Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Solid dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

DESORPTION OF SORBATES FROM MST, MMST, AND CST UNDER VARIOUS CONDITIONS

The Small Column Ion Exchange (SCIX) Program (formerly referred to as the Modular Salt Processing (MSP) Project) seeks to deploy equipment to remove the {sup 134,137}Cs, {sup 90}Sr, and alpha-emitting radionuclides (principally {sup 238,239,240}Pu and {sup 237}Np) from the high level waste salt solutions. The equipment is installed within a high level waste tank to take advantage of the shielding provided by the waste tank. The process will involve adding monosodium titanate (MST) to the waste tank (i.e., Tank 41H) to sorb the Sr and select actinides, removing the MST and entrained sludge with in-riser rotary microfilters, and subsequently using ion-exchange columns containing crystalline silicotitanate (CST) to remove the Cs. After being loaded with Cs, the CST will be ground to reduce the particle size and then transferred into another waste tank (e.g., Tank 40H). The MST and sludge solids stream will be transported to a sludge batch preparation tank (i.e., Tank 42H or Tank 51H) once the SCIX batch is processed. Both streams, MST/solids and CST, will ultimately be transported into and vitrified inside the Defense Waste Processing Facility (DWPF). A series of experiments were performed to examine desorption from monosodium titanate (MST), modified monosodium titanate (mMST), and crystalline silicotitanate (CST) under various conditions. The first two experiments examined desorption from MST and CST under two different sludge treatment processes, aluminum dissolution and sludge washing. Desorption of all sorbates was observed to varying degrees under the aluminum dissolution conditions. The extent of desorption ranged from < 3% to about 50% after 4 weeks, with Pu exhibiting the lowest desorption. At the end of the experiment, the temperature was reduced from 65 C to 25 C and the tests monitored for an additional two weeks. After reducing the temperature, partial resorption of the sorbates was observed with both MST and CST. Under the sludge washing conditions, no desorption of sorbates was observed with MST; however, some additional sorption did occur. For CST, a small amount of Cs leached from the material during the first day of testing, but no further leaching was observed over the remaining test period. The final test was designed to examine the possibility of desorption from both MST and mMST upon increasing the solid to liquid phase ratio. The results of these tests indicated some desorption of Pu from MST within the first two weeks after changing the phase ratio, then resorption of some of the leached Pu over the remaining 4 weeks of the experiment. No desorption of any sorbates was observed for mMST under these conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Investigation of nanostructured Al-10 wt.% Zr material prepared by ball milling for high temperature applications

Ground chips of as-cast Al-10 wt.% Zr alloy were subjected to mechanical alloying (MA) with 5 vol.% of nanodiamond addition in a high energy planetary ball-mill. The aim of this work was to investigate the microstructure, phase transformation and mechanical properties of the material both after MA and after subsequent annealing. Optical and transmission electron microscopes were used for morphological and microstructural analysis. The effect of milling time on powder microhardness, Al lattice parameter, lattice microstrain and crystallite size was determined. It was shown that mechanical alloying of as-cast Al-10wt.%Zr alloy during 20 h leads to a complete dissolution of the primary tetragonal Al{sub 3}Zr crystals in aluminum. At the same time, the powder microhardness increases to 370 HV. Metastable cubic Al{sub 3}Zr phase nanoparticles precipitate from the Al solution due to its decomposition after annealing, however, the Al solid solution remains supersaturated and nanocrystalline. Compression tests at room temperature and at 300 °C showed that the strength values of the hot-pressed samples reach 822 MPa and 344 MPa, respectively. - Highlights: •As-cast Al-10 wt.% Zr alloy was mechanically alloyed with 5 vol.% nanodiamond. •The primary tetragonal Al{sub 3}Zr crystals were completely dissolved in Al after 20 h. •Cubic Al{sub 3}Zr phase nanoparticles precipitated from Al solution after aging. •The aged bulk material showed a high strength at room and elevated temperatures.

36 MATERIALS SCIENCE↗

On the dissolution of a borosilicate glass with the use of isotopic tracing – Insights into the mechanism for the long-term dissolution rate

An understanding of the mechanisms responsible for controlling the long-term corrosion rate of nuclear waste glass is paramount if reliable glass dissolution models are to be used to calculate the controlled release of radionuclides from nuclear waste glass under geologic disposal conditions. Additionally, understanding silicate glass dissolution is also important for natural glasses to understand the role from the dissolution of these glasses has on the composition of natural aquatic systems. Two general mechanisms appear to be responsible for the elemental release from glass to the surrounding biosphere - ion exchange (release principally of alkalis) and matrix dissolution (release of the structural components of the glass). Key unknowns related to these mechanisms are the impact of surface layers on the altered glass and how these layers participate in corrosion. To better understand the impact of these layers on glass corrosion, we made two glasses of the same elemental composition, but with selected elements enriched in specific isotopes, e.g. more 10 B than 11 B. We reacted these glasses for 1 y then the solutions from each were exchanged and the chemistry of the solutions and the solids were followed for another 2 y and in some cases 3 y. This allowed us to follow changes in the glasses with respect to these elements and how these elements were transported through the alteration layers with time and, for at least one element, into the glass. Results from these experiments demonstrate that the release behavior of different elements is strongly dependent on their structural role in the glass (e.g. network formers and modifiers), but, more importantly, the role of water transport and subsequent ion exchange has in the long-term dissolution of the glass studied here. In this article, we highlight the behavior of four elements: lithium, sodium, silicon, and boron. Lithium and sodium, network modifying elements, have similar chemistries. The behavior of Li could be tracked in more detail by following both 6 Li and 7 Li; Li penetrates through the gel layer in both directions without hinderance and into and released from the glass deeper than sodium. Silicon, a network forming element, reacts with the silica-rich alteration layer. Boron, a network forming element, does not accumulate in the gel or the pristine glass and has a very sharp elemental profile between the pristine glass and alteration layer. Boron, lithium, and sodium elemental profiles suggest that there is little if any transport control within the alteration layer. The correlation between the Li and Na profiles and that of a water species suggest that the limiting release is a steady state between the diffusion of a water species and matrix dissolution that results in a low release rate for alkali and this provides a steady driving force for the long-term dissolution of glass.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Technetium Stabilization in Low-Solubility Sulfide Phases: A Review

We report that technetium contamination remains a major environmental problem at nuclear reprocessing sites, e.g., the Hanford Site, Washington, USA. At these sites, Tc is present in liquid waste destined for immobilization in a waste form or has been released into the subsurface environment. The high environmental risk associated with Tc is due to its long half-life (214 000 years) and the mobility of the oxidized anionic species Tc(VII)O 4 - . Under reducing conditions, TcO 4 - is readily reduced to Tc(IV), which commonly exists as a relatively insoluble and therefore immobile, hydrous Tc-oxide (TcO 2 · n H 2 O). The stability of Tc(IV) sequestered as solid phases depends on the solubility of the solid and susceptibility to reoxidation to TcO 4 - , which in turn depend on the (biogeo)chemical conditions of the environment and/or nuclear waste streams. Unfortunately, the solubility of crystalline TcO 2 or amorphous TcO 2 ·H 2 O is still above the maximum contaminant level (MCL) established by the U.S. EPA (900 pCi/L), and the kinetics of TcO 2 oxidative dissolution can be on the order of days to years. In addition to oxygen, sulfur can form complexes that significantly affect the adsorption, solubility, and reoxidation potential of Tc, especially Tc(IV). The principal technetium sulfides are TcS 2 and Tc 2 S 7 , but much less is known about the mechanisms of formation, stabilization, and reoxidation of Tc-sulfides. A common assumption is that sulfides are less soluble than their oxyhydrous counterparts. Determination of the molecular structure of Tc 2 S 7 in particular has been hampered by the propensity of this phase to precipitate as an amorphous substance. Recent work indicates that the oxidation state of Tc in Tc 2 S 7 is Tc(IV), in apparent contradiction to its nominal stoichiometry. Technetium is relatively immobile in reduced sediments and soils, but in many cases the exact sink for Tc has not been identified. Experiments and modeling have demonstrated that both abiotic and biologic mechanisms can exert strong controls on Tc mobility and that Tc binding or uptake into sulfide phases can occur. These and similar investigations also show that extended exposure to oxidizing conditions results in transformation of sulfide-stabilized Tc(IV) to a Tc(IV)O 2 -like phase without formation of measurable dissolved TcO 4 - , suggesting a solid-state transformation in which Tc(IV)-associated sulfide is preferentially oxidized before the Tc(IV) cation. This transformation of Tc(IV)-sulfides to Tc(IV)-oxides may be the main process that limits remobilization of Tc as Tc(VII)O 4 - . The efficacy of the final waste form to retain Tc also strongly depends on the ability of oxidizing species to enter the waste and convert Tc(IV) to Tc(VII). Finally, many waste form designs are reducing (e.g., cementitious waste forms such as salt stone) and, therefore, attempt to restrict access of oxidizing species such that diffusion is the rate-limiting step in remobilization of Tc.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Understanding the Importance of Labile Fe(III) during Fe(II)-Catalyzed Transformation of Metastable Iron Oxyhydroxides

Transformation of metastable Fe(III) oxyhydroxides is a prominent process in natural environments and can be significantly accelerated by the coexisting aqueous Fe(II) (Fe(II) aq ). Recent evidence points to the solution mass transfer of labile Fe(III) (Fe(III) labile ) as the primary intermediate species of general importance. However, a mechanistic aspect that remains unclear is the dependence of phase outcomes on the identity of the metastable Fe(III) oxyhydroxide precursor. Here, we compared the coupled evolution of Fe(II) species, solid phases, and Fe(III) labile throughout the Fe(II)-catalyzed transformation of lepidocrocite (Lp) versus ferrihydrite (Fh) at equal Fe(III) mass loadings with 0.2–1.0 mM Fe(II) aq at pH = 7.0. Similar to Fh, the conversion of Lp to product phases occurs by a dissolution–reprecipitation mechanism mediated by Fe(III) labile that seeds the nucleation of products. Though for Fh we observed a transformation to goethite (Gt), accompanied by the transient emergence and decline of Lp, for initial Lp we observed magnetite (Mt) as the main product. Further, a linear correlation between the formation rate of Mt and the effective supersaturation in terms of Fe(III) labile concentration shows that Fe(II)-induced transformation of Lp into Mt is governed by the classical nucleation theory. When Lp is replaced by equimolar Gt, Mt formation is suppressed by opening a lower barrier pathway to Gt by heterogeneous nucleation and growth on the added Gt seeds. The collective findings add to the mechanistic understanding of factors governing phase selections that impact iron bioavailability, system redox potential, and the fate and transport of coupled elements.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Irradiation Effect on Noble Metal Particles in Water Using in situ Liquid Cell STEM Observation

During geologic disposal of spent nuclear fuel (SNF) in an engineered nuclear waste repository, once all other barriers have degraded, oxidizing may occur at the solid-water interface owing to a self-generated radiolytic field. The repository design includes large quantities of iron (Fe), that is anticipated to corrode under an anoxic environment, and generate hydrogen (H 2 ) gas. This H 2 gas is thought to be able to suppress the dissolution of SNF through a catalytic reaction with noble metal particles (NMP) that are pre-existing in the SNF. This interaction leads to the decomposition of the major oxidant, hydrogen peroxide (H 2 O 2 ). In conclusion, these processes are described in the Fuel Matrix Degradation (FMD) model that is being used to predict SNF degradation rates. The NMP, therefore, plays an important role within the FMD model.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Utilization of municipal solid waste incineration fly ash for sulfoaluminate cement clinker production

Highlights: > The replacement can be taken up to 30% of MSWI fly ash in the raw mix. > The novelty compositional parameters were defined, their optimum values were determined. > Expansive property of SAC is strongly depended on gypsum content. > Three leaching test methods are used to assess the environmental impact. - Abstract: The feasibility of partially substituting raw materials with municipal solid waste incineration (MSWI) fly ash in sulfoaluminate cement (SAC) clinker production was investigated by X-ray diffraction (XRD), compressive strength and free expansion ratio testing. Three different leaching tests were used to assess the environmental impact of the produced material. Experimental results show that the replacement of MSWI fly ash could be taken up to 30% in the raw mixes. The good quality SAC clinkers are obtained by controlling the compositional parameters at alkalinity modulus (C{sub m}) around 1.05, alumina-sulfur ratio (P) around 2.5, alumina-silica ratio (N) around 2.0{approx}3.0 and firing the raw mixes at 1250 deg. C for 2 h. The compressive strengths of SAC are high in early age while that develop slowly in later age. Results also show that the expansive properties of SAC are strongly depended on the gypsum content. Leaching studies of toxic elements in the hydrated SAC-based system reveal that all the investigated elements are well bounded in the clinker minerals or immobilized by the hydration products. Although some limited positive results indicate that the SAC prepared from MSWI fly ash would present no immediate thread to the environment, the long-term toxicity leaching behavior needs to be further studied.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Accelerated carbonation of steel slags in a landfill cover construction

Steel slags from high-alloyed tool steel production were used in a full scale cover construction of a municipal solid waste (MSW) landfill. In order to study the long-term stability of the steel slags within the final cover, a laboratory experiment was performed. The effect on the ageing process, due to i.e. carbonation, exerted by five different factors resembling both the material characteristics and the environmental conditions is investigated. Leaching behaviour, acid neutralization capacity and mineralogy (evaluated by means of X-ray diffraction, XRD, and thermogravimetry/differential thermal analysis, TG/DTA) are tested after different periods of ageing under different conditions. Samples aged for 3 and 10 months were evaluated in this paper. Multivariate data analysis was used for data evaluation. The results indicate that among the investigated factors, ageing time and carbon dioxide content of the atmosphere were able to exert the most relevant effect. However, further investigations are required in order to clarify the role of the temperature.

54 ENVIRONMENTAL SCIENCES↗

Manganese: The overlooked contaminant in the world largest mine tailings dam collapse

Manganese (Mn) is an abundant element in terrestrial and coastal ecosystems and an essential micronutrient in the metabolic processes of plants and animals. Mn is generally not considered a potentially toxic element due to its low content in both soil and water. However, in coastal ecosystems, the Mn dynamic (commonly associated with the Fe cycle) is mostly controlled by redox processes. Here, we assessed the potential contamination of the Rio Doce estuary (SE Brazil) by Mn after the world’s largest mine tailings dam collapse, potentially resulting in chronic exposure to local wildlife and humans. Estuarine soils, water, and fish were collected and analyzed seven days after the arrival of the tailings in 2015 and again two years after the dam collapse in 2017. Using a suite of solid-phase analyses including X-ray absorption spectroscopy and sequential extractions, our results indicated that a large quantity of Mn II arrived in the estuary in 2015 bound to Fe oxyhydroxides. Over time, dissolved Mn and Fe were released from soils when Fe III oxyhydroxides underwent reductive dissolution. Due to seasonal redox oscillations, both Fe and Mn were then re-oxidized to Fe III , Mn III , and Mn IV and re-precipitated as poorly crystalline Fe oxyhydroxides and poorly crystalline Mn oxides. In 2017, redox conditions (Eh: -47 ± 83 mV; pH: 6.7 ± 0.5) favorable to both Fe and Mn reduction led to an increase (~880%) of dissolved Mn (average for 2015: 66 ± 130 μg L -1 ; 2017: 582 ± 626 μg L -1 ) in water and a decrease (~75%, 2015: 547 ± 498 mg kg -1 ; 2017: 135 ± 80 mg kg -1 ) in the total Mn content in soils. The crystalline Fe oxyhydroxides content significantly decreased while the fraction of poorly ordered Fe oxides increased in the soils limiting the role of Fe in Mn retention. The high concentration of dissolved Mn found within the estuary two years after the arrival of mine tailings indicates a possible chronic contamination scenario, which is supported by the high levels of Mn in two species of fish living in the estuary. Our work suggests a high risk to estuarine biota and human health due to the rapid Fe and Mn biogeochemical dynamic within the impacted estuary.

54 ENVIRONMENTAL SCIENCES↗

Radiocarbon analysis as a method for verifying atmospheric CO 2 uptake during carbon mineralization

Sequestration of atmospheric CO 2 is required to constrain the warming of Earth’s climate. Carbon mineralization refers to the precipitation of carbonate minerals by reaction of CO 2 and Mg- and Ca-rich rocks; if the source of the CO 2 is atmospheric and the precipitated carbonate is protected from subsequent dissolution, this process at sufficient scale may be able to reliably draw down atmospheric greenhouse gas levels. Such reactions occur passively in ultramafic settings and previous work has demonstrated that they actively draw down local CO 2 (g) concentrations. However, a method for unambiguously attributing the sequestered carbon solid product to atmospheric sources is still lacking. Here, we test if radiocarbon can be used to verify that the carbon being incorporated into carbonate minerals during carbon mineralization is atmospheric in origin. Additionally, samples from recently exposed ultramafic sites are analyzed and the results demonstrate the utility of this technique for verifying true atmospheric carbon reduction.

58 GEOSCIENCES↗

Effects of alloying elements on the formation of < c >-component loops in Zr alloy Excel under heavy ion irradiation.

We report here the microstructural changes occurring in the zirconium alloy Excel (Zr-3.5 wt% Sn-0.8Nb-0.8Mo-0.2Fe) during heavy ion irradiation. In situ irradiation experiments were conducted at reactor operating temperatures on two Zr Excel alloy microstructures with different states of alloying elements, with the states achieved by different solution heat treatments. In the first case, the alloying elements were mostly concentrated in the beta (beta) phase, whereas, in the second case, large Zr-3(Mo,Nb,Fe)(4) secondary phase precipitates (SPPs) were grown in the alpha (alpha) phase by long term aging. The heavy ion induced damage and resultant compositional changes were examined using transmission electron microscopy (TEM) in combination with scanning transmission electron microscope (STEM)-energy dispersive x-ray spectroscopy (EDS) mapping. Significant differences were seen in microstructural evolution between the two different microstructures that were irradiated under similar conditions. Nucleation and growth of < c >-component loops and their dependence on the alloying elements are a major focus of the current investigation. It was observed that the < c >-component loops nucleate readily at 100, 300, and 400 degrees C after a threshold incubation dose (TID), which varies with irradiation temperature and the state of alloying elements. It was found that the TID for the formation of < c >-component loops increases with decrease in irradiation temperature. Alloying elements that are present in the form of SPPs increase the TID compared to when they are in the beta phase solid solution. Dose and temperature dependence of loop size and density are presented. Radiation induced redistribution and clustering of alloying elements (Sn, Mo, and Fe) have been observed and related to the formation of < c >-component loops. It has been shown that at the higher temperature tests, irradiation induced dissolution of precipitates occurs whereas irradiation induced amorphization occurs at 100 degrees C. Furthermore, dose and temperature seem to be the main factors governing the dissolution of SPPs and redistribution of alloying elements, which in turn controls the nucleation and growth of < c >-component loops. The correlation between the microstructural evolution and microchemistry has been found by EDS and is discussed in detail.

Idrees, Yasir↗

Microstructure, microstructural stability and mechanical properties of sand-cast Mg–4Al–4RE alloy

This paper presents a methodology for assessing the phase composition and the results of structural stability tests of the sand-cast Mg–4Al–4RE alloy after annealing it at 175 and 250 °C for 3000 h. The microstructure was analyzed with optical, scanning electron, and transmission electron microscopy. The phase composition was determined with X-ray diffraction. The structure of the Mg–4Al–4RE (AE44) alloy is composed of large grains of α-Mg solid solution, needle-shaped precipitates of the Al{sub 11}RE{sub 3}phase, polyhedral precipitates of the Al{sub 2}RE phase and Al{sub 10}RE{sub 2}Mn{sub 7} phase. After annealing at 175 °C for 3000 h, no changes in the alloy structure are observed, whereas after annealing at 250 °C the precipitates of the Al{sub 11}RE{sub 3} phase are found to be in the initial stages of spheroidization. The coarse-grained structure and unfavorable morphology of the intermetallic phases in the sand-cast AE44 alloy, which are caused by low solidification rates, result in low creep resistance up to 200 °C and low mechanical properties at ambient temperature and at 175 °C. - Highlights: • Complement the knowledge about the microstructure of Mg-Al-RE alloys. • Clarify the mechanism of formation of Mg17Al12 phase above 180 °C. • Applying a chemical dissolution of the α-Mg in order to phase identification. • Applying a statistical test to assess the spheroidization of precipitates. • Quantitative description of microstructure of Mg-Al-RE alloys.

36 MATERIALS SCIENCE↗

Lithium oxidation and electrolyte decomposition at Li-metal/liquid electrolyte interfaces

In this work, we examine the evolution of events occurring when a Li metal surface is in contact with a 2 M solution of a Li salt in a solvent or mixture of solvents, via classical molecular dynamics simulations with a reactive force field allowing bond breaking and bond forming. The main events include Li oxidation and electrolyte reduction along with expansion of the Li surface layers forming a porous phase that is the basis for the formation of the solid-electrolyte interphase (SEI) components. Nucleation of the main SEI components (LiF, Li oxides, and some organics) is characterized. The analysis clearly reveals the details of these physical–chemical events as a function of time, during 20 nanoseconds. The effects of the chemistry of the electrolyte on Li oxidation and dissolution in the liquid electrolyte, and SEI nucleation and structure are identified by testing two salts: LiPF 6 and LiCF 3 SO 3 , and various solvents including ethers and carbonates and mixtures of them. The kinetics and thermodynamics of Li 6 F, the core nuclei in the LiF crystal, are studied by analysis of the MD trajectories, and via density functional theory calculations respectively. The SEI formed in this computational experiment is the “native” film that would form upon contact of the Li foil with the liquid electrolyte. As such, this work is the first in a series of computational experiments that will help elucidate the intricate interphase layer formed during battery cycling using metal anodes.

25 ENERGY STORAGE↗

Separation and Speciation of Mercury from Hanford 241-AP-107 Tank Waste Supernatant

Mercuric nitrate, Hg(NO 3 ) 2 , was introduced into the Hanford flowsheet when it was used to catalyze nitric acid dissolution of certain aluminum alloy fuels and to suppress radioiodine volatilization during nitric acid dissolution of short-cooled uranium metal fuel. Inventory estimates, based primarily on Hanford process-knowledge, suggest a total mercury inventory of 2,100 kg 1 in the Hanford Tank Farms. Aside from the obvious human exposure concerns via tank vapors, mercury species in the tank waste liquid and solid fraction pose risk to the implementation and execution of the River Protection Project mission due to mercury limits imposed under waste acceptance criteria, toxicity characteristic leaching procedure restrictions for secondary waste disposal, and air emission permits. Although there is currently no processing of tank waste at Hanford, waste processing is imminent and representative mercury inventory tracking will be important to anticipate and mitigate stack emissions and secondary liquid waste disposal issues like those experienced at the Savannah River Site.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

TANK 7 CHARACTERIZATION AND WASHING STUDIES

A 3-L PUREX sludge sample from Tank 7 was characterized and then processed through a series of inhibited water washes to remove oxalate, sodium, and other soluble ions. Current plans use Tank 7 as one of the feed sources for Sludge Batch 7 (SB7). Tank 7 is high in oxalate due to the oxalic acid cleaning of the sludge heels from Tanks 5 and 6 and subsequent transfer to Tank 7. Ten decant and nine wash cycles were performed over a 47 day period at ambient temperature. Initially, seven decants and seven washes were completed based on preliminary estimates of the number of wash cycles required to remove the oxalate in the sludge. After reviewing the composition data, SRNL recommended the completion of 2 or 3 more decant/wash cycles to ensure all of the sodium oxalate had redissolved. In the first 7 washes, the slurry oxalate concentration was 12,300 mg/kg (69.6% oxalate removal compared to 96.1% removal of the other soluble ions). After all ten decants were complete, the slurry oxalate concentration was 3,080 mg/kg (89.2% oxalate removal compared to 99.0% of the other soluble ions). The rate of dissolution of oxalate increased significantly with subsequent washes until all of the sodium oxalate had been redissolved after seven decant/wash cycles. The measured oxalate concentrations agreed very well with LWO predictions for washing of the Tank 7 sample. Highlights of the analysis and washing of the Tank 7 sample include: (1) Sodium oxalate was detected in the as-received filtered solids. 95% of the oxalate was insoluble (undissolved) in the as-received slurry. (2) No sodium oxalate was detected in the post-wash filtered solids. (3) Sodium oxalate is the last soluble species that redissolves during washing with inhibited water. In order to significantly reduce the sodium oxalate concentration, the sludge must be highly washed, leaving the other soluble anions and cations (including sodium) very low in concentration. (4) The post-wash slurry had 1% of the soluble anions and cations remaining, with the exception of sodium and oxalate, for which the percentages were 2.8% and 10.8% respectively. The post-wash sodium concentration was 9.25 wt% slurry total solids basis and 0.15 M supernate. (5) The settling rate of slurry was very fast allowing the completion of one decant/wash cycle each day. (6) The measured yield stress of as-received (6.42 wt% undissolved solids) and post-wash (7.77 wt% undissolved solids) slurry was <1 Pa. For rapidly settling slurries, it can be hard to measure the yield stress of the slurry so this result may be closer to the supernate result than the slurry. The recommended strategy for developing the oxalate target for sludge preparation for Sludge Batch 7 includes the following steps: (1) CPC simulant testing to determine the percent oxalate destruction and acid mix needed to produce a predicted redox of approximately 0.2 Fe{sup +2}/{Sigma}Fe in a SME product while meeting all DWPF processing constraints. (2) Perform a DWPF melter flammability assessment to ensure that the additional carbon in the oxalate together with other carbon sources will not lead to a flammability issue. (3) Perform a DWPF glass paper assessment to ensure the glass produced will meet all DWPF glass limits due to the sodium concentration in the sludge batch. The testing would need to be repeated if a significant CPC processing change, such as an alternative reductant to formic acid, is implemented.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

SEI formation mechanisms and Li + dissolution in lithium metal anodes: Impact of the electrolyte composition and the electrolyte-to-anode ratio

The lithium metal battery is one of today's most promising high-energy-density storage devices. Its full-scale implementation depends on solving operational and safety issues intrinsic to the Li metal high reactivity leading to uncontrolled electrolyte decomposition and uneven Li deposition. In this work, we study the spontaneous formation of the solid electrolyte interphase (SEI) upon contact of Li metal with the electrolyte and describe the heterogeneous SEI morphological features. Multiple electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethoxyethane (DME), dimethyl carbonate (DMC), 1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) and bis(2,2,2-trifluoroethyl) ether (BTFE) are used. Findings include the description of the SEI evolution from dispersed LiO, LiS, LiN, and LiF clusters to a continuous and compact inorganic phase in which the LiO and LiF content depend on the presence of fluorine diluents. Further, the role of the DME ether solvent helping the growth of a “wet-SEI” is compared to that of the highly unstable carbonate DMC, which decomposes into complex radical oligomers that might contribute to further electrolyte decomposition. The impact of the electrolyte-to-anode ratio on LiFSI decomposition is highlighted. Finally, we suggest the existence of a critical LiFSI concentration and electrolyte-to-anode ratio that could potentially balance the rate of electrolyte depletion and lithium consumption.

25 ENERGY STORAGE↗

Chemical durability of multicomponent lanthanide zirconate solid solutions

Multicomponent zirconate solid solutions A 2 Zr 2 O 7 (A= (Sm,Yb), (Sm,Yb,Gd), (Sm,Yb,Gd,Er), and (Sm,Yb,Gd,Er,Dy)) were synthesized through spark plasma sintering and their chemical durability was investigated via semi-dynamic leaching tests in pH = 1 nitric acid at 90°C. Incongruent dissolution occurred for all samples with the preferential elemental release of zirconium in all A 2 Zr 2 O 7 except for high entropy (Sm,Yb,Gd,Er,Dy)Zr 2 O 7 which displays a congruent release of the A-site elements and Zr. A strong positive correlation was found between the lanthanide elemental release rates and the A-site cation size disorder, whereas a negative correlation was observed between the elemental release rates and mixing entropy.

36 MATERIALS SCIENCE↗