Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “EMBRITTLEMENT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

HYDROGEN EMBRITTLEMENT OF METALS: A PRIMER FOR THE FAILURE ANALYST

Hydrogen reduces the service life of many metallic components. Such reductions may be manifested as blisters, as a decrease in fatigue resistance, as enhanced creep, as the precipitation of a hydride phase and, most commonly, as unexpected, macroscopically brittle failure. This unexpected, brittle fracture is commonly termed hydrogen embrittlement. Frequently, hydrogen embrittlement occurs after the component has been is service for a period of time and much of the resulting fracture surface is distinctly intergranular. Many failures, particularly of high strength steels, are attributed to hydrogen embrittlement simply because the failure analyst sees intergranular fracture in a component that served adequately for a significant period of time. Unfortunately, simply determining that a failure is due to hydrogen embrittlement or some other form of hydrogen induced damage is of no particular help to the customer unless that determination is coupled with recommendations that provide pathways to avoid such damage in future applications. This paper presents qualitative and phenomenological descriptions of the hydrogen damage processes and outlines several metallurgical recommendations that may help reduce the susceptibility of a particular component or system to the various forms of hydrogen damage.

08 HYDROGEN↗

Applicability of the fracture toughness master curve to irradiated highly embrittled steel and intergranular fracture

The Heavy-Section Steel Irradiation (HSSI) Program at Oak Ridge National Laboratory has evaluated a submerged-arc (SA) weld irradiated to a high level of embrittlement and a temper embrittled base metal that exhibits significant intergranular fracture (IGF) relative to representation by the Master Curve. The temper embrittled steel revealed that the intergranular mechanism significantly extended the transition temperature range up to 150 C above To. For the irradiated highly embrittled SA weld study, a total of 21 1T compact specimens were tested at five different temperatures and showed the Master Curve to be nonconservative relative to the results, although that observation is uncertain due to evidence of intergranular fracture.

36 MATERIALS SCIENCE↗

On High-Fluence Irradiation Hardening of Nine RPV Surveillance Steels in the UCSB ATR-2 Experiment: Implications for Extended-Life Embrittlement Predictions

Nine archival reactor pressure vessel (RPV) surveillance steels from commercial nuclear power plants were irradiated in the University of California, Santa Barbara Advanced Test Reactor 2 (ATR-2) experiment to evaluate irradiation embrittlement under low-flux surveillance capsule versus higher flux test reactor (ATR-2) conditions. The postirradiation measurements of irradiation hardening, measured as increases in yield stress (Δσy), and corresponding conversions of Δσy to Charpy V-notch 41-J transition temperature shifts (ΔTc) are compared with various embrittlement trend curve (ETC) model predictions for the nine steels. Tensile and converted shear punch and microhardness measurements of Δσy generally show a continuing increase between intermediate and high ATR-2 fluences. The Eason-Odette-Nanstad-Yamamoto and ASTM E900 ETC models underpredict embrittlement at the ATR-2 irradiation condition: irradiation temperature (Ti) of 292°C, neutron fluence (ϕt) of 1.4 × 1020 n/cm2 (E > 1 MeV), and neutron flux (ϕ) of 3.68 × 1012 n/cm2-s. On average, the French FIS and Japanese JAEC ETCs slightly overpredict the ATR-2 data. The increase in Δσy with higher fluence is primarily due to Ni-Mn-Si precipitates, which slowly evolve in both nearly copper-free and copper-bearing steels. Finally, a new Odette-Wells-Almirall-Yamamoto embrittlement model is shown that yields good predictions for the nine steels at high fluences (ϕt > 5.5 × 1019 n/cm2).

Nanstad, Randy K.↗

Hydrogen Embrittlement of Structural Steels

Carbon-manganese steels are candidates for the structural materials in hydrogen gas pipelines; however, it is well known that these steels are susceptible to hydrogen embrittlement. Decades of research and industrial experience have established that hydrogen embrittlement compromises the structural integrity of steel components. This experience has also helped identify the failure modes that can operate in hydrogen containment structures. As a result, there are tangible ideas for managing hydrogen embrittlement in steels and quantifying safety margins for steel hydrogen containment structures. For example, fatigue crack growth aided by hydrogen embrittlement is a well-established failure mode for steel hydrogen containment structures subjected to pressure cycling. This pressure cycling represents one of the key differences in operating conditions between current hydrogen pipelines and those anticipated in a hydrogen delivery infrastructure. Applying structural integrity models in design codes coupled with measurement of relevant material properties allows quantification of the reliability/integrity of steel hydrogen pipelines subjected to pressure cycling. Furthermore, application of these structural integrity models is aided by the development of physics-based predictive models, which provide important insights such as the effects of microstructure on hydrogen-assisted fatigue crack growth. Successful implementation of these structural integrity and physics-based models enhances confidence in the design codes and enables decisions about materials selection and operating conditions for reliable and efficient steel hydrogen pipelines.

36 MATERIALS SCIENCE↗

Environmental hydrogen embrittlement of an alpha-beta titanium alloy - Effect of microstructure.

Study of environmental hydrogen embrittlement of a Ti-6 Al-4 alloy as a function of test displacement rate and of variations in alpha-beta microstructure. Embrittlement in low-pressure (about 1 atm) gaseous hydrogen was inversely dependent on test displacement rate and strongly dependent on microstructure. At a given displacement rate, microstructures having a continuous alpha-phase matrix were less severely embrittled than those having a continuous beta-phase matrix. Further, brittle fracture occurred in the former microstructures by transgranular cleavage and in the latter microstructures by intergranular separation. These observations are consistent with previous studies made on slow strain-rate embrittlement of hydrogen-charged titanium alloys and are explained in terms of relative hydrogen transport rates within the alpha-phase and beta-phase titanium.

Nelson, H. G.↗

Effects of alloy composition in alleviating embrittlement problems associated with the tantalum alloy T-111

The causes of aging embrittlement in T-111 (Ta-8W-2Hf) and the effect of alloy modification were investigated. Results show that T-111 possesses a critical combination of tungsten and hafnium that leads to loss in ductility at -196 C after aging near 1040 C. It was found that this occurs because tungsten enhances hafnium segregation to grain boundaries, which also leads to increased susceptibility to hydrogen embrittlement. Aging embrittlement was not observed in tantalum alloys with reduced tungsten or hafnium contents; most of the alloys studied have lower strengths than T-111 and exhibit susceptibility to hydrogen embrittlement.

Stephens, J. R.↗

Effects of alloy composition in alleviating embrittlement problems associated with the tantalum alloy T-111

The causes of aging embrittlement in T-111 (Ta-8W-2Hf) and the effects of alloy modification were investigated. Results showed that T-111 contains a critical combination of tungsten and hafnium that leads to loss of ductility at -196 C after aging near 1040 C. This appears to occur because tungsten enhances hafnium segregation to grain boundaries and this also leads to increased susceptibility to hydrogen embrittlement. Aging embrittlement was not observed in tantalum alloys with reduced tungsten or hafnium contents; however, most of the alloys studied have lower strengths than T-111 and exhibit susceptibility to hydrogen embrittlement.

Stephens, J. R.↗

Technique to Predict Ultraviolet Radiation Embrittlement of Polymers in Space

In the low-Earth-orbit environment, solar ultraviolet (UV) radiation embrittles polymer materials through bond breaking and crosslinking. This UV embrittlement increases the surface hardness of the polymer. Before the durability of polymer materials in the low- Earth-orbit environment can be predicted, the extent of UV embrittlement needs to be determined. However, traditional techniques for measuring the microhardness of materials cannot be employed to measure changes in the hardness of UV-embrittled surfaces because traditional techniques measure bulk hardness and are not sensitive enough to surface changes. A unique technique was used at the NASA Lewis Research Center to quantify polymer surface damage that had been induced by UV radiation. The technique uses an atomic force microscope (AFM) to measure surface microhardness. An atomic force microscope measures the repulsive forces between the atoms in a microscopic cantilevered tip and the atoms on the surface of a sample. Typically, an atomic force microscope produces a topographic image of a surface by monitoring the movement of the tip over features of the surface. The force applied to the cantilevered tip, and the indention of the tip into the surface, can be measured. The relationship between force and distance of indentation, the quantity force/distance (newtons/meter), provides a measure of the surface hardness. Under identical operating conditions, direct comparisons of surface hardness values can be made.

Source record↗

Nickel-Based Superalloy Resists Embrittlement by Hydrogen

A nickel-based superalloy that resists embrittlement by hydrogen more strongly than does nickel alloy 718 has been developed. Nickel alloy 718 is the most widely used superalloy. It has excellent strength and resistance to corrosion as well as acceptably high ductility, and is recognized as the best alloy for many high-temperature applications. However, nickel alloy 718 is susceptible to embrittlement by hydrogen and to delayed failure and reduced tensile properties in gaseous hydrogen. The greater resistance of the present nickel-based superalloy to adverse effects of hydrogen makes this alloy a superior alternative to nickel alloy 718 for applications that involve production, transfer, and storage of hydrogen, thereby potentially contributing to the commercial viability of hydrogen as a clean-burning fuel. The table shows the composition of the present improved nickel-based superalloy in comparison with that of nickel alloy 718. This composition was chosen to obtain high resistance to embrittlement by hydrogen while maintaining high strength and exceptional resistance to oxidation and corrosion. The most novel property of this alloy is that it resists embrittlement by hydrogen while retaining tensile strength greater than 175 kpsi (greater than 1.2 GPa). This alloy exhibits a tensile elongation of more than 20 percent in hydrogen at a pressure of 5 kpsi (approximately equal to 34 MPa) without loss of ductility. This amount of elongation corresponds to 50 percent more ductility than that exhibited by nickel alloy 718 under the same test conditions.

Lee, Jonathan↗

On High-Fluence Irradiation Hardening of Nine RPV Surveillance Steels in the UCSB ATR-2 Experiment: Implications for Extended-Life Embrittlement Predictions

Nine archival reactor pressure vessel (RPV) surveillance steels from commercial nuclear power plants were irradiated in the University of California, Santa Barbara Advanced Test Reactor 2 (ATR-2) experiment to evaluate irradiation embrittlement under low-flux surveillance capsule versus higher flux test reactor (ATR-2) conditions. The postirradiation measurements of irradiation hardening, measured as increases in yield stress (Δσy), and corresponding conversions of Δσy to Charpy V-notch 41-J transition temperature shifts (ΔTc) are compared with various embrittlement trend curve (ETC) model predictions for the nine steels. Tensile and converted shear punch and microhardness measurements of Δσy generally show a continuing increase between intermediate and high ATR-2 fluences. The Eason-Odette-Nanstad-Yamamoto and ASTM E900 ETC models underpredict embrittlement at the ATR-2 irradiation condition: irradiation temperature (Ti) of 292°C, neutron fluence (ϕt) of 1.4 × 1020 n/cm2 (E > 1 MeV), and neutron flux (ϕ) of 3.68 × 1012 n/cm2-s. On average, the French FIS and Japanese JAEC ETCs slightly overpredict the ATR-2 data. The increase in Δσy with higher fluence is primarily due to Ni-Mn-Si precipitates, which slowly evolve in both nearly copper-free and copper-bearing steels. Finally, a new Odette-Wells-Almirall-Yamamoto embrittlement model is shown that yields good predictions for the nine steels at high fluences (ϕt > 5.5 × 1019 n/cm2).

Nanstad, Randy↗

Rethinking of Zircaloy Embrittlement Criteria for Improving Safety Margin of Light Water Reactor

Zircaloy embrittlement criteria have become a basis for the current emergency core cooling system (ECCS) criteria to maintain the coolable geometry. U.S. NRC has considered that retaining adequate cladding ductility is a simple and effective way for ensuring the structural integrity of fuel rods under the accident conditions. Considering this, the current ECCS criteria limits the peak cladding temperature(PCT) to be 1204 deg. C, and equivalent cladding reacted (ECR) to be 17%, calculated by the Baker-Just equation. However, the criteria were established based on the experimental investigations in early 1970's and it has inevitably limitations, in particular, about hydrogen embrittlement with burnup. As a consequence, the new draft-rule proposes a relation that gives rise to a decreasing ECR limit with respect to pre-transient hydrogen content by U.S NRC. The regulation of Japan is quite different from that of U.S. NRC. This rule is set to assure structural integrity of ruptured fuel rods upon water-quenching. Recently, Japanese Atomic Energy Agency (JAEA) conducted integral fuel rod thermal shock tests with high burnup claddings. These investigations confirmed that the original criteria (PCT 1200 deg. C, ECR 15% calculated by Baker-Just equation ) still successfully guarantee fuel rod structural integrity upon thermal shock and concluded that the high-burnup effects are inconsiderable as the thermal-shock fracture boundary is not significantly reduced. Hence, there exists an obvious disagreement between the embrittlement-based and the thermal shock fracture-based criterion particularly when it comes to the high burnup consideration. The one of them can be adopted to define safety limit and safety margin which is the difference between the regulation limit and actual value of the parameter. Also, it is worth noting that the temperature limit (1204 deg. C) of the Zircaloy embrittlement criteria has not been altered since it was first determined in 1970's. Such a qualitative concern alone should not limit further discussions on the potential increase in the temperature limit. Indeed, there is ample experimental evidence that supports the possibility that Zircaloy ductility can be maintained beyond 1204 deg. C if it is oxidized for a limited time period. The increase in the temperature margin can lead to a reactor power uprate, or allow an increased accident coping time. This paper aims to achieve a comprehensive understanding of an engineering compatibility between nuclear fuel behaviors, safety system, and safety criteria, in the pursuit of increasing safety margin of LWRs. Specifically, this study presents a revision the current temperature limit (1204 deg. C) with adjustable ECR levels through an extensive literature review. And the impact of this temperature limit on the actual design basis accident margin is discussed. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Evaluation of the Role of Metallic Matrix on Environmentally Assisted Embrittlement of Austempered Ductile Iron (ADI) Using High Si Steel

The objective of this work stems from the environmentally assisted embrittlement suffered by austempered ductile iron (ADI) when its surface is submerged in water. This phenomenon leads to a drop in elongation and ultimate tensile strength of about 75% and 10%, respectively, while the 0.2% offset strain stress remains unaffected. Heat-treating a high Si steel, an ausferritic matrix similar to that present in the ADI under study is obtained, yielding giving a very good combination of tensile strength and elongation. In this manner, it was possible to examine the influence of the metallic matrix such as that present in ADI, though without nodules and cell boundaries, also called last to freeze zones (LTF). Tensile test evaluations on ADI and steel samples under dry and wet conditions were carried out. Additionally, a very specific test, introducing surface cracks, was conducted with the purpose of expanding the current knowledge on this particular kind of fracture. Earlier investigations on ADI have suggested that the process of embrittlement starts in a surface crack generated at the early stages of plastic deformation in LTF zones, which results from the solidification process, where pores, inclusions and unreacted austenite are present. In this manner, water penetrates and weakens the material strength, making the crack grow very fast and leading to an instantaneous samples failure. The main results obtained in this work include the confirmation of the deleterious effect of the LTF zones in the embrittlement process and the fracture surface analysis showing characteristic features of this kind of failure.

36 MATERIALS SCIENCE↗

Experimental and Numerical Analysis of Liquid Metal Embrittlement Crack Location

Advanced high-strength steels used in automotive structural components are commonly protected using zinc coatings. However, the steel/zinc system creates the potential for liquid metal embrittlement during welding. Although liquid metal embrittlement cracks are known to form, the current literature does not include crack location when assessing crack severity. In this work, TRIP1100 joints showed that LME cracks decreased strength from 7.8 to 42.2%, depending on location, between the coated (cracked) and uncoated (non-cracked) condition. Liquid metal embrittlement cracks in critical locations were observed to propagate until fracture from lap shear testing. However, cracks in non-critically loaded areas were not part of the fracture path and did not result in a significant loss in strength. This shows LME crack location can be controlled to improve joint performance and vehicle safety. In addition, a model of lap shear testing in a cracked sample showed how the presence of a crack can affect the internal stress field depending on its location.

36 MATERIALS SCIENCE↗

Characterizing the flux effect on the irradiation embrittlement of reactor pressure vessel steels using machine learning

In-service exposure to high-energy neutrons embrittles reactor pressure vessel (RPV) steels. An increase in the yield stress (Δσ y ) results in a corresponding increase in the brittle to ductile transition temperature (ΔT c ). Most existing models underpredict ΔT c at higher fluence following accelerated irradiations in test reactors. High fluence, up to 10 20 n/cm 2 in some cases, will be reached over extended RPV vessel operation of 80 years, or more, at low service flux. Embrittlement has been extensively studied in accelerated, higher flux test reaction irradiations. However, the use of test reactor data naturally raises the question of flux effects. Here, this study used a machine learning approach trained on a set of hardening data, covering a wide range of flux, fluence, and steel compositions to determine the interactive effects of both irradiation and material variables on Δσ y . The analysis included machine learning-based cross-plots of the variable dependence of Δσ y for six core steels (i.e., CM6, LC, LD, LG, LH, and LI), with controlled differences in their Cu and Ni contents. A primary objective is to evaluate an effective to actual fluence (Φt e /Φt) ratio, as a function of flux, fluence, and steel composition. This is information critical to properly use intermediate flux-high fluence data in calibrating a low flux-high fluence embrittlement model. The predicted Φt e /Φt is reasonably consistent with estimates previously derived from a physics-based solute recombination trap model.

36 MATERIALS SCIENCE↗

Detection of voids in hydrogen embrittled iron using transmission X-ray microscopy

Hydrogen embrittlement remains a barrier to widespread adoption of hydrogen as a carbon-neutral energy source. Here, hydrogen embrittlement mechanisms are investigated across length scales in iron using transmission X-ray microscopy (TXM), digital image correlation (DIC), and notched tensile testing during in-situ electrochemical hydrogen charging. TXM reveals void size and spatial distribution ahead of a propagating crack. We find hydrogen charging leads to voids within ~10 μm of the crack tip and suppression of voids beyond this distance. Near the crack tip, voids are elongated in the direction of the crack and are smaller than voids in an uncharged sample. In the presence of hydrogen, these voids lead to quasi-cleavage fracture and a sharper crack tip. DIC shows localization and reduction of plastic strain with hydrogen charging, and tensile testing reveals a reduction in fracture energy and elongation at failure. Finally, these results are discussed in the context of hydrogen embrittlement mechanisms.

08 HYDROGEN↗

Hydrogen Embrittlement of Medium Mn Steels

Recent research efforts to develop advanced–/ultrahigh–strength medium-Mn steels have led to the development of a variety of alloying concepts, thermo-mechanical processing routes, and microstructural variants for these steel grades. However, certain grades of advanced–/ultrahigh–strength steels (A/UHSS) are known to be highly susceptible to hydrogen embrittlement, due to their high strength levels. Hydrogen embrittlement characteristics of medium–Mn steels are less understood compared to other classes of A/UHSS, such as high Mn twinning–induced plasticity steel, because of the relatively short history of the development of this steel class and the complex nature of multiphase, fine-grained microstructures that are present in medium–Mn steels. The motivation of this paper is to review the current understanding of the hydrogen embrittlement characteristics of medium or intermediate Mn (4 to 15 wt pct) multiphase steels and to address various alloying and processing strategies that are available to enhance the hydrogen-resistance of these steel grades.

36 MATERIALS SCIENCE↗

A Review of Recent Advances in the Understanding of Liquid Metal Embrittlement

Significant advances in the study of liquid metal embrittlement have occurred since 2000 but there have been few reviews of the liquid metal embrittlement literature since that time. This paper discusses recent advances in modelling and testing. Specific solid - liquid systems (including steel exposed to molten lead-bismuth and aluminum - gallium ) are reviewed. Relationships between various studies are considered and the need for careful test protocols is emphasized. The individual effects of wetting, crack initiation and propagation are discussed. Finally, mechanisms of liquid metal embrittlement including interatomic and mass-transport based phenomena are analyzed.

36 MATERIALS SCIENCE↗

A Mechanical Study of T91 Embrittlement by Liquid Lead-bismuth Eutectic

The susceptibility of liquid metal embrittlement of the T91 martensitic steel is investigated from slow deformation rate (6.67x10{sup -8} m.s{sup -1}) to high deformation rate (6.67x10{sup -3} m.s{sup -1}), using a Center Cracked in Tension geometry. Brittle fracture, characterized by elongated river cracks on all the fracture surfaces, indicates that T91 is sensitive to the Embrittlement by LBE. This embrittlement effect is very marked at the low deformation rate ({approx}10{sup -5} mm.s{sup -1}). A ductile-brittle transition is observed in the high strain rate range investigated. In this transition regime, there is a competition between the growth of dimples and the cracking induced by the liquid metal. Ductility recovery is complete at the highest investigated displacement rate. This dependence of T91/LBE susceptibility to LME on the displacement rate and the brittle to ductile transition at high strain rate is confirmed by a fracture mechanics analysis. (authors)

36 MATERIALS SCIENCE↗