At least 55 records · Page 3

Large-area low-temperature ultrananocrystaline diamond (UNCD) films and integration with CMOS devices for monolithically integrated diamond MEMD/NEMS-CMOS systems.

Because of exceptional mechanical, chemical, and tribological properties, diamond has a great potential to be used as a material for the development of high-performance MEMS and NEMS such as resonators and switches compatible with harsh environments, which involve mechanical motion and intermittent contact. Integration of such MEMS/NEMS devices with complementary metal oxide semiconductor (CMOS) microelectronics will provide a unique platform for CMOS-driven commercial MEMS/NEMS. The main hurdle to achieve diamond-CMOS integration is the relatively high substrate temperatures (600-800 C) required for depositing conventional diamond thin films, which are well above the CMOS operating thermal budget (400 C). Additionally, a materials integration strategy has to be developed to enable diamond-CMOS integration. Ultrananocrystalline diamond (UNCD), a novel material developed in thin film form at Argonne, is currently the only microwave plasma chemical vapor deposition (MPCVD) grown diamond film that can be grown at 400 C, and still retain exceptional mechanical, chemical, and tribological properties comparable to that of single crystal diamond. We have developed a process based on MPCVD to synthesize UNCD films on up to 200 mm in diameter CMOS wafers, which will open new avenues for the fabrication of monolithically integrated CMOS-driven MEMS/NEMS based on UNCD. UNCD films were grown successfully on individual Si-based CMOS chips and on 200 mm CMOS wafers at 400 C in a MPCVD system, using Ar-rich/CH4 gas mixture. The CMOS devices on the wafers were characterized before and after UNCD deposition. All devices were performing to specifications with very small degradation after UNCD deposition and processing. A threshold voltage degradation in the range of 0.08-0.44V and transconductance degradation in the range of 1.5-9% were observed.

36 MATERIALS SCIENCE↗

Self-composite comprised of nanocrystalline diamond and a non-diamond component useful for thermoelectric applications

One provides nanocrystalline diamond material that comprises a plurality of substantially ordered diamond crystallites that are sized no larger than about 10 nanometers. One then disposes a non-diamond component within the nanocrystalline diamond material. By one approach this non-diamond component comprises an electrical conductor that is formed at the grain boundaries that separate the diamond crystallites from one another. The resultant nanowire is then able to exhibit a desired increase with respect to its ability to conduct electricity while also preserving the thermal conductivity behavior of the nanocrystalline diamond material.

36 MATERIALS SCIENCE↗

Self-composite comprised of nanocrystalline diamond and a non-diamond component useful for thermoelectric applications

One provides nanocrystalline diamond material that comprises a plurality of substantially ordered diamond crystallites that are sized no larger than about 10 nanometers. One then disposes a non-diamond component within the nanocrystalline diamond material. By one approach this non-diamond component comprises an electrical conductor that is formed at the grain boundaries that separate the diamond crystallites from one another. The resultant nanowire is then able to exhibit a desired increase with respect to its ability to conduct electricity while also preserving the thermal conductivity behavior of the nanocrystalline diamond material.

36 MATERIALS SCIENCE↗

The laser micro-machining system for diamond anvil cell experiments and general precision machining applications at the High Pressure Collaborative Access Team

We report we have designed and constructed a new system for micro-machining parts and sample assemblies used for diamond anvil cells and general user operations at the High Pressure Collaborative Access Team, sector 16 of the Advanced Photon Source. The new micro-machining system uses a pulsed laser of 400 ps pulse duration, ablating various materials without thermal melting, thus leaving a clean edge. With optics designed for a tight focus, the system can machine holes any size larger than 3 μm in diameter. Unlike a standard electrical discharge machining drill, the new laser system allows micro-machining of non-conductive materials such as: amorphous boron and silicon carbide gaskets, diamond, oxides, and other materials including organic materials such as polyimide films (i.e., Kapton). An important feature of the new system is the use of gas-tight or gas-flow environmental chambers which allow the laser micro-machining to be done in a controlled (e.g., inert gas) atmosphere to prevent oxidation and other chemical reactions in air sensitive materials. The gas-tight workpiece enclosure is also useful for machining materials with known health risks (e.g., beryllium). Specialized control software with a graphical interface enables micro-machining of custom 2D and 3D shapes. The laser-machining system was designed in a Class 1 laser enclosure, i.e., it includes laser safety interlocks and computer controls and allows for routine operation. Though initially designed mainly for machining of the diamond anvil cell gaskets, the laser-machining system has since found many other micro-machining applications, several of which are presented here.

47 OTHER INSTRUMENTATION↗

Diamond synthesis at atmospheric pressure by microwave capillary plasma chemical vapor deposition

Polycrystalline diamond has been synthesized on silicon substrates at atmospheric pressure, using a microwave capillary plasma chemical vapor deposition technique. The CH{sub 4}/Ar plasma was generated inside of quartz capillary tubes using 2.45 GHz microwave excitation without adding H{sub 2} into the deposition gas chemistry. Electronically excited species of CN, C{sub 2}, Ar, N{sub 2}, CH, H{sub β}, and H{sub α} were observed in the emission spectra. Raman measurements of deposited material indicate the formation of well-crystallized diamond, as evidenced by the sharp T{sub 2g} phonon at 1333 cm{sup −1} peak relative to the Raman features of graphitic carbon. Field emission scanning electron microscopy images reveal that, depending on the growth conditions, the carbon microstructures of grown films exhibit “coral” and “cauliflower-like” morphologies or well-facetted diamond crystals with grain sizes ranging from 100 nm to 10 μm.

36 MATERIALS SCIENCE↗

Growth and Isolation of Large Area Boron-Doped Nanocrystalline Diamond Sheets: A Route toward Diamond-on-Graphene Heterojunction

Many material device applications would benefit from thin diamond coatings, but current growth techniques, such as chemical vapor deposition (CVD) or atomic layer deposition require high substrate and gas-phase temperatures that would destroy the device being coated. The development of freestanding, thin boron-doped diamond nanosheets grown on tantalum foil substrates via microwave plasma-assisted CVD is reported. These diamond sheets (measuring up to 4 × 5 mm in planar area, and 300–600 nm in thickness) are removed from the substrate using mechanical exfoliation and then transferred to other substrates, including Si/SiO 2 and graphene. The electronic properties of the resulting diamond nanosheets and their dependence on the free-standing growth, the mechanical exfoliation and transfer processes, and ultimately on their composition are characterized. To support this, a prototypical diamond nanosheet–graphene field effect transistor-like (DNGfet) device is developed and its electronic transport properties are studied as a function of temperature. The resulting DNGfet device exhibits thermally activated transport (thermionic conductance) above 50 K. Below 50 K a transition to variable range hopping is observed. Finally, these findings demonstrate the first step towards a low-temperature diamond-based transistor.

36 MATERIALS SCIENCE↗

High quality x-ray absorption spectroscopy measurements with long energy range at high pressure using diamond anvil cell

We describe an approach for acquiring high quality x-ray absorption fine structure (XAFS) spectroscopy spectra with wide energy range at high pressure using diamond anvil cell (DAC). Overcoming the serious interference of diamond Bragg peaks is essential for combining XAFS and DAC techniques in high pressure research, yet an effective method to obtain accurate XAFS spectrum free from DAC induced glitches has been lacking. It was found that these glitches, whose energy positions are very sensitive to the relative orientation between DAC and incident x-ray beam, can be effectively eliminated using an iterative algorithm based on repeated measurements over a small angular range of DAC orientation, e.g., within {+-}3{sup o} relative to the x-ray beam direction. Demonstration XAFS spectra are reported for rutile-type GeO{sub 2} recorded by traditional ambient pressure and high pressure DAC methods, showing similar quality at 440 eV above the absorption edge. Accurate XAFS spectra of GeO{sub 2} glass were obtained at high pressure up to 53 GPa, providing important insight into the structural polymorphism of GeO{sub 2} glass at high pressure. This method is expected be applicable for in situ XAFS measurements using a diamond anvil cell up to ultrahigh pressures.

36 MATERIALS SCIENCE↗

Polymorphism and second harmonic generation in a novel diamond-like semiconductor: Li{sub 2}MnSnS{sub 4}

High-temperature, solid-state synthesis in the Li{sub 2}MnSnS{sub 4} system led to the discovery of two new polymorphic compounds that were analyzed using single crystal X-ray diffraction. The α-polymorph crystallizes in Pna2{sub 1} with the lithium cobalt (II) silicate, Li{sub 2}CoSiO{sub 4}, structure type, where Z=4, R1=0.0349 and wR2=0.0514 for all data. The β-polymorph possesses the wurtz-kesterite structure type, crystallizing in Pn with Z=2, R1=0.0423, and wR2=0.0901 for all data. Rietveld refinement of synchrotron X-ray powder diffraction was utilized to quantify the phase fractions of the polymorphs in the reaction products. The α/β-Li{sub 2}MnSnS{sub 4} mixture exhibits an absorption edge of ∼2.6–3.0 eV, a wide region of optical transparency in the mid- to far-IR, and moderate SHG activity over the fundamental range of 1.1–2.1 μm. Calculations using density functional theory indicate that the ground state energies and electronic structures for α- and β-Li{sub 2}MnSnS{sub 4}, as well as the hypothetical polymorph, γ-Li{sub 2}MnSnS{sub 4} with the wurtz-stannite structure type, are highly similar. - Graphical abstract: Two polymorphs, α- and β-Li{sub 2}MnSnS{sub 4}, have been discovered using single crystal X-ray diffraction. Rietveld refinement of synchrotron X-ray powder diffraction data indicates the presence of both polymorphs in the samples that were analyzed. - Highlights: • Li{sub 2}MnSnS{sub 4} exists as two polymorphs crystallizing in the Pna2{sub 1} and Pn space groups. • The α- and β-Li{sub 2}MnSnS{sub 4} mixture exhibits a moderate SHG response over a broad range. • The α- and β-Li{sub 2}MnSnS{sub 4} mixture exhibits an optical absorption edge of ∼2.6–3.0 eV. • Synchrotron powder diffraction data are necessary to distinguish α- and β-Li{sub 2}MnSnS{sub 4.} • Electronic structure calculations show similar total energies for α- and β-Li{sub 2}MnSnS{sub 4}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Extreme Metastability of Diamond and its Transformation to the BC8 Post-Diamond Phase of Carbon

Diamond possesses exceptional physical properties due to its remarkably strong carbon–carbon bonding, leading to significant resilience to structural transformations at very high pressures and temperatures. Despite several experimental attempts, synthesis and recovery of the theoretically predicted post-diamond BC8 phase remains elusive. Through quantum-accurate multimillion atom molecular dynamics (MD) simulations, we have uncovered the extreme metastability of diamond at very high pressures, significantly exceeding its range of thermodynamic stability. We predict the post-diamond BC8 phase to be experimentally accessible only within a narrow high pressure–temperature region of the carbon phase diagram. The diamond to BC8 transformation proceeds through premelting followed by BC8 nucleation and growth in the metastable carbon liquid. Here we propose a double-shock compression pathway for BC8 synthesis, which is currently being explored in experiments at the National Ignition Facility.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Controlling the work function of a diamond-like carbon surface by fluorination with XeF{sub 2}

Thin diamond-like carbon films were subjected to fluorination with gaseous XeF{sub 2} under ultrahigh vacuum conditions in order to increase the work function of the diamond-like carbon surface. Changes in the work function and surface composition were monitored with UV photoemission spectroscopy and x-ray photoemission spectroscopy, respectively. Successive XeF{sub 2} exposures raised the work function by as much as 1.55 eV. Surprisingly, approximately half of the increase in the work function occurred while the coverage of fluorine remained below 0.02 monolayers (ML). This suggests that initial doses of XeF{sub 2} remove extrinsic adsorbates from the diamond-like carbon film and that fluorine desorbs with the reaction products. Increasing the exposure of the diamond-like carbon to XeF{sub 2} leads to the expected covalent fluorination of the surface, which saturates at fluorine coverages of 6 F atoms/nm{sup 2} ({approx}0.3 ML). Annealing of the diamond-like carbon to temperatures above 850 K was required to reduce the surface fluorine concentration to undetectable levels. This did not, however, cause the work function to return to its original, prefluorination value.

36 MATERIALS SCIENCE↗

Influence of diamond surface termination on thermal boundary conductance between Al and diamond

The effect of diamond surface treatment on the Thermal Boundary Conductance (TBC) between Al and diamond is investigated. The treatments consist in either of the following: exposition to a plasma of pure Ar, Ar:H and Ar:O, and HNO{sub 3}:H{sub 2}SO{sub 4} acid dip for various times. The surface of diamond after treatment is analyzed by X-ray Photoelectron Spectroscopy, revealing hydrogen termination for the as-received and Ar:H plasma treated samples, pure sp{sup 2} termination for Ar treated ones and oxygen (keton-like) termination for the other treatments. At ambient, all the specific treatments improve the TBC between Al and diamond from 23 {+-} 2 MW m{sup -2} K{sup -1} for the as-received to 65 {+-} 5, 125 {+-} 20, 150 {+-} 20, 180 {+-} 20 MW m{sup -2} K{sup -1} for the ones treated by Ar:H plasma, acid, pure Ar plasma, and Ar:O plasma with an evaporated Al layer on top, respectively. The effect of these treatments on temperature dependence are also observed and compared with the most common models available in the literature as well as experimental values in the same system. The results obtained show that the values measured for an Ar:O plasma treated diamond with Al sputtered on top stay consistently higher than the values existing in the literature over a temperature range from 78 to 290 K, probably due a lower sample surface roughness. Around ambient, the TBC values measured lay close to or even somewhat above the radiation limit, suggesting that inelastic or electronic processes may influence the transfer of heat at this metal/dielectric interface.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of the Surface Modification of Synthetic Diamond with Nickel or Tungsten on the Properties of Copper–Diamond Composites

Tungsten- and nickel-containing coatings have been produced on the surface of synthetic diamond crystals by rotary chemical vapor deposition (RCVD) using tungsten hexacarbonyl, W(CO){sub 6}, and nickelocene, Ni(C{sub 5}H{sub 5}){sub 2}, as gaseous precursors. The thickness, composition, and morphology of the coatings have been shown to depend on the RCVD process duration and reactant concentrations in the vapor phase. The synthetic diamond microcrystals with tungsten- and nickel-containing coatings have been used to produce copper–diamond heat-conducting composites. Powder mixtures containing 50 vol % diamond with a particle size of 50, 100, or 200 μm have been consolidated by spark plasma sintering or hot pressing. It has been shown that the highest relative density (97%) and thermal conductivity (340 W/(m K)) are offered by the composites produced by spark plasma sintering using tungsten carbide-coated 50-μm diamond crystals.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗