Refractive index of Nd:CaF2 and some Nd doped glasses as a function of wavelength, % neodymium, and temperature
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Phase transitions and equations of state of the alkaline earth fluorides CaF{sub 2}, SrF{sub 2}, and BaF{sub 2} were examined by static compression to pressures as high as 146 GPa. Angle-dispersive x-ray diffraction experiments were performed on polycrystalline samples in the laser-heated diamond-anvil cell. We confirmed that at pressures less than 10 GPa all three materials undergo a phase transition from the cubic (Fm3{sup -}m) fluorite structure to the orthorhombic (Pnam) cotunnite-type structure. This work has characterized an additional phase transition in CaF{sub 2} and SrF{sub 2}: these materials were observed to transform to a hexagonal (P6{sub 3}/mmc) Ni{sub 2}In-type structure between 63-79 GPa and 28-29 GPa, respectively, upon laser heating. For SrF{sub 2}, the Ni{sub 2}In-type phase was confirmed by Rietveld refinement. Volumes were determined as a function of pressure for all high-pressure phases and fit to the third-order Birch-Murnaghan equation of state. For CaF{sub 2} and SrF{sub 2}, the fluorite-cotunnite transition results in a volume decrease of 8-10%, while the bulk modulus of the cotunnite-type phase is the same or less than that of the fluorite phase within uncertainty. For all three fluorides, the volume reduction associated with the further transition to the Ni{sub 2}In-type phase is {approx}5%. The percentage increase in the bulk modulus ({Delta}K) across the transition is greater when the cation is smaller. While for BaF{sub 2}, {Delta}K is 10-30%, {Delta}K values for SrF{sub 2} and CaF{sub 2} are 45-65% and 20-40%. Although shock data for CaF{sub 2} have been interpreted to show a transition to a highly incompressible phase above 100 GPa, this is not consistent with our static equation of state data.
Abstract not provided.
Abstract not provided
Abstract not provided.
Abstract not provided.
Abstract not provided.
Atomization of a molten mixture of BaF2 and CaF2 has been found to be superior to crushing of bulk solid BaF2- CaF2 as a means of producing eutectic BaF2-CaF2 powder for use as an ingredient of the powder feedstock of a high-temperature solid lubricant material known as PS304. Developed to reduce friction and wear in turbomachines that incorporate foil air bearings, PS304 is applied to metal substrates by plasma spraying. The constituents of PS304 are: a) An alloy of 80 weight percent Ni and 20 weight percent Cr, b) Cr2O3, c) Ag, and d) The BaF2-CaF2 eutectic, specifically, 62 weight percent BaF2 and 38 weight percent CaF2. The superiority of atomization as a means of producing the eutectic BaF2-CaF2 powder lies in (1) the shapes of the BaF2-CaF2 particles produced and (2) the resulting flow properties of the PS304 feedstock powder: The particles produced through crushing are angular, whereas those produced through atomization are more rounded. PS304 feedstock powder containing the more rounded BaF2-CaF2 particles flows more freely and more predictably, as is preferable for plasma spraying.
Explore the source record for details and available documents.
The effects of BaF2-CaF2 particle size and size distribution on PS304 feedstock powder flowability have been investigated. Angular BaF2-CaF2 eutectic powders were produced by comminution and classified by screening to obtain 38 to 45 microns 45 to 106 microns, 63 to 106 microns, 45 to 53 microns, 63 to 75 microns, and 90 to 106 microns particle size distributions. The fluorides were added incrementally from 0 to 10 wt% to the other powder constituents of the PS304 feedstock: nichrome, chromia, and silver powders. The flow rate of the powder blends decreased linearly with increasing concentration of the fluorides. Flow was degraded with decreasing BaF2-CaF2 particle size and with increasing BaF2-CaF2 particle size distribution. A semiempirical relationship is offered to describe the PS304 powder blend flow behavior. The Hausner Ratio confirmed the funnel flow test results, but was slightly less sensitive to differences in BaF2-CaF2 particle size and size distribution. These findings may have applicability to other powders that do not flow easily, such as ceramic powders.
Carboxylic acid is a common ligand anchoring group to functionalize nanoparticle surfaces. Its binding structures and mechanisms as a function of the oxidation states of metal oxide nanoparticle surfaces are not well characterized experimentally. We present an in situ sum frequency generation vibrational spectroscopy (SFG-VS) study on the binding of deuterated acetic acid on ceria nanoparticles in the aqueous solution. In the SFG experiment, ceria nanoparticles were deposited on the flat surface of a CaF2 hemisphere in contact with acetic acid solutions. While the ceria nanoparticle deprotonated the acetic acid, the CaF2 surface could not. Thus, the binding of the deprotonated acetic acid on ceria can be selectively probed. SFG spectra revealed that the binding modes of the carboxylate group depend on the oxidation states of the ceria surfaces. SFG polarization analysis suggested that the bidentate chelating and bridging binding modes co-exist on the reduced ceria surfaces, while the oxidized ceria surfaces are dominated by the bidentate bridging mode. The direct spectroscopic evidence helps to clarify the binding structures and mechanisms on the ceria nanoparticles. Furthermore, the middle-infrared (IR) transparent CaF2 and its chemical inertness make CaF2 and similar substrate materials good candidates for direct SFG-VS measurement of nanoparticle surface reactions and binding chem-istry.
As a part of a program for the development of a sulfur probe for monitoring the sulfur potential in coal gasification reactors, an investigation was conducted regarding the efficiency of the solid electrolyte cell Ar+H2+H2S/CaS+CaF2+(Pt)//CaF2//Pt)+CaF2+CaS/H2S+H2+Ar. A demonstration is provided of the theory, design, and operation of a solid-state sulfur probe based on CaF2 electrolyte. It was found that the cell responds to changes in sulfur potential in a manner predicted by the Nernst equation. The response time of the cell at 1225 K, after a small change in temperature or gas composition, was 2.5 Hr, while at a lower temperature of 990 K the response time was approximately 9 hr. The cell emf was insensitive to a moderate increase in the flow rate of the test gas and/or the reference gas. The exact factors affecting the slow response time of galvanic cells based on a CaF2 electrolyte have not yet been determined. The rate-limiting steps may be either the kinetics of electrode reactions or the rate of transport through the electrolyte.
The deformation behavior of CaF2 and LiF single crystals compressed in the 111 and the 100 line directions, respectively, are compared with the mechanical properties of polycrystalline LiF-22 (mol pct) CaF2 eutectic mixture in the temperature range 300 to 1275 K for strain rates varying between 7 x 10 to the -7th and 0.2/s. The true stress-strain curves for the single crystals were found to exhibit three stages in an intermediate range of temperatures and strain rates, whereas those for the eutectic showed negative work-hardening rates after a maximum stress. The true stress-strain rate data for CaF2 and LiF-22 CaF2 could be represented by a power-law relation with the strain rate sensitivities lying between 0.05 and 0.2 for both materials. A similar relation was found to be unsatisfactory in the case of LiF.
The lubricating properties of some experimental ceramic coatings, diffusion-bonded fluoride coatings, and ceramic-bonded fluoride coatings were determined. The experiments were conducted in an air atmosphere at a sliding velocity of 430 feet per minute and at temperatures from 75 to 1500 F. Several ceramic coatings provided substantial reductions in friction coefficient and rider wear (compared with the unlubricated metals). For example, a cobaltous oxide (CoO) base coating gave friction coefficients of 0.24 to 0.36 within the temperature range of 75 to 1400 F; serious galling and welding of the metal surfaces were prevented. The friction coefficients were higher than the arbitrary maximum (0.2) usually considered for effective boundary lubrication. However, when a moderately high friction coefficient can be tolerated, this type of coating may be a useful antiwear composition. Diffusion-bonded calcium fluoride (CaF2) on Haynes Stellite 21 and on Inconel X gave friction coefficients of 0.1 to 0.2 at 1500 F. Endurance life was dependent on the thermal history of the coating; life improved with increased exposure time at elevated temperatures prior to running. Promising results were obtained with ceramic-bonded CaF2 on Inconel X. Effective lubrication and good adherence were obtained with a 3 to 1 ratio of CaF2 to ceramic. A very thin sintered and burnished film of CaF2 applied to the surface of this coating further improved lubrication, particularly above 1350 F. The friction coefficient was 0.2 at 500 F and decreased with increasing temperature to 0.06-at 1500 F. It was 0.25 at 75 F and 0.22 at 250 F.