Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “DIFFUSION WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Weldability and Impact Energy Properties of High-Hardness Armor Steel

In this study, the weldability of high-hardness armor steel by the gas metal arc welding method has been investigated. The study was aimed at determining the weakness points of manual welding compared to automated welding through microhardness testing, the cooling rate, tensile characteristics and nondestructive analysis. Detailed studies were performed for automated welding on the impact energy and microhardness in the fusion line, as the most sensitive zone of the armor steel weld joint. It was demonstrated that the selection of the preheating and interpass temperature is important in terms of the cooling rate and quantity of diffusible and retained hydrogen in the weld joint. The tensile strength was higher than 800 MPa. The width of the heat-affected zone did not exceed 15.9 mm, measured from the weld centerline, while the impact energy results were 74 and 39 J at 20 and – 40 °C, respectively.

36 MATERIALS SCIENCE↗

Characterization of the Interface of an Alloy 625 Overlay on Steels Using Nanoindentation

Industry standards require postweld heat treatment (PWHT) to reduce the heat-affected zone hardness of steels such as F22 (2.25Cr-1Mo) and AISI 8630 overlaid (clad) with Alloy 625 weld metal. PWHT results in carbon diffusion and accumulation at the interface between the steel and overlay. The accumulation of carbon in a planar solidification growth zone adjacent to the fusion boundary results in high hardness and the potential for hydrogen-assisted cracking. The planar growth zone (PGZ) is so narrow that normal Vickers hardness testing cannot fully reveal the hardness distribution in this zone. This study focused on the application of nanoindentation to characterize the hardness in the narrow microstructural regions adjacent to the fusion boundary. The development of nanohardness maps revealed that the PGZ is not necessarily the region that exhibits peak hardness after PWHT. The highest hardness values were associated with clusters of M{sub 7}C{sub 3} carbides in specific subregions in the PGZ and also in the partially-mixed zone adjacent to the fusion boundary or in steel “swirl” structures. It was also confirmed in this study that nanohardness has a linear correlation with Vickers hardness values. The results presented here provide new insight into the role of carbon diffusion during PWHT and its effect on interface embrittlement associated with Alloy 625 overlays on steel.

36 MATERIALS SCIENCE↗

Summary of Prior Work on Joining of Oxide Dispersion-Strengthened Alloys

There is a range of joining techniques available for use with ODS alloys, but care should be exercised in matching the technique to the final duty requirements of the joint. The goal for joining ODS alloys is a joint with no local disruption of the distribution of the oxide dispersion, and no significant change in the size and orientation of the alloy microstructure. Not surprisingly, the fusion welding processes typically employed with wrought alloys produce the least satisfactory results with ODS alloys, but some versions, such as fusion spot welding, and the laser and electron-beam welding technologies, have demonstrated potential for producing sound joints. Welds made using solid-state spot welding reportedly have exhibited parent metal properties. Thus, it is possible to employ processes that result in significant disruption of the alloy microstructure, as long as the processing parameters are adjustment to minimize the extent of or influence of the changes in the alloy microstructure. Selection among these joining approaches largely depends on the particular application and component configuration, and an understanding of the relationships among processing, alloy microstructure, and final properties is key. Recent developments have resulted in friction welding evolving to be a prime method for joining ODS sheet products, and variants of brazing/diffusion bonding have shown excellent promise for use with tubes and pipes. The techniques that come closest to the goal defined above involve solid-state diffusion bonding and, in particular, it has been found that secondary recrystallization of joints made by pulsed plasma-assisted diffusion can produce the desired, continuous, large alloy grain structure through the joint. Such joints have exhibited creep rupture failure at >82% of the load needed to fail the monolithic parent alloy at 1000 C.

36 MATERIALS SCIENCE↗

Interfacial microstructure and mechanical properties of rotary inertia friction welded dissimilar 422 martensitic stainless steel to 4140 low alloy steel joints

In this work, dissimilar rotary inertia friction welds between 422 martensitic stainless steel and 4140 martensitic low-alloy steel were made to fabricate prototype heavy-duty diesel engine pistons. The influence of the inertia friction welding process and post weld heat treatment (PWHT) temperature on the interfacial microstructure evolutions and corresponding effects on mechanical properties of the 422/4140 welds were evaluated in detail. Carbon diffused from the 4140 side to the 422 side during PWHT at 650 °C for 1.5 h, causing the formation of a hard carbide-rich layer on the 422 side, and a softer but discontinuous C-depleted layer the 4140 side. PWHT at 700 °C for 1.5 h greatly accelerated C diffusion across the interface relative to 650 °C, resulting in a thicker hard carbide-rich layer and a relatively thick and continuous layer of coarse C-depleted grains (ferrite) on the 4140 side. In addition, the PWHT temperature greatly influenced the tensile properties and fracture behavior of the welds, with the 650 °C PWHT-ed samples failing predominately in a ductile manner in the 4140 heat affected zone during tensile testing. Conversely, the 700 °C PWHT specimens exhibited a strength reduction compared with the 650 °C PWHT specimens because of additional coarsening of the interfacial ferrite layer and softening of the base materials during PWHT, with brittle fracture between the hard and soft layers the predominate failure mechanism. Based on the findings, a reduced PWHT temperature and/or time, minimizing the hardness differential of the base metals, and pre-heating the 422 steel prior to welding are the potential pathways to achieve a more optimal balance between desirable tempering and stress relief of the weld microstructure and undesirable C migration across the weld interface, and to reduce the strength mismatch across the weld.

36 MATERIALS SCIENCE↗

Corrosion behaviors of friction welded dissimilar aluminum alloys

Highlights: • Corrosion properties of friction welded dissimilar aluminum alloys seem to be governed by the anode part in the weld. • Intense corrosion near the interface has the limited region due to insufficient ionic transport. • Self-formation of a micro-galvanic cell is a main reason for the inferior corrosion performance. - Abstract: Corrosion behaviors of the friction welded dissimilar aluminum alloys were investigated to understand how galvanic effect plays a role in altering corrosion properties of the dissimilar weld. From the fact that the weld had the similar OCP value to that of AA2017, it can be inferred that the corrosion characteristics of the weld is under the control of the AA2017 part in the weld and as a result, only the AA2017 part in the weld had experienced severe corrosion, leaving AA6063 under cathodic protection. Intense corrosion occurring near the interface implies that the area near the interface is placed under the effect of galvanic corrosion and there was the effective distance where the galvanic effect exerts an impact due to the increase in the resistance of the electrolyte with the distance from the interface. The disappearance of Warburg diffusion plot in Nyquist plots for the weld seemed to be the breakdown of the passivation layer related to the formation of the micro-galvanic cell, which in turn presented the shrinkage in the capacitance response, indicating that charge reactions in the form of corrosion occurred.

36 MATERIALS SCIENCE↗

Characterization of Alloy 600 joints exposed to a high-temperature supercritical-carbon dioxide environment

Highlights: • Diffusion-bond showed similar corrosion and carburization behavior as parent matrix. • Diffusion-bond line migrated due to the Cr-depletion induced recrystallization. • Alloy 182 fusion-weld showed larger weight gains with outer Mn-rich oxides. • The presence of SiO{sub 2} in chromia suppressed carburization at the oxide/matrix interface. • Despite larger weight gains, Alloy 182 fusion-weld showed negligible tensile property changes. - Abstract: Two types of Alloy 600 joints, such as diffusion-bonded joint and Alloy 182 fusion-weld, were exposed to supercritical-CO{sub 2} environment at 550 and 650 °C (20 MPa) for 1000 h. The diffusion-bond region showed similar oxidation characteristics as parent Alloy 600, but the migration of diffusion bond line below oxide layer was observed due to the Cr-depletion induced recrystallization. For Alloy 182 fusion-weld, outer Mn-rich oxides (Mn{sub 3}O{sub 4} and MnCr{sub 2}O{sub 4}) and a small amount of inner SiO{sub 2} mixed with chromia were formed due to high Mn and Si contents. The presence of SiO{sub 2} in chromia suppressed carburization at the oxide/matrix interface, which resulted in the formation of an amorphous C layer between the outer Mn-rich oxide and inner Cr-rich oxide. For Alloy 182 fusion-weld, tensile property changes after exposure to supercritical-CO{sub 2} environment were negligible.

36 MATERIALS SCIENCE↗

Characterization of the interaction layer in diffusion couples U-7 wt.%Mo/Al 6061 alloy at 550 deg. C and 340 deg. C

Solid state reaction between U-7 wt.%Mo and Al 6061 alloys at 550 deg. C and 340 deg. C was characterized in chemical diffusion couples made by Friction Stir Welding. Results were obtained from optical and scanning electron microscopy, electron probe microanalysis and X-ray diffraction. At 550 deg. C the interaction layer in {gamma}U(Mo)/Al 6061 is formed by U(Al,Si){sub 3} phase but when {gamma}U(Mo) cellular decomposition occurs, UAl{sub 3} and Al{sub 43}Mo{sub 4}U{sub 6} also appear in the interaction layer. At 340 deg. C the use of X-ray diffraction with synchrotron radiation made it possible to analyze the interaction layer. It was found that it is only formed by U{sub 3}Si{sub 5} phase with its cell volume enlarged respect to the original one.

36 MATERIALS SCIENCE↗

Microstructures and mechanical properties of the welded AA5182/HC340LA joint by magnetic pulse welding

Highlights: • The magnetic pulse welding of 5× aluminum alloy with high strength steel is performed. • The microstructure evolution of welding interface under different parameters is investigated. • The intermediate layer is characterized by high-resolution transmission electron microscope and electron diffraction pattern. - Abstract: Magnetic pulse welding (MPW) is an innovative joining technology for dissimilar materials. The MPW with high joining qualities could be realized between high strength steel and 5× aluminum alloys. In this work, the MPW joints between aluminum alloy (AA 5182) sheet and high-strength low alloy steel (HC340LA) sheet were prepared under various discharge energies. The mechanical properties and microstructure observations were employed to evaluate the joint performance. Results showed that a lower discharge voltage tended to cause joints with poor quality. When the discharge energy increased, the failure position gradually changed from the weld zone to the weaker base metal (Al) during quasi-static tensile tests. In addition, the effect of discharge energies on microstructure evolution in the intermediate layer was revealed by high-resolution transmission electron microscopy (HRTEM) and scanning electron microscope (SEM). Atomic-scale diffusion was found to be the mainly welding mechanism of the Al/Fe joint. The intermetallic compound (IMC) FeAl{sub 2} and ultra-fine grains (UFG) were found in the intermediate layer under high discharge energy.

36 MATERIALS SCIENCE↗

Evaluation of intermetallic compound layer at aluminum/steel interface joined by friction stir scribe technology

Heat input and high strain rate deformation during friction stir welding of aluminum and steel resulted in the diffusion-based formation of a Fe x Al y intermetallic compound (IMC) layer. Compared with conventional friction stir welding tools, a friction stir scribe tool can reduce heat input significantly limiting the IMC layer thickness (~100–750 nm). Friction stir scribe joined lap joints fractured either through the welded interface or within the base aluminum alloy on the loading side, depending on IMC layer thickness during tensile lap shear testing. In addition, a modified effective heat of formation model predicted that Al 13 Fe 4 formed first at aluminum/steel interface and, during welding process, was substituted by Al 5 Fe 2 with local silicon enrichment, which was verified via microstructural characterization.

36 MATERIALS SCIENCE↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel

Highlights: • The fresh martensite formed in P92-sided CGHAZ during PWHT due to high Ni content. • Transition from type I to type IV cracking was observed with increasing temperature. • Creep damaged area changed depending on the dominant creep mechanism. • The transition value of Larson-Miller parameter would be within 25,063–26,168. - Abstract: Characterization of microstructures and creep fracture characteristics of dissimilar welds between Ni-based Inconel 740H superalloy and ferritic/martensitic P92 steel has been investigated. The welds were produced by shielded metal arc (SMA) welding process with the AWS A5.11 Class ENiCrFe-3 filler metal, commonly known as Inconel 182 superalloy. Postweld heat treatment (PWHT) at 760 °C for 4 h was conducted to temper the martensite in heat-affected zone (HAZ) of P92 and to form γ′ strengthener in Inconel 740H. The deposited Inconel 182 austenitic weld metal had a columnar microstructure, and grew epitaxially from the Inconel 740H base metal. The weld interface between P92 and weld metal was characterized by the discrete line with a minimal inter-diffusion, where the fresh untempered martensite was found to be formed during PWHT due to higher Ni contents diffused from Inconel 182 into P92. The P92 base metal and Inconel 182 weld metal displayed low hardness values (~240 Hv), and the sharp hardness increase was detected at coarse-grained HAZ of P92 while the hardness minimum occurred at the fine-grained HAZ (FGHAZ). Fracture location after creep was found to shift from the P92-sided fusion line to the FGHAZ of P92 with increasing creep temperature. The carbon migration from the P92 into the weld metal was not significant at lower creep temperature (600 °C), where the crack initiation at the P92-sided fusion line appeared to be related with a significant strain incompatibility across the fusion line. At both 650 °C and 700 °C where diffusion-controlled creep was more pronounced, the type IV cracking was observed. This may be attributed to the strain localization at the weak grain boundaries of FGHAZ due to the smaller grain size as well as the lack of grain boundary strengthening by carbides.

36 MATERIALS SCIENCE↗

Investigation of Interfacial Layer for Friction Stir Scribe Welded Aluminum to Steel Joints

Friction stir scribe (FSS) welding as a recent derivative of friction stir welding has successfully fabricated a linear joint between automotive Al and steel sheets. However, there is a lack of understanding on its bonding mechanism. In this paper, the microstructures and phases at the bonding interface of FSS welded Al to ultra-high strength steel joints were studied using scanning electron microscopy and transmission electron microscopy. Based on the microstructural analysis, it is found that both mechanical and chemical bonding occurred simultaneously, and the energy-dispersive X-ray spectroscopy revealed that a thin intermetallic compound (IMC) layer was formed at the interface. Owing to the varied material flow and heat generation, the IMC layer thickness gradually decreased from the advancing side to the retreating side, and two IMCs (i.e. Fe2Al5 and Fe4Al13) were confirmed in different weld regions using diffraction pattern (or 1D fast Fourier transform pattern). Also, a Fe/Al solid solution was noticed in the IMC layer, and several Al fringes were found in the Fe-rich side in the scribe stir zone.

friction stir scribe welding, interfacial layer, i↗

Facet-Dependent Cold Welding of Au Nanorods Revealed by Liquid Cell Transmission Electron Microscopy

Cold welding of metals at the nanoscale has been demonstrated to play a significant role in bottom-up manufacturing and self-healing processes of nanostructures and nanodevices. However, the welding mechanism at the nanoscale is not well understood. In this study, a comprehensive demonstration of the cold welding process of gold nanorods with different modes is presented through in situ liquid cell transmission electron microscopy. The experimental results and molecular dynamics simulations reveal that the nanorods are welded through the facet-dependent atomic surface diffusion and rearrangement along {100} facets. The density functional theory calculations indicate that the preferred coalescence of two {100} surfaces is thermodynamically favorable. Unlike the prevalent “oriented attachment” in the nanoparticle coalescence, the misalignment of nanorod orientations and local stresses can induce grain boundaries and stacking faults in the welded interface.

42 ENGINEERING↗

Microstructural Modeling of the α + β Phase in Ti-6Al-4V: A Diffusion-Based Approach

Complex heat treatment operations and advanced manufacturing processes such as laser or electron-beam welding will see the metallic workpiece experience a considerable range of temperatures and heating/cooling rates. These intrinsic conditions will have a significant bearing upon the microstructure of the material, and in turn upon the thermo-mechanical properties. In this work, a diffusion-based approach to model the growth and shrinkage of precipitates in the alpha + beta field of the common titanium alloy Ti-6Al-4V is established. Further, the numerical model is extended using a JMA-type approach to explore the dependency of the beta-transus temperature on extremely high heating rates, whereby dissolution alone is too slow to accurately describe the alpha to beta-phase transformation. Experimental heat treatments at rates of 5, 50, and 500 °C/s were performed, and metallographic analysis of the samples was used to validate the numerical modeling framework predictions for lamellar shrinkage, while data from the literature has been used to evaluate the numerical modeling framework for the growth of equiaxed microstructures. The agreement between measurements and numerical predictions was found to be good.

36 MATERIALS SCIENCE↗

Evaluation of Tungsten—Steel Solid-State Bonding: Options and the Role of CALPHAD to Screen Diffusion Bonding Interlayers

Critical aspects of innovative design in engineering disciplines like infrastructure, transportation, and medical applications require the joining of dissimilar materials. This study investigates the literature on solid-state bonding techniques, with a particular focus on diffusion bonding, as an effective method for establishing engineering bonds. Welding and brazing, while widely used, may pose challenges when joining materials with large differences in melting temperature and can lead to mechanical property degradation. In contrast, diffusion bonding offers a lower temperature process that relies on solid-state interactions to develop bond strength. The joining of tungsten and steel, especially for fusion reactors, presents a unique challenge due to the significant disparity in melting temperatures and the propensity to form brittle intermetallics. Here, diffusion characteristics of tungsten–steel interfaces are examined and the influence of bonding parameters on mechanical properties are investigated. Additionally, CALPHAD modeling is employed to explore joining parameters, thermal stability, and diffusion kinetics. The insights from this research can be extended to join numerous dissimilar materials for specific applications such as aerospace, automobile industry, power plants, etc., enabling advanced and robust design with high efficiency.

36 MATERIALS SCIENCE↗

Understanding radiation effects in friction stir welded MA956 using ion irradiation and a rate theory model

We report an outstanding challenge in the manufacturing and joining of oxide dispersion strengthened steels is retaining the nanofeatures in the alloy throughout the fabrication and welding process. MA956 was friction stir welded with two different sets of welding parameters, resulting in a medium and high heat input. After welding, 5 MeV Fe ++ ion irradiations were performed at doses ranging from 50 to 200 dpa in the temperature range of 400 to 500°C. Post-irradiation characterization was performed with scanning transmission electron microscopy and energy-dispersive x-ray spectroscopy to investigate the Y-Al-O dispersoids, voids, and dislocations. After welding, the dispersoid microstructure coarsened, resulting in fewer and larger dispersoids regardless of heat input. After irradiation, the dispersoid behavior in the welded material was sensitive to temperature, exhibiting growth behavior attributed to Ostwald coarsening at 500 °C but a mixture of nucleation and more muted growth at 400 and 450 °C, attributed to competing mechanisms of radiation-enhanced diffusion and Ostwald coarsening. Void swelling correlated to heat input; being more prevalent in the welded conditions occurring at lower doses and in higher values relative to the base material. The low values of swelling despite microstructure coarsening caused by welding demonstrate the excellent swelling resistance of MA956, even after welding with the highest swelling values of 0.5% noted in the stir zone high heat input condition at 450 °C, 200 dpa. The dislocation behavior was inconsistent: the strongest trend was that network density was higher for welded versus base material, and an increase in loop diameter with temperature was observed. A rate theory model based on the observed microstructure suggests at high temperature interstitial loss to sinks was more likely to be dominant compared to mutual annihilation via point defect recombination, because of an increase of the radiation diffusion coefficient with temperature regardless of initial welded microstructure.

36 MATERIALS SCIENCE↗