Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ELECTRON BEAM WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

The effect of electron beam welding on the creep rupture properties of a Nb-Zr-C alloy

Creep rupture tests of electron beam welded PWC-11 sheet were conducted at 1350 K. Full penetration, single pass welds were oriented transverse to the testing direction in 1 mm thick sheet. With this orientation, stress was imposed equally on the base metal, weld metal, and heat-affected zone. Tests were conducted in both the postweld annealed and aged conditions. Unwelded specimens with similar heat treatments were tested for comparative purposes. It was found that the weld region is stronger than the base metal for both the annealed and aged conditions and that the PWC-11 material is stronger in the annealed condition than in the aged condition.

Moore, T. J.↗

Exploration Extravehicular Mobility Unit (xEMU): Electron Beam Welding of the Portable Life Support System (PLSS) Ti-6Al-4V Backplate with Integrated Cooling Channels

The Exploration Extravehicular Mobility Unit (xEMU) is the first clean sheet redesign of the astronaut spacesuit in approximately 40 years. NASA Langley Research Center’s electron beam welding team, of which the author is a member, is leading the development of the weld technology required to manufacture the backplate component of the Portable Life Support System (PLSS). This backplate will provide both structural support and integral cooling for the life support systems, communications, and other electronics inside the spacesuit.

electron beam welding↗

Detecting overpenetration of electron-beam welds

Gold plate beneath weldment reveals areas of excess penetration during X-ray inspection. Technique is applicable to critical electron-beam welds, such as those in gas turbines and pressure vessels.

Macfarlane, D. I.↗

Preventing Contamination In Electron-Beam Welds

Simple expedient eliminates time-consuming, expensive manual hand grinding. Use of groove and backup tube greatly reduces postweld cleanup in some electron-beam welding operations. Tube-backup method developed for titanium parts, configurations of which prevents use of solid-block backup. In new welding configuration, tube inserted in groove to prevent contact between alumina beads and molten weld root. When welding complete and beads and tube removed, only minor spatter remains and is ground away easily.

Goodin, Wesley D.↗

Electron Beam Welding to Join Gamma Titanium Aluminide Articles

A method is provided for welding two gamma titanium aluminide articles together. The method includes preheating the two articles to a welding temperature of from about 1700 F to about 2100 F, thereafter electron beam welding the two articles together at the welding temperature and in a welding vacuum to form a welded structure, and thereafter annealing the welded structure at an annealing temperature of from about 1800 F to about 2200 F, to form a joined structure.

Kelly, Thomas Joseph↗

Manufacturing Full-Scale High Gradient Copper Accelerators: Electron Beam Welding and Allied Processes

This DOE ARDAP-funded study examines the technical and business feasibility of manufacturing high-gradient normal conducting RF (NCRF) copper accelerating structures using electron beam welding (EBW) instead of conventional high-temperature brazing. The core motivation is material performance: brazing softens copper significantly, while hard copper alloys have demonstrated ~75% higher operational gradients in SLAC tests, making cold-joining techniques highly attractive. EBW, applied to split-cell (half or quadrant) structure designs, preserves copper hardness away from the weld joint and simplifies machining — but industrial process optimization remains immature and a substantial learning curve is expected. The business case was modeled for two scenarios: a greenfield EBW linac company (> $10M upfront costs, viable above ~30 units/year) and an EBW division added to an existing accelerator firm to reduce risk and upfront costs, at the expense of being less optimal structure for the higher volume production. The study concludes that without a significant increase in demand, private investment alone cannot sustain this capability, and recommends federal support through R&D grants, procurement incentives, and CAPEX cost-sharing to incubate domestic EBW-NCRF manufacturing — with the existing-company model.

43 PARTICLE ACCELERATORS↗

Power distribution for electron beam welding

The power distribution of an electron seam is analyzed. Digital computer techniques are used to evaluate the radial distribution of power detected by a wire probe circulating through the beam. Results are reported.

Edwards, E.↗

Microstructure and 77K mechanical properties of electron beam welded Cu101- Inconel 625 joints

In developing large-scale next-generation superconducting radio frequency (SRF) linear accelerators using superconducting films on Cu, the design and development of dissimilar welding and joining metals, such as Cu to Inconel, stainless steel, and Nb, are essential. In this talk, we present the development of procedures for electron-beam welding of Cu¿Inconel 625 and evaluation of the microstructure and 77K mechanical properties of the weld and base material in the welded condition and heat treatments in the 750°C ¿950°C heat treatment range. The results will be presented in the context of developing joining techniques for low-temperature applications where high conductivity and strength, vacuum hygiene, and magnetic properties of the material need consideration. The methods presented here are being deployed to thin film SRF Cu cavities at Jefferson Lab. Acknowledgment: This material is based upon work supported by the U.S. Department of Energy, Office of Science, Office of Nuclear

Khanal, Bashu↗

Electron Beam Welding of Pure Tungsten Hex Cans for Nuclear Thermal Propulsion Engines

Nuclear thermal propulsion (NTP) is an in-space propulsion method currently being developed at the NASA Marshall Space Flight Center (MSFC). NTP systems are a high specific impulse (750–1,100 s), high thrust (15,000–250,000 lbf ) method of propulsion which have the potential to allow for faster transit times when optimizing for high ΔV. In the nuclear rocket engine, the heat from the nuclear fission reaction is transferred to a low molecular mass propellant (such as hydrogen). Hot propellant is expanded through a nozzle to generate thrust. Development of ceramic metal (cermet) fuel systems for NTP applications is currently ongoing at MSFC. In cermet fuel systems, ceramic fissile fuel particles such as uranium nitride or uranium dioxide are dispersed within a net-shaped, high-density structural matrix. The composite material is cladded by a protective metal structure to make up an NTP fuel element. Cladding materials must be able to withstand the demanding operating conditions required of the engine as well as retain a hermetic seal to allow for retention of fuel element structural integrity, prevent hydrogen attack or migration of the ceramic fuel, and limit release of fission products during operation. For NTP applications, tungsten is a prime material for both the metal matrix and cladding in cermet fuel systems because of its high melting point, high temperature strength, and compatibility with hot hydrogen. If a weld in tungsten with the capability of holding a hermetic seal is achievable, tungsten becomes a strong candidate for NTP applications. This Technical Memorandum focuses on determining the weldability of pure tungsten using electron beam welding (EBW). Tungsten appears well suited for NTP applications, but it has a high ductile to brittle transition temperature (DBTT) dependent upon chemical composition, structure/stress distribution, and mechanical conditions. Therefore, it is highly subject to brittle fracture. Because of its high susceptibility to brittle fracture, it is very difficult to weld. EBW was chosen for joining pure tungsten because of its low heat input compared to gas tungsten arc welding. Reduced heat input can be directly correlated with an increase in ductility of a tungsten weld. EBW is a high energy density welding process in which a stream of electrons penetrates a weld joint in a deep, narrow spike in contrast to a broad gas tungsten arc weld pool. The investigation initially focused on EBW of tungsten plates of both 0.01 in and 0.03 in thickness to determine if EBW could weld pure tungsten without the presence of visual defects—particularly cracking—in the welds. Variation in the weld procedure and post-weld heat treatment (PWHT) was used to improve the surface appearance of flat EBWs on a pure tungsten sheet. The investigation moved on to weld 0.05-in-thick hexagonal tungsten cans with a weld joint thickness of 0.025 in. The goal for welding the pure tungsten hex cans was to avoid any visual surface defects and generate a weld capable of a hermetic seal. This proved difficult. Cold welds commonly exhibited porosity that leaked air. Hot welds exhibited cracks, typically observed immediately after welding. Later welds were preheated to increase ductility and decrease the likelihood of through-thickness cracking. PWHT was used to arrest microcrack growth both in the flat weld samples and hexagonal weld samples.

Courtright, Z. S.↗

Electron Beam Welding of Additively Manufactured Niobium Alloy Heat Pipes

Additively manufactured refractory alloy-liquid metal heat pipes are being developed and tested for thermal management systems within nuclear propulsion and power applications. This study investigated electron beam (EB) welded joints on a laser powder bed fusion printed niobium alloy (C-103) and the impact of multiple joined heat pipe sections on working fluid flow and container leak-tightness. Results showed that EB welded joints connecting multiple heat pipe sections do not impact working fluid wicking behavior and the printed C-103 material and the EB welds joining the tubular sections created a leak-tight container. Interestingly, CT data showed an order of magnitude greater number and volume of porosity indications in the ground mating surface weld compared to the as-printed mating surface weld. The work concluded that AM is a viable manufacturing process for niobium alloy heat pipes and provided valuable insights for future AM heat pipe research and development.

Electron beam welding↗

Performance of 75-millimeter-bore bearings using electron-beam-welded hollow balls with a diameter ratio of 1.26

An experimental investigation was performed to determine the rolling element fatigue life of electron beam-welded hollow balls with a diameter ratio (o.d./i.d.) of 1.26 and to determine the operating characteristics of bearings using these hollow balls. Similar bearings with solid balls were also tested and the data compared. The bearings were operated at shaft speeds up to 28,000 rpm with a thrust load of 2200 N (500 lb). Ball failures during the bearing tests were due to flexure fatigue. The solid and hollow ball bearings tested showed little difference in outer race temperatures and indicated the same bearing torque. The 17.5-mm (0.6875-in.) diameter balls were also tested in the five-ball fatigue tester and showed no significant difference in life when compared with the life of a solid ball.

Coe, H. H.↗

Investigations for the improvement of space shuttle main engine electron beam welding equipment

Progress made in the testing, evaluation, and correction of MSFC's 7.5 kW electron beam welder in support of space shuttle main engine component welding is summarized. The objective of this project was to locate and correct the deficiencies in the welder. Some 17 areas were deficient in the 7.5 kW ERI welding system and the associated corrective action was taken to improve its operational performance. An overall improvement of 20 times the original reliability was obtained at full rated capacity after the modifications were made.

Smock, R. A.↗

Onorbit electron beam welding experiment definition

The proposed experiment design calls for six panels to be welded, each having unique characteristics selected to yield specific results and information. The experiment is completely automated and the concept necessitated the design of a new, miniaturized, self-contained electron beam (EB) welding system, for which purpose a separate IR and D was funded by the contractor, Martin Marietta Corporation. Since future tasks beyond the proposed experiment might call for astronauts to perform hand-held EB gun repairs or for the gun to be interfaced with a dexterous robot such as the planned flight telerobotic servicer (FTS), the EB gun is designed to be dismountable from the automated system. In the experiment design, two separate, identical sets of weld panels will be welded, one on earth in a vacuum chamber and the other onorbit in the aft cargo bay of an orbiter. Since the main objective of the experiment is to demonstrate that high quality welds can be achieved under onorbit conditions, the welds produced will be subjected to a wide range of discriminating non-destructive Q.C. procedures and destructive physical tests. However, advantage will be taken of the availability of a fairly large quantity of welded material in the two series of welded specimens to widen the circle of investigative talent by providing material to academic and scientific institutions for examination.

William H. Hooper↗

Controlling Electron-Beam-Weld Focus

Control loop measures weld-spot temperature to regulate focus current. Square-wave generator modulates current in electron-beam focus coil so that focal point is varied between points slightly above and below surface of weld. Sensor detects intensity of light emitted by weld, proportional to fourth power of temperature at hottest part of weld spot. Sensor signal is detected by chopper demodulator synchronized by square-wave generator, to determine whether average position of focal point is higher than, coincident with, or lower than optimum point; and focus coil current is adjusted accordingly.

Coate, F. M.↗

Assessment of Corona/Arcing Hazard for Electron Beam Welding in Space Shuttle Bay at LEO for ISWE: Test Results

Test welds were made in argon over a range of pressures from 10-5 to 10-3 torr (the latter pressure an order of magnitude above pressures anticipated in the space shuttle bay during welding) with and without plasma on 304 stainless steel, 6Al-4V titanium, and 5456 aluminum in search of any possible unwanted electrical discharges. Only a faint steady glow of beam-excited atoms around the electron beam and sometimes extending out into the vacuum chamber was observed. No signs of current spiking or of any potentially dangerous electrical discharge were found.

Nunes, A. C., Jr.↗