Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “HEAT TREATMENTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Microstructural Evaluation of KM4 and SR3 Samples Subjected to Various Heat Treatments

The gamma-gamma microstructures of two advanced powder metallurgy disk alloys, KM4 and SR3, were quantified after a series of heat treatments using transmission electron microscopy and image analysis. Relationships between the heat treatments and the resulting gamma distributions were evaluated. Statistical correlations between the gamma distributions and the reported tensile strengths, creep resistances, and dwell crack growth resistances were separately assessed for each alloy. To avoid the effects of grain size related mechanisms, the grain size of the samples used in the correlations for each alloy were limited to narrow ranges of about 1.5 in ASTM grain size number. In both alloys, yield and tensile strength increased with increasing fraction of medium sized gamma. The strength increased as the size of the medium gamma decreased and the size of the fine gamma increased. Time to 0.2 percent creep in SR3 increased with increasing medium gamma volume fraction, and decreasing fine gamma sizes. However, 0.2 percent creep time was not clearly correlated with the gamma microstructures of KM4 specimens, apparently due to effects of stabilization heat treatments which greatly suppress creep resistance. Dwell fatigue crack growth rate decreased with increasing medium gamma volume fraction, indicating more medium gamma is beneficial. The crack growth rate also decreased with decreasing gamma size, indicating finer gamma is better.

Ellis, David↗

The Effects of Heat Treatment and Microstructure Variations on Disk Superalloy Properties at High Temperature

The effects of heat treatment and resulting microstructure variations on high temperature mechanical properties were assessed for a powder metallurgy disk superalloy LSHR. Blanks were consistently supersolvus solution heat treated and quenched at two cooling rates, than aged at varying temperatures and times. Tensile, creep, and dwell fatigue crack growth tests were then performed at 704 C. Gamma' precipitate microstructures were quantified. Relationships between heat treatment-microstructure, heat treatment-mechanical properties, and microstructure-mechanical properties were assessed.

Gabb, Timothy P.↗

The Effect of Heat Treatment on Residual Stress and Machining Distortions in Advanced Nickel Base Disk Alloys

This paper describes an extension of NASA's AST and IDPAT Programs which sought to predict the effect of stabilization heat treatments on residual stress and subsequent machining distortions in the advanced disk alloy, ME-209. Simple "pancake" forgings of ME-209 were produced and given four heat treats: 2075F(SUBSOLVUS)/OIL QUENCH/NO AGE; 2075F/OIL QUENCH/1400F@8HR;2075F/OIL QUENCH/1550F@3HR/l400F@8HR; and 2160F(SUPERSOLVUS)/OIL QUENCH/1550F@3HR/ 1400F@8HR. The forgings were then measured to obtain surface profiles in the heat treated condition. A simple machining plan consisting of face cuts from the top surface followed by measurements of the surface profile opposite the cut were made. This data provided warpage maps which were compared with analytical results. The analysis followed the IDPAT methodology and utilized a 2-D axisymmetric, viscoplastic FEA code. The analytical results accurately tracked the experimental data for each of the four heat treatments. The 1550F stabilization heat treatment was found to significantly reduce residual stresses and subsequent machining distortions for fine grain (subsolvus) ME209, while coarse grain (supersolvus) ME209 would require additional time or higher stabilization temperatures to attain the same degree of stress relief.

Gayda, John↗

Effects of Heat Treatment on Microstructure, Thermal Transport and Stability in SRF Niobium

Efficient heat transfer and thermal stability are critical for preventing thermal quench and ensuring the high performance and reliability of superconducting radiofrequency (SRF) cavities, especially under high RF fields. In this article, we investigate thermal conductivity and heat capacity of high-purity cold-worked niobium used in SRF applications, with a particular focus on the effects of high-temperature heat treatments. Our measurements reveal a pronounced sensitivity of thermal transport and thermodynamic properties to the underlying microstructure such as grain size and dislocation density. The results show the critical role of controlled heat treatment processes in optimizing the thermal performance of SRF niobium, providing valuable insights for improving cavity fabrication and processing.

36 MATERIALS SCIENCE↗

Fracture characteristics and heat treatment of laser powder bed fusion additively manufactured GRCop-84 copper

Laser Powder Bed Fusion (LPBF) of Glenn Research Copper 84 (GRCop-84), a Cr 2 Nb (8 at. % Cr, 4 at. % Nb) precipitation hardened alloy, produces a fully dense high conductivity alloy with a yield strength of 500 MPa and ultimate tensile strength (UTS) of 740 MPa, superior to other competing copper alloys, and 20% elongation at fracture for material stressed perpendicular to the build direction. The high thermal stability of the Cr 2 Nb precipitate in the copper matrix reduces coarsening and maintains a 300 MPa yield, 520 MPa UTS and 26% elongation after a 900 °C, 5-h heat treatment, while a 3 h 450 °C heat treatment increases yield to 810 MPa, UTS to 970 MPa with 9% elongation at fracture, for samples stressed perpendicular to the build direction. Tensile strength anisotropy based on print direction was attributed to internal stress and columnar grain formation. Void nucleation during tensile fracture was initiated by brittle fracture of precipitate particles within the copper matrix. Fracture cusps contain matching precipitate fragment geometry on opposing sides located near the cusp center in at least 80% of fracture cusps. An optimal precipitate size of 100 nm is predicted for maximum tensile strength from precipitates on fracture surfaces, while tensile testing with varying heat treatments shows maximum strength with 100 nm and smaller precipitates. Cr2Nb precipitates are shown to transition between polycrystalline and monocrystalline structures at high temperature.

36 MATERIALS SCIENCE↗

Thermomagnetic Processing of Aluminum Alloys During Heat Treatment

Processing materials under magnetic fields is an underexplored technique to improve structure and mechanical properties in metals and alloys. Magnetic fields can alter phase stability, modify diffusion characteristics, and alter material flow substantially. In castings, magnetic fields can be used during melting of the alloy, during solidification, or during postprocessing operations such as heat treatment to achieve structural changes. This work investigates the effectiveness of thermomagnetic processing during heat treatment of Al alloys containing in the Al–Cu, Al–Si–Cu, and Al–Mg–Ce systems. We demonstrate an improvement in mechanical properties and a reduction in required heat treatment times for all alloys.

36 MATERIALS SCIENCE↗

Enhancement of Nanostructured Ferritic Alloy 14YWT Properties via Heat Treatment for Post-Consolidation Processing

The nanostructured ferritic alloy 14YWT is a promising candidate for in-core use in generation IV nuclear reactors, due to a dense dispersion of insoluble, ultrafine-scale Y-Ti-O nano-oxides, which provide a high degree of irradiation tolerance and thermal stability. This work investigates the effects of heat treatment on the workability of 14YWT, along with the effect of processing history on abnormal grain structures and radial microstructural uniformity. In this study, a 14YWT rod consolidated at 850 °C was heat treated in argon at 1100 °C, 1150 °C, 1200 °C, or 1250 °C for 1 or 8 hours and changes in mechanical properties and microstructure were examined using microhardness and electron backscattered diffraction (EBSD). Two distinct types of large abnormal grains were observed, each with unique processing origins, including one with high and the other with low strain energy. Consolidation via direct extrusion resulted in radial microstructural gradients, where the center of the rod was softer with larger grain sizes and lower strain energies. These gradients persisted and intensified throughout heat treatment. Based upon this work, the recommended heat treatment for increased workability with minimal microstructural change is 1150 °C for 1 hours.

36 MATERIALS SCIENCE↗

Effects of ZrN Coating and Heat Treatment on U-Mo Dispersion Fuel under Irradiation

The stability of U-Mo fuel particles in Al matrix can be improved using ZrN coating and heat treatment. This study investigated irradiation behaviors of fuel plates containing U-Mo fuel particles fabricated with different conditions including heat treatment and the thickness of ZrN coating. Additionally, different fission densities were applied to each fuel plate to understand how varying fission densities affect its irradiation behaviors. This study showed that more recrystallization of grains and development of high burnup structure (HBS) occurred in irradiated fuel particles with higher fission densities. Heat treatment reduced the accumulation of fission gas bubbles in the fuel particles by coarsening their grains. The fuel particles with a ZrN coating thickness of 1.2-1.8 µm showed less significant development of U-Mo/Al interaction layers than the particles with a coating thickness of 0.5 µm after irradiation. This might indicate the existence of a critical thickness of ZrN coating to minimize the formation of the interaction layers. Fission gas bubbles were observed at grain boundaries of irradiated U-Mo fuel particles at low fission densities, and the formation of dendritic features with a darker contrast was identified in backscattered electron images. These features stemmed from grain boundaries with fission gas bubbles or HBS, and some of them contained the bubbles, indicating that they might represent an early stage of HBS propagation in the fuel particles.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Heat treatment study 2

The microstructural variations in nickel based superalloys that result from modifications in processing were examined. These superalloys include MAR-M246(HF) and PWA1480. Alternate heat treatments for equiaxed as-cast specimens were studied and a sample matrix of 42 variations in the heat treatments were processed, as well as different directional solidification parameters. Variation in temperature and times for both solution and aging were performed. Photomicrographs were made of the microstructure and volume fraction analysis of primary gamma-prime and aged gamma-prime precipitates were performed. The results of the heat treatment, cooling rate, and directional solidification experiments are discussed.

Workman, Gary L.↗

The heat treatment of duralumin

When certain light aluminum alloys are heat-treated, quenched and aged, there is considerable improvement in their tensile properties. This paper presents different methods of accomplishing these heat treatments.

DURALUMIN - HEAT TREATMENT↗

Aging heat treatment design for Haynes 282 made by wire-feed additive manufacturing using high-throughput experiments and interpretable machine learning

Wire-feed additive manufacturing (WFAM) produces superalloys with complex thermal cycles and unique microstructures, often requiring optimized heat treatments. To address this challenge, we present a hybrid approach that combines high-throughput experiments, precipitation simulation, and machine learning to design effective aging conditions for the WFAM Haynes 282 superalloy. Our results demonstrate that the γ’ radius is the critical microstructural feature for strengthening Haynes 282 during post-heat treatment compared with the matrix composition and γ’ volume fraction. New aging conditions at 770°C for 50 hours and 730°C for 200 hours were discovered based on the machine learning model and were applied to enhance yield strength, bringing it on par with the wrought counterpart. This approach has significant implications for future AM alloy production, enabling more efficient and effective heat treatment design to achieve desired properties.

CALPHAD↗

Heat treatment for superalloy

A cobalt-free nickel-base superalloy composed of in weight % 15 Cr-5 Mo-3.5 Ti-4 Al-0.07 (max) C-remainder Ni is given a modified heat treatment. With this heat treatment the cobalt-free alloy achieves certain of the mechanical properties of the corresponding cobalt-containing nickel-base superalloy at 1200 F (650 C). Thus, strategic cobalt can be replaced by nickel in the alloy.

Harf, Fredric H.↗

IMPACT OF MEDIUM TEMPERATURE HEAT TREATMENT ON FLUX TRAPPING SENSITIVITY IN SRF CAVITIES

The effect of mid-T heat treatment on flux trapping sensitivity was measured on several 1.3 GHz single cell cavities subjected to medium temperature vacuum annealing at temperature of 150 - 400 ?C for a duration of 3 hours. The cavity was cooldown with residual magnetic field ?0 and ?20 mG in Dewar with cooldown condition of full flux trapped. The quality factor as a function of accelerating gradient was measured. The results show the correlation between the treatment temperature, quality factor, and sensitivity to flux trapping. Sensitivity increases with increasing heat treatment temperatures within the range of (200 - 325 ?C/3h).Moreover, variations in the effective penetration depth ofthe magnetic field and the density of quasi-particles can occur,influencing alterations in the cavity?s electromagneticresponse and resonance frequency.

Dhakal, P.↗

Effects of ZrN coating and heat treatment on U-Mo dispersion fuel systems under irradiation

The stability of U-Mo fuel particles embedded in an Al matrix under irradiation can be enhanced through ZrN coatings and/or heat treatment. Here, the present study investigates the irradiation behavior of fuel plates containing U-Mo fuel particles fabricated under various heat-treatment conditions and ZrN coating thicknesses. Different fission densities were also applied to each fuel plate to evaluate the effects of these variables. Results indicate that higher fission densities lead to more grain recrystallization and high burnup structure (HBS) development in the fuel particles. Heat treatment was found to mitigate the accumulation of fission gas bubbles in fuel particles at low fission densities by coarsening their grains. Fuel particles with ZrN coatings of a 1.2 μm thickness or above exhibited reduced formation of U-Mo/Al interaction layers, suggesting the existence of a critical ZrN coating thickness that minimizes the development of these layers. Fission gas bubbles were predominantly observed at grain boundaries of U-Mo fuel particles irradiated at low fission densities. Subgrain boundaries, which appeared to originate from the original grain boundaries containing fission gas bubbles or HBSs, were also observed, indicating the early stage of HBS propagation in the fuel particles.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Dual Microstructure Heat Treatment of a Nickel-Base Disk Alloy Assessed

Gas turbine engines for future subsonic aircraft will require nickel-base disk alloys that can be used at temperatures in excess of 1300 F. Smaller turbine engines, with higher rotational speeds, also require disk alloys with high strength. To address these challenges, NASA funded a series of disk programs in the 1990's. Under these initiatives, Honeywell and Allison focused their attention on Alloy 10, a high-strength, nickel-base disk alloy developed by Honeywell for application in the small turbine engines used in regional jet aircraft. Since tensile, creep, and fatigue properties are strongly influenced by alloy grain size, the effect of heat treatment on grain size and the attendant properties were studied in detail. It was observed that a fine grain microstructure offered the best tensile and fatigue properties, whereas a coarse grain microstructure offered the best creep resistance at high temperatures. Therefore, a disk with a dual microstructure, consisting of a fine-grained bore and a coarse-grained rim, should have a high potential for optimal performance. Under NASA's Ultra-Safe Propulsion Project and Ultra-Efficient Engine Technology (UEET) Program, a disk program was initiated at the NASA Glenn Research Center to assess the feasibility of using Alloy 10 to produce a dual-microstructure disk. The objectives of this program were twofold. First, existing dual-microstructure heat treatment (DMHT) technology would be applied and refined as necessary for Alloy 10 to yield the desired grain structure in full-scale forgings appropriate for use in regional gas turbine engines. Second, key mechanical properties from the bore and rim of a DMHT Alloy 10 disk would be measured and compared with conventional heat treatments to assess the benefits of DMHT technology. At Wyman Gordon and Honeywell, an active-cooling DMHT process was used to convert four full-scale Alloy 10 disks to a dual-grain microstructure. The resulting microstructures are illustrated in the photomicrographs. The fine grain size in the bore can be contrasted with the coarse grain size in the rim. Testing (at NASA Glenn) of coupons machined from these disks showed that the DMHT approach did indeed produce a high-strength, fatigue resistant bore and a creep-resistant rim. This combination of properties was previously unobtainable using conventional heat treatments, which produced disks with a uniform grain size. Future plans are in place to spin test a DMHT disk under the Ultra Safe Propulsion Project to assess the viability of this technology at the component level. This testing will include measurements of disk growth at a high temperature as well as the determination of burst speed at an intermediate temperature.

Gayda, John↗

Insights into the Effect of Heat Treatment and Carbon Coating on the Electrochemical Behaviors of SiO Anodes for Li-Ion Batteries

The use of SiO as an anode material has attracted significant interest due to its high capacity and long cycling life. Many promising approaches, including structural design and carbon coating at high temperatures, effectively improve its intrinsic low electrical conductivity and poor Coulombic efficiency. However, the “heat treatment process-composition and microstructure-electrochemical properties” relationship of the SiO anode is not fundamentally understood. Here the structure and composition evolution in amorphous SiO and graphene-coated SiO is investigated using different heat-treatment conditions. X-ray absorption near-edge structure techniques are also employed to analyze the surface and bulk composition change during the initial lithiation process, supplemented by physical or chemical characterization and electrochemical testing. Here results reveal the structural transition of SiO during heat treatment, from amorphous to disproportionated hierarchical structure, where the as-formed dielectric exterior SiO 2 shell and interior SiO 2 matrix severely polarizes electrodes, hindering the lithiation process. Carbon coating on SiO effectively restricts the growth of the SiO 2 shell and facilitates charge transfer, leading to improved electrochemical performance. A schematic model is proposed to reveal the relationship between the treatments, the resultant structural evolutions, and corresponding electrochemical behaviors.

36 MATERIALS SCIENCE↗

Heat treatments for high temperature cast aluminum alloys

Disclosed herein are embodiments of an aging heat treatment that can be used to replace conventional aging steps when making alloy embodiments of the present disclosure. Embodiments of the disclosed aging heat treatment reduce cost and complexity in producing aluminum alloy-based components while also promoting and/or improving microstructure stability of the aluminum alloys.

Shyam, Amit↗

Hardness and Second Phase Percentage of Ni-Ti-Hf Compounds After Heat Treatment at 700C

The Vickers hardness and second phase precipitation of three ternary intermetallic Ni-Ti-Hf compounds containing either 1, 3 or 5 at.% Hf were compared to 60-Nitinol (55 at.% Ni - 45 at.% Ti). Heat treatment either at 700 C or with a subsequent aging step, hardened the 3 and 5 at.% Hf-containing ternaries to approximately 620 HV (56 HRC). Heat treatment increased the hardness of the 1 at.% Hf compound by more than 25 percent. Average hardness of the 3 and 5 at.% Hf ternaries, though higher than that of the binary Ni-Ti or the Ni-Ti-Hf compound containing 1 at.% Hf, appeared to be fairly insensitive to the different heat treatments. There was a drastic reduction of fatigue-enhancing second phase precipitates for the 5 at.% Hf ternaries compared to the other compounds. These results should guide materials selection for development of aerospace componentry.

intermetallics↗