Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “High Temperature Oxidation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

The microscopic mechanisms of high temperature oxidation of Haynes 282

Nickel-based superalloy finds widespread applications in aerospace and extreme environments. They are known for their high temperature oxidation resistance under extended periods. However, the oxide formation and evolution which sets the stages for the later parabolic oxidation kinetics is not fully understood. This paper aims to provide new insights into the transient stage oxidation mechanism and kinetics of a typical Ni-based superalloy (Haynes 282). While tracking the chemical and microstructural evolution under micrometer scale at 800°C, we show that the oxide scale and its grain boundary species change significantly during the initial stages of oxidation and can have a profound impact on the oxidation kinetics. Cr 2 O 3 forms initially at the grain boundary along with minor amount of Al 2 O 3 . Then, the grain boundary region is enriched with copious amounts TiO 2 while Cr migrates away from the grain boundary. A noticeable change in the isothermal oxidation kinetics observed likely results from a mechanistic change from uniform surface oxidation to preferential outward diffusion of Ti 4+ ions through the grain boundary. Through first-principles calculations combined with energy dispersive spectroscopy, we confirmed the preferential outward diffusion of Ti 4+ ions as the diffusion barrier is lower for Ti than Cr along the grain boundaries. In conclusion, these findings highlight the critical role of early-stage grain boundary oxidation dynamics in dictating the long-term oxidation resistance of Ni-based superalloys and provide a foundation for future strategies to enhance their performance in extreme environments.

DFT↗

Ceramic problems/challenges in high temperature oxide superconductors - Hysteretic force measurements as a new analysis tool

A technique is presented for analyzing high-temperature oxide superconductors using hysteretic magnetic force/distance measurements. Emphasis is placed on developing low weight, highly robust superconducting materials for space applications. Bi-Ca-Sr-Cu superconductors are prepared and characterized by standard techniques. It is found that standard techniques such as XRD, SEM, and TEM are insufficient to completely characterize superconductors. The magnetic properties of the superconductors are studied with the new technique, based on measuring the force between a magnet and the superconductor as a function of their separation.

Morgan, P. E. D.↗

High temperature oxidation of PCD coated Zr alloy

Polycrystalline diamond (PCD) coating is a promising possibility for prevention, or reduction of high temperature oxidation of zirconium alloys and decrease corrosion rate of zirconium alloy during standard operation. Zirconium alloys are widely used as cladding and construction material in almost all types of nuclear reactors, where usually creates a barrier between nuclear fuel and cooling water in the primary circuit. Hydrogen and considerable amount of heat is released during steam oxidation that may occur in an eventual accident. In this paper zirconium alloy was covered by polycrystalline diamond layer using Plasma Enhanced Linear Antennas Microwave Chemical Vapor Deposition system reactor. X-Ray Diffraction and Raman spectroscopy measurements confirmed coverage of the surface area with crystalline and amorphous carbon layer. Characterizations (Raman spectroscopy) were done for zirconium alloy covered with polycrystalline diamond layer before and after high temperature steam exposure. Weight increase and hydrogen release were measured during steam exposure. The results show that the oxidation kinetics of PCD coated samples is similar to kinetics of uncoated samples at almost all temperatures, but with lower hydrogen production and lower weight gains. Most important difference is in later beginning of breakaway oxidation at 1000 Celsius degrees, when breakaway oxidation starts on PCD coated sample 15 minutes later. Raman spectroscopy revealed graphitization of the PCD layer and the diamond sp{sup 3} bounds are lost and the Raman signal consists only from the two graphite-related D bounds. It implies conversion of PCD layer to the homogeneous non-crystalline carbon layer with a large content of graphitic phase. Overall hydrogen production and weight gain values are generally lower then for uncoated samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High temperature oxidation of Ni alloys in CO 2 containing impurities

Next-generation power systems need structural alloys resistant to high-temperature oxidation in CO 2 containing combustion impurities. In this report we evaluate the oxidation performance of several commercial Ni alloys exposed to 95%CO 2 -4%H 2 O-1%O 2 , with/without 0.1% SO 2 , at 750°C and 1 atm. All alloys formed protective chromia layers and showed no signs of carburization or sulfidation, and minimal chromia volatilization. The microstructural evolution of the alloy surface, secondary oxidants, and minor alloy additions all played a part in promoting protective chromia formation/growth. The results show that Ni alloys are promising candidates for high-temperature portions of next-generation CO 2 -based power systems.

36 MATERIALS SCIENCE↗

High Temperature Oxidation Behavior of Ni-based High Entropy Superalloys

A new class of polycrystalline gamma-prime strengthened superalloys with alloy compositions of (wt%) Ni-20Co-13Cr-6Fe-4Al-3W-2Mo-(4-x)Nb-(x)Ti (x = 0,1,2) were subjected to cyclic oxidation exposures in dry air at 800 °C for 3600 h. The alloys were borderline chromia/alumina formers, showing good oxidation resistance relative to commercially available materials of similar composition. While all alloys formed alumina scales initially, only the alloy with the lowest Ti/Nb ratio retained an alumina scale for the duration of the exposure. Formation of a continuous layer of rutile TiO 2 at the alumina/alloy interface is proposed to cause eventual alumina failure for the alloys containing Ti.

36 MATERIALS SCIENCE↗

Quantitative characterization of high temperature oxidation using electron tomography and energy-dispersive X-ray spectroscopy

We report quantitative characterization of the high temperature oxidation process by using electron tomography and energy-dispersive X-ray spectroscopy. As a proof of principle, we performed 3D imaging of the oxidation layer of a model system (Mo 3 Si) at nanoscale resolution with elemental specificity and probed the oxidation kinetics as a function of the oxidation time and the elevated temperature. Our tomographic reconstructions provide detailed 3D structural information of the surface oxidation layer of the Mo 3 Si system, revealing the evolution of oxidation behavior of Mo 3 Si from early stage to mature stage. Based on the relative rate of oxidation of Mo 3 Si, the volatilization rate of MoO 3 and reactive molecular dynamics simulations, we propose a model to explain the mechanism of the formation of the porous silica structure during the oxidation process of Mo 3 Si. We expect that this 3D quantitative characterization method can be applied to other material systems to probe their structure-property relationships in different environments.

36 MATERIALS SCIENCE↗

High-Temperature Oxidation Study in a Multi-Oxidant Environment Using 18 O Tracer

The goal of this study was to use 18 O-enriched water to better understand the role of H 2 O in high-temperature oxidation. Seven model and three commercial M-Cr and M-Cr-Al alloys were studied in air with 10% of H 2 O at 800 °C for 5 h. Oxygen from water vapor was more reactive than oxygen from the air and 18 O enriched at the outermost layers of the formed Cr- and Al-rich oxides. Alloys with Al and/or Ti additions showed signs of internal oxidation but 18 O was not enriched inside the alloy in locations with internal oxidation. In conclusion, depending on the alloy Al content, the oxide went from Al oxidation beneath a chromia scale to external alumina scale formation.

18O-enriched water↗

Effect of Surface Finish on High-Temperature Oxidation of Steels in CO 2 , Supercritical CO 2 , and Air

Current and future power systems require steels resistant to high-temperature oxidation in CO 2 -rich environments. The introduction of structural defects by various surface treatments can profoundly affect the oxidation/corrosion behavior of steels in many environments. This effect is largely unexplored for steels exposed to high-temperature CO 2 , which is the focus of this work. We prepared Grade 22, Grade 91, 347H, and 310S steels with three different surface finishes, ranging from little to substantial surface damage, and exposed the steels to 1 bar CO 2 , 200 bar supercritical CO 2 , and laboratory air at 550 °C for up to 1500 h. Surface finish had little impact on the oxidation behavior of low-Cr (2 wt%) Grade 22 and high-Cr (25 wt%) 310S steels. In contrast, intermediate-Cr steels Grade 91 (8 wt%) and 347H (17 wt%) generally showed improved oxidation and carburization resistance with increasing extent of surface damage, which was attributed to the delay or prevention of the onset of Fe-rich oxide nodule growth. Comparison between exposure environments suggests that this effect is more complex for CO 2 compared to air and that it is additionally affected by CO 2 pressure. In conclusion, the results suggest that surface treatments should be considered as one approach to achieve improved corrosion resistance in high-temperature CO 2 , particularly for steels containing Cr levels near the transition that is required to form and maintain a protective Cr-rich oxide scale.

36 MATERIALS SCIENCE↗

Sputter-ion plating of coatings for protection of gas-turbine blades against high-temperature oxidation and corrosion

Considerable effort is being devoted to the development of overlay coatings for protecting critical components such as turbine blades against high-temperature oxidation, corrosion, and erosion damage in service. The most commercially advanced methods for depositing coatings are electron-beam evaporation and plasma spraying. Sputter-ion plating (SIP) offers a potentially cheaper and simpler alternative method for depositing overlays. Experimental work on SIP of Co-Cr-Al-Y and Ni-Cr-Al-Ti alloy coatings is described. Results are presented of metallographic assessment of these coatings, and of the results obtained from high-velocity testing using a gas-turbine simulator rig.

Coad, J. P.↗

High Temperature Oxidation Lifetime Modelling of thin-walled components

High temperature material solutions for future power generation applications require longer component lifetimes at higher temperatures to improve durability and efficiency. From a research and development point of view, the lifetimes are too long for experimental verification. Thus, accurate lifetime models are needed. Examples are provided where modeling is being applied to lifetime prediction of thin-walled NiCr wrought alloy components. Specific laboratory experiments have been conducted for alloy X at 900°-950°C in dry air and air with water vapor with cycle times from 1 to 500 h. Along with microstructure characterization, comparisons are made between experiment and model predictions. The eventual goal is to predict both oxidation and mechanical behavior.

Pillai, Rishi↗

Alloying effect of Nb and Sn on the Zirconium alloy fuel claddings behavior at high temperature oxidation in steam - 6.1 STP-2016-0072

As the material of fuel claddings for water cooled reactors most commonly used binary and multicomponent zirconium alloys Zr-Nb (E110,M5), Zr-Sn-Fe (Zircaloy-2,-4) and Zr-Nb-Sn-Fe (E635, Zirlo) are used, which improvement extends, in particular, by varying their composition by Nb, Sn and Fe. At the same time, the importance is given to ensuring the safe operation of the fuel rods not only in normal conditions but also in emergency situations such as LOCA. In this paper the researches results of the studies of influence of alloying elements Nb, Sn (and Fe) on corrosion resistance and embrittlement at high temperature steam oxidation of fuel claddings based on alloys types Zr-xNb (x=1.0/2.5) and Zr-xNb-ySn-zFe (x=0.6/2.4; y=0.24/1.1; z=0.18/0.34) made with using zirconium sponge are presented. High temperature steam oxidation tests were carried out at temperatures of 1000, 1100 and 1200 deg. C with continuous measurement of the weight gain during the experiment and subsequent cooling in steam with rate ∼ 20 deg. C/s. The studies of kinetics of high-temperature oxidation in steam, structural-phase state changes, alloying elements distribution, absorbed hydrogen content and residual ductility after rapid cooling of the oxidized specimens were made. The difference in the oxidation kinetics of the materials studied was revealed, it decreases with the oxidation temperature increase. At the same time, an increase of the Sn content in the alloy influences on specimens 'breakaway' oxidation intensification at 1000 deg. C. It is shown that the mechanical properties of fuel claddings oxidized under the same conditions depend on their alloying composition, the hydrogen fraction absorbed by the specimen and formed by the oxidation ZrO2, a-Zr(O) and 'ex-β' layers structure, which in turn varies depending on the alloy composition. The increase of Nb, Sn and Fe content in the zirconium alloy leads to decrease in residual ductility of fuel claddings after high temperature steam oxidation. According to obtained results the most resistant to high-temperature steam oxidation and embrittlement at temperatures of 1000-1200 deg. C among the materials studied is Zr-1Nb alloy. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Combining Raman Microprobe and XPS to Study High Temperature Oxidation of Metals

Raman microprobe spectroscopy was applied in studies of high-temperature air oxidation of a ferritic alloy (HT-9) in the absence and presence of zirconia coatings with the objective of evaluating the technique as a way to quickly screen candidate cladding materials and actinide-based mixed oxide fuel mixtures for advanced nuclear reactors. When oxidation was relatively uniform, Raman spectra collected using microscope optics with low spatial resolution were found to be similar to those collected with conventional Raman spectroscopy. These spectra could be used to identify major oxide corrosion products and follow changes in the composition of the oxides due to heating. However, when the oxidation films were comprised of multiple layers of varying composition, or with layers containing metallic phases, techniques with higher depth resolution and sensitivity to zero-valence metals were necessary. The requirements were met by combining Raman microprobe using different optical configurations and x-ray photoelectron spectroscopy.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High Temperature Oxidation of Silicon Carbide and Advanced Iron-Based Alloys in Steam-Hydrogen Environments

A side by side comparison of the oxidation behavior of zirconium alloys with SiC materials and advanced iron-based alloys is provided. Oxidation tests were conducted in steam and steam-hydrogen environments at 800-1350 C and 0.34-2MPa for durations up to 48 hours. Monolithic SiC specimens as well as SiC/SiC composites were examined during the study where the material recession mechanism appeared to be governed by silica layer volatilization at the surface for CVD SiC. A wide set of austenitic and ferritic steels were also examined where a critical Cr content (>20 wt.%) was shown to be necessary to achieve oxidation resistance at high temperatures. SiC materials and alumina-forming ferritic steels exhibited slowest oxidation kinetics; roughly two orders of magnitude lower than zirconium alloys.

Terrani, Kurt A↗

The high-temperature oxidation of aromatic hydrocarbons

Chemical mechanisms of the atmospheric pressure, high-temperature (875-1500 K) gas-phase oxidation of benzene, toluene, ethylbenzene, and propylbenzene are described and discussed. Oxidation trends evident from turbulent flow reactor experiments serve as the basis for the mechanisms of the oxidation of benzene and alkylated aromatics. The potential effects of very high temperatures and pressures on the chemistry of oxidation of aromatics are described. The oxidation of benzene and phenyl radical has been found to proceed in a stepwise C6-C5-C4 sequence. Species profiles obtained from flow-reactor experiments suggest that the oxidation of benzene and phenyl radical follows the generalized route via phenoxy, cyclopentadienyl and butadienyl radical. The oxidation of the C4 species branches into multiple pathways that yield copious amounts of ethylene and acetylene. Certain major trends are evident: the alkylated aromatics on initial attack either form styrene, benzyl radical or benzene. The styrene reacts further to produce a benzyl radical or benzene. The oxidation of an alkylated aromatic hydrocarbon appears eventually to reduce to the oxidation of either phenyl radical or benzene.

Brezinsky, K.↗

High-Temperature Oxidation Behavior of FeCoCrNi+(Cu/Al)-Based High-Entropy Alloys in Humid Air

Previous studies showed some transition metal high-entropy alloy (HEA) compositions can have good oxidation resistance in air up to 800 °C. Four equiatomic HEAs have been developed based on FeCoCrNi with additions of Mn, Cu, Al or Al+Cu. The oxidation behavior of these HEAs was compared in humid (10 vol.% H2O) air at 800 °C for 100–500 h to investigate the influence of water vapor on the oxidation mechanisms. The Cu- and Al-containing alloys exhibited improved oxidation resistance over the Mn composition. For the Cu-containing alloy, a local attack of the Cu-rich phase was observed, which formed an Fe/Ni/Co/Cr spinel that was surrounded by Cr2O3. This oxide was thicker for the humid air atmosphere when compared to dry air, and the transition of the Cu oxide to the spinel was accelerated. The Al-containing HEA formed a thin Al2O3 scale with humidity suppressing AlN formation and forming a smoother oxide layer. The Al+Cu composition had the highest overall oxidation resistance (minimal local attack, no nitridation) and also showed a smooth oxide scale topography under humid air oxidation as opposed to a plate-like, rougher scale under dry air.

Crystallography↗

Alloying effect of niobium and tin on the zirconium alloy fuel cladding behavior at high temperature oxidation in steam - 2016-0072

As the materials for fuel claddings for water-cooled reactors, binary and multicomponent zirconium alloys zirconium-niobium (Zr-Nb) (E110, M5), zirconium-tin-iron (Zr-Sn-Fe) (Zircaloy-2,-4), and zirconium-niobium-tin-iron (Zr-Nb-Sn-Fe) (E635, ZIRLO{sup R} ) most commonly are used. Improvement extends, in particular, by varying their composition by niobium, tin, and iron. At the same time, importance is given to ensuring the safe operation of the fuel rods not only in normal conditions but also in emergency situations such as a loss of coolant accident. In this paper, we present the research results of studies of the influence of alloying elements niobium, tin, and iron on corrosion resistance and embrittlement at high-temperature steam oxidation of fuel claddings based on the alloy types Zr-xNb (x=1.0/2.5) and Zr-xNb-ySn-zFe (x=0.6/2.4; y=0.24/1.1; z=0.18/0.34) made by using zirconium sponge. We conducted high-temperature steam oxidation tests at temperatures of 1,000 deg. C, 1,100 deg. C, and 1,200 deg. C with continuous measurement of the weight gain during the experiment and subsequent cooling in steam with rate ∼ 20 deg. C/s. We conducted studies of kinetics of high-temperature oxidation in steam, structural-phase state changes, alloying elements distribution, absorbed hydrogen content, and residual ductility after rapid cooling of the oxidized specimens. We revealed the difference in the oxidation kinetics of the materials studied, which decreased as the oxidation temperature increased. Likewise, an increase of the tin content in the alloy influenced a specimen's breakaway oxidation intensification at 1,000 deg. C. This shows that the mechanical properties of fuel claddings oxidized under the same conditions depend on their alloying composition, and the hydrogen fraction is absorbed by the specimen and formed by the oxidation of ZrO{sub 2}, α-Zr(O), and ex-β layer structures, which in turn varies depending on the alloy composition. The increase of niobium, tin, and iron content in the zirconium alloy leads to a decrease in the residual ductility of fuel claddings after high-temperature steam oxidation. According to obtained results, among the materials studied, Zr-1.0Nb alloy is the most resistant to embrittlement during high-temperature steam oxidation at temperatures of 1,000-1,200 deg. C. (authors)

36 MATERIALS SCIENCE↗

Evidence for redispersion of Ni on LaMnO 3 films following high-temperature oxidation

LaMnO 3 films, 0.5-nm thick, were deposited by atomic layer deposition (ALD) onto γ-Al 2 O 3 that had been modified with 15-wt% CaO. The CaO was shown to be effective in preventing formation of LaAlO 3 that formed when La 2 O 3 was deposited directly onto γ-Al 2 O 3 . Lattice fringes on the resulting CaAl 2 O 4 /γ-Al 2 O 3 substrate were weakly resolved, allowing a detailed characterization of the LaMnO 3 films. High-resolution transmission electron microscopy (HR-TEM) images showed that the LaMnO 3 formed two-dimensional crystallites, ~10 to 15 nm wide, that covered most of the surface. Crystallites with (001) and (111) orientation were clearly identified. High-temperature oxidation caused Ni to spread over the LaMnO 3 film, suggesting there is a reaction of the Ni 2+ cations with the perovskite lattice. Ni formed by high-temperature reduction on these films remained well dispersed and significantly more active for CO 2 reforming of CH 4 compared to Ni on MgAl 2 O 4 , even after repeated oxidation and reduction cycles at 1073 K. Finally, the implications of these results for understanding metal-support interactions between Ni and LaMnO 3 are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗