At least 55 records · Page 3

Connector for Composite Tubes

Difficulties in joining tubular structural members made of composite materials are overcome by improved conectors. Connectors are made from same composite as structural shapes, eliminating stress and weight problems experienced with metal connectors. Composites allow joint strength to be optimized by properly choosing fiber orientation and fabric. Only two basic shapes are required to make 90 degrees and T-joints in plane. Used to assemble strong, lightweight, three-dimensional structures.

Harrison, E. J.↗

The behavior of bonded doubler splices for composite sandwich panels

The results of an investigation into the behavior of adhesively bonded doubler splices of two composite material sandwich panels are presented. The splices are studied from three approaches: analytical; numerical (finite elements); and experimental. Several parameters that characterize the splice are developed to determine their influence upon joint strength. These parameters are: doubler overlap length; core stiffness; laminate bending stiffness; the size of the gap between the spliced sandwich panels; and room and elevated temperatures. Similarities and contrasts between these splices and the physically similar single and double lap joints are discussed. The results of this investigation suggest several possible approaches to improving the strength of the sandwich splices.

Zeller, T. A.↗

Latent Hardeners for the Assembly of Epoxy Composites

Large-scale composite structures are commonly joined by secondary bonding of molded-and-cured thermoset components. This approach may result in unpredictable joint strengths. In contrast, assemblies made by co-curing, although limited in size by the mold, result in stable structures, and are certifiable for commercial aviation because of structural continuity through the joints. Multifunctional epoxy resins were prepared that should produce fully-cured subcomponents with uncured joining surfaces, enabling them to be assembled by co-curing in a subsequent out-of-autoclave process. Aromatic diamines were protected by condensation with a ketone or aldehyde to form imines. Properties of the amine-cured epoxy were compared with those of commercially available thermosetting epoxy resins and rheology and thermal analysis were used to demonstrate the efficacy of imine protection. Optimum conditions to reverse the protecting chemistry in the solid state using moisture and acid catalysis were determined. Alternative chemistries were also investigated. For example, chain reaction depolymerization and photoinitiated catalysts would be expected to minimize liberation of volatile organic content upon deprotection and avoid residual reactive species that could damage the resin. Results from the analysis of protected and deprotected resins will be presented.

Palmieri, Frank↗

Design, fabrication and test of graphite/polymide composite joints and attachments: Summary

The design, analysis and testing performed to develop four types of graphite/polyimide (Gr/PI) bonded and bolted composite joints for lightly loaded control surfaces on advanced space transportation systems that operate at temperatures up to 561K (550 F) are summarized. Material properties and 'small specimen' tests were conducted to establish design data and to evaluate specific design details. 'Static discriminator' tests were conducted on preliminary designs to verify structural adequacy. Scaled up specimens of the final joint designs, representative of production size requirements, were subjected to a series of static and fatigue tests to evaluate joint strength. Effects of environmental conditioning were determined by testing aged (125 hours 589K (600 F)) and thermal cycled (116K to 589K (-250 F to 600 F), 125 times) specimens. It is concluded Gr/PI joints can be designed and fabricated to carry the specified loads. Test results also indicate a possible resin loss or degradation of laminates after exposure to 589K (600 F) for 125 hours.

Cushman, J. B.↗

Design, fabrication and test of graphite/polyimide composite joints and attachments

The design, analysis, and testing performed to develop four types of graphite/polyimide (Gr/PI) bonded and bolted composite joints for lightly loaded control surfaces on advanced space transportation systems that operate at temperatures up to 561 K (550 F) are summarized. Material properties and small specimen tests were conducted to establish design data and to evaluate specific design details. Static discriminator tests were conducted on preliminary designs to verify structural adequacy. Scaled up specimens of the final joint designs, representative of production size requirements, were subjected to a series of static and fatigue tests to evaluate joint strength. Effects of environmental conditioning were determined by testing aged (125 hours at 589 K (600 F)) and thermal cycled (116 K to 589 K (-250 F to 600 F), 125 times) specimens. It is concluded Gr/PI joints can be designed and fabricated to carry the specified loads. Test results also indicate a possible resin loss or degradation of laminates after exposure to 589 K (600 F) for 125 hours.

Cushman, J. B.↗

Effects of fiber/matrix interactions on the properties of graphite/epoxy composites

A state-of-the-art literature review of the interactions between fibers and resin within graphite epoxy composite materials was performed. Emphasis centered on: adhesion theory; wetting characteristics of carbon fiber; load transfer mechanisms; methods to evaluate and measure interfacial bond strengths; environmental influence at the interface; and the effect of the interface/interphase on composite performance, with particular attention to impact toughness. In conjunction with the literature review, efforts were made to design experiments to study the wetting behavior of carbon fibers with various finish variants and their effect on adhesion joint strength. The properties of composites with various fiber finishes were measured and compared to the base-line properties of a control. It was shown that by tailoring the interphase properties, a 30% increase in impact toughness was achieved without loss of mechanical properties at both room and elevated temperatures.

Mcmahon, P. E.↗

Explosive Welding of Tubular Configurated Joints for Critical Applications

Explosive welding can provide the answer to problems of permanently joining metals typically used in the aerospace industry. The explosive bonding process is a solid state bonding process enabling material incompatibility problems associated with fusion welding to be overcome. In addition, heat affected zones are eliminated thus, enhancing joint strength, properties and performance. The process requires the parts being joined to be impelled, by means of explosives, to collide with each other. Certain critical collision parameters must be met and controlled and these parameters are defined. Various component geometries which satisfy the collision parameters are described. Examples of transition joints used in the aerospace industry are described and illustrated.

Hardwick, R.↗

Predicting Strength and Fatigue for Suited and Unsuited Conditions from Empirical Data

The need for longer and more labor-intensive extra-vehicular activities (EVA) is required for construction and maintenance of the International Space Station (ISS). Issues pertaining to human performance while wearing a space suit (EMU) for prolonged periods have become more important. This project was conducted to investigate how a pressurized Extra-vehicular Mobility Unit (EMU) affects human upper body joint strength and fatigue and how to predict it from computer models based on the data collected.

Maida, James C.↗

Development of a gas pressure bonded four-pole alternator rotor

Methods were developed for fabrication of a solid four pole alternator rotor by hot isostatic pressure welding. The rotor blanks welded in this program had complex geometrical mating interfaces and were of considerable bulk, being approximately 3-1/2 inches (0.089 meters) in diameter and 14 inches (0.356 meters) long. Magnetic end pieces were machined from AlSl 4340 steel, while the non-magnetic central section was of Inconel 718. Excellent welds were produced which were shown to be responsive to post weld heat treatments which substantially improved joint strength. Prior to welding the rotors, test specimens of complex geometry were welded to demonstrate that complex surfaces with intentional mechanical misfit could be readily joined using HIP welding. This preliminary work demonstrated not only that interface compliance is achieved during welding but that welding pressure is developed in these thick sections sufficient to produce sound joints. Integral weld-heat treatment cycles were developed that permitted the attainment of magnetic properties while minimizing residual stress associated with the allotropic transformation of 4340 steel.

Lessmann, G. G.↗

Applications of gap welding

Gap welding of electronic interconnections yields high strength joints, is easy to use, and allows visual inspection of the welding process. It is easily adaptable to automated circuit assembly.

Adams, G. D.↗

Retort braze bonding of borsic/aluminum composite sheet to titanium

Braze bonding studies between Borsic/aluminum composite and titanium sheet were conducted to establish acceptable brazing techniques and to assess potential joint efficiencies. Excellent braze joints were produced which exhibited joint strengths exceeding 117 MPa (17,000 psi) and which retained up to 2/3 of this strength at 589 K (600 F). Noticeable composite strength degradation resulting from the required high temperature braze cycle was found to be a problem.

Webb, B. A.↗

Resistance welding graphite-fiber composites

High-strength joints are welded in seconds in carbon-reinfored thermoplastic beams. Resistance-welding electrode applies heat and pressure to joint and is spring-loaded to follow softening material to maintain contact; it also holds parts together for cooling and hardening. Both transverse and longitudinal configurations can be welded. Adhesive bonding and encapsulation are more time consuming methods and introduce additional material into joint, while ultrasonic heating can damage graphite fibers in composite.

Lamoureux, R. T.↗

The effects of inherent flaws on the time and rate dependent failure of adhesively bonded joints

Inherent flaws, as well as the effects of rate and time, are shown by tests on viscoelastic adhesive-bonded single lap joints to be as critical in joint failure as environmental and stress concentration effects, with random inherent flaws and loading rate changes resulting in an up to 40% reduction in joint strength. It is also found that the asymptotic creep stress, below which no delayed failure may occur, may under creep loading be as much as 45% less than maximum adhesive strength. Attention is given to test results for the case of titanium-LARC-3 adhesive single-lap specimens.

Sancaktar, E.↗

End effects in scarf joints

Scarf joints with small scarf angles are especially sensitive to stiffness mismatch between adherends and to adherend tip bluntness. Pre-assembly breakage of an adherend tip where it is only a few microns thick can cause significant reduction in joint strength. Mathematically, the reason for such sensitivity is that the solutions to the governing differential equation develop boundary layer character when the scarf angles are small. The boundary layers are regions with large adhesive stresses. Experimental strength data for laminated composite adherends agree with the results of this analysis.

Adkins, D. W.↗

Aligning Plasma-Arc Welding Oscillations

Tool aids in alignment of oscillator probe on variable-polarity plasma-arc welding torch. Probe magnetically pulls arc from side to side as it moves along joint. Tensile strength of joint depends on alignment of weld bead and on alignment of probe. Operator installs new tool on front of torch body, levels it with built-in bubble glass, inserts probe in slot on tool, and locks probe in place. Procedure faster and easier and resulting alignment more accurate and repeatable.

Norris, Jeff↗

Stress analysis method for clearance-fit joints with bearing-bypass loads

Within a multi-fastener joint, fastener holes may be subjected to the combined effects of bearing loads and loads that bypass the hole to be reacted elsewhere in the joint. The analysis of a joint subjected to search combined bearing and bypass loads is complicated by the usual clearance between the hole and the fastener. A simple analysis method for such clearance-fit joints subjected to bearing-bypass loading has been developed in the present study. It uses an inverse formulation with a linear elastic finite-element analysis. Conditions along the bolt-hole contact arc are specified by displacement constraint equations. The present method is simple to apply and can be implemented with most general purpose finite-element programs since it does not use complicated iterative-incremental procedures. The method was used to study the effects of bearing-bypass loading on bolt-hole contact angles and local stresses. In this study, a rigid, frictionless bolt was used with a plate having the properties of a quasi-isotropic graphite/epoxy laminate. Results showed that the contact angle as well as the peak stresses around the hole and their locations were strongly influenced by the ratio of bearing and bypass loads. For single contact, tension and compression bearing-bypass loading had opposite effects on the contact angle. For some compressive bearing-bypass loads, the hole tended to close on the fastener leading to dual contact. It was shown that dual contact reduces the stress concentration at the fastener and would, therefore, increase joint strength in compression. The results illustrate the general importance of accounting for bolt-hole clearance and contact to accurately compute local bolt-hole stresses for combined bearings and bypass loading.

Naik, R. A.↗