The influence of grain size and composition on slow plastic flow in FeAl between 1100 and 1400 K

The slow plastic flow properties of a series of binary B2 FeAl intermetallics at elevated temperatures, and ranging in aluminum content from 39.8 to 48.7 at. pct, were investigated using constant-velocity compression tests at strain rates from 2 x 10 to the -3rd to 2 x 10 to the -7th. Two deformation mechanisms with the same activation energy are found. For the mode with a stress component of 6, the strength increases with decreasing grain size, probably as a result of Hall-Petch behavior, while for the mode with stress component of 3, the strength increases with increasing grain size, probably due to the action of diffusional creep. Creep in the high stress exponent mode can be described in terms of the initial grain size because the large-angle grain structure is replaced by a small-angle grain microstructure of similar grain diameter during deformation.

Whittenberger, J. D.↗

Fatigue life and crack growth prediction methodology

This paper reviews the capabilities of a plasticity-induced crack-closure model and life-prediction code to predict fatigue crack growth and fatigue lives of metallic materials. Crack-tip constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective stress-intensity factor range (Delta K(sub eff)) under constant amplitude loading. Some modifications to the Delta K(sub eff)-rate relations were needed in the near threshold regime to fit small-crackgrowth rate behavior and endurance limits. The model was then used to calculate small- and large-crack growth rates, and in some cases total fatigue lives, for several aluminum and titanium alloys under constant-amplitude, variable-amplitude, and spectrum loading. Fatigue lives were calculated using the crack-growth relations and microstructural features like those that initiated cracks. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

A Progressive Damage Methodology for Residual Strength Predictions of Center-Crack Tension Composite Panels

An investigation of translaminate fracture and a progressive damage methodology was conducted to evaluate and develop a residual strength prediction capability for laminated composites with through penetration notches. This is relevant to the damage tolerance of an aircraft fuselage that might suffer an in-flight accident such as an uncontained engine failure. An experimental characterization of several composite materials systems revealed an R-curve type of behavior. Fractographic examinations led to the postulate that this crack growth resistance could be due to fiber bridging, defined here as fractured fibers of one ply bridged by intact fibers of an adjacent ply. The progressive damage methodology is currently capable of predicting the initiation and growth of matrix cracks and fiber fracture. Using two difference fiber failure criteria, residual strength was predicted for different size panel widths and notch lengths. A ply discount fiber failure criterion yielded extremely conservative results while an elastic-perfectly plastic fiber failure criterion showed that the fiber bridging concept is valid for predicting residual strength for tensile dominated failure loads. Furthermore, the R-curves predicted by the model using the elastic-perfectly plastic fiber criterion compared very well with the experimental R-curves.

Coats, Timothy William↗

Analyses of Fatigue and Fatigue-Crack Growth under Constant- and Variable-Amplitude Loading

Studies on the growth of small cracks have led to the observation that fatigue life of many engineering materials is primarily crack growth from micro-structural features, such as inclusion particles, voids, slip-bands or from manufacturing defects. This paper reviews the capabilities of a plasticity-induced crack-closure model to predict fatigue lives of metallic materials using small-crack theory under various loading conditions. Constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective stress-intensity factor range (delta K(sub eff)) under constant-amplitude loading. Modifications to the delta K(sub eff)-rate relations in the near-threshold regime were needed to fit measured small-crack growth rate behavior. The model was then used to calculate small- and large-crack growth rates, and to predict total fatigue lives, for notched and un-notched specimens under constant-amplitude and spectrum loading. Fatigue lives were predicted using crack-growth relations and micro-structural features like those that initiated cracks in the fatigue specimens for most of the materials analyzed. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

Nonisothermal elasto-visco-plastic response of shell-type structures

A mathematical model and solution methodologies for analyzing structural response of thin, metallic shell-type structures under large transient, cyclic or static thermomechanical loads is disussed. Among the system responses, which are associated with these load conditions, are thermal buckling and creep buckling. Thus, geometric as well as material-type nonlinearities (of high order) can be anticipated and have been considered in the development of the mathematical model. Furthermore, this was accommodated in the solution procedures. A complete true ab-inito rate theory of kinematics and kinetics for continuum and curved thin structures, without any restriction on the magnitude of the strains or the deformation, was formulated. The time dependence and large strain behavior are incorporated through the introduction of the time rates of the metric and curvature in two coordinate systems, a fixed (spatial) one and a convected (material) coordinate system. The relations between the time derivative and the covariant derivatives (gradients) have been developed for curved space and motion, so that the velocity components supply the connection between the equations of motion and the time rate of change of the metric and curvature tensors.

Simitses, G. J.↗

Understanding Variability in Mechanical Behavior of Adhesively Bonded Sandwich Joints due to Stochastic Material Damage

A mesoscale progressive damage analysis was applied to the analysis of recently tested adhesively bonded sandwich panels, in which ten nominally identical tension loaded panels failed in three different failure modes, with peakloads ranging from 13.0 –16.1 kips. A parametric finite element model for progressive damage analysis of an adhesively bonded joint (ABJ) considering matrix and fiber damage, and delamination cracks in unidirectional and fabric composite sections of the joint, as well as core crushing, and adhesive fracture was developed. The model was developed using Abaqus/Explicit and utilized continuum damage mechanics material models for intralaminar damage in the facesheet and doubler plies, cohesive elements for delamination and adhesive debonding, and discretized cells considering plasticity to model crushing of the aluminum honeycomb core. Analysis predictions obtained with a pristine model agreed well with the average experimental peak load, strain in the joint, and post-test damage states. Then, various methods to incorporate stochastic material variability into ABJ model were evaluated. These methods included simulation of pre-existing matrix damage, pre-existing adhesive porosity, and uniform modification of adhesive properties. These material and manufacturing defects changed the damage mode predictions in some cases. The analysis of stochastic strength due to the considered defects revealed unintuitive damage mode interaction in the ABJ, explaining some structure-property relationships observed experimentally.

Richard Larson↗

Fracture mechanics; Proceedings of the Seventeenth National Symposium, Albany, NY, August 7-9, 1984

The present conference gives attention to topics in the application of fracture mechanics, subcritical crack growth phenomena, fracture testing methods, ductile fracture behavior, and fracture mechanisms and their analysis. Specific papers treat the resistance curve approach to composite materials characterization, fracture toughness in ductile iron and cast steel, hold-time effects in elevated temperature fatigue crack propagation, creep crack growth under nonsteady conditions, viscoplastic fatigue in a superalloy at elevated temperatures, fracture testing with arc bend specimens, one-point bend impact test application, and a compact mode II fracture specimen. Also discussed are the computation of stable crack growth using the J-integral, the use of plastic energy dissipation to characterize crack growth, the extension of surface cracks under cyclic loading, the minimum time criterion for crack instability in structural materials, dynamic crack propagation and branching under biaxial loading, and boundary layer effects in cracked bodies.

Underwood, J. M.↗

Jet Engine Fan Blade Containment Using an Alternate Geometry

With a goal of reducing jet engine weight, simulations of a fan blade containment system with an alternate geometry were tested and analyzed. A projectile simulating a fan blade was shot at two alternate geometry containment case configurations using a gas gun. The first configuration was a flat plate representing a standard case configuration. The second configuration was a flat plate with a radially convex curve section at the impact point. The curved surface was designed to force the blade to deform plastically, dissipating energy before the full impact of the blade is received by the plate. The curved case was able to tolerate a higher impact velocity before failure. The computational model was developed and correlated with the tests and a weight savings assessment was performed. For the particular test configuration used in this study the ballistic impact velocity of the curved plate was approximately 60 m/s (200 ft/s) greater than that of the flat plate. For the computational model to successfully duplicate the test, the very high strain rate behavior of the materials had to be incorporated.

Carney, K.S.↗

Fatigue life and crack growth prediction methodology

The capabilities of a plasticity-induced crack-closure model and life-prediction code to predict fatigue crack growth and fatigue lives of metallic materials are reviewed. Crack-tip constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective-stress-intensity factor range (delta(K(sub eff))) under constant-amplitude loading. Some modifications to the delta(K(sub eff))-rate relations were needed in the near threshold regime to fit small-crack growth rate behavior and endurance limits. The model was then used to calculate small- and large-crack growth rates, and in some cases total fatigue lives, for several aluminum and titanium alloys under constant-amplitude, variable-amplitude, and spectrum loading. Fatigue lives were calculated using the crack growth relations and microstructural features like those that initiated cracks. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

Elevated temperature compressive steady state deformation and failure in the oxide dispersion strengthened alloy MA 6000E

The compressive flow strength-strain rate behavior of the oxide-dispersion-strengthened alloy MA 6000E has been studied in the temperature range 1144-1366 K, with strain rates ranging from 2.1 x 10 to the -5th to 2.1 x 10 to the -7th per s. It is found that the inherent strength of the alloy is essentially the same in all test directions and that the low strength observed in tensile tests results from the inability of grain boundaries to support high tensile stresses. The failure of MA 6000E under high-temperature, slow plastic flow conditions is shown to be the result of concentrated slip. Slow plastic deformation in MA 6000E can be described by a threshold stress model of creep where threshold stresses are calculated from relatively fast testing procedures and the effective stress exponent for creep is assumed to be 3.5.

Whittenberger, J. D.↗

High-Temperature Shape Memory Polymers

physical conformation changes when exposed to an external stimulus, such as a change in temperature. Such materials have a permanent shape, but can be reshaped above a critical temperature and fixed into a temporary shape when cooled under stress to below the critical temperature. When reheated above the critical temperature (Tc, also sometimes called the triggering or switching temperature), the materials revert to the permanent shape. The current innovation involves a chemically treated (sulfonated, carboxylated, phosphonated, or other polar function group), high-temperature, semicrystalline thermoplastic poly(ether ether ketone) (Tg .140 C, Tm = 340 C) mix containing organometallic complexes (Zn++, Li+, or other metal, ammonium, or phosphonium salts), or high-temperature ionic liquids (e.g. hexafluorosilicate salt with 1-propyl-3- methyl imidazolium, Tm = 210 C) to form a network where dipolar or ionic interactions between the polymer and the low-molecular-weight or inorganic compound forms a complex that provides a physical crosslink. Hereafter, these compounds will be referred to as "additives". The polymer is semicrystalline, and the high-melt-point crystals provide a temporary crosslink that acts as a permanent crosslink just so long as the melting temperature is not exceeded. In this example case, the melting point is .340 C, and the shape memory critical temperature is between 150 and 250 C. PEEK is an engineering thermoplastic with a high Young fs modulus, nominally 3.6 GPa. An important aspect of the invention is the control of the PEEK functionalization (in this example, the sulfonation degree), and the thermal properties (i.e. melting point) of the additive, which determines the switching temperature. Because the compound is thermoplastic, it can be formed into the "permanent" shape by conventional plastics processing operations. In addition, the compound may be covalently cross - linked after forming the permanent shape by S-PEEK by applying ionizing radiation ( radiation, neutrons), or by chemical crosslinking to form a covalent permanent network. With respect to other shape memory polymers, this invention is novel in that it describes the use of a thermoplastic composition that can be thermally molded or solution-cast into complex "permanent" shapes, and then reheated or redissolved and recast from solution to prepare another shape. It is also unique in that the shape memory behavior is provided by a non-polymer additive.

Yoonessi, Mitra↗

Effects of High Mean Stress on High-cycle Fatigue Behavior of PWA 1480

PWA 1480 is a potential candidate material for use in the high-pressure fuel turbine blade of the space shuttle main engine. As an engine material it will be subjected to high-cycle fatigue loading superimposed on a high mean stress due to combined centrifugal and thermal loadings. The present paper describes the results obtained in an ongoing program at the Argonne National Laboratory, sponsored by NASA Lewis, to determine the effects of a high mean stress on the high-cycle fatigue behavior of this material. Straight-gauge high-cycle fatigue specimens, 0.2 inch in diameter and with the specimen axis in the 001 direction, were supplied by NASA Lewis. The nominal room temperature yield and ultimate strength of the material were 146 and 154 ksi, respectively. Each specimen was polished with 1-micron diamond paste prior to testing. However, the surface of each specimen contained many pores, some of which were as large as 50 micron. In the initial tests, specimens were subjected to axial-strain-controlled cycles. However, very little cyclic plasticity was observed.

Majumdar, S.↗

Nonlinear probabilistic finite element models of laminated composite shells

A probabilistic finite element analysis procedure for laminated composite shells has been developed. A total Lagrangian finite element formulation, employing a degenerated 3-D laminated composite shell with the full Green-Lagrange strains and first-order shear deformable kinematics, forms the modeling foundation. The first-order second-moment technique for probabilistic finite element analysis of random fields is employed and results are presented in the form of mean and variance of the structural response. The effects of material nonlinearity are included through the use of a rate-independent anisotropic plasticity formulation with the macroscopic point of view. Both ply-level and micromechanics-level random variables can be selected, the latter by means of the Aboudi micromechanics model. A number of sample problems are solved to verify the accuracy of the procedures developed and to quantify the variability of certain material type/structure combinations. Experimental data is compared in many cases, and the Monte Carlo simulation method is used to check the probabilistic results. In general, the procedure is quite effective in modeling the mean and variance response of the linear and nonlinear behavior of laminated composite shells.

Engelstad, S. P.↗

Fatigue-Life Prediction Methodology Using Small-Crack Theory

This paper reviews the capabilities of a plasticity-induced crack-closure model to predict fatigue lives of metallic materials using 'small-crack theory' for various materials and loading conditions. Crack-tip constraint factors, to account for three-dimensional state-of-stress effects, were selected to correlate large-crack growth rate data as a function of the effective-stress-intensity factor range (delta K(eff)) under constant-amplitude loading. Some modifications to the delta k(eff)-rate relations were needed in the near-threshold regime to fit measured small-crack growth rate behavior and fatigue endurance limits. The model was then used to calculate small- and large-crack growth rates, and to predict total fatigue lives, for notched and un-notched specimens made of two aluminum alloys and a steel under constant-amplitude and spectrum loading. Fatigue lives were calculated using the crack-growth relations and microstructural features like those that initiated cracks for the aluminum alloys and steel for edge-notched specimens. An equivalent-initial-flaw-size concept was used to calculate fatigue lives in other cases. Results from the tests and analyses agreed well.

Newmann, James C., Jr.↗

Slow and fast motion of cracks in inelastic solids. Part 1: Slow growth of cracks in a rate sensitive tresca solid. Part 2: Dynamic crack represented by the Dugdale model

An extension is proposed of the classical theory of fracture to viscoelastic and elastic-plastic materials in which the plasticity effects are confined to a narrow band encompassing the crack front. It is suggested that the Griffith-Irwin criterion of fracture, which requires that the energy release rate computed for a given boundary value problem equals the critical threshold, ought to be replaced by a differential equation governing the slow growth of a crack prior to the onset of rapid propagation. A new term which enters the equation of motion in the dissipative media is proportional to the energy lost within the end sections of the crack, and thus reflects the extent of inelastic behavior of a solid. A concept of apparent surface energy is introduced to account for the geometry dependent and the rate dependent phenomena which influence toughness of an inelastic solid. Three hypotheses regarding the condition for fracture in the subcritical range of load are compared. These are: (1) constant fracture energy (Cherepanov), (2) constant opening displacement at instability (Morozov) and (3) final stretch criterion (Wnuk).

Wnuk, M. P.↗

Slow growth of cracks in a rate sensitive Tresca solid.

Extension of the classical theory of fracture to viscoelastic and elastic-plastic materials in which the plasticity effects are confined to a narrow band encompassing the crack front. It is suggested that the Griffith-Irwin criterion of fracture, which requires that the energy release rate computed for a given boundary value problem equal the critical threshold, ought to be replaced by a differential equation governing the slow growth of a crack prior to the onset of rapid propagation. A new term which enters the equation of motion in the dissipative media is proportional to the energy lost within the end sections of the crack, and thus it reflects the extent of inelastic behavior of a solid. A concept of 'apparent' surface energy is introduced to account for the geometry-dependent and the rate-dependent phenomena which influence toughness of an inelastic solid. Three hypotheses regarding the condition for fracture in the subcritical range of load are compared.

Wnuk, M. P.↗

A study on thermal barrier coatings including thermal expansion mismatch and bond coat oxidation

The present investigation deals with a plasma-sprayed thermal barrier coating (TBC) intended for high temperature applications to advanced gas turbine blades. Typically, this type of coating system consists of a zirconia-yttria ceramic layer with a nickel-chromium-aluminum bond coat on a superalloy substrate. The problem on hand is a complex one due to the fact that bond coat oxidation and thermal mismatch occur in the TBC. Cracking in the TBC has also been experimentally illustrated. A clearer understanding of the mechanical behavior of the TBC is investigated. The stress states in a model thermal barrier coating as it cools down in air is studied. The powerful finite element method was utilized to model a coating cylindrical specimen. Four successively refined finite element models were developed. Some results obtained using the first two models have been reported previously. The major accomplishment is the successful development of an elastic TBC finite element model known as TBCG with interface geometry between the ceramic layer and the bond coat. An equally important milestone is the near-completion of the new elastic-plastic TBC finite element model called TBCGEP which yielded initial results. Representative results are presented.

Chang, George C.↗

Fracture behavior of large-scale thin-sheet aluminum alloy

A series of fracture tests on large-scale, pre-cracked, aluminum alloy panels is being carried out to examine and to characterize the process by which cracks propagate and link up in this material. Extended grips and test fixtures were specially designed to enable the panel specimens to be loaded in tension, in a 1780-kN-capacity universal testing machine. Twelve panel specimens, each consisting of a single sheet of bare 2024-T3 aluminum alloy, 3988 mm high, 2286 mm wide, and 1.016 mm thick are being fabricated with simulated through-cracks oriented horizontally at mid-height. Using existing information, a test matrix has been set up that explores regions of failure that are controlled by fracture mechanics, with additional tests near the boundary between plastic collapse and fracture. In addition, a variety of multiple site damage (MSD) configurations have been included to distinguish between various proposed linkage mechanisms. All tests but one use anti-buckling guides. At this writing seven specimens have been tested. Three were fabricated with a single central crack, three others had multiple cracks on each side of the central crack, and one had a single crack but no anti-buckling guides. Each fracture event was recorded on film, video, computer, magnetic tape, and occasionally optical microscopy. The visual showed the crack tip with a load meter in the field of view, using motion picture film for one tip and SVHS video tape for the other. The computer recorded the output of the testing machine load cell, the stroke, and twelve strain gages at 1.5 second intervals. A wideband FM magnetic tape recorder was used to record data from the same sources. The data were analyzed by two different procedures: (1) the plastic zone model based on the residual strength diagram; and (2) the R-curve. The first three tests were used to determine the basic material properties, and these results were then used in the analysis of the two subsequent tests with MSD cracks. There is good agreement between measured values and results obtained from the model.

Dewit, Roland↗