Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Dislocation Lines”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

53 records · Page 3

The Fast Radio Burst Luminosity Function and Death Line in the Low-Twist Magnetar Model

We explore the burst energy distribution of fast radio bursts(FRBs)in the low-twist magnetar model ofWadiasingh & Timokhin(WT19). Motivated by the power-lawfluence distributions of FRB121102, we proposean elementary model for the FRB luminosity function of individual repeaters with an inversion protocol thatdirectly relates the power-law distribution index of magnetar short burstfluences to that for FRBs. The protocolindicates that the FRB energy scales virtually linearly with crust/field dislocation amplitude, if magnetar shortbursts prevail in the magnetoelastic regime. Charge starvation in the magnetosphere during bursts(required inWT19)for individual repeaters implies the predicted burstfluence distribution is narrow,3 decades for yieldingstrains and oscillation frequencies feasible in magnetar crusts. Requiring magnetic confinement and chargestarvation, we obtain a death line for FRBs, which segregates magnetars from the normal pulsar population,suggesting only the former will host recurrent FRBs. We convolve the burst energy distribution for individualmagnetars to define the distribution of luminosities in evolved magnetar populations. The broken power-lawluminosity function’s low-energy character depends on the population model, while the high-energy index tracesthat of individual repeaters. Independent of the evolved population, the broken power-law isotropic-equivalentenergy/luminosity function peaks at∼1037–1040erg with a low-energy cutoff at∼1037erg. Lastly, we considerthe localfluence distribution of FRBs andfind that it can constrain the subset of FRB-producing magnetarprogenitors. Our model suggests that improvements in sensitivity may reveal aflattening of the global FRBfluencedistribution and saturation in FRB rates.

Cosmology↗

Correlations between critical current density, j(sub c), critical temperature, T(sub c),and structural quality of Y1B2Cu3O(7-x) thin superconducting films

Correlations between critical current density (j(sub c)) critical temperature (T(sub c)) and the density of edge dislocations and nonuniform strain have been observed in YBCO thin films deposited by pulsed laser ablation on (001) LaAlO3 single crystals. Distinct maxima in j(sub c) as a function of the linewidths of the (00 l) Bragg reflections and as a function of the mosaic spread have been found in the epitaxial films. These maxima in j(sub c) indicate that the magnetic flux lines, in films of structural quality approachingthat of single crystals, are insufficiently pinned which results in a decreased critical current density. T(sub c) increased monotonically with improving crystalline quality and approached a value characteristic of a pure single crystal. A strong correlation between j(sub c) and the density of edge dislocations ND was found. At the maximum of the critical current density the density of edge dislocations was estimated to be N(sub D) approximately 1-2 x 10(exp 9)/sq cm.

Chrzanowski, J.↗

Fatigue and creep-fatigue deformation of several nickel-base superalloys at 650 C

Transmission electron microscopy has been used to study the bulk deformation characteristics of seven nickel-base superalloys tested in fatigue and creep-fatigue at 650 C. The alloys were Waspalloy, HIP Astroloy, H plus F Astroloy, H plus F Rene 95, IN 100, MERL 76, and NASA IIB-7. The amount of bulk deformation observed in all the alloys was low. In tests with inelastic strain amplitudes less than about 0.003, only some grains exhibited yielding and the majority of those had the 110 line near the tensile axis. Deformation occurred on octahedral systems for all of the alloys except MERL 76 which also showed abundant primary cube slip. Creep-fatigue cycling occasionally produced extended faults between partial dislocations, but otherwise deformation was much the same as for fatigue cycling.

Miner, R. V.↗

Interaction between a circular inclusion and an arbitrarily oriented crack

The plane interaction problem for a circular elastic inclusion imbedded into an elastic matrix which contains an arbitrarily oriented crack is considered. Using the existing solutions for the edge dislocations as Green's functions, first the general problem of a through crack in the form of an arbitrary smooth arc located in the matrix in the vicinity of the inclusion is formulated. The integral equations for the line crack are then obtained as a system of singular integral equation with simple Cauchy kernels. The singular behavior of the stresses around the crack tips is examined and the expressions for the stress intensity factors representing the strength of the stress singularities are obtained in terms of the asymptotic values of the density functions of the integral equations. The problem is solved for various typical crack orientations and the corresponding stress intensity factors are given.

Erdogan, F.↗

Interaction between a circular inclusion and an arbitrarily oriented crack

The plane interaction problem for a circular elastic inclusion embedded in an elastic matrix which contains an arbitrarily oriented crack is considered. Using the existing solutions for the edge dislocations as Green's functions, first the general problem of a through crack in the form of an arbitrary smooth arc located in the matrix in the vicinity of the inclusion is formulated. The integral equations for the line crack are then obtained as a system of singular integral equations with simple Cauchy kernels. The singular behavior of the stresses around the crack tips is examined and the expressions for the stress-intensity factors representing the strength of the stress singularities are obtained in terms of the asymptotic values of the density functions of the integral equations. The problem is solved for various typical crack orientations and the corresponding stress-intensity factors are given.

Erdogan, F.↗

Analysis of plastic deformation in silicon web crystals

Numerical calculation of 111-plane 110-line slip activity in silicon web crystals generated by thermal stresses is in good agreement with etch pit patterns and X-ray topographic data. The data suggest that stress redistribution effects are small and that a model, similar to that proposed by Penning (1958) and Jordan (1981) but modified to account for dislocation annihilation and egress, can be used to describe plastic flow effects during silicon web growth.

Spitznagel, J. A.↗

Mechanism of slip and twinning

The objectives are to: (1) demonstrate the mechanisms of deformation in body centered cubic (BCC), face centered cubic (FCC), and hexagonal close-packed (HCP)-structure metals and alloys and in some ceramics as well; (2) examine the deformed microstructures (slip lines and twin boundaries) in different grains of metallic and ceramic specimens; and (3) study visually the deformed macrostructure (slip and twin bands) of metals and alloys. Some of the topics covered include: deformation behavior of materials, mechanisms of plastic deformation, slip bands, twin bands, ductile failure, intergranular fracture, shear failure, slip planes, crystal deformation, and dislocations in ceramics.

Rastani, Mansur↗

Low-temperature photoluminescence studies of chemical-vapor-deposition-grown 3C-SiC on Si

Low-temperature photoluminescence studies of 26 cubic SiC films, ranging in thickness from 600 A to 25 microns, grown by CVD on (100)Si are presented. It is suggested that the G band near 1.90-1.92 eV and its phonon side bands G1 and G2 are related to dislocations and extended defects. Formulas for the band-gap shift due to an axial stress have been obtained and applied to the CVD 3C-SiC/Si system. The results indicate that a 1-3-micron transition layer greatly reduces the interface misfit strain, and that biaxial stress in the SiC/Si system depresses the intensity of the no-phonon line.

Choyke, W. J.↗

Simplex GPS and InSAR Inversion Software

Changes in the shape of the Earth's surface can be routinely measured with precisions better than centimeters. Processes below the surface often drive these changes and as a result, investigators require models with inversion methods to characterize the sources. Simplex inverts any combination of GPS (global positioning system), UAVSAR (uninhabited aerial vehicle synthetic aperture radar), and InSAR (interferometric synthetic aperture radar) data simultaneously for elastic response from fault and fluid motions. It can be used to solve for multiple faults and parameters, all of which can be specified or allowed to vary. The software can be used to study long-term tectonic motions and the faults responsible for those motions, or can be used to invert for co-seismic slip from earthquakes. Solutions involving estimation of fault motion and changes in fluid reservoirs such as magma or water are possible. Any arbitrary number of faults or parameters can be considered. Simplex specifically solves for any of location, geometry, fault slip, and expansion/contraction of a single or multiple faults. It inverts GPS and InSAR data for elastic dislocations in a half-space. Slip parameters include strike slip, dip slip, and tensile dislocations. It includes a map interface for both setting up the models and viewing the results. Results, including faults, and observed, computed, and residual displacements, are output in text format, a map interface, and can be exported to KML. The software interfaces with the QuakeTables database allowing a user to select existing fault parameters or data. Simplex can be accessed through the QuakeSim portal graphical user interface or run from a UNIX command line.

Donnellan, Andrea↗

1000 to 1200 K time-dependent compressive deformation of single-crystalline and polycrystalline B2 Ni-40Al

The 1000-K and 1200-K time-dependent deformation of 100-line-oriented and non-100-line-oriented single crystals of Ni-40Al (made by a modified Bridgman technique) was examined over a large range of strain rates (from 0.1 to 10 to the -7th per sec). The results were compared with those for polycrystalline Ni-40Al made by hot pressing XD synthesized powder. The results from measurements of slow-plastic-strain-rate properties of the two materials show that single crystals offer no strength advantage over polycrystalline material. Both forms were found to deform via a dislocation climb mechanism.

Whittenberger, J. D.↗

Structure development in silicon sheet by shaped crystallization

Models are presented for the development of a parallel twinned structure of the 110 plane type and the 112 line type in silicon ribbons. The models are believed to be mutually compatible and operable. The first model relates the requirements for super-cooling during crystallization. The existence of reentrant angles associated with the twin structure is proposed to provide a rough interface to reduce super-cooling. The spacing of the twins is proposed to be limited by the geometrical relationship between the thermal gradient in the liquid and the dimensions of the twinned crystallization front. The second model relates the thermal stress configuration to detail dislocation reactions which would be expected to develop twins. While a specific dislocation mechanism cannot yet be defined, a number of alternatives are presented. All of these various dislocation mechanisms would result in the observed crystalline configuration and the choice among them is not critical.

Leipold, M. H.↗

Crystal-melt interface shape of Czochralski-grown large diameter germanium crystals

Crystal-melt interface shapes of 100 to 200 mm diameter 111-line Ge grown by the Czochralski technique have been examined using the method of fast withdrawal from the melt. Initially, the interface shape is convex, then transforms gradually into a sigmoidal shape, becomes nearly planar at about one third of the final crystal length, and finally assumes a concave profile with progressively increasing curvature. The nearly planar interface has a double-facet structure, with an annular facet at the edge of the crystal in addition to the central (111) facet. Formation of the annular facet is accompanied by a giant oscillation of the pull rate when the maximum average pull rate is exceeded. Such oscillation is detrimental to crystal quality, since it introduces a region of high dislocation density. An average pull rate maximum of 2 cm/h has been found to allow for a smooth growth of 200 mm diameter crystals. The origin of the pull rate perturbation is discussed in terms of an instantaneous change in the equilibrium shape of the meniscus.

Roth, M.↗

TEM Analyses of Itokawa Regolith Grains and Lunar Soil Grains to Directly Determine Space Weathering Rates on Airless Bodies

Samples returned from the moon and Asteroid Itokawa by NASA's Apollo Missions and JAXA's Hayabusa Mission, respectively, provide a unique record of their interaction with the space environment. Space weathering effects result from micrometeorite impact activity and interactions with the solar wind. While the effects of solar wind interactions, ion implantation and solar flare particle track accumulation, have been studied extensively, the rate at which these effects accumulate in samples on airless bodies has not been conclusively determined. Results of numerical modeling and experimental simulations do not converge with observations from natural samples. We measured track densities and rim thicknesses of three olivine grains from Itokawa and multiple olivine and anorthite grains from lunar soils of varying exposure ages. Samples were prepared for analysis using a Leica EM UC6 ultramicrotome and an FEI Quanta 3D dual beam focused ion beam scanning electron microscope (FIB-SEM). Transmission electron microscope (TEM) analyses were performed on the JEOL 2500SE 200kV field emission STEM. The solar wind damaged rims on lunar anorthite grains are amorphous, lack inclusions, and are compositionally similar to the host grain. The rim width increases as a smooth function of exposure age until it levels off at approximately 180 nm after approximately 20 My (Fig. 1). While solar wind ion damage can only accumulate while the grain is in a direct line of sight to the Sun, solar flare particles can penetrate to mm-depths. To assess whether the track density accurately predicts surface exposure, we measured the rim width and track density in olivine and anorthite from the surface of rock 64455, which was never buried and has a surface exposure age of 2 My based on isotopic measurements. The rim width from 64455 (60-70nm) plots within error of the well-defined trend for solar wind amorphized rims in Fig. 1. Measured solar flare track densities are accurately reflecting the surface exposure of the grains. Track densities correlate with the amorphous rim thicknesses. While the space-weathered rims of anorthite grains are amorphous, the space-weathered rims on both Itokawa and lunar olivine grains show solar wind damaged rims that are not amorphous. Instead, the rims are nanocrystalline with high dislocation densities and sparse inclusions of nanophase Fe metal. The rim thicknesses on the olivine grains also correlate with track density. The Itokawa olivine grains have track densities that indicate surface exposures of approximately 10(exp 5) years. Longer exposures (up to approximately 10(exp 7) years) do not amorphize the rims, as evidenced by lunar soil olivines with high track densities (approximately 10(exp 11) cm(exp -2)). From the combined data, shown in Fig. 1, it is clear that olivine is damaged (but not amorphized) more rapidly by the solar wind compared to anorthite. The olivine damaged rim forms quickly (in approximately 10(exp 6) y) and saturates at approximately 120nm with longer exposure time. The anorthite damaged rims form more slowly, amorphize, and grow thicker than the olivine rims. This is in agreement with numerical modeling data which predicts that solar wind damaged rims on anorthite will be thicker than olivine. However, the models predict that both olivine and anorthite rims will amorphize and reach equilibrium widths in less than 10(exp 3) y, in contrast to what is observed for natural samples. Laboratory irradiation experiments, which show rapid formation of fully amorphous and blistered surfaces from simulated solar wind exposures are also in contrast to observations of natural samples. These results suggest that there is a flux dependence on the type and extent of irradiation damage that develops in olivine. This flux dependence suggests that great caution be used in extrapolating between high-flux laboratory experiments and the natural case, as demonstrated by. We constrain the space weathering rate through analysis of returned samples. Provided that the track densities and the solar wind damaged rim widths exhibited by the Itokawa grains are typical of the fine-grained regions of Itokawa, then the space weathering rate is on the order of 10(exp 5) y. Space weathering effects in lunar soils saturate within a few My of exposure while those in Itokawa regolith grains formed in approximately 10(exp 5) y. Olivine and anorthite respond differently to solar wind irradiation. The space weathering effects in olivine are particularly difficult to reconcile with laboratory irradiation studies and numerical models. Additional measurements, experiments, and modeling are required to resolve the discrepancies among the observations and calculations involving solar wind amorphization of different minerals on airless bodies.

Berger, Eve L.↗

InGaAsP/InP laser development for single-mode, high-data-rate communications

Materials studies as well as general and specific device development were carried out in the InGaAsP system. A comparison was made of three standard methods of evaluating substrate quality by means of dislocation studies. A cause of reduced yield of good wafers, the pullover of melt from one bin to the next, has been analyzed. Difficulties with reproducible zinc acceptor doping have been traced to segregation of zinc in the In/Zn alloy used for the doping source. Using EBIC measurments, the pn junction was shown to drift in location depending on factors not always under control. An analysis of contact structures by SIMS showed that the depth to which the sintered Au/Zn contact penetrates into the structure is typically 0.13 microns, or well within the cap layer and out of the p-type cladding and thus not deleterious to laser prformance. The problem of single-mode laser development was investigated and it was shown to be related to the growth habit over four different possible substrate configurations. The fabrication of constricted double heterojunctions, mesa stripe buried heterostructures, and buried heterostructures was discussed, and measurements were presented on the device properties of single-mode buried heterostructure lasers. Results include single spectral line emission at 3 mW and a threshold current of 60 mA.

Ladany, I.↗

X-ray analysis of fatigue damage in copper

A Warren-Averbach x-ray line profile analysis was applied to, broadened x-ray diffraction peaks from copper deformed in fatigue. The copper specimens were fatigued by four point bending at various strain amplitudes, and measurements were made at various fractions of the total fatigue life. The analysis results in an estimation of 1) an average coherently diffracting domain size in a direction normal to the diffracting planes; and 2) a strain distribution function. The strain distribution function is in terms of the root mean square strain, <ϵ^(2)> where ϵ is averaged over a given distance at all points in the diffracting crystals. This rms strain is expressed as a function of averaging distance for a direction normal to the diffracting planes. The rms strains were found to be a function of the fatigue strain amplitude level, increasing with amplitude and reaching a maximum limiting value during the first 2% of the fatigue life. The strains were normally larger in the 4lO0 direction compared to the <111> direction and the absolute values were quite small. These results may be explained by assuming the dislocations are present in the form of dipoles because the lattice strain around a dipole is much less than around single dislocations. Conclusions arrived at in this analysis are in agreement with current theories of fatigue damage in metals. The result that maximum hardening is achieved during the initial few percent of the fatigue life is confirmed by many other investigators using entirely different analytical techniques. It is felt that the structure of the material is changing during this initial hardening stage to an eventual steady state characteristic of the testing conditions. A unique substructure is developed which thereafter persists, and the remainder of the fatigue test is taken up by crack propagation through this substructure until ultimate failure occurs by fracture. The formation of this steady state structure is dependent on the maximum fatigue strain amplitude and on the frequency and temperature of cycling for a particular material.

COPPER↗

The 1999 Hector Mine Earthquake, Southern California: Vector Near-Field Displacements from ERS InSAR

Two components of fault slip are uniquely determined from two line-of-sight (LOS) radar interferograms by assuming that the fault-normal component of displacement is zero. We use this approach with ascending and descending interferograms from the ERS satellites to estimate surface slip along the Hector Mine earthquake rupture. The LOS displacement is determined by visually counting fringes to within 1 km of the outboard ruptures. These LOS estimates and uncertainties are then transformed into strike- and dip-slip estimates and uncertainties; the transformation is singular for a N-S oriented fault and optimal for an E-W oriented fault. In contrast to our previous strike-slip estimates, which were based only on a descending interferogram, we now find good agreement with the geological measurements, except at the ends of the rupture. The ascending interferogram reveals significant west-sidedown dip-slip (approximately 1.0 m) which reduces the strike-slip estimates by 1 to 2 m, especially along the northern half of the rupture. A spike in the strike-slip displacement of 6 m is observed in central part of the rupture. This large offset is confirmed by subpixel cross correlation of features in the before and after amplitude images. In addition to strike slip and dip slip, we identify uplift and subsidence along the fault, related to the restraining and releasing bends in the fault trace, respectively. Our main conclusion is that at least two look directions are required for accurate estimates of surface slip even along a pure strike-slip fault. Models and results based only on a single look direction could have major errors. Our new estimates of strike slip and dip slip along the rupture provide a boundary condition for dislocation modeling. A simple model, which has uniform slip to a depth of 12 km, shows good agreement with the observed ascending and descending interferograms.

Sandwell, David T.↗

New AFM Techniques for Investigating Molecular Growth Mechanisms of Protein Crystals

Atomic Force Microscopy (AFM) has emerged as a powerful technique for investigating protein crystal growth. Earlier AFM studies were among the first to demonstrate that these crystals grew by dislocation and 2D nucleation growth mechanisms [1]. These investigations were restricted to the micron range where only surface features, such as dislocation hillocks and 2D islands are visible. Most AFM instruments can scan at higher resolutions and have the potential to resolve individual protein molecules at nanometer ranges. Such scans are essential for determining the molecular packing arrangements on crystal faces and for probing the growth process at the molecular level. However, at this resolution the AFM tip influences the image produced, with the resulting image being a convolution of the tip shape and the surface morphology [2]. In most studies this problem is resolved by deconvoluting the image to obtain the true surface morphology. Although deconvolution routines work reasonably well for simple one- dimensional shapes, for complex surfaces this approach does not produce accurate results. In this study we devised a new approach which takes advantage of the precise molecular order of crystal surfaces, combined with the knowledge of individual molecular shapes from the crystallographic data of the protein and the AFM tip shape. This information is used to construct expected theoretical AFM images by convoluting the tip shape with the constructed crystal surface shape for a given surface packing arrangement. By comparing the images from actual AFM scans with the constructed ones for different possible surface packing arrangements, the correct packing arrangement can be conclusively determined. This approach was used in this study to determine the correct one from two possible packing arrangements on (I 10) faces of tetragonal lysozyme crystals. Another novel AFM technique was also devised to measure the dimension of individual growth units of the crystal faces. Measuring these units was not attempted before and most studies have assumed that the growth unit consisted of individual protein molecules. The linescan mode of AFM instruments allows the crystal surface to be scanned along a single line. By scanning across a growth step an image showing the motion of the step is obtained. Normally such an image shows a straight line for continuous and constant step velocity. In this study by increasing the scan rate and by decreasing the step velocity (by decreasing the supersaturation), we were able to capture images of individual growth events, shown by jump discontinuities in the step line. By suitable integration of the image the growth unit dimension in the scanned direction can be obtained. Since multiple units can be involved in the growth process it is necessary to collect a statistically relevant sample before drawing conclusions about the growth mechanism. This technique was successfully employed to obtain the dimensions of growth units for the (110) face, showing that they consisted of various aggregates corresponding to the 43 helices in the crystal structure.

Li, Huayu↗