Secondary Ion Mass Spectrometry Bias on Isotope Ratios in Dolomite-Ankerite, Part II: δ 13 C Matrix Effects
Here, this study is Part II of a series that documents the development of a suite of calibration reference materials for in situ SIMS analysis of stable isotope ratios in Ca-Mg-Fe carbonates. Part I explored the effects of Fe 2+ substitution on SIMS δ18O bias measured from the dolomite–ankerite solid solution series [CaMg(CO3)2–CaFe(CO 3 ) 2 ], whereas this complementary work explores the compositional dependence of SIMS δ 13 C bias (calibrated range: Fe# = 0.004–0.789, where Fe# = molar Fe/(Mg+Fe)). Under routine operating conditions for carbonate δ 13 C analysis at WiscSIMS (CAMECA IMS 1280), the magnitude of instrumental bias increased exponentially by 2.5–5.5‰ (session-specific) with increasing Fe-content in the dolomite structure, but appeared insensitive to minor Mn substitution [< 2.6 mole % Mn/(Ca+Mg+Fe+Mn)]. The compositional dependence of bias (i.e., the matrix effect) was expressed using the Hill equation, yielding calibration residual values ≤ 0.3‰ relative to CRM NBS-19 for eleven carbonate reference materials (6-μm-diameter spot size measurements). Based on the spot-to-spot repeatability of a drift monitor material that ‘bracketed’ each set of ten sample-spot analyses, the analytical precision was ± 0.6–1.2‰ (2s, standard deviations). The analytical uncertainty for individual sample analyses was approximated by combining the precision and calibration residual values (propagated in quadrature), suggesting an uncertainty of ± 1.0–1.5‰ (2s).