuring slightly higher in temperature, was established.

36 MATERIALS SCIENCE↗

Aluminothermic Reduction Process Under Nitrogen Gas Pressure for Preparing High Nitrogen Austenitic Steels

The aluminothermic reduction casting process under nitrogen gas pressure to make austenitic Cr-Mn-N (Ni-free) and Cr-N (Ni/Mn-free) high nitrogen stainless steels was investigated. Thermodynamic simulation of the redox reaction depending on process parameters was performed. As a result, the optimal ratio of aluminum to oxygen in the initial powder mixture to obtain the highest yield of metal product with minimal aluminum nitride contamination was predicted to be slightly greater than the stoichiometric ratio of 1.125. Microstructures of aluminothermic 26Cr1N and 23Cr9Mn1N steels, prepared taking into account the results of thermodynamic simulation, were investigated by X-ray diffraction, metallography, and transmission electron microscopy. The as-cast microstructure was a pseudo-pearlite (layered ferrite-nitride mixture) in 26Cr1N steel and a ferrite-austenite with signs of discontinuous austenite decomposition in 23Cr9Mn1N steel. After hot forging and subsequent water quenching from 1200 °C, the microstructure was fully austenitic in both steels. Tensile tests of quenched 23Cr9Mn1N steel showed a combination of high strength (ultimate strength of 1324 MPa) and ductility (elongation of 27 pct). The results illustrate that the aluminothermic casting process for producing high nitrogen steel is competitive with the commonly used methods, such as pressure electroslag remelting, both in terms of cost and mechanical properties of manufactured steel.

36 MATERIALS SCIENCE↗

Dynamic Recrystallization and Grain Refinement of Fe-P-C-Si and Fe-P-C-Si-N Steels

Grain refinement is an effective technique to improve the mechanical properties of steels. In the present work, single-pass hot compression experiments have been conducted on two different compositions of high phosphorous steels to study the microstructural evolution and ferrite grain refinement at various strain rates and deformation temperatures, i.e., 0.01-10 s{sup −1} and 750-1050 °C, respectively. Optical metallography has been employed to understand the physical processes that take place during hot deformation process. The results indicate that when these compositions of high phosphorous steels are worked at relatively low temperatures in the intercritical regions, a ferrite grain size of 5-7 µm is obtained. It is observed that the grain size decreases with an increase in strain rate and with the decrease in deformation temperature. Based on the values of stress exponent (n) obtained in the present work, dislocation creep is identified as the deformation mechanism. The activation energies for deformation of these two types of high phosphorous steels have been calculated. The effect of the alloying elements on the stress–strain curve, microstructure, and grain refinement has been discussed.

36 MATERIALS SCIENCE↗

Microstructural Characteristics of DU-xMo Alloys with x = 7-12wt%

Microstructural, phase, and impurity analyses of six depleted uranium-molybdenum alloys were obtained using optical metallography, x-ray diffraction, and carbon/nitrogen/oxygen determination. Uranium-molybdenum alloy foils are currently under investigation for the possible conversion of high-power research reactors to accommodate the use of low-enriched uranium fuel. Understanding basic microstructural behavior of these foils is an important consideration in determining the impact of fabrication processes and in anticipating performance of the foils in a reactor. Average grain diameter decreased with increasing molybdenum content, while the degree of mechanical deformation banding increased with increasing molybdenum content. A lattice parameter, which provided information on stress-corrosion cracking behavior, decreased with increasing molybdenum content, and no significant degree of crystallographic ordering was caused by processing and post-processing conditions employed in this study. Impurity concentration, specifically carbon when it is in solution with the host matrix, inhibited the degree of microstructural recrystallization but did not appear to impact other microstructural traits, such as ?-phase retention or lattice parameter.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural Development in Irradiated U-7Mo/6061 Al Alloy Matrix Dispersion Fuel

A U-7Mo alloy/6061 Al alloy matrix dispersion fuel plate was irradiated in the Advanced Test Reactor and then destructively examined using optical metallography and scanning electron microscopy to characterize the developed microstructure. Results were compared to the microstructures of as-fabricated dispersion fuel to identify changes that occurred during irradiation. The interaction layers that formed on the surface of the fuel U-7Mo particles during fuel fabrication exhibited stable irradiation performance as a result of the ~0.88 wt% Si present in the fuel meat matrix. During irradiation, the interaction layers changed very little in thickness and composition. The overall irradiation performance of the fuel plate to moderate power and burnup was considered excellent.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of Irradiation on the Microstructure of U-7Mo Dispersion Fuel with Al-2Si Matrix

The Reduced Enrichment for Research and Test Reactor program is developing low-enriched uranium U-Mo dispersion fuels for application in research and test reactors around the world. As part of this development, fuel plates have been irradiated in the Advanced Test Reactor and then characterized using optical metallography (OM) and scanning electron microscopy (SEM) to determine the as-irradiated microstructure. To demonstrate the irradiation performance of U-7Mo dispersion fuel plates with 2 wt% Si added to the matrix, fuel plates were tested to medium burnups at intermediate fission rates as part of the RERTR-6 experiment. Further testing was performed to higher fission rates as part of the RERTR-7A experiment, and very aggressive testing (high temperature, high fission density, high fission rate) was performed in the RERTR-9A, RERTR-9B and AFIP-1 experiments. As-irradiated microstructures were compared to those observed after fabrication to determine the effects of irradiation on the microstructure. Based on comparison of the microstructural characterization results for each irradiated sample, some general conclusions can be drawn about how the microstructure evolves during irradiation: there is growth of the fuel/matrix interaction layer (FMI), which was present in the samples to some degree after fabrication, during irradiation; Si diffuses from the FMI layer to deeper depths in the U-7Mo particles as the irradiation conditions are made more aggressive; lowering of the Si content in the FMI layer results in an increase in the size of the fission gas bubbles; as the FMI layer grows during irradiation more Si diffuses from the matrix to the FMI layer/matrix interface, and interlinking of fission gas bubbles in the fuel plate microstructure that may indicate breakaway swelling is not observed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Proton irradiation damage of an annealed Alloy 718 beam window

Mechanical testing and microstructural analysis was performed on an Alloy 718 window that was in use at the Los Alamos Neutron Science Center (LANSCE) Isotope Production Facility (IPF) for approximately 5 years. It was replaced as part of the IPF preventive maintenance program. The window was transported to the Wing 9 hot cells at the Chemical and Metallurgical Research (CMR) LANL facility, visually inspected and 3-mm diameter samples were trepanned from the window for mechanical testing and microstructural analysis. Shear punch testing and optical metallography was performed at the CMR hot cells. The 1-mm diameter shear punch disks were cut into smaller samples to further reduce radiation exposure dose rate using Focus Ion Beam (FIB) and microstructure changes were analyzed using a Transmission Electron Microscopy (TEM). Irradiation doses were determined to be ~0.2–0.7 dpa (edge) to 11.3 dpa (peak of beam intensity) using autoradiography and MCNPX calculations. The corresponding irradiation temperatures were calculated to be ~34–120 °C with short excursion to be ~47–220 °C using ANSYS. Mechanical properties and microstructure analysis results with respect to calculated dpa and temperatures show that significant work hardening occurs but useful ductility still remains. The hardening in the lowest dose region (~0.2–0.7 dpa) was the highest and attributed to the formation of γ" precipitates and irradiation defect clusters/bubbles whereas the hardening in the highest dose region (~11.3 dpa) was lower and attributed mainly to irradiation defect clusters and some thermal annealing.

36 MATERIALS SCIENCE↗

The ternary system cerium-rhodium-silicon

Phase relations have been established in the ternary system Ce-Rh-Si for the isothermal section at 800 deg. C based on X-ray powder diffraction and EPMA on about 80 alloys, which were prepared by arc melting under argon or by powder reaction sintering. From the 25 ternary compounds observed at 800 deg. C 13 phases have been reported earlier. Based on XPD Rietveld refinements the crystal structures for 9 new ternary phases were assigned to known structure types. Structural chemistry of these compounds follows the characteristics already outlined for their prototype structures: tau{sub 7}-Ce{sub 3}RhSi{sub 3}, (Ba{sub 3}Al{sub 2}Ge{sub 2}-type), tau{sub 8}-Ce{sub 2}Rh{sub 3-x}Si{sub 3+x} (Ce{sub 2}Rh{sub 1.35}Ge{sub 4.65}-type), tau{sub 10}-Ce{sub 3}Rh{sub 4-x}Si{sub 4+x} (U{sub 3}Ni{sub 4}Si{sub 4}-type), tau{sub 11}-CeRh{sub 6}Si{sub 4} (LiCo{sub 6}P{sub 4}-type), tau{sub 13}-Ce{sub 6}Rh{sub 30}Si{sub 19.3} (U{sub 6}Co{sub 30}Si{sub 19}-type), tau{sub 18}-Ce{sub 4}Rh{sub 4}Si{sub 3} (Sm{sub 4}Pd{sub 4}Si{sub 3}-type), tau{sub 21}-CeRh{sub 2}Si (CeIr{sub 2}Si-type), tau{sub 22}-Ce{sub 2}Rh{sub 3+x}Si{sub 1-x} (Y{sub 2}Rh{sub 3}Ge-type) and tau{sub 24}-Ce{sub 8}(Rh{sub 1-x}Si{sub x}){sub 24}Si (Ce{sub 8}Pd{sub 24}Sb-type). For tau{sub 25}-Ce{sub 4}(Rh{sub 1-x}Si{sub x}){sub 12}Si a novel bcc structure was proposed from Rietveld analysis. Detailed crystal structure data were derived for tau{sub 3}-CeRhSi{sub 2} (CeNiSi{sub 2}-type) and tau{sub 6}-Ce{sub 2}Rh{sub 3}Si{sub 5} (U{sub 2}Co{sub 3}Si{sub 5}-type) by X-ray single crystal experiments, confirming the structure types. The crystal structures of tau{sub 4}-Ce{sub 22}Rh{sub 22}Si{sub 56}, tau{sub 5}-Ce{sub 20}Rh{sub 27}Si{sub 53} and tau{sub 23}-Ce{sub 33.3}Rh{sub 58.2-55.2}Si{sub 8.5-11.5} are unknown. High temperature compounds with compositions Ce{sub 10}Rh{sub 51}Si{sub 33} (U{sub 10}Co{sub 51}Si{sub 33}-type) and CeRhSi (LaIrSi-type) have been observed in as-cast alloys but these phases do not participate in the phase equilibria at 800 deg. C. - Graphical abstract: Phase relations in the ternary system Ce-Rh-Si have been established for the isothermal section at 800 deg. C based on X-ray powder and single-crystal diffraction, metallography, SEM and EMPA techniques on about 80 alloys. 25 ternary compounds were observed.

36 MATERIALS SCIENCE↗

Examination of the solidification macrostructure of spheroidal and flake graphite cast irons using DAAS and ESBD

This investigation focuses on the study of the solidification macrostructure of sand cast flake and spheroidal graphite cast irons. The macrostructure is revealed by using a special technique developed earlier by the authors, called Direct Austempering After Solidification. The observations make use of conventional metallography and Electron Back Scattering Diffraction. The latter technique allows a more detailed observation of the morphology of the austenite grains and the microstructure of the matrix. The results of Electron Back Scattering Diffraction validate the observations made using the macrographic technique. It is verified that the solidification of both flake and spheroidal graphite cast irons is dominated by the growth of large austenite dendrites that form a grain pattern similar to that usually found in most metallic alloys.

36 MATERIALS SCIENCE↗

Influence of heat treatment on microstructure and hot crack susceptibility of laser-drilled turbine blades made from Rene 80

Turbine components from conventionally cast nickel-base alloy Rene 80 show different hot cracking susceptibilities depending on their heat treatment conditions leading to slightly different microstructures. Electron probe micro-analysis, focused ion beam technique and analytical transmission electron microscopy were applied to reveal and identify grain boundary precipitates and the {gamma}-{gamma}'-microstructure. The distribution of borides along grain boundaries was evaluated statistically by quantitative metallography. The following features could be correlated with an increase of cracking susceptibility: i) Increasing grain size, ii) increasing fraction of grain boundaries with densely spaced borides, iii) lack of secondary {gamma}'-particles in matrix channels between the coarse cuboidal {gamma}'-precipitates. The latter feature seems to be responsible for linking-up of cracked grain boundary precipitates which occurred as an additional cracking mechanism after one heat treatment, whereas decohesion at the boride-matrix-interface in the heat affected zone of laser-drilled holes was observed for both heat treatments.

36 MATERIALS SCIENCE↗