Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Cold sintering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Microstructural features underpinning the mechanical behavior of powder metallurgy Cr-based alloys

Refractory materials such as Cr-based alloys offer the potential of enhanced elevated temperature performance but have been limited by their poor formability. However, powder metallurgy has been shown to be a viable pathway to fabricate these alloys. Nanophase separation sintering (NPSS) in particular has been used in the literature to accelerate the densification of powder metallurgy Cr- and W-based alloys. Here, we explore microstructure evolution during NPSS in a binary Cr 85 Ni 15 alloy consolidated via (i) cold pressing & pressureless sintering and (ii) hot isostatic pressing followed by hot extrusion & hot upsetting, and the role of these different processing routes on resulting material properties. The alloy lacked room temperature tensile ductility regardless of consolidation process, with multi-length scale characterization, including scanning electron microscopy, transmission electron microscopy, atom probe tomography, X-ray diffraction, and uniaxial tensile testing, revealing that brittleness was due to intrinsically poor Cr grain boundary cohesion. Tensile testing conducted at 760 °C showed marked strength reduction for the extruded & upset (94 %) condition compared to the pressed & sintered (18 %). The formation of orthorhombic CrNi 2 intermetallics functioned as precipitate strengtheners and prevented elevated temperature softening in the pressed and sintered condition. The findings offer foundational insights into aiding the future development of Cr-based alloys.

36 MATERIALS SCIENCE↗

High-performance and flexible thermoelectric films by screen printing solution-processed nanoplate crystals

Screen printing allows for direct conversion of thermoelectric nanocrystals into flexible energy harvesters and coolers. However, obtaining flexible thermoelectric materials with high figure of merit ZT through printing is an exacting challenge due to the difficulties to synthesize high-performance thermoelectric inks and the poor density and electrical conductivity of the printed films. Here, we demonstrate high-performance flexible films and devices by screen printing bismuth telluride based nanocrystal inks synthesized using a microwave-stimulated wet-chemical method. Thermoelectric films of several tens of microns thickness were screen printed onto a flexible polyimide substrate followed by cold compaction and sintering. The n-type films demonstrate a peak ZT of 0.43 along with superior flexibility, which is among the highest reported ZT values in flexible thermoelectric materials. A flexible thermoelectric device fabricated using the printed films produces a high power density of 4.1 mW/cm 2 with 60°C temperature difference between the hot side and cold side. In conclusion, the highly scalable and low cost process to fabricate flexible thermoelectric materials and devices demonstrated here opens up many opportunities to transform thermoelectric energy harvesting and cooling applications.

30 DIRECT ENERGY CONVERSION↗

Titanium Sheet Fabricated from Powder for Industrial Applications

In collaboration with Ametek and Commonwealth Scientific and Industrial Research Organization (CSIRO), Oak Ridge National Laboratory has evaluated three different methods for converting titanium hydride-dehydride (HDH) powder into thin gauge titanium sheet from a roll compacted preform. Methodologies include sintering, followed by cold rolling and annealing; direct hot rolling of the roll-compacted sheet; and hot rolling of multiple layers of roll compacted sheet that are encapsulated in a steel can. All three methods have demonstrated fully consolidated sheet, and each process route has the ability to produce sheet that meets ASTM B265 specifications. However, not every method currently provides sheet that can be highly formed without tearing. The degree of sintering between powder particles, post processing density, and the particle to particle boundary layer where compositional variations may exist, have a significant effect on the ability to form the sheet into useful components. Uniaxial tensile test results, compositional analysis, bend testing, and biaxial testing of the titanium sheet produced from hydride-dehydride powder will be discussed. Multiple methods of fabrication and the resulting properties can then be assessed to determine the most economical means of making components for industrial applications.

36 MATERIALS SCIENCE↗

Mechanical and electrical properties of low temperature phase MnBi

Low temperature phase (LTP) manganese bismuth (MnBi) is a promising rare-earth-free permanent magnet material due to its high intrinsic coercivity and large positive temperature coefficient. While scientists are making progress on fabricating bulk MnBi magnets, engineers have begun considering MnBi magnets for motor applications. Physical properties other than magnetic ones could significantly affect motor design. Here, we report results of our investigation on the mechanical and electrical properties of bulk LTP MnBi and their temperature dependence. A MnBi ingot was prepared using an arc melting technique and subsequently underwent grinding, sieving, heat treatment, and cryomilling. The resultant powders with a particle size of ∼5 μm were magnetically aligned, cold pressed, and sintered at a predefined temperature. Micro-hardness testing was performed on a part of original ingot and we found that the hardness of MnBi was 109 ± 15 HV. The sintered magnets were subjected to compressive testing at different temperatures and it was observed that a sintered MnBi magnet fractured when the compressive stress exceeded 193 MPa at room temperature. Impedance spectra were obtained using electrochemical impedance spectroscopy at various temperatures and we found that the electrical resistance of MnBi at room temperature was about 6.85 μΩ m.

Jiang, Xiujuan↗

Compaction and Sintering of Mo Powders

To support the development of Mo-99 production by NorthStar Medical Technologies, LLC, Mo metal powders were evaluated for compaction and sintering characteristics as they relate to Mo-100 accelerator target disk fabrication. Powders having a natural isotope distribution and enriched Mo-100 powder were examined. Various powder characteristics are shown to have an effect on both the compaction and sintering behavior. Natural Mo powders could be cold pressed directly to >90% density. All of the powders, including the Mo-100 samples, could be sintered after cold pressing to >90% density. As an example, a compacted Mo-100 disk reached 89.7% density (9.52 g/cm3) after sintering at 1000 C for 1 hr. in flowing Ar/4%H2. Higher sintering temperatures were required for other powder samples. The relationships between processing conditions and the resulting densities of consolidated Mo disks will be presented.

Nunn, Stephen D↗

Preparation of amine-impregnated silica foams using agar as the gelling agent

In this work we successfully prepared amine-impregnated gel-cast silica foams using agar and atmospheric air as the gelling agent and heat treatment atmosphere, respectively. The concentration of 3,6-anhydrogalactose in agar was evaluated by ultraviolet–visible spectroscopy (UV–Vis). The obtained foams were examined by Fourier transform infrared spectroscopy (FTIR), thermogravimetric analysis (TG) coupled to mass spectrometry (TG-MS), scanning electron microscopy (SEM), X-ray microtomography (micro-CT), and Archimedes method. The cold crushing strength of the materials prepared in this work was assessed using a mechanical testing stage available in the micro-CT system. The obtained foams exhibited a highly interconnected pore network, with an expressive presence of open pores. Samples heat-treated at 1300 °C for 2 h showed both an expressive porosity (≈ 77%) and a significant cold crushing strength (≈ 1.4 MPa). It was observed that the calcination of the prepared materials at 1200 °C for times as long as 16 h may lead to the rupture of pore walls. FTIR and TG-MS revealed that amine groups were properly incorporated into the foams structure. - Highlights: •Successful preparation of amine-impregnated gel-cast silica foams •Agar used as the gelling agent •Samples with expressive porosity and cold crushing strength •Sintering times as long as 16 h led to the rupture of the pore network.

36 MATERIALS SCIENCE↗

Al{sub 2}TiO{sub 5}-Al{sub 2}O{sub 3}-TiO{sub 2} nanocomposite: Structure, mechanical property and bioactivity studies

Novel biomaterials are of prime importance in tissue engineering. Here, we developed novel nanostructured Al{sub 2}TiO{sub 5}-Al{sub 2}O{sub 3}-TiO{sub 2} composite as a biomaterial for bone repair. Initially, nanocrystalline Al{sub 2}O{sub 3}-TiO{sub 2} composite powder was synthesized by a sol-gel process. The powder was cold compacted and sintered at 1300-1500 {sup o}C to develop nanostructured Al{sub 2}TiO{sub 5}-Al{sub 2}O{sub 3}-TiO{sub 2} composite. Nano features were retained in the sintered structures while the grains showed irregular morphology. The grain-growth and microcracking were prominent at higher sintering temperatures. X-ray diffraction peak intensity of {beta}-Al{sub 2}TiO{sub 5} increased with increasing temperature. {beta}-Al{sub 2}TiO{sub 5} content increased from 91.67% at 1300 {sup o}C to 98.83% at 1500 {sup o}C, according to Rietveld refinement. The density of {beta}-Al{sub 2}TiO{sub 5} sintered at 1300 {sup o}C, 1400 {sup o}C and 1500 {sup o}C were computed to be 3.668 g cm{sup -3}, 3.685 g cm{sup -3} and 3.664 g cm{sup -3}, respectively. Nanocrystalline grains enhanced the flexural strength. The highest flexural strength of 43.2 MPa was achieved. Bioactivity and biomechanical properties were assessed in simulated body fluid. Electron microscopy confirmed the formation of apatite crystals on the surface of the nanocomposite. Spectroscopic analysis established the presence of Ca and P ions in the crystals. Results throw light on biocompatibility and bioactivity of {beta}-Al{sub 2}TiO{sub 5} phase, which has not been reported previously.

36 MATERIALS SCIENCE↗

Magnetic and magneto elastic properties of cobalt ferrite ceramic compacted through cold isostatic pressing

Nano crystalline CoFe{sub 2}O{sub 4} powder was prepared by combustion synthesis method. As synthesized powder was calcined at an appropriate condition to remove the impurities and to promote phase formation. Phase pure CoFe{sub 2}O{sub 4} powder was pressed into cylindrical rod at an applied pressure of 200 MPa using a cold isostatic pressing. Sintering of the green compact at 1350°c for 12 hrs resulted in sintered cylindrical rod with ~85% of the theoretical density. Single phase cubic spinel structure was observed in the powder x-ray diffraction pattern of the sintered pellet. Scanning electron micrographs (SEM) of the as sintered pellet revealed the microstructure to be composed of ferrite grains of average size ~4 µm. Saturation magnetization of 72 emu/g and coercivity of 355 Oe were observed for cobalt ferrite sample. The magnetostriction was measured on a circular disc (12 mm diameter and 12 mm length) with the strain gauge (350 Ω) mounted on the flat surface of the circular disc. Magnetostriciton of 180 ppm and strain derivative of 1 × 10{sup −9} m/A were observed for the sintered CoFe{sub 2}O{sub 4} sample.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Porous Titanium Parts Fabricated by Sintering of TiH{sub 2} and Ti Powder Mixtures

A new simple powder metallurgy process by sintering TiH{sub 2} powders was used to manufacture porous Ti components. The effects of the processing parameters (pressure of cold isostatic pressing and sintering temperature) and the TiH{sub 2}/Ti ratio in the powder mixtures on the impurities, the linear shrinkage and the pore properties (including overall and open porosities) were comprehensively determined. The addition of TiH{sub 2} as a reactant has been found beneficial for the synthesis of porous Ti components. The formation mechanisms of pores were demonstrated based on the dehydrogenation process of TiH{sub 2} during sintering, resulting in highest reactivity due to the “in statu nascendi” generation of the metal. In addition, the hardness and corrosion resistance of all the sintered samples were evaluated, related to the overall and open porosities. As a result, an optimal composition of Ti-40 wt.% TiH{sub 2} was defined, as its maximum open porosity was about 23%.

36 MATERIALS SCIENCE↗

Synthesis and Characterization of Natural Nano-hydroxyapatite Derived from Turkey Femur-Bone Waste

Hydroxyapatite (HAp) is a bioactive and vital material which has found many applications in the biomedical and clinical fields. This bio-ceramic powder can be synthesized via different bio-waste materials. In this study, the production of natural nanohydroxyapatite was produced through calcination of untreated turkey femur-bone waste powder at 850 °C followed by ball milling the powder. The obtained powder was characterized using X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR) analysis. The morphology, size, and elemental composition of obtained turkey hydroxyapatite (THA) particles were investigated by scanning electron microcopy (SEM), transmission electron microcopy (TEM), and energy dispersive spectroscopy (EDS) analysis, in which the average particle size of ball milled THA was found to be about 85 nm with a Ca/P ratio of 1.63. The powder was then cold pressed and later sintered at 850, 950, 1050, and 1150 °C to evaluate its mechanical properties in terms of compressive strength and hardness. The results revealed that the strength and hardness of the samples increased by increasing the sintering temperature up to 1150 °C. Finally, the maximum values of hardness and compressive strength of the sintered THA were obtained at 1150 °C (37.44 MPa and 3.2 GPa, respectively).

60 APPLIED LIFE SCIENCES↗

Raspberry colloid-templated approach for the synthesis of palladium-based oxidation catalysts with enhanced hydrothermal stability and low-temperature activity

It is becoming increasingly urgent to develop and utilize novel, more efficient and stable materials for mobile and stationary emission control applications as the deleterious consequences of anthropogenic air pollution are becoming more evident and pressing. Tightening regulations, particularly related to automotive exhaust treatment, together with continued improvements in engine design, that result in lowering the engine operating temperatures and inadvertently lead to the release of an overwhelming proportion of pollutants during the cold start, present new challenges for materials design, specifically for oxidation catalysts. In particular, improvements in the low-temperature activity while maintaining catalyst stability at high temperatures are required from the next-generation catalyst. Typical catalysts for removal of pollutants from automotive exhaust streams incorporate platinum group metals (PGMs). They tend to be inefficient at low temperatures (below 250 °C), thus accounting for the cold start problem, yet sinter and lose their activity at high temperatures that are frequently encountered during catalyst operation. High PGM loadings are often employed to compensate for catalyst inefficiencies and fast degradation, ultimately resulting in high-cost catalytic converters. Here, we have developed a new approach for the design and formation of catalytic materials that allows for both significantly more efficient PGM incorporation and improved overall catalyst performance at reduced PGM loadings. The method provides control over the composition and geometry of the support through self-assembly of sacrificial composite template — “raspberry” polymeric colloids decorated with catalytic particles — accompanied by infiltration with metal-oxide precursor and subsequent removal of the colloids. This method simultaneously structures the porous network and organizes the catalytic particles within it. Uniquely, the resulting catalytic particles are partially embedded in the support matrix and partially exposed to the pore interior, producing catalytic sites that are both stable and accessible. Herein, the feasibility of this novel and versatile approach for automotive catalytic conversion is demonstrated: the studies include testing alumina-based raspberry-colloid-templated (RCT) catalysts containing Pd nanoparticles (RCT Pd/Al2O3) for oxidation of propane and carbon monoxide under simulated diesel exhaust conditions and hydrothermal aging at 800 °C for 50 h in the simulated stream. The RCT Pd/Al2O3 catalysts exhibit exceptional activity toward CO oxidation, reduced reaction onset temperature, and high stability to elevated temperatures (demonstrated through prolonged exposure to temperatures up to 950 °C) and reactive gas streams, without migration, sintering or loss of the precious metal NPs. Notably, the novel catalyst shows the same or slightly better performance than the commercial catalysts even when the PGM load is reduced by ~80 % compared to the commercial counterparts. These results provide confidence for the utilization of the RCT approach for the fabrication of robust nanostructured catalysts for next-generation, energy-efficient catalytic converters with improved performance at low and high temperatures and reduced costs. The RCT methodology is, in addition, highly generalizable, and can thus be applied for the design of a wide range of catalytic systems in the automotive sector and beyond.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanically alloyed Mo-Si-B alloys with a continuous a-Mo matrix and improved mechanical properties

Mechanical alloying (MA) followed by cold isostatic pressing (CIPing), sintering and hot isostatic pressing (HIPing) was used to prepare Mo-base silicide alloys consisting of a Mo(Si) solid solution and the intermetallic phases Mo{sub 3}Si and Mo{sub 5}SiB{sub 2}. The microstructural development during milling of both binary Mo-Si and Mo-B and ternary Mo-Si-B powder mixtures was evaluated. While obtaining a supersaturated solid solution requires rather long milling times, domain size (which correlates with the grain size) is reduced to below 100 {angstrom} after about 10 h of milling. After heat treatment and consolidation the microstructure reveals a continuous {alpha}-Mo matrix with embedded, uniformly distributed intermetallic particles. The establishment of such a microstructure is beneficial for the mechanical properties since, as compared to a discontinuous {alpha}-Mo matrix, it decreases the brittle-to-ductile transition temperature (BDTT) by about 150 K.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Consolidation Process in Near Net Shape Manufacturing of Armstrong CP-Ti/Ti-6Al-4V Powders

This paper summarizes our recent efforts to develop the manufacturing technologies of consolidated net-shape components by using new low-cost commercially pure titanium (CP-Ti) and Ti-6Al-4V alloy powders made by the Armstrong process. Fabrication processes of net shape/ near net shape components, such as uniaxial die-pressing, cold isostatic pressing (CIP), sintering, roll compaction and stamping, have been evaluated. The press-and-sinter processing of the powders were systematically investigated in terms of theoretical density and microstructure as a function of time, pressure, and temperature. Up to 96.4% theoretical density has been achieved with the press-and-sinter technology. Tensile properties of the consolidated samples exhibit good ductility as well as equivalent yield/ultimate tensile strengths to those of fully consolidate materials, even with the presence of a certain amount of porosity. A consolidation model is also under development to interpret the powder deformation during processing. Net shape components made of the Armstrong powder can successfully be fabricated with clearer surface details by using press-and-sinter processing.

36 MATERIALS SCIENCE↗

Tunning of microstructure and thermoelectric properties of Ca{sub 3}Co{sub 4}O{sub 9} ceramics by high-magnetic-field sintering

The structural, magnetic, electrical, and thermal transport properties of Ca{sub 3}Co{sub 4}O{sub 9} ceramics sintered under high magnetic field were investigated. Crystal grain texturing and densification were achieved through cold-pressing and high-magnetic-field sintering techniques. The c-axis of the layered crystal grain was partly oriented along the c-axis of the pressed samples via a cold-pressing technique, and the degree of orientation was further increased while applying the magnetic field in the sample sintering progress. The easy magnetization axis of Ca{sub 3}Co{sub 4}O{sub 9} polycrystalline ceramics was found to be the c-axis. The room-temperature resistivity along the ab-plane of the sample sintered under 8 T magnetic field was about 30% smaller than that of the sample sintered without magnetic field, and the Seebeck coefficient of the former reached 177.7 {mu}V/K at the room temperature, which is about 50% larger than that of the latter. Consequently, for the sample sintered at 8 T magnetic field, the power factor along the ab-plane was enhanced by about 1.8 times compared to the sample without magnetic field sintering. The obtained result is suggested to originate from the variations of the carrier mobility and spin-orbital degeneracy due to high-magnetic-field sintering in the progress of the sample preparation.

36 MATERIALS SCIENCE↗

In situ formation of sintered cordierite–mullite nano–micro composites by utilizing of waste silica fume

Highlights: ► We succeeded to obtain in situ formed sintered cordierite–mullite nano–macro composites from waste and pure materials at 1400 °C. ► Their sinterability was greatly dependent on both firing temperature and composition. ► XRD patterns showed that the optimum temperature required for formation of sintered cordierite–mullite nano–macro composites was achieved at 1400 °C. ► The batch containing 70 wt.% cordierite and 30 wt.% mullite exhibited the best properties. ► Microstructures of the densified composites were composed of nano–macro cordierite–mullite structures. -- Abstract: This study aims at in situ formation of sintered cordierite–mullite nano–macro composites having high technological properties using waste silica fume, calcined ball clay, calcined alumina, and magnesia as starting materials. The starting materials were mixed in different ratios to obtain different cordierite–mullite composite batches in which the cordierite contents ranged from 50 to 100 wt.%. The batches were uni-axially pressed at 100 MPa and sintered at 1350, 1400 and 1450 °C to select the optimum temperature required for cordierite–mullite nano–macro composites formation. The formed phases were identified by X-ray diffraction (XRD) pattern. The sintering parameters in terms of bulk density (BD) and apparent porosity (AP) were determined. The microstructure of composites has been investigated by scanning electron microscope (SEM). Cold crushing strength (CCS) of the sintered batches was evaluated. The result revealed that the cordierite–mullite nano–macro composites were in-situ formed at 1400 °C. The batch containing 70 wt.% cordierite showed good physical and mechanical properties.

36 MATERIALS SCIENCE↗

Progress in development of SiC-based joints resistant to neutron irradiation

This study fills a knowledge gap regarding neutron-irradiation resistance of SiC joints for nuclear applications, by investigating high-dose neutron irradiation effects on the strength of selected joints and low-dose neutron irradiation effects on recently developed joints fabricated by state of the art processing methods. The joining methods used for the high-dose radiation study included pressure-assisted liquid-phase sintering (LPS) of SiC nanopowder, pressureless calcia-alumina glass ceramics joining, and reaction sintering of Ti-Si-C powders with hot-pressing. The joints were neutron-irradiated at 530 °C to 20 displacements per atom (dpa). Other joining methods included low-pressure LPS of cold-pressed SiC green body, pressureless reaction sintered Ti-Si-C powder joint, spark plasma–sintered Ti diffusion bond, and hot-pressed Ti diffusion bond, which were irradiated at ~500 °C to ~2 dpa. There was no notable degradation of torsional strengths of the joints following the high-dose irradiation. The irradiation-induced degradation at low neutron dose was highly dependent on joint type.

36 MATERIALS SCIENCE↗

Study of microstructure and electrical properties of bulk YBCO prepared by melt textured growth technique

Bulk YBCO components were prepared using Melt Texture Growth (MTG) technique. Components were fabricated using MTG by addition of Y{sub 2}BaCuO{sub 5} (Y211) and Ag to YBCO, which leads to improved grain size without affecting superconducting properties. Green compacts prepared by cold isostatic pressing were pre-sintered at 930°C before subjecting melt texturing. Cooling rates lower than 1 °C.h{sup −1} was used, in between (peritectic) temperature of about 995 and 1025°C, to obtain large grained components. Microstructure studies in details were carried out by Scanning Electron Microscope (SEM), Electron Probe Micro Analysis (EPMA), Orientation Imaging Microscope (OIM) and TEM correlated with electrical properties like Critical current density (J{sub c})

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗