Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Hydrogen separation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Hydrogen separation membrane on a porous substrate

A hydrogen permeable membrane is disclosed. The membrane is prepared by forming a mixture of metal oxide powder and ceramic oxide powder and a pore former into an article. The article is dried at elevated temperatures and then sintered in a reducing atmosphere to provide a dense hydrogen permeable portion near the surface of the sintered mixture. The dense hydrogen permeable portion has a higher initial concentration of metal than the remainder of the sintered mixture and is present in the range of from about 20 to about 80 percent by volume of the dense hydrogen permeable portion.

36 MATERIALS SCIENCE↗

Pd3Ag(111) as a Model System for Hydrogen Separation Membranes: Combined Effects of CO Adsorption and Surface Termination on the Activation of Molecular Hydrogen

Abstract The co-adsorption of hydrogen and carbon monoxide on Pd 3 Ag(111) alloy surfaces has been studied as a model system for Pd-Ag alloys in membrane and catalysis applications using periodic density functional theory calculations (PW91-GGA). We explored the effects of Pd–Ag surface composition, since segregation of silver towards and away from the surface has been suggested to explain the experimentally observed changes in H 2 activation, CO inhibition and reactivity. We found that CO pre-adsorbed on the surface weakens the adsorption of H on Pd 3 Ag(111) alloy surfaces irrespective of whether the surface termination corresponds to the bulk Pd 3 Ag composition, or is purely Pd-terminated. A higher coverage of H with CO present is obtained for the Pd-terminated surface; this surface also exhibits a larger range of chemical potentials for co-adsorbed hydrogen and CO. The barrier for H 2 activation increases with increasing CO coverage, but the surface composition has the largest impact on H 2 activation at intermediate CO coverage. The results imply that Pd-based membranes with typically ~ 23 wt% Ag are less prone to CO poisoning if the surface becomes Pd-terminated.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

PdAu/YSZ composite hydrogen separation membranes with enhanced stability in the presence of CO

The effects of gold composition on the tolerance of palladium-based composite membranes to CO exposure was studied under the presence of high CO concentrations. Membranes with PdAu compositions ranging up to 41% by mass were exposed to binary 50/50 H 2 /CO gas atmospheres and both hydrogen flux and purity were monitored over time. It was observed that the highest gold composition (41%) suffered no degradation in membrane performance in terms of permeate hydrogen purity and hydrogen permeation flux during the 48 h exposure. Furthermore, for lower gold compositions, X-ray diffraction patterns suggested that carbon entered the film and could be removed by exposure to a non-CO containing gas mixture over time. However, removal of the carbon adversely affected purity; interestingly, some of the purity decline could be reversed upon re-exposure to the CO gas mixture. It is hypothesized that carbon loading in the palladium films causes lattice expansion and may even fill pore defects, thus lowering leaks through the Pd films. Furthermore, this study suggests that a membrane exposed to a CO mixture should not be cycled between CO and non-CO environments, but rather run continuously for best performance. Additionally, the choice of Pd-alloy and metal composition should be considered in regard to its carbon solubility to best predict lifetime performance.

08 HYDROGEN↗

Novel dense membrane for hydrogen separation for energy applications

The main objectives of this project are: (1) Characterization of the thermo mechanical properties of the novel dense HTM bulk sample; (2) Development of a correlation among the intrinsic factors (such as grain size and phase distribution), and the extrinsic factors (such as temperature and atmosphere) and the thermo-mechanical properties (such as strengths and stress) to predict the performance of a HTM system (HTM membrane and porous substrate) ; and (3) Evaluation of the stability of the novel HTM membrane and its property correlations after thermal cycling. Based on all results and analysis of the thermo mechanical properties for the HTM cermet bulk samples, several important conclusions were made. The mean σfs at room temperature is approximately 356 MPa for the HTM cermet. The mean σfs value decreases to 284 MPa as the temperature increases to 850?C. The Difference difference in atmosphere, such as air or N2, had an insignificant effect on the flexural strength values at 850?C for the HTM cermet. The HTM cermet samples at room temperature and at 500?C fractured without any significant plastic deformation. Whereas, at 850?C, the HTM cermet samples fractured, preceded by an extensive plastic deformation. It seems that the HTM cermet behaves more like an elastic material such as a nonmetal ceramic at the room temperature, and more like a ductile material at increased temperature (850?C). The exothermic peak during the TG/DTA tests centered at 600?C is most likely associated with both the enthalpy change of transformation from the amorphous phase into crystalline zirconia and the oxidation of Pd phase in HTM cermet in air. The endothermic peak centered at 800?C is associated with the dissociation of PdO to Pd for the HTM cermet sample in both inert N2 environment and air. There is a corresponding weight gain as oxidation occurs for palladium (Pd) phase to form palladium oxide (PdO) and there is a weight loss as the unstable PdO is dissociated back to Pd and oxygen. The normal stress and shear stresses from the Mohr?s circle indicate that the residual stress in the HTM cermet sample is mainly as compressive residual stress in the magnitude of -135 to -155 MP, and with very little shear stress (in the magnitude of 10 MPa). The magnitude of change in the normal stress and the shear stress is insignificant in the HTM after 120 thermal cycles. However, the principle normal stress changes from compressive to tensile residual stress and there is a significant increase in the shear stress after 500 thermal cycles. The calculated value based on the equation and the Mohr?s circle is found to be consistent with the experimental value for the as-received HTM cermet samples. At some rotation (φ) angle, the residual stress was found to be as tensile stress. Most ceramic material is weak in tension, and develops microscopic cracks. With treatment of 120 thermal cycles between 50?850?C, the HTM- sample exhibited thermally-induced cracks on the surface. Visually observable cracks appeared on the surface of HTM cermet with continuous thermal cycling, after 500 thermal cycles. The XRD powder diffraction analysis indicated an increased amount of crystalline PdO crystalline in HTM cermet after 120 and 500 thermal cycles as compare to the as-received samples. The Pd crystalline peaks were found to significantly decrease in peak intensity with thermal cycling. Higher peak intensity for PdO phase was observed with increased number of thermal cycles. A Monoclinic monoclinic zirconia phase was first identified in the as-received HTM as-received sample. However, with thermal cycling treatment of both 120 and 500 thermal cycles, the M-ZrO2 phase is transformed to the tetragonal YSZ, which is consistent with the thermal analysis results by TG/DTA. Correlations of the microstructural and thermo-mechanical properties of both selected reference material and ANL-3e HTM cermet bulk sample are affected mainly by porosity and microstructural features, such as grain size and pore size/distribution. The Young?s Modulus (E-value), especially, is positively proportional to the flexural strength for materials with similar crystallographic structure. For different crystallographic materials, physical properties such as E and density are independent of mechanical properties, such as flexural strength.. Microstructural properties, particularly, grain size and crystallographic structure, and thermodynamic properties are the main factors affecting the mechanical properties at both room and high temperatures. The oxidation and the plasticity of Pd phase mainly affect the mechanical properties of HTM cermet at high temperature or with thermal cycling treatment. Changes in the residual stress and microstructure affect the mechanical properties of HTM when subjected to high temperature or thermal cycling treatment.

08 HYDROGEN↗

Thermal method for fabricating a hydrogen separation membrane on a porous substrate

A thermal method of making a hydrogen permeable composition is disclosed. A mixture of metal oxide powder and ceramic oxide powder and optionally a pore former is formed and pressed to form an article. The article is dried at elevated temperatures and then sintered in a reducing atmosphere to provide a dense hydrogen permeable portion near the surface of the sintered mixture. The dense hydrogen permeable portion has a higher initial concentration of metal than the remainder of the sintered mixture and is present in the range of from about 20 to about 80 percent by volume of the dense hydrogen permeable portion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Nickel-hydrogen separator development

The separator technology is a critical element in the nickel-hydrogen (Ni-H2) systems. Previous research and development work carried out at NASA Lewis Research Center has determined that separators made from zirconium oxide (ZrO2) and potassium titanate (PKT) fibers will function satisfactorily in Ni-H2 cells without exhibiting the problems associated with the asbestos separators. These separators and their characteristics were previously discussed. A program was established to transfer the separator technology into a commercial production line. A detailed plan of this program will be presented and the preliminary results will be discussed.

Gonzalez-Sanabria, O. D.↗

Nickel-hydrogen separator development

The separator technology is a critical element in the nickel-hydrogen (Ni-H2) systems. Previous research and development work carried out at NASA Lewis Research Center has determined that separators made from zirconium oxide (ZrO2) and potassium titanate (PKT) fibers will function satisfactorily in Ni-H2 cells without exhibiting the problems associated with the asbestos separators. A program has been established to transfer the separator technology into a commercial production line. A detailed plan of this program will be presented and the preliminary results will be discussed.

Gonzalez-Sanabria, O. D.↗

Simulation of 12-bed vacuum pressure-swing adsorption for hydrogen separation from methanol-steam reforming off-gas

This study focuses on analysis of a 12-bed vacuum pressure-swing adsorption (VPSA) process capable of purifying hydrogen from a ternary mixture (H 2 /CO 2 /CO 75/24/1 mol%) derived from methanol-steam reforming. The process produces 9 kmol H 2 /h with less than 2 ppm and 0.2 ppm of CO2 and CO, respectively, to supply a polymer electrolyte membrane fuel cell. The process model is developed in Aspen Adsorption® using the “uni-bed” approach. A parametric study of H 2 purity and recovery with respect to adsorption pressure, adsorbent height, activated carbon:zeolite ratio, feed composition, and number of beds is performed. Results show 12-bed VPSA can meet the H 2 purity goals, with H 2 recovery as high as 75.75%. Adsorption occurs at 7 bar, the column height is 1.2 m, and the adsorbent ratio is 70%:30%. Furthermore, a 4-bed VPSA can achieve the same purity goals as the 12-bed process, but H 2 recovery decreases to 61.34%.

03 NATURAL GAS↗

Proton conducting ceramic membranes for hydrogen separation

A multi-phase proton conducting material comprising a proton-conducting ceramic phase and a stabilizing ceramic phase. Under the presence of a partial pressure gradient of hydrogen across the membrane or under the influence of an electrical potential, a membrane fabricated with this material selectively transports hydrogen ions through the proton conducting phase, which results in ultrahigh purity hydrogen permeation through the membrane. The stabilizing ceramic phase may be substantially structurally and chemically identical to at least one product of a reaction between the proton conducting phase and at least one expected gas under operating conditions of a membrane fabricated using the material. In a barium cerate-based proton conducting membrane, one stabilizing phase is ceria.

36 MATERIALS SCIENCE↗

Development of membranes for hydrogen separation: Pd-coated V-10Pd

Numerous Group IVB and VB alloys were prepared and tested as potential membrane materials but most of these materials were brittle or exhibited cracking during hydrogen exposure. One of the more ductile alloys, V-10Pd (at. %), was fabricated into a thin (107-{micro}m thick) composite membrane coated with 100 nm of Pd on each side. The material was tested for hydrogen permeability, resistance to hydrogen embrittlement, and long term hydrogen flux stability. The hydrogen permeability, {phi}, of the V-10Pd membrane was 3.86 x 10{sup -8} mol H{sub 2} m{sup -1} s{sup -1} Pa{sup -0.5} (avg. of three different samples) at 400 C, which is slightly higher than the permeability of Pd-23Ag at that temperature. A 1400 h hydrogen flux test at 400 C demonstrated that the rate of metallic interdiffusion was slow between the V-10Pd foil and the 100-nm-thick Pd coating on the surface. However, at the end of testing the membrane cracked at 118 C because of hydrogen embrittlement.

08 HYDROGEN↗