Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Anodic Stripping”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Room-Temperature Calcium Plating and Stripping Using a Perfluoroalkoxyaluminate Anion Electrolyte

Multivalent ion chemistries, like Ca 2+ , used in energy storage boast the potential to utilize solid metallic anodes and provide high volumetric energy density. The promise of such systems relies on the ability to incorporate high-voltage cathode materials while sustaining robust plating and stripping at the anode. These processes are dependent on an electrochemically stable electrolyte for ion transport and storage. In this work, we report an addition to the limited pool of nonaqueous electrolytes capable of plating and stripping calcium at room temperature. The synthesis and structural properties of calcium tetrakis(perfluoro-tert-butoxy) aluminate (Ca[TPFA] 2 ) are described along with the electrochemical performance during plating and stripping (up to 55% Coulombic efficiency) and a proof of concept for full cell viability with a CuS cathode material. X-ray experiments were used to study both the bulk solvation structure around calcium and possible decomposition pathways of the weakly coordinating TPFA anion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crossover Effects in Lithium–Metal Batteries with a Localized High Concentration Electrolyte and High–Nickel Cathodes

While crossover effects, such as transition–metal dissolution, are well–understood in lithium–ion batteries, there is a limited understanding of the effect of crossed–over chemical species in cells with oxide cathodes and lithium–metal anodes. In this work, the effects of cathode–to–anode and anode–to–cathode crossover are explored in cells with a high–nickel cathode, lithium–metal anode, and a localized high–concentration electrolyte (LHCE). Dramatic differences are found among cells; a lithium–metal anode paired with a high–nickel cathode has three times less solid–electrolyte interphase growth than a lithium–metal anode paired with lithium metal. Meanwhile, the cathode paired with lithium metal has 2–3 times higher capacity fade than the same cathode paired with graphite. Decomposition and crossover of the FSI salt is identified as the main source of these changes. The fluorine in the salt is first stripped off at the lithium–metal anode, and the remaining sulfur and nitrogen cross over to the cathode. Although the reduction in fluorine content harms the surface stability of the cathode, the lithium–metal anode benefits from the increased fluorine content. Furthermore, because the lithium–metal anode is typically the bottleneck for cells with thin lithium, crossover is a major factor in the enhanced performance of lithium–metal batteries with LHCE.

25 ENERGY STORAGE↗

Structural and electrochemical evolution of alloy interfacial layers in anode-free solid-state batteries

“Anode-free” solid-state batteries feature high energy density since there is no anode active material. Although the beneficial effects of interfacial layers at the anode-solid electrolyte interface have been demonstrated, the mechanisms through which they influence lithium plating/stripping are unclear. Here, in this study, we reveal the evolution of 100-nm silver and gold interfacial layers during lithium plating/stripping using electrochemical methods, electron microscopy, X-ray microcomputed tomography, and modeling. The alloy layers improve Coulombic efficiency and resistance to short circuiting, even though the alloys form solute regions or particulates that detach from the current collector during plating. In situ electrochemical impedance spectroscopy shows that the alloys return to the interface and mitigate contact loss at the end of stripping, avoiding a critical vulnerability of anode-free cells. Contact retention is driven by even Li thickness that promotes spatially uniform stripping, as well as local alloy delithiation in response to current concentrations that homogenizes current and diminishes voiding.

25 ENERGY STORAGE↗

Performance degradation due to anodic failure mechanisms in lithium-ion batteries

Here, we report a mechano-chemical model for anodic degradation during fast-charging of nickel-manganese-cobalt (NMC)/graphite (C) cell due to SEI growth, lithium plating/stripping, dead lithium storage, and film fracture of composite SEI and plated lithium film. Degradation of the battery is analyzed for a range of charging rates from 1 to 6 C-rates, and the influence of plating mechanisms – lithium plating and dead lithium deposition and recovery during stripping – on the film resistance of the anode are accounted for in the model. Dynamic evolution of the interfacial properties is modeled using rule-of-mixture approach. Model predictions of plating associated stress fields are used to compute critical energy release rate for film cracking. The results indicate an increased tendency of fracture for thinner SEI film with lithium plating at higher charging rates. The process of reforming the cracked film absorbs a significant portion of the electrode current thereby reducing the cell capacity and plating efficiency. The mechano-chemical model provides an extensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, prognosticating conditions of SEI failure, and evaluating the capacity fade and efficiency of lithium-ion battery.

25 ENERGY STORAGE↗

High-efficiency, anode-free lithium–metal batteries with a close-packed homogeneous lithium morphology

Anode-free lithium–metal batteries (LMBs) are ideal candidates for high-capacity energy storage as they eliminate the need for a conventional graphite electrode or excess lithium–metal anode. Current anode-free LMBs suffer from low Coulombic efficiency (CE) due to poor lithium stripping efficiency. Advanced electrolyte development is a promising route to maximize lithium plating and stripping CE and minimize capacity fade. However, a poor understanding of the mechanisms by which advanced electrolytes improve performance hampers progress in the practical development of anode-free LMBs. Here, we use synchrotron techniques and other tools to analyze the influence of three commercially available electrolytes on the composition, heterogeneity, kinetics, morphology, and electrochemistry of anode-free LMBs. Advanced electrolytes improve the electrochemical performance of anode-free LMBs by forming much denser and better-packed Li morphologies on a Cu current collector than on the conventional electrolyte. Li plates uniformly over the electrode area with the advanced electrolytes rather than in a few active sites. Inactive crystalline Li with heterogeneous distribution dominates the capacity degradation of anode-free cells, especially with the conventional electrolyte, indicating that reducing the amount of “dead” crystalline Li will significantly improve the cycling stability of anode-free cells. Finally, the understanding of the Li plating and stripping process obtained from this work will accelerate the development of anode-free LMBs with high efficiency.

25 ENERGY STORAGE↗

Combined density functional theory/kinetic Monte Carlo investigation of surface morphology during cycling of Li-Cu electrodes

In this work, we employed a combined density functional theory and kinetic Monte Carlo approach in order to investigate the nanoscale behavior of lithium stripping and plating on lithium-copper nanoalloys. Density functional theory calculations were used to develop an atom-by-atom understanding of the nucleation behavior of lithium on copper surfaces with different surface morphologies. We found that nanometric pits resulted in significantly more favorable lithium deposition when compared to pristine or lightly-defective Cu surfaces, which is in agreement with previous experimental studies. We then used density functional theory and constrained ab initio molecular dynamics to develop interaction and reaction parameters for a larger-scale kinetic Monte Carlo model in order to provide insight into the stripping and plating behavior of nanostructured Li-Cu nanoalloy anodes. Substantial losses in capacity and strong indications of morphological change were observed for a wide range of Cu:Li ratios over 100 cycles. We observed a complex relationship between the nanoparticle composition and the properties of the formed solid-electrolyte interphase.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tuning Solid Electrolyte Interphase Formation before Plating Onset in Anode-Free Sodium Batteries

Sodium (Na) batteries are of growing interest due to the higher earth abundance of sodium than lithium, as well as their promising theoretical energy density when metallic Na anodes are used. However, Na plating and stripping are heavily influenced by the physicochemical properties of the solid electrolyte interphase (SEI), which is directly influenced by the solvent and salt used for the electrolyte. While most studies focus on the SEI that forms on the surface of Na metal after plating, we expand this analysis by identifying a nanoscale “pre-plating” SEI that forms on the current collector (CC) prior to the onset of Na plating. Here, we systematically investigate an array of Na salt and glyme solvents in the electrolyte and determine the associated impacts on pre-plating SEI formation on aluminum CCs. By combining analytical electrochemistry approaches with a multimodal suite of spectroscopy techniques (X-ray, infrared, and Raman), supported by density functional theory calculations, we reveal a direct correlation between the Na + coordination environment and pre-plating SEI composition. We find that longer-chain glymes produce larger proportions of organic alkoxide products in the interphase, consistent with increased Na + −glyme interactions, while the fraction of salt-derived inorganic products (e.g., NaF) correlates with Na + −anion coordination. These insights highlight the critical influence of electrolyte composition particularly solvent identity and Na + coordination on the initial SEI formation in anode-free Na batteries.

anode-free batteries↗

The DUNE Far Detector Vertical Drift Technology. Technical Design Report

DUNE is an international experiment dedicated to addressing some of the questions at the forefront of particle physics and astrophysics, including the mystifying preponderance of matter over antimatter in the early universe. The dual-site experiment will employ an intense neutrino beam focused on a near and a far detector as it aims to determine the neutrino mass hierarchy and to make high-precision measurements of the PMNS matrix parameters, including the CP-violating phase. It will also stand ready to observe supernova neutrino bursts, and seeks to observe nucleon decay as a signature of a grand unified theory underlying the standard model. The DUNE far detector implements liquid argon time-projection chamber (LArTPC) technology, and combines the many tens-of-kiloton fiducial mass necessary for rare event searches with the sub-centimeter spatial resolution required to image those events with high precision. The addition of a photon detection system enhances physics capabilities for all DUNE physics drivers and opens prospects for further physics explorations. Given its size, the far detector will be implemented as a set of modules, with LArTPC designs that differ from one another as newer technologies arise. In the vertical drift LArTPC design, a horizontal cathode bisects the detector, creating two stacked drift volumes in which ionization charges drift towards anodes at either the top or bottom. The anodes are composed of perforated PCB layers with conductive strips, enabling reconstruction in 3D. Light-trap-style photon detection modules are placed both on the cryostat's side walls and on the central cathode where they are optically powered. This Technical Design Report describes in detail the technical implementations of each subsystem of this LArTPC that, together with the other far detector modules and the near detector, will enable DUNE to achieve its physics goals.

47 OTHER INSTRUMENTATION↗

Overcoming Anode Instability in Solid‐State Batteries through Control of the Lithium Metal Microstructure

Abstract Enabling the lithium metal anode (LMA) in solid‐state batteries (SSBs) is the key to developing high energy density battery technologies. However, maintaining a stable electrode–electrolyte interface presents a critical challenge to high cycling rate and prolonged cycle life. One such issue is the interfacial pore formation in LMA during stripping. To overcome this, either higher stack pressure or binary lithium alloy anodes are used. Herein, it is shown that fine‐grained ( d = 20 µm) polycrystalline LMA can avoid pore formation by exploiting the microstructural dependence of the creep rates. In a symmetric cell set‐up, i.e., LiǀLi 6.25 Al 0.25 La 3 Zr 2 O 12 (LLZO)ǀLi, fine‐grained LMA achieves > 11.0 mAh cm −2 compared to ≈ 3.6 mAh cm −2 for coarse‐grained LMA ( d = 295 µm) at 0.1 mA cm −2 and at moderate stress of 2.0 MPa. Smaller diffusion lengths (≈ 20 µm) and higher diffusivity pathway along dislocations ( D d ≈ 10 −7 cm 2 s −1 ), generated during cell fabrication, result in enhanced viscoplastic deformation in fine‐grained polycrystalline LMA. The electrochemical performances corroborate well with estimated creep rates. Thus, microstructural control of LMA can significantly reduce the required stack pressure during stripping. These results are particularly relevant for “anode‐free” SSBs wherein both the microstructure and the mechanical state of the lithium are critical parameters.

25 ENERGY STORAGE↗

Design strategies for nonaqueous multivalent-ion and monovalent-ion battery anodes

The inability of current battery technologies to keep up with the performance requirements of industry is pushing forward developments in electrochemistry. Specifically, the battery's negative electrode, the anode, presents many unique chemical, physical and engineering challenges. Lithium-based battery technologies have dominated the past decade, but concerns about the limited supply of lithium in the Earth's crust have led researchers to look towards alternative metal-ion technologies. Furthermore, various alkali metals (such as sodium and potassium) and alkali earth metals (such as magnesium and calcium) have attracted significant research interest. In this Review, we analyse these technologies in a coherent manner, addressing the problems of each type of anode, rather than those of specific types of metal-ion batteries. Covering direct metal plating and stripping, intercalation-based, alloy-based and conversion-reaction-based anode technologies, this analysis will offer the reader a comprehensive understanding of the behaviour of different metal-ion anodes and of what can be learned by transferring knowledge between these different systems. Increasing demand for energy-storage systems will inevitably stress the Earth's lithium supply; thus, the research focus is shifting towards other alkali and alkali earth metals. In summary, this Review compares and connects strategies to enable different multivalent and monovalent metal-ion battery anodes, including metal anodes and intercalation-based, alloy-based and conversion-reaction-based anodes.

36 MATERIALS SCIENCE↗

Interfacial Issues and Modification of Solid Electrolyte Interphase for Li Metal Anode in Liquid and Solid Electrolytes

Abstract The high energy density required for the next generation of lithium batteries will likely be enabled by a shift toward lithium metal anode from the conventional intercalation‐based anode such as graphite. However, several critical challenges for Li metal originate from its highly reactive nature and the hostless reaction of deposition and stripping impede the practical use of Li metal as an anode. The role of the solid electrolyte interphase (SEI) is very important for the Li metal anode where the SEI must protect the dynamically changing surface of the Li metal. Since the SEI‐generating reaction mechanisms for the two different electrolyte systems, liquid and solid, are considerably different, the SEI layers formed between the Li metal and the electrolytes in the two electrolyte systems have substantially different properties, causing different interfacial issues. Inhibition of the interfacial problems requires different strategies to reinforce the SEI layer for each of the electrolyte systems. However, the differences in the two electrolyte systems have not been clearly compared in the prior literature. In this report, the interfacial issues for the two different electrolyte systems are compared and different strategies for SEI modification are provided to overcome the issues.

25 ENERGY STORAGE↗

Working Principle of an Ionic Liquid Interlayer During Pressureless Lithium Stripping on Li 6.25 Al 0.25 La 3 Zr 2 O 12 (LLZO) Garnet‐Type Solid Electrolyte

Abstract Solid‐state‐batteries employing lithium metal anodes promise high theoretical energy and power densities. However, morphological instability occurring at the lithium/solid–electrolyte interface when stripping and plating lithium during cell cycling needs to be mitigated. Vacancy diffusion in lithium metal is not sufficiently fast to prevent pore formation at the interface above a certain current density during stripping. Applied pressure of several MPa can prevent pore formation, but this is not conducive to practical application. This work investigates the concept of ionic liquids as “self‐adjusting” interlayers to compensate morphological changes of the lithium anode while avoiding the use of external pressure. A clear improvement of the lithium dissolution process is observed as it is possible to continuously strip more than 70 μm lithium (i. e., 15 mAh cm −2 charge) without the need for external pressure during assembly and electrochemical testing of the system. The impedance of the investigated electrodes is analyzed in detail, and contributions of the different interfaces are evaluated. The conclusions are corroborated with morphology studies using cryo‐FIB‐SEM and chemical analysis using XPS. This improves the understanding of the impedance response and lithium stripping in electrodes employing liquid interlayers, acting as a stepping‐stone for future optimization.

Fuchs, Till↗

A low-cost, fluorine-free electrolyte for improved sodium batteries

Sodium batteries are an attractive alternative to lithium-ion technologies due to sodium’s lower cost and natural abundance—over 1,000 times greater than lithium, comprising approximately 2.4% of the Earth’s crust. However, most current electrolytes rely on fluorine-containing components, which raise economic and environmental concerns. This study explores fluorine-free, borate-based electrolytes that offer improved cycling stability and significant cost and sustainability benefits. We demonstrate stable sodium metal stripping and plating on aluminum foil, enabling anode-free cell configurations with over 50% capacity retention after 700 cycles. Spectroscopic and electrochemical analyses reveal the effects of solvents and salt composition on solvation, ionic conductivity, and oxidative stability. In full-cell configurations, the fluorine-free electrolyte maintains more than 98% capacity retention after 400 cycles. Furthermore, these findings represent a critical step toward the development of cost-effective, environmentally friendly, and high-performance sodium battery systems suitable for future electrification.

anode-free sodium batteries↗

Cracking the failure of lithium batteries

Lithium batteries that use a solid electrolyte have the potential to improve safety and increase the amount of stored energy . This makes solid-state electrochemical cells a promising option for electric vehicles and wearable devices. However, nonuniform plating or stripping of lithium at the interface between an anode (negative electrode) and the electrolyte during charging and discharging leads to growth of detrimental lithium filaments (dendrites) that short-circuit the battery cell. This problem even occurs when the battery operates at small currents. The underlying mechanism of this failure is not well understood. On page 311 of this issue, Wang et al. (1) report that structural defects accumulate in the lithium metal anode under repeated charging and discharging at a small current. This is similar to mechanical fatigue that is observed over longer periods of intermittent straining of a material. Here, the observation could guide the design of lithium batteries with increased life span.

25 ENERGY STORAGE↗

The Impact of Lithium Anode Interface on Capacity Fade in Polymer Electrolyte-Based Solid-State Batteries

This study investigates the Li stripping-plating morphology and failure mechanisms in full cells consisting of a solid polymer electrolyte (SPE) with two commercial Li anodes: Li chip and Li foil. The primary identified failure mechanism of the SPE cell is capacity fade, regardless of the Li manufacturer. While the cathode’s role in capacity fade is evident, the Li anode significantly influences cycling performance, with Li foil cells cycling 50% longer than Li chip cells, a statistical difference. Further, post-mortem scanning electron microscopy and X-ray photoelectron spectroscopy results attribute the Li chip’s faster capacity fade to a loss of contact and continuous growth of the solid electrolyte interphase (SEI). Conversely, Li foil maintains consistent contact with the solid polymer, displaying a thin and stable SEI. Additionally, failure mechanisms between a gel electrolyte in previous work and the dry SPE are compared.

25 ENERGY STORAGE↗

Interfacial Atomistic Mechanisms of Lithium Metal Stripping and Plating in Solid–State Batteries

All-solid-state batteries based on a Li metal anode represent a promising next-generation energy storage system, but are currently limited by low current density and short cycle life. Further research to improve the Li metal anode is impeded by the lack of understanding in its failure mechanisms at lithium–solid interfaces, in particular, the fundamental atomistic processes responsible for interface failure. Here, using large-scale molecular dynamics simulations, the first atomistic modeling study of lithium stripping and plating on a solid electrolyte is performed by explicitly considering key fundamental atomistic processes and interface atomistic structures. In the simulations, the interface failure initiated with the formation of nano-sized pores, and how interface structures, lithium diffusion, adhesion energy, and applied pressure affect interface failure during Li cycling are observed. By systematically varying the parameters of solid-state lithium cells in the simulations, the parameter space of applied pressures and interfacial adhesion energies that inhibit interface failure during cycling are mapped to guide selection of solid-state cells. Furthermore, this study establishes the atomistic modeling for Li stripping and plating, and predicts optimal solid interfaces and new strategies for the future research and development of solid-state Li-metal batteries.

25 ENERGY STORAGE↗

Dual Passivation of Cathode and Anode through Electrode–Electrolyte Interface Engineering Enables Long-Lifespan Li Metal–SPAN Batteries

The reliability and durability of lithium metal (Li 0 )–sulfur batteries are largely limited by the undesired Li 0 plating-stripping irreversibility and the detrimental polysulfide dissolution, yet approaches that can simultaneously address the above anodic and cathodic problems are scarce. In this study, we report the stable operation of a Li 0 -SPAN (sulfurized polyacrylonitrile) battery via an anode–cathode dual-passivation approach. By combination of a fluorinated localized high concentration electrolyte (LHCE) and a Li 3 N-forming additive (TMS-N 3 ), robust and highly conductive electrode passivation layers are formed in situ on the surface of both the Li 0 anode and the SPAN cathode. The resulting highly reversible, dendrite-free, and high-density Li 0 plating morphology enables a high Coulombic efficiency of 99.4%. Advanced tender energy X-ray spectroscopy also reveals the eliminated Li 2 S formation and minimized polysulfide dissolution in SPAN cathodes, leading to a high capacity of 580 mAh/g SPAN and stable cycling with negligible capacity decay (0.7%) for 800 cycles. This electrode–electrolyte interphase engineering strategy has tackled the major limitations of Li–S batteries in both ether- and carbonate-based electrolyte systems and under a wide temperature range from –10 to +50 °C, thus providing insightful guidelines for the rational design of highly durable and high-energy-density Li 0 -S batteries.

25 ENERGY STORAGE↗