Moisture-Induced Delamination Video of an Oxidized Thermal Barrier Coating
PVD TBC coatings were thermally cycled to near-failure at 1150 C. Normal failure occurred after 200-300 1-hr cycles with only moderate weight gains (0.5 mg/cm2). Delamination and buckling was often delayed until well after cooldown (desktop spallation), but could be instantly induced by the application of water drops, as shown in an accompanying video-recording. Moisture therefore plays a primary role in delayed desktop TBC failure. Hydrogen embrittlement is proposed as the underlying mechanism.