At least 55 records · Page 3

Influence of Wear Test Parameters on the Electrical Contact Performance of Brass Alloy/Copper Contactors Under Fretting Wear

Fretting of mated electronic connectors may be due to extreme increase in contact resistance. We present a detailed analysis of contact resistance by fretting experiments using brass alloys/copper contact pairs. The relationship between wear mechanisms and contact resistance was determined. The influence of fundamental factors such as normal load, displacement amplitude, and current on contact resistance change was also evaluated. It was found out that displacement amplitude, normal load, and current are important parameters for infinite lifetime or stable electrical resistance during fretting condition. Influence of displacement amplitude on the electrical contact performance might be affected by wear debris in the contact area. Electric contact performance could be improved by increasing the power current, which could break down the thick oxide film formed. The predicted working lifetime and reliability requirements of the connector were determined to optimize and extend the service life under the working condition.

36 MATERIALS SCIENCE↗

The role of local strains from prior cold work on stress corrosion cracking of α-brass in Mattsson's solution

The dynamic strain rate ahead of a crack tip formed during stress corrosion cracking (SCC) under a static load is assumed to arise from the crack propagation. The strain surrounding the crack tip would be redistributed as the crack grows, thereby having the effect of dynamic strain. Recently, several studies have shown cold work to cause accelerated crack growth rates during SCC, and the slip-dissolution mechanism has been widely applied to account for this via a supposedly increased crack-tip strain rate in cold worked material. While these interpretations consider cold work as a homogeneous effect, dislocations are generated inhomogeneously within the microstructure during cold work. The presence of grain boundaries results in dislocation pile-ups that cause local strain concentrations. The local strains generated from cold working α-brass by tensile elongation were characterized using electron backscatter diffraction (EBSD). The role of these local strains in SCC was studied by measuring the strain distributions from the same regions of the sample before cold work, after cold work, and after SCC. Though, the cracks did not always initiate or propagate along boundaries with pre-existing local strains from the applied cold work, the local strains surrounding the cracked boundaries had contributions from both the crack propagation and the prior cold work. - Highlights: • Plastic strain localization has a complex relationship with SCC susceptibility. • Surface relief created by cold work creates its own granular strain localization. • Cold work promotes crack growth but several other factors are involved.

36 MATERIALS SCIENCE↗

Spectroscopic characterization of laser ablation brass plasma

We present optical emission studies of the laser ablation brass plasma generated by the fundamental, second, and third harmonics of a neodymium doped yttrium aluminum garnet laser. The spectra predominantly reveal the spectral lines of the neutral and singly ionized copper and zinc. The excitation temperatures are determined by the Boltzmann plot method, whereas the electron number densities have been extracted from the Stark broadened line profiles. The spatial variations in the spectral line intensities and the plasma parameters at 1000, 500, and 100 mbar air pressures have been evaluated. Besides, the effect of the ambient gases (He, Ne, and Ar), the laser irradiance, and the laser wavelengths on the plasma parameters have been investigated.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Ambient dependence of the phase of nanowires grown by annealing brass

The growth of oxide nanowires has been studied by the annealing of brass (Cu 65%, Zn 35%) at different annealing temperatures and in different ambient. The annealing temperature was varied from 400 deg. C to 650 deg. C. Scanning Electron Microscope (SEM) results showed that the temperature has a significant effect on the density and size of the nanowires. The annealing temperature of 600 deg. C was found to be optimum for the growth of nanowires. The growth at 600 deg. C was observed in two ambient-air and moist nitrogen. Selected Area Electron Diffraction (SAED) and Energy Dispersive Spectroscopy (EDS) results on Transmission Electron Microscope (TEM) showed that with changing the ambient from air to moist nitrogen, the phase of the nanowires changed from Zn doped CuO to Cu doped ZnO. This result can be of significance importance as it suggests the use of ambient for the tuning of phase of oxide nanowires and in turn for the tuning of their physical properties.

36 MATERIALS SCIENCE↗

Femtosecond laser ablation of brass in air and liquid media

Laser ablation of brass in air, water, and ethanol was investigated using a femtosecond laser system operating at a wavelength of 785 nm and a pulse width less than 130 fs. Scanning electron and optical microscopy were used to study the efficiency and quality of laser ablation in the three ablation media at two different ablation modes. With a liquid layer thickness of 3 mm above the target, ablation rate was found to be higher in water and ethanol than in air. Ablation under water and ethanol showed cleaner surfaces and less debris re-deposition compared to ablation in air. In addition to spherical particles that are normally formed from re-solidified molten material, micro-scale particles with varying morphologies were observed scattered in the ablated structures (craters and grooves) when ablation was conducted under water. The presence of such particles indicates the presence of a non-thermal ablation mechanism that becomes more apparent when ablation is conducted under water.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Brass plasmoid in external magnetic field at different air pressures

The behavior of expanding brass plasmoid generated by 266 nm wavelength of Nd:YAG laser in nonuniform magnetic field at different air pressures has been examined using optical emission spectroscopy and fast imaging of plasma plumes. The splitting of the plasma plumes and enhancement of intensity of Cu I at 510.5 nm in the presence of magnetic field at lower pressures are discussed. The threading and expulsion of the magnetic field lines through the plasmoid are correlated with the ambient pressure. The stoichiometry of the plasma plume is not significantly influenced by the magnetic field; however, the abundance of neutral to ionic species of Cu and Zn is greatly influenced by the magnetic field.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Combined DNA Typing and Protein Identification from Unfired Brass Cartridges

Biological evidence in the form of contact traces is of major importance in forensic laboratories but success rates are affected by the low amounts and degraded state of the DNA present on these items. Combining DNA polymorphisms with markers individualizing the more abundant protein fraction is a promising new approach. In this study touched brass cartridges were successfully tested for DNA polymorphisms and signature peptides after a single collection and enzyme digestion step. A comparison between moistened swabs and adhesive tape for the collection step resulted in slightly better quality DNA profiles for the tape samples, but no significant difference for protein identifications. The detected proteins showed the expected prominence of different keratins and were generally consistent with previously described skin proteomes.

59 BASIC BIOLOGICAL SCIENCES↗

Structure Determination of Two Modulated g-Brass Structures in the Zn-Pd System through a (3+1)-Dimensional Space Description

The structure determination of two composite compounds in the Zn-Pd system with close relationships to the cubic g-brass structure Zn11-dPd2+d is reported. Their structures have been solved from single crystal X-ray diffraction data within a (3 + 1)-dimensional [(3 + 1)D] formalism. Zn75.7(7)Pd24.3 and Zn78.8(7)Pd21.2 crystallize with orthorhombic symmetry, super space group Xmmm(00g)0s0 X=[(1/2,1/2,0,0);(0,1/2,1/2,1/2); (1/2,0,1/2,1/2)], with the following lattice parameters, respectively: as = 12.929(3) , bs = 9.112(4) , cs = 2.5631(7) , q = 8/13 c* and Vs = 302.1(3) A3 and as = 12.909(3) , bs = 9.115(3) , cs = 2.6052(6) , q = 11/18 c* and Vs = 306.4(2) A3. Their structures may be considered as commensurate because they can be refined in the conventional 3D space groups (Cmcm and Cmce, respectively) using super cells, but they also refined within the (3 + 1)D formalism to residual factors R = 3.22% for 139 parameters and 1184 independent reflections for Zn75.7(7)Pd24.3 and R = 3.46% for 197 parameters and 1804 independent reflections for Zn78.8(7)Pd21.2. The use of the (3 + 1)D formalism improves the results of the refinement and leads to a better understanding of the complexity of the atomic arrangement through the various modulations (occupation waves and displacive waves). Our refinements emphasize a unique Pd/Zn occupation modulation at the center of the icosahedra which is correlated with the distortion of the sites.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pd2.28(1)Zn10.37(1)Al0.35(1), a ternary γ-brass-type structure

Palladium zinc aluminium (2.28/10.37/0.35), Pd{sub 2.28(1)}Zn{sub 10.37(1)}Al{sub 0.35(1)}, represents the upper limit of Al substitution into the parent cubic {gamma}-brass Pd{sub 2+x}Zn{sub 11-x}. The structure can be described in terms of a 26-atom cluster consisting of an inner tetrahedron (IT), an outer tetrahedron (OT), an octahedron (OH) and a cuboctahedron (CO), with the substituted Al atoms partially occupying the IT (.3m) and CO (..m) sites.

36 MATERIALS SCIENCE↗

Initial stages of cavitation damage and erosion on copper and brass tested in a rotating disk device

In view of the differences in flow and experimental conditions, there has been a continuing debate as to whether or not the ultrasonic method of producing cavitation damage is similar to the damage occurring in cavitating flow systems, namely, venturi and rotating disk devices. In this paper, the progress of cavitation damage during incubation periods on polycrystalline copper and brass tested in a rotating disk device is presented. The results indicate several similarities and differences in the damage mechanism encountered in a rotating disk device (which simulates field rotary devices) and a magnetostriction apparatus. The macroscopic erosion appears similar to that in the vibratory device except for nonuniform erosion and apparent plastic flow during the initial damage phase.

Rao, P. V.↗

Thermal conductance of pressed brass contacts at liquid helium temperatures

An apparatus has been designed and fabricated which will measure the thermal conductance of pressed contacts at liquid helium temperatures as a function of applied force, with surface finish as a parameter. The apparatus is automated and was used to measure thermal conductance at temperatures from 1.5 to 6.5 K at applied forces up to 700 N for brass sample pairs having surface finishes from 0.1 to 1.6 micron rms. The experimental data were found to fit a simple power law where the thermal conductance is given by k = alpha T exp n, where k is the thermal conductance, T is the absolute temperature, and alpha and n are empirically determined constants.

Salerno, L. J.↗

Further observations of SCC in alpha-beta brass Considerations regarding the appearance of crack arrest markings during SCC

A series of constant displacement and constant extension rate stress corrosion cracking (SCC) tests was performed on an alpha-beta brass alloy in 1 N Na2SO4 solutions. The chosen mechanical and electrochemical conditions resulted in predominantly transgranular, cleavage-like failure at high (about 8 to 50 microns/s) average crack propagation rates. Crack arrest markings were observed on selected transgranular facets, which almost exclusively bordered regions of ductile overload failure. It is proposed that the observed crack velocities and the specific nature of the arrest mark appearance are most consistent with a cracking mechanism involving adsorption or some other interaction with a damaging environmental species.

Hintz, M. B.↗

Grain boundary sliding behaviour of copper and alpha brass at intermediate temperatures

The role of grain boundary sliding in copper and Cu-30 pct Zn in the temperature range 0.50-0.72 Tm, where Tm is the absolute melting point of the material, is examined. First, sliding data obtained on these materials are presented. The results indicate that the stress exponent for sliding is similar to that for lattice deformation, while the activation energy for sliding varies between 0.5 and 1.6 of the activation energy for creep. Several models proposed for grain boundary sliding are discussed, and it is shown that they do not account for the observed results on copper and alpha brass. A phenomenological model is proposed, where it is assumed that grain boundary sliding results from the glide of dislocations on secondary slip planes.

Raj, S. V.↗

R-damage cassette (incorporated brass sleeve)

The R-Damage series of ten experiments is part of a long-term collaboration with RFNC/VNIIEF in pulsed power technology. These experiments use a cylindrical configuration to study spallation damage, which allows for a natural recollection of the damaged material under proper driving conditions and post-shot collection of the damaged target material for subsequent metallographic analysis. Dynamic in-situ experimental velocimetry diagnostics are also employed. LANL is responsible for the design of the experimental load and velocimetry system. VNIIEF is responsible for the design and construction of the driving explosive magnetic generator. Eight of the experiments in the planned series have been completed. Thus far, data has been collected about failure initiation of a well-characterized material (aluminum) in a cylindrical geometry, the behavior of material recollected after damage from pressures in the damage initiation regime, and the behavior of material recollected after complete failure. The final two experiments will continue the study of material recollected after complete failure. The load assembly shown is similar to that employed in the previous two experiments, with some modiflications for easier assembly.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗