Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Stable magnesium zinc oxide by reactive Co-Sputtering for CdTe-based solar cells

Magnesium zinc oxide (MZO) is a promising front contact material for CdTe solar cells. Due to its higher band gap than traditional CdS, MZO can reduce parasitic absorption to significantly increase short-circuit current density while also providing a benefit of conduction band offset tuning through Mg:Zn ratio optimization. MZO has been successfully implemented into CdTe devices, however its stability has been of concern. The MZO stability issue has been attributed to the presence of oxygen in the CdTe device processing ambient, leading to double-diode behavior (S-kink) in the current density-voltage curves. Here we report on MZO thin films deposited by reactive co-sputtering. The reactively co-sputtered MZO thin films have encouraging stability, show no significant variation in work function of the surface over a period of 6 months, as measured by Kelvin probe. Energy conversion efficiencies of around 16% have been achieved both with and without presence of oxygen in device processing ambients across multiple research facilities. Finally, these efficiencies should be possible to increase further by tuning of the thin film deposition and device processing parameters, especially through optimization of the back contact.

14 SOLAR ENERGY↗

Probing layered structure of Inconel 625 coatings prepared by magnetron sputtering

Coating/substrate interface and oxide layers present in Inconel 625 film may cause significant impacts on its corrosion behavior. However, layered structure of Inconel 625 coatings remains poorly understood due to its requirement of high spatial resolution. Here we have applied X-ray reflectometry (XRR) to probe the layered structure of magnetron-sputtered Inconel 625 film with atomic spatial resolution. Our results indicate that there exists a 2 nm thick Cr-rich Inconel sublayer underneath the principal film. On top of the principal film, it is found a 2 nm thick oxide layer mainly consisting of NiO. In addition, we detected ~2 Å contamination layer on the sapphire substrate, although argon ion sputter cleaning had been applied to the substrate prior to deposition. By comparing the coatings with different deposition time, we observed that the thickness of principal Inconel 625 layer grows linearly with deposition time, with all other layers remaining constant. Our findings provide insight into the layered structures of Inconel 625 coatings with atomic-scale spatial resolution, and provide directions for future efforts that aim to improve the corrosion resistance of Inconel 625 coatings.

14 SOLAR ENERGY↗

Effect of substrate temperature on sputter-deposited boron carbide films

Sputter deposition of B4C films with tailored physical properties remains a challenge. Here, we systematically study how substrate temperature influences the properties of B4C films deposited by direct current magnetron sputtering onto planar substrates held at temperatures in the range of 100-510°C. Results show that all films are amorphous stoichiometric B4C, with low O content of ~1 at. %. Films deposited onto substrates at 100°C exhibit high compressive residual stress and decreased mechanical properties. Therefore, for elevated substrate temperatures in the range of 180-510°C, film mass density, surface roughness, Young’s modulus, and hardness are weakly dependent on substrate temperature. However, in this temperature range, an increase in substrate temperature leads to larger residual compressive stress accompanied by a corresponding reduction in the concentration of nanoscale inhomogeneities. At least for the landing atom ballistics conditions studied here, a substrate temperature range of ~185-250°C is optimum for growing films with near-zero intrinsic residual stress. The overall weak substrate temperature dependence of film properties revealed in this work is favorable for the development of a robust deposition process, particularly for the case of deposition onto non-planar substrates where temperature control is often challenging.

36 MATERIALS SCIENCE↗

Growth of microscopic cones on titanium cathodes of sputter-ion pumps driven by sorption of large argon quantities

Microscopic cones have been observed on titanium cathodes of sputter-ion pumps (SIPs) after pump operation. The cones were studied by means of scanning electron microscopy and energy dispersive x-ray analysis. Size and morphology of these cones are clearly correlated with the nature and the relative amount of each gas species pumped by each SIP during its working life. In particular, their growth was found to be fed by sputtering mechanisms, mostly during Ar pumping, and to be driven by the electromagnetic field applied to the Penning cells of each SIP. Experimental findings suggest that the formation and extent of such conic structures on cathode surfaces might play a leading role in the onset of phenomena typically related to the functioning of SIPs, e.g., the so-called argon instability.

36 MATERIALS SCIENCE↗

Self-sputtering far above the runaway threshold: an extraordinary metal ion generator

When self-sputtering is driven far above the runaway threshold voltage, energetic electrons are made available to produce"excess plasma" far from the magnetron target. Ionization balance considerations show that the secondary electrons deliver the necessary energy to the"remote" zone. Thereby, such a system can be an extraordinarily prolific generator of useable metal ions. Contrary to other known sources, the ion current to a substrate can exceed the discharge current. For gasless self-sputtering of copper, the useable ion current scales exponentially with the discharge voltage.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Time-Resolved Grazing Incidence X-Ray Absorption Spectroscopy for the In Situ Investigation of the Initial Stages of Sputter-Deposited Copper Thin Films

The sputter deposition and the growth of thin copper films on float glass substrates are in situ studied using grazing incidence, reflection mode X-ray absorption fine structure spectroscopy with subsecond time resolution. The experimental data are compared with model calculations, assuming the presence of crystalline, face-centered cubic metallic Cu nanostructures. From a detailed analysis of the measured spectra, the film thickness as well as the surface roughness is determined, leading to a detailed understanding of the films growth as a function of the sputter deposition time. In particular, different stages of film growth can clearly be distinguished from the fits of the experimental data. The results suggest the formation of isolated, approximately nm-sized copper clusters in the initial phase of the film deposition for the first few seconds, a coalescence phase with a nominal thickness of ≈1.5–2.8 nm, constant roughness of about 1.4 nm for the subsequent ≈5 s, and finally 3D growth of the Cu crystallites in the film for later stages of film growth. Further prospects of the methodology are given.

36 MATERIALS SCIENCE↗

Stoichiometry of Silicon Dioxide Films Obtained by Ion-Beam Sputtering

The composition of SiO{sub x} films produced by ion-beam sputtering (IBS) of silicon and quartz targets were studied by infrared spectrometry. Films with thicknesses of 150–390 nm were formed on silicon substrates. It was found that increase in the partial pressure of oxygen in the working gas, increase in the temperature of the substrate, and the presence of a positive potential on the target during reactive IBS of silicon shifted the main absorption band ν{sub as} into the high-frequency region and increased the composition index from 1.41 to 1.85. During IBS of a quartz target the stoichiometry of the films deteriorates with increase of the energy of the sputtering argon ions. This may be due to increase of the deposition rate. Increase in the current of the thermionic compensator, increase of the substrate temperature, and addition of oxygen led to the formation of SiO{sub x} films with improved stoichiometry.

36 MATERIALS SCIENCE↗

Properties of Molybdenum Films Produced by High-Power Impulse Magnetron Sputtering

Results of experiments on deposition of thin molybdenum films on glass substrates by high-power impulse magnetron sputtering are presented. Two high-current modes with different pulse frequencies and durations are used. Properties of the produced molybdenum films are compared with those of films produced by magnetron sputtering at a direct current. It is shown that this method allows the resistivity of molybdenum films to be decreased and their reflectance in the visible range to be increased.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thermodynamic Investigation of the Effect of Target Compositions and Conditions of Their Magnetron Sputtering on Phase Compositions of the Resulting Films

A thermodynamic investigation of plasmochemical processes taking place in a magnetron during sputtering of the targets consisting of indium and dysprosium ions is performed, which allowed identifying the feasibility of forming under the given conditions certain amounts of the chemical compounds In{sub 2}O{sub 3}, Dy{sub 2}O{sub 3}, DyInO{sub 3}. In the thermodynamic analysis of the equilibrium compositions during magnetron sputtering of the films, a universal TERRA software program is used.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Investigation of Corrosion Behavior of Ti/TiN Multilayers on Al7075 Deposited by High-Vacuum Magnetron Sputtering in 3.5% NaCl Solution

Although Al 7075 has many favorable mechanical properties such as the large strength-to-weight ratio, the relatively poor corrosion resistance has restricted industrial applications. In this work, Ti/TiN as hard multilayered and nanostructured coatings are deposited on the relatively soft Al 7075 structure by high-vacuum radio-frequency magnetron sputtering and the phase, structure, and morphology are investigated in details. The corrosion behavior is evaluated by electrochemical impedance spectroscopy in 3.5% NaCl at a pH of 7.5 for 1, 6, 12, 24, 36, 48, 60, and 72 h. At time points of 1, 6, 12, and 24 h, primary oxide layers and double layers are formed, but the corrosive medium penetrates the primary titanium nitride columnar structure. At longer time points of 24, 36, 48, 60, and 72 h, formation of stronger oxide and double layers leads to better corrosion resistance which is 14.8 times better than that observed from the uncoated substrate after immersion for 36 h. According to R{sub ct}, the corrosion resistances of the short and long immersion groups are 808.5-1984 and 808.5-1248 kΩ cm{sup 2}, respectively, thereby confirming the effectiveness of the Ti/TiN coating against corrosion in comparison with the corrosion resistance of 84.3 kΩ cm{sup 2} observed from the uncoated Al 7075. The smallest corrosion resistance of 808.5 kΩ cm{sup 2} observed at the time point of 24 h is 9.6 times that of the uncoated substrate. Graphical Abstract: A 1.4-µm-thick Ti/TiN hard nanostructured coating comprising six layers is deposited on the relatively soft Al 7075 substrate by high-vacuum radio-frequency magnetron sputtering at 100 °C. The first layer of the intermediate Ti layer cannot improve the corrosion resistance of the TiN super hard coating with a columnar structure. The second and third intermediate Ti layers play an important role in improving the corrosion resistance of Al 7075 by obstructing defects and coating damage from aggressive Cl{sup −} ions and penetration of water. The mechanism involves self-healing of defects by oxide formation and Warburg resistance by diffusion control. .

36 MATERIALS SCIENCE↗

Sputter-Deposited Mo Thin Films: Multimodal Characterization of Structure, Surface Morphology, Density, Residual Stress, Electrical Resistivity, and Mechanical Response

Multimodal datasets of materials are rich sources of information which can be leveraged for expedited discovery of process–structure–property relationships and for designing materials with targeted structures and/or properties. For this data descriptor article, we provide a multimodal dataset of magnetron sputter-deposited molybdenum (Mo) thin films, which are used in a variety of industries including high temperature coatings, photovoltaics, and microelectronics. In this dataset we explored a process space consisting of 27 unique combinations of sputter power and Ar deposition pressure. Here, the phase, structure, surface morphology, and composition of the Mo thin films were characterized by x-ray diffraction, scanning electron microscopy, atomic force microscopy, and Rutherford backscattering spectrometry. Physical properties—namely, thickness, film stress and sheet resistance—were also measured to provide additional film characteristics and behaviors. Additionally, nanoindentation was utilized to obtain mechanical load-displacement data. The entire dataset consists of 2072 measurements including scalar values (e.g., film stress values), 2D linescans (e.g., x-ray diffractograms), and 3D imagery (e.g., atomic force microscopy images). An additional 1889 quantities, including film hardness, modulus, electrical resistivity, density, and surface roughness, were derived from the experimental datasets using traditional methods. Minimal analysis and discussion of the results are provided in this data descriptor article to limit the authors’ preconceived interpretations of the data. Overall, the data modalities are consistent with previous reports of refractory metal thin films, ensuring that a high-quality dataset was generated. The entirety of this data is committed to a public repository in the Materials Data Facility.

36 MATERIALS SCIENCE↗

Sputtering of neutral clusters from silver-gold alloys.

Polycrystalline Ag, Ag{sub 20}Au{sub 80}, Ag{sub 40}Au{sub 60}, Ag{sub 80}Au{sub 20} and Au samples were bombarded with 15 keV Ar{sup +} at 60{sup o} incidence and the resulting secondary neutral yield distribution was studied by non-resonant laser post-ionization mass spectrometry. Neutral clusters containing up to 21 atoms were observed for the targets. The yield of neutral clusters, Ag{sub m}Au{sub n-m}, containing n atoms, Y{sub n}, was found to follow a power in n, i.e. Y{sub n} {proportional_to} n{sup -{delta}}, where the exponent {delta} varied from 3.2 to 4.0. For a fixed n, the cluster yields showed a variation with number of gold atoms similar to that expected for a binomial distribution. In addition, the cluster compositions from the sputtered alloys were indicative of sputtering from a gold rich surface.

36 MATERIALS SCIENCE↗

Growth, microstructure and electrical properties of sputter-deposited hafnium oxide (HfO2) thin films grown using HfO2 ceramic target

Hafnium oxide (HfO₂) thin films have been made by radio-frequency (rf) magnetron-sputtering onto Si(100) substrates under varying growth temperature (Ts). HfO₂ ceramic target has been employed for sputtering while varying the Ts from room temperature to 500⁰C during deposition. The effect of Ts on the growth and microstructure of deposited HfO₂ films has been studied using grazing incidence x-ray diffraction (GIXRD), X-ray photoelectron spectroscopy (XPS), and high-resolution scanning electron microscopy (HR-SEM) coupled with energy dispersive x-ray spectrometry (EDS). The results indicate that the effect of Ts is significant on the growth, surface and interface structure, morphology and chemical composition of the HfO₂ films. Structural characterization indicates that the HfO₂ films grown at Ts<200 ⁰C are amorphous while films grown at Ts>200 ⁰C are nanocrystalline. An amorphous-to-crystalline transition occurs at Ts=200 ⁰C. Nanocrystalline HfO₂ films crystallized in a monoclinic structure with a (-111) orientation. XPS measurements indicated the high surface-chemical quality and stoichiometric nature of the grown HfO₂ films. An interface layer (IL) formation occurs due to reaction at the HfO₂-Si interface for HfO₂ films deposited at Ts>200 ⁰C. The thickness of IL increases with increasing Ts. XPS and EDS at the HfO₂-Si cross-section indicate the IL is a (Hf, Si)-O compound. The electrical characterization using capacitance-voltage measurements indicate that the dielectric constant decreases from 25 to 16 with increasing Ts.

36 MATERIALS SCIENCE↗

Effects of sample bias on adhesion of magnetron sputtered Cr coatings on SiC

Swelling of SiC at 300 C due to in-service neutron irradiation causes tensile residual stresses in coatings which are expected to adversely affect the performance of coated SiC composite fuel cladding for light water reactors. Matching the coating swelling with the substrate, a solution common for thermal expansion, is not practical in the case of neutron irradiation. Biasing samples during magnetron sputtering deposition induces compressive residual stress which may counteract this. In this study, chromium coatings were deposited on SiC by DC magnetron sputtering with no external heating at bias voltages of –50V, –75V, and –100V. The effects of the bias voltage on morphology, residual stress, microstrain, texture, and adhesion are shown. The low deposition temperature resulted in the coating microstructure evolution following an energetic particle bombardment dominated trend. Additionally, at the two lower bias voltages knock-on implantation dominated increasing the residual stress and microstrain while at the highest bias voltage, thermal spike migration allowed for defect relaxation. When the knock-on induced compressive residual stress exceeded 0.8 GPa microcrack formation in the SiC substrate decreased coating adhesion. While no microcracks formed at the lowest bias voltage, insufficient atomic mobility during coating growth lead to voids forming in the coating. A balance is needed to form void-free coatings that have high compressive residual stress.

36 MATERIALS SCIENCE↗

Effects of substrate temperature on properties of ITO-ZnO composition spread films fabricated by combinatorial RF magnetron sputtering

We have fabricated ITO-ZnO composition spread films to investigate the effects of substrate temperature on their electrical and optical properties by using combinatorial RF magnetron sputtering. It turned out by X-ray measurement that the film with zinc contents above 16.0 at% [Zn/(In+Zn+Sn)] showed amorphous phase regardless of substrate temperature. The amorphous ITO-ZnO film had lower resistivity than polycrystalline films. When the films were deposited at 250 deg. C, the minimum resistivity of 3.0x10{sup -4} OMEGA cm was obtained with the zinc contents of 16.0 at%. The indium content could be reduced as high as {approx}30 at% compared to that of ITO for the films having similar resistivity ({approx}10{sup -4} OMEGA cm). However, a drastic increase of resistivity was observed for the ITO-ZnO films deposited at 350 deg. C, having zinc contents below 15.2 at%. - Graphical abstract: The effects of substrate temperature on properties of ITO-ZnO films were investigated by using combinatorial RF magnetron sputtering. The amorphous ITO-ZnO film had lower resistivity than polycrystalline films. The minimum resistivity of 3.0x10{sup -4} OMEGA cm was obtained with the substrate temperature of 250 deg. C and the zinc contents of 16.0 at%. The electronic states of ITO-ZnO films were discussed with related to the formation of transparent amorphous oxide semiconductor (TAOS).

36 MATERIALS SCIENCE↗

Combinatorial study of WInZnO films deposited by rf magnetron co-sputtering

The compositional dependence of co-sputtered tungsten indium zinc oxide (WInZnO) film properties was first investigated by means of a combinatorial technique. Indium zinc oxide (IZO) and WO{sub 3} targets were used with different target power. W composition ratio [W/(In+Zn+W)] was varied between 3 and 30 at% and film thickness was reduced as the sample position moved toward WO{sub 3} target. Furthermore, the optical bandgap energy increased gradually, which might be affected by the reduction in film thickness. All the WInZnO films showed an amorphous phase regardless of the W/(In+Zn+W) ratio. As the W/(In+Zn+W) ratio in WInZnO films increased, the carrier concentration was restricted, causing the increase in electrical resistivity. W cations worked as oxygen binders in determining the electronic properties, resulting in suppressing the formation of oxygen vacancies. Consequentially, W metal cations were effectively incorporated into the WInZnO films as a suppressor against the oxygen vacancies and the carrier generation by employing the combinatorial technique. - Graphical abstract: The film thickness and the sheet resistance (R{sub s}) with respect to the sample position of WInZnO films, which is compositionally graded by rf power for each target, are exhibited. Highlights: > The compositional dependence of co-sputtered WInZnO film properties is first investigated. > W cations work as oxygen binders in determining the electronic properties. > All the WInZnO films show an amorphous phase regardless of the W/(In+Zn+W) ratio. > W metal cations are effectively incorporated into the WInZnO films by the combinatorial technique.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of annealing on Curie temperature and phase transition in La{sub 0.55}Sr{sub 0.08}Mn{sub 0.37}O{sub 3} epitaxial films grown on SrTiO{sub 3} (100) substrates by reactive radio frequency magnetron sputtering

Mn-poor LaSrMnO{sub 3} (LSMO) epitaxial films were grown on SrTiO{sub 3} (100) substrates by radio frequency magnetron sputtering in an argon and oxygen gas mix, and then the samples were annealed in air at various temperatures (T{sub a}). 2 theta-chi X-ray diffraction mapping, nano-beam diffraction analysis through transmission electron microscopy, and electron back scatter diffraction through scanning electron microscopy revealed that the crystal symmetry of the LSMO films changed from monoclinic/orthorhombic to rhombohedral on annealing in air. Curie temperature (T{sub C}) of the LSMO films was found to increase with increasing T{sub a}, and become higher than the room temperature at T{sub a} ≥ 861 °C, indicating that the cause of these changes was the filling of oxygen and the transition of the crystal symmetry into rhombohedral. - Highlights: •Mn-poor LSMO changed from monoclinic/orthorhombic to rhombohedral by oxygen supply. •Mn-poor LSMO was increased T{sub C} by changed crystal symmetry, and it showed T{sub C} above RT. •Annealed in air effectively supplied O{sub 2} more than O{sub 2} gas during sputtering •EBSD is useful to evaluate crystal symmetry of complex oxide film from the substrate.

36 MATERIALS SCIENCE↗

Recrystallization and martensitic transformation in nanometric grain size Cu-Al-Ni thin films grown by DC sputtering at room temperature

Highlights: • Polycrystalline Cu-Al-Ni thin films with nanometric grain size are grown by DC sputtering. • Influence of thermal annealing process at low temperatures on the microstructure is analyzed. • Strained martensitic transformation is observed for films with grain size average of 30 nm. - Abstract: We report the recrystallization of metastable hexagonal and body centered cubic BCC phase in free-standing 6 μm thick Cu-Al-Ni films grown by DC sputtering at room temperature. The results show that the BCC phase recrystallizes to L2{sub 1} at around 533 K together with precipitation of γ{sub 2}-phase. Annealing temperatures (533 K–623 K) at short times (0–30 min) produce systematic increment of the fraction of γ{sub 2}-phase. Films with phase coexistence of hexagonal, γ{sub 2} and L2{sub 1} structure display temperature driven martensitic transformation. This transformation is observed for samples with austenite grain size of around 30 nm. In all cases, the martensitic transformation temperature (M{sub S}) notoriously decreases (compared to bulk) and systematically increases with the annealing temperatures and annealing time. In addition, the films display extended transformation and retransformation ranges along with asymmetric hysteresis, which may be associated to restitutive forces due to elastic deformations at martensite – martensite and martensite – austenite interfaces. Annealing temperatures above 623 K produce fast precipitation to equilibrium α- and γ{sub 2}-phases. The austenitic phase can be recovered after annealing over 1000 K and fast quenching in ice-water.

77 NANOSCIENCE AND NANOTECHNOLOGY↗