Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Optical Microscopy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Effect of a copper filler metal on the microstructure and mechanical properties of electron beam welded titanium-stainless steel joint

Cracking in an electron beam weld of titanium to stainless steel occurred during the cooling process because of internal thermal stress. Using a copper filler metal, a crack free joint was obtained, which had a tensile strength of 310 MPa. To determine the reasons for cracking in the Ti/Fe joint and the function of the copper filler metal on the improvement of the cracking resistance of the Ti/Cu/Fe joint, the microstructures of the joints were studied by optical microscopy, scanning electron microscopy and X-ray diffraction. The cracking susceptibilities of the joints were evaluated with microhardness tests on the cross-sections. In addition, microindentation tests were used to compare the brittleness of the intermetallics in the welds. The results showed that the Ti/Fe joint was characterized by continuously distributed brittle intermetallics such as TiFe and TiFe(Cr){sub 2} with high hardness ({approx} 1200 HV). For the Ti/Cu/Fe joint, most of the weld consisted of a soft solid solution of copper with dispersed TiFe intermetallics. The transition region between the weld and the titanium alloy was made up of a relatively soft Ti-Cu intermetallic layer with a lower hardness ({approx} 500 HV). The formation of soft phases reduced the cracking susceptibility of the joint. - Highlights: Black-Right-Pointing-Pointer Electron beam welded Ti/Fe joint cracked for the brittleness and residual stress. Black-Right-Pointing-Pointer Electron beam welded Ti/Cu/Fe joint with tensile strength of 310 MPa was obtained. Black-Right-Pointing-Pointer Cu diluted Ti and Fe contents in weld and separated the TiFe{sub 2} into individual blocks. Black-Right-Pointing-Pointer Interfacial hard Ti-Fe compounds were replaced by soft Ti-Cu compounds in the weld. Black-Right-Pointing-Pointer A large amount of solid solution of copper formed in the weld.

36 MATERIALS SCIENCE↗

Microstructural Characterization of Irradiated U{sub 0.17}ZrH{sub 1.6} Using Ultrasonic Techniques

In recent years, there has been an increased level of effort to understand the changes in microstructure that occur due to irradiation of nuclear fuel. The primary driver for this increased effort is the potential for designing new fuels that are safer and more reliable, in turn enabling new and improved reactor technologies. Much of the data on microstructural change in irradiated fuels is generated through a host of post irradiation examination techniques such as optical microscopy (OM), scanning electron microscopy (SEM), and transmission electron microscopy (TEM) to determine grain structure, porosity, crack geometry, etc. in irradiated fuels. Such 'traditional' examination techniques were recently used to characterize a novel new fuel consisting of U{sub 0.17}ZrH{sub 1.6} pellets bonded to zircaloy-2 cladded with lead-bismuth eutectic before and after irradiation. In addition to the conventional suite of post-irradiation examination tools, several nondestructive interrogation techniques exist which bring the potential for in-situ assessment of microstructural changes. One such method, ultrasonic examination, was tested on each of the samples. This paper describes the results of this examination. Ultrasonic measurements have a long and successful history of use for nondestructive materials characterization, including nondestructive evaluation (NDE) of degradation and damage, microstructure characterization, and measurement of physical parameters for process control. Ultrasonic NDE is critical to the nuclear power industry's in-service inspection program for maintaining pressure boundary integrity, and is being actively investigated for PIE of fuels. Ultrasonic measurements, typically performed at 10 MHz or higher, performed post irradiation show that fuel microstructural parameters, such as porosity and grain size, can be correlated to ultrasonic velocity. The objective of this examination was to assess the feasibility of using ultrasonic measurements on irradiated fuel to determine sensitivity to microstructural changes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Well-aligned polycrystalline lanthanum silicate oxyapatite grown by reactive diffusion between solid La{sub 2}SiO{sub 5} and gases [SiO+1/2O{sub 2}]

The c-axis-oriented polycrystalline lanthanum silicate oxyapatite, La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} (□ denotes a vacancy in the Si site), was successfully prepared by the reactive diffusion between randomly grain-oriented La{sub 2}SiO{sub 5} polycrystal and [SiO+1/2O{sub 2}] gases at 1873 K in Ar atmosphere. The polycrystal was characterized using optical microscopy, scanning electron microscopy equipped with energy dispersive X-ray spectroscopy, micro-Raman spectroscopy, X-ray diffractometry, and impedance spectroscopy. The crystal structure (space group P6{sub 3}/m) showed the deficiency of Si site at ca. 1.9%. The bulk oxide-ion conductivity along the grain-alignment direction steadily increased from 9.2 × 10{sup −3} to 1.17 × 10{sup −2} S/cm with increasing temperature from 923 to 1073 K. The activation energy of conduction was 0.23(2) eV. - Graphical abstract: We have successfully prepared the highly c-axis-oriented polycrystalline La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} by the reactive diffusion between randomly grain-oriented La{sub 2}SiO{sub 5} polycrystal and [SiO + 1/2O{sub 2}] gases at 1873 K in Ar atmosphere. The crystal structure (space group P6{sub 3}/m) showed the deficiency of Si site of ca. 1.9%. - Highlights: • The c-axis-oriented polycrystalline La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} is successfully prepared. • Crystal structure of La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} is determined by single-crystal XRD. • The polycrystal shows relatively high oxide ion conductivity along the common c-axis. • Reactive diffusion is successfully used for the preparation of grain-aligned ceramics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dielectric strength of parylene HT

The dielectric strength of parylene HT (PA-HT) films was studied at room temperature in a wide thickness range from 500 nm to 50 μm and was correlated with nano- and microstructure analyses. X-ray diffraction and polarized optical microscopy have revealed an enhancement of crystallization and spherulites development, respectively, with increasing the material thickness (d). Moreover, a critical thickness d{sub C} (between 5 and 10 μm) is identified corresponding to the beginning of spherulite developments in the films. Two distinct behaviors of the dielectric strength (F{sub B}) appear in the thickness range. For d ≥ d{sub C}, PA-HT films exhibit a decrease in the breakdown field following a negative slope (F{sub B} ∼ d{sup −0.4}), while for d < d{sub C}, it increases with increasing the thickness (F{sub B} ∼ d{sup 0.3}). An optimal thickness d{sub optim} ∼ 5 μm corresponding to a maximum dielectric strength (F{sub B} ∼ 10 MV/cm) is obtained. A model of spherulite development in PA-HT films with increasing the thickness is proposed. The decrease in F{sub B} above d{sub C} is explained by the spherulites development, whereas its increase below d{sub C} is induced by the crystallites growth. An annealing of the material shows both an enhancement of F{sub B} and an increase of the crystallites and spherulites dimensions, whatever the thickness. The breakdown field becomes thickness-independent below d{sub C} showing a strong influence of the nano-scale structural parameters. On the contrary, both nano- and micro-scale structural parameters appear as influent on F{sub B} for d ≥ d{sub C}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of cooling rate on the microstructure and microhardness of the CuZrAgAl alloy

The effect of cooling rate on the microstructure and microhardness of the Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} (at.%) alloy has been studied. The crystalline phases were characterized by X-ray diffraction, optical microscopy and scanning electron microscopy with energy dispersive X-ray spectroscopy, and identified as AlCu{sub 2}Zr, Cu{sub 10}Zr{sub 7} and CuZr{sub 2}. The solidification sequence was established as following: the Cu{sub 10}Zr{sub 7} phase forms first in the periphery of the rod, then following with AlCu{sub 2}Zr phase in the rod center and finally CuZr{sub 2} crystals in Cu-depleted areas. The effect of crystals on the mechanical properties of the Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} alloy was also estimated through the microhardness. According to the value of microhardness, inhomogeneous structure of the amorphous matrix is more easily formed for the alloy in the low cooling rate (i.e., 9 mm) as compared with the alloy with fully amorphous state in the large cooling rate (i.e., 3 mm). This inhomogeneous structure was attributed to the composition change of amorphous matrix arising from the forming of crystalline phases due to the low cooling rate. - Highlights: Black-Right-Pointing-Pointer The crystalline phases in the Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} alloy were identified. Black-Right-Pointing-Pointer The solidification sequence of Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} alloy was verified. Black-Right-Pointing-Pointer The softening and hardening of alloy could be observed due to the crystallization.

36 MATERIALS SCIENCE↗

Effect of Nb Content on Microstructures and Mechanical Properties of Ti-xNb-2Fe Alloys

β-Type Ti-Nb-based alloys exhibit satisfactory biocompatibility and low Young’s modulus for biomedical applications. The microstructure and mechanical properties of a series of Ti-(14, 16, 18, 20, 22, 24)Nb-2Fe alloys fabricated by arc melting were investigated by XRD, optical microscopy, and tensile tests. Both ω and α″ phases existed in the Ti-14Nb-2Fe alloy, while just a single β phase existed in the other alloys. Twinning is an important deformation mechanism that causes work hardening and twinning-induced plasticity. It was found in the Ti-(14, 16, 18, 20)Nb-2Fe alloys and not in the Ti-22Nb-2Fe alloy. The Ti-14Nb-2Fe alloy exhibited the highest tensile strength and the highest Young’s modulus owing to the existence of the ω phase. The tensile strength decreased gradually from 830 MPa (highest) for the Ti-14Nb-2Fe alloy to 540 MPa (lowest) for the Ti-24Nb-2Fe alloy with an increase in the Nb content. The Young’s modulus decreased from 90 GPa for the Ti-14Nb-2Fe alloy to 63 GPa for the Ti-22Nb-2Fe alloy and then increased to 71 GPa for the Ti-24Nb-2Fe alloy. Elongation shows the same trend as the Young’s modulus. The Ti-22Nb-2Fe alloy, with a low Young’s modulus of 63 GPa, tensile strength of 570 MPa, and 15% elongation, was found suitable for biomedical applications. The Ti-20Nb-2Fe alloy also exhibits a high tensile strength, a Young’s modulus ratio of 9.24 × 10{sup −3}, and 18% elongation and is thus considered another valuable Ti alloy for biomedical applications.

36 MATERIALS SCIENCE↗

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by super duplex filler metal

In the present paper, microstructural changes across an as-welded dissimilar austenitic/duplex stainless steel couple welded by a super duplex stainless steel filler metal using gas tungsten arc welding process is characterized with optical microscopy and electron back-scattered diffraction techniques. Accordingly, variations of microstructure, texture, and grain boundary character distribution of base metals, heat affected zones, and weld metal were investigated. The results showed that the weld metal, which was composed of Widmanstätten austenite side-plates and allotriomorphic grain boundary austenite morphologies, had the weakest texture and was dominated by low angle boundaries. The welding process increased the ferrite content but decreased the texture intensity at the heat affected zone of the super duplex stainless steel base metal. In addition, through partial ferritization, it changed the morphology of elongated grains of the rolled microstructure to twinned partially transformed austenite plateaus scattered between ferrite textured colonies. However, the texture of the austenitic stainless steel heat affected zone was strengthened via encouraging recrystallization and formation of annealing twins. At both interfaces, an increase in the special character coincident site lattice boundaries of the primary phase as well as a strong texture with <100> orientation, mainly of Goss component, was observed. - Graphical abstract: Display Omitted - Highlights: • Weld metal showed local orientation at microscale but random texture at macroscale. • Intensification of <100> orientated grains was observed adjacent to the fusion lines. • The austenite texture was weaker than that of the ferrite in all duplex regions. • Welding caused twinned partially transformed austenites to form at SDSS HAZ. • At both interfaces, the ratio of special CSL boundaries of the primary phase increased.

36 MATERIALS SCIENCE↗

Microstructural characterisation of friction stir welding joints of mild steel to Ni-based alloy 625

In this study, 6-mm-thick mild steel and Ni-based alloy 625 plates were friction stir welded using a tool rotational speed of 300 rpm and a travel speed of 100 mm·min{sup −1}. A microstructural characterisation of the dissimilar butt joint was performed using optical microscopy, scanning and transmission electron microscopy, and energy dispersive X-ray spectroscopy (XEDS). Six different weld zones were found. In the steel, the heat-affected zone (HAZ) was divided into three zones and was composed of ferrite, pearlite colonies with different morphologies, degenerated regions of pearlite and allotriomorphic and Widmanstätten ferrite. The stir zone (SZ) of the steel showed a coarse microstructure consisting of allotriomorphic and Widmanstätten ferrite, degenerate pearlite and MA constituents. In the Ni-based alloy 625, the thermo-mechanically affected zone (TMAZ) showed deformed grains and redistribution of precipitates. In the SZ, the high deformation and temperature produced a recrystallised microstructure, as well as fracture and redistribution of MC precipitates. The M{sub 23}C{sub 6} precipitates, present in the base material, were also redistributed in the stir zone of the Ni-based alloy. TMAZ in the steel and HAZ in the Ni-based alloy could not be identified. The main restorative mechanisms were discontinuous dynamic recrystallisation in the steel, and discontinuous and continuous dynamic recrystallisation in the Ni-based alloy. The interface region between the steel and the Ni-based alloy showed a fcc microstructure with NbC carbides and an average length of 2.0 μm. - Highlights: • Comprehensive microstructural characterisation of dissimilar joints of mild steel to Ni-based alloy • Friction stir welding of joints of mild steel to Ni-based alloy 625 produces sound welds. • The interface region showed deformed and recrystallised fcc grains with NbC carbides and a length of 2.0 μm.

36 MATERIALS SCIENCE↗

On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: Investigating microstructure, microhardness, wear and tensile behavior

The main aim of this study is to produce copper reinforced metal matrix composite (MMC) layers using micron sized SiC particles via friction stir processing (FSP) in order to enhance surface mechanical properties. Microstructural evaluation using optical microscopy (OM) and scanning electron microscopy (SEM) indicated that an increase in traverse speed and a decrease in rotational speed cause a reduction in the grain size of stir zone (SZ) for the specimens friction stir processed (FSPed) without SiC particles. With the aim of determining the optimum processing parameters, the effect of traverse speed as the main processing variable on microstructure and microhardness of MMC layers was investigated. Higher traverse speeds resulted in poor dispersion of SiC particles and consequently reduced the microhardness values of MMC layers. It was found that upon addition of SiC particles, wear properties were improved. This behavior was further supported by SEM images of wear surfaces. Results demonstrated that the microcomposite produced by FSP exhibited enhanced wear resistance and higher average friction coefficient in comparison with pure copper. Tensile properties and fracture characteristics of the specimens FSPed with and without SiC particles and pure copper were also evaluated. According to the results, the MMC layer produced by FSP showed lower strength and elongation than pure copper while a remarkable elongation was observed for FSPed specimen without SiC particles. Research Highlights: {yields} Decrease in traverse speed leads to good dispersion of SiC particles in composites. {yields} No distinct TMAZ in side regions of SZ of FSPed specimens with SiC particles. {yields} Microhardness of FSPed specimens with SiC particles shows a remarkable increase. {yields} Reinforcement of Cu with SiC particles improves wear and friction behavior of surface. {yields} A weak bonding in tensile due to probable agglomeration for SiC containing samples.

36 MATERIALS SCIENCE↗

Hemicellulose Modulates Nanoscale Lignin Architecture in Synthetic Plant Cell Walls

Cellulose, hemicellulose, and lignin─the most abundant biopolymers on Earth─compose the structural matrix of plant biomass, providing renewable resources critical to bioenergy and sustainable materials. Despite their importance, the nanoscale mechanochemical processes underlying lignocellulose assembly during plant secondary cell wall formation remain poorly understood, hindering advancements in biomass conversion technologies. Here, in this study, we synthesize a biomimetic model system comprising cellulose–hemicellulose nanofibrils (CHN) to examine guaiacyl lignin polymerization in a physiologically relevant context. Using advanced nanocharacterization─scattering-type scanning near-field optical microscopy (s-SNOM) with infrared nanospectroscopy coupled to solid-state nuclear magnetic resonance (NMR)─we reveal that hemicellulose presence considerably modulates lignin deposition and alters its interunit bond distribution. Specifically, hemicellulose-rich environments dramatically reduce lignin deposition by approximately 50% and yield highly condensed lignin structures characterized by severely reduced β–O–4′ linkages (<2%) and suppressed β–β′ linkages. Conversely, cellulose-alone scaffolds support notably higher β–O–4′ content (∼10%), resulting in a more uniform nanoscale lignin coating. Our work helps explain how accessible hemicellulose sites, both sterically and chemically, direct radical coupling during lignification, fundamentally reshaping lignin’s nanoscale architecture. These findings deepen our mechanistic understanding of plant cell wall biosynthesis and inform strategies aimed at enhancing biomass deconstruction efficiency for sustainable bioenergy applications.

NMR↗

Microstructures of ancient and modern cast silver–copper alloys

The microstructures of modern cast Sterling silver and of cast silver objects about 2500 years old have been compared using optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), scanning transmission electron microscopy (STEM), energy dispersive X-ray microanalysis (EDX) and electron backscatter diffraction (EBSD). Microstructures of both ancient and modern alloys were typified by silver-rich dendrites with a few pools of eutectic and occasional cuprite particles with an oxidised rim on the outer surface. EBSD showed the dendrites to have a complex internal structure, often involving extensive twinning. There was copious intragranular precipitation within the dendrites, in the form of very fine copper-rich rods which TEM, X-ray diffraction (XRD), SEM and STEM suggest to be of a metastable face-centred-cubic (FCC) phase with a cube–cube orientation relationship to the silver-rich matrix but a higher silver content than the copper-rich β in the eutectic. Samples from ancient objects displayed a wider range of microstructures including a fine scale interpenetration of the adjoining grains not seen in the modern material. Although this study found no unambiguous evidence that this resulted from microstructural change produced over archaeological time, the copper supersaturation remaining after intragranular precipitation suggests that such changes, previously proposed for wrought and annealed material, may indeed occur in ancient silver castings. - Highlights: • Similar twinned structures and oxidised surfaces seen in ancient and modern cast silver • General precipitation of fine Cu-rich rods apparently formed by discontinuous precipitation is characteristic of as-cast silver. • The fine rods are cube-cube related to the matrix in contrast with the eutectic. • The silver-rich phase remains supersaturated with copper. • Possibly age-related grain boundary features seen in ancient cast silver.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and texture evolution of AZ31 alloy containing trace levels of strontium

The effect of low levels of Sr (0.01, 0.03, 0.05 wt.%) on the microstructure, mechanical properties and texture of AZ31 magnesium alloy has been investigated. Thermodynamic modeling has been used to study the effect of Sr on phase precipitation at different temperatures. Cooling curve analysis reveals a decrease in solidification superheat with the addition of 0.03 wt.% Sr to AZ31. The as-cast microstructures of the alloys have been studied using optical microscopy (OM) and electron probe micro analysis (EPMA). Results show the refining effect of Sr on the grain size and on the {beta}-Mg{sub 17}Al{sub 12} precipitates through growth poisoning and inoculation, respectively. To investigate the mechanical properties of the alloys, as-cast samples were compression tested at elevated temperatures. Hot compression peak stress ({sigma}{sub max}) and critical strain before recrystallization ({epsilon}{sub c}) initially drop but then increase. {sigma}{sub max} first decreases due to the depletion of Al from solid solution and then increases when the amount of the Al-Sr precipitates reach a significant amount. {epsilon}{sub c} drops due to the acceleration of dynamic recrystallization kinetics as a result of grain refinement. It increases with increasing Sr when the concentration Sr in solid solution is increased leading to dislocation pinning and retardation of recrystallization. X-ray texture measurements on the hot compressed and extruded samples show a decrease in maximum intensity of the basal pole figures with increasing Sr as a result of reduced twining and the changes in Al and Sr concentrations in solid solution. - Research Highlights: {yields} Microstructures/precipitates of AZ31+trace levels of Sr were examined by OM and EPMA. {yields} Thermodynamic calculations and cooling curve analysis were used to predict ppt formation. {yields} It has been shown that Sr refines the grains and Mg17Al12 precipitates. {yields} Mechanical properties and texture were studied using hot compression and X-ray diffraction. {yields} Different micro-mechanisms were responsible for mechanical and texture changes.

36 MATERIALS SCIENCE↗

Effects of rare earth yttrium on microstructure and properties of Ni–16Mo–7Cr–4Fe nickel-based superalloy

Effects of rare earth yttrium on microstructure of Ni–16Mo–7Cr–4Fe alloy were examined by optical microscopy, scanning electron microscopy, transmission electron microscopy and X-ray fluorescence. M{sub 6}C phase was observed in the alloys with and without yttrium addition, and Ni{sub 17}Y{sub 2} phase existed in the alloys containing 0.05–0.43 wt.% yttrium simultaneously. The amount of Ni{sub 17}Y{sub 2} phase increased as yttrium concentration increased. When the concentration of yttrium increased to 0.43 wt.%, some multi-precipitated phase regions appeared in the form of large amount of coarse Ni{sub 3}Y phase surrounded by M{sub 6}C phase and γ phase in the alloy. Influences of rare earth yttrium on high temperature static oxidation and mechanical properties of Ni–16Mo–7Cr–4Fe alloy were also investigated. The alloy containing 0.05 wt.% yttrium showed the best oxidation resistance and mechanical properties simultaneously. The adequate concentration of yttrium at grain boundary and in the solid-solution (γ phase) and the adhesion enhancement of the outer oxidation scale to the substrate are key factors for the improvements in the mechanical properties and oxidation resistance respectively. - Highlights: • When the content of yttrium reaches to 0.43%, some multiphase regions appear. • When the content of yttrium reaches to 0.43%, some Ni{sub 17}Y{sub 2} chains appear. • The morphology of M{sub 6}C changes with increasing concentration of yttrium. • The Ni–16Mo–7Cr–4Fe alloy with 0.05% yttrium performs the best mechanical property. • The Ni–16Mo–7Cr–4Fe alloy with 0.05% yttrium performs the best oxidation resistance.

36 MATERIALS SCIENCE↗

Effects of metallic nanoparticle doped flux on the interfacial intermetallic compounds between lead-free solder ball and copper substrate

Lead free solders currently in use are prone to develop thick interfacial intermetallic compound layers with rough morphology which are detrimental to the long term solder joint reliability. A novel method has been developed to control the morphology and growth of intermetallic compound layers between lead-free Sn–3.0Ag–0.5Cu solder ball and copper substrate by doping a water soluble flux with metallic nanoparticles. Four types of metallic nanoparticles (nickel, cobalt, molybdenum and titanium) were used to investigate their effects on the wetting behavior and interfacial microstructural evaluations after reflow. Nanoparticles were dispersed manually with a water soluble flux and the resulting nanoparticle doped flux was placed on copper substrate. Lead-free Sn–3.0Ag–0.5Cu solder balls of diameter 0.45 mm were placed on top of the flux and were reflowed at a peak temperature of 240 °C for 45 s. Angle of contact, wetting area and interfacial microstructure were studied by optical microscopy, field emission scanning electron microscopy and energy-dispersive X-ray spectroscopy. It was observed that the angle of contact increased and wetting area decreased with the addition of cobalt, molybdenum and titanium nanoparticles to flux. On the other hand, wettability improved with the addition of nickel nanoparticles. Cross-sectional micrographs revealed that both nickel and cobalt nanoparticle doping transformed the morphology of Cu{sub 6}Sn{sub 5} from a typical scallop type to a planer one and reduced the intermetallic compound thickness under optimum condition. These effects were suggested to be related to in-situ interfacial alloying at the interface during reflow. The minimum amount of nanoparticles required to produce the planer morphology was found to be 0.1 wt.% for both nickel and cobalt. Molybdenum and titanium nanoparticles neither appear to undergo alloying during reflow nor have any influence at the solder/substrate interfacial reaction. Thus, doping of flux with appropriate metallic nanoparticles can be successfully used to control the morphology and growth of intermetallic compound layers at the solder/substrate interface which is expected to lead to better reliability of electronic devices. - Highlights: • A novel nanodoped flux method has been developed to control the growth of IMCs. • Ni doped flux improves the wettability, but Co, Mo and Ti deteriorate it. • Ni and Co doped flux gives planer IMC morphology through in-situ alloying effect. • 0.1 wt.% Ni and Co addition into flux gives the lowest interfacial IMC thickness. • Mo and Ti doped flux does not have any influence at the interfacial reaction.

36 MATERIALS SCIENCE↗

Correlative characterization of primary particles formed in as-cast Al-Mg alloy containing a high level of Sc

Primary particles formed in as-cast Al-5Mg-0.6Sc alloy and their role in microstructure and mechanical properties of the alloy were investigated using optical microscopy (OM), scanning electron microscopy (SEM), electron back-scatter diffraction (EBSD) and tensile testing. It was found that primary particles due to a close orientation to matrix could serve as the potent heterogeneous nucleation sites for α-Al during solidification and thus impose a remarkable grain refinement effect. Eutectic structure consisted of layer by layer of ‘Al{sub 3}Sc + α-Al + Al{sub 3}Sc + ⋯’ and cellular-dendritic substructure were simultaneously observed at the particles inside, indicating that these particles could be identified as the eutectics rather than individual Al{sub 3}Sc phase. A calculating method, based on EBSD results, was introduced for the spatial distribution of these particles in matrix. The results showed that these eutectic particles randomly distributed in matrix. In addition, the formation of primary eutectic particles significant improved the strength of the Al-Mg alloy in as-cast condition, which is ascribed to the structural evolution from coarse dendrites to prefect fine equiaxed grains. On the other hand, these large-sized particles due to the tendency to act as the microcrack sources could cause a harmful effect in the ductility of Al-Mg-Sc alloy. - Highlights: •Primary particles exhibit an ‘Al{sub 3}Sc + α-Al + Al{sub 3}Sc + ⋯’ multilayer feature with a cellular-dendritic mode of growth. •EBSD analyses the mechanism of grain refinement and the distribution of primary particles in α-Al matrix. •A computational method was presented to calculate the habit planes of primary particles.

36 MATERIALS SCIENCE↗

Inhibition of Polyimide Photodegradation by Incorporation of Titanate Nanotubes into a Composite

The effect of UV light exposure on the properties of hexafluoroisopropylidene-diphthalic anhydride–oxydianiline (6FDA–ODA) polyimide (PI) and polyimide–titanate nanotube (TiNT/PI) composites has been studied using Raman spectroscopy, optical microscopy, nanoidentation and TEM. The degree of polymer photodegradation was estimated by measuring the change in affinity to a positively charged dye (methylene blue, MB). The mechanism of photoassisted transformations in polyimides usually involves scission of polymer chains accompanied by appearance of active radicals, which undergo further rapid transformations to more stable phenol, amine, and carboxylic functional groups. The accumulation of these groups can increase the degree of adsorption of charged dyes in the photodegraded polymer. It was found that neat PI showed a significantly increased capacity to adsorb MB after irradiation with UV, reaching a plateau after 1 h. In contrast, TiNT/PI composite demonstrated a much slower rise in concentration of adsorbed MB even after 4 h of UV exposure. Raman spectra indicated cleavage of C=O and C–F bonds in PI while only the C–F bond was damaged in TiNT/PI. Shorter cracks (≈ 40 µm long) appeared in TiNT/PI composites whereas macro cracks (> 100 µm) were visible in neat PI after 3 h of UV exposure. Brittleness was studied by comparing plasticity index which varied from 0 to 1 (0 corresponding to the most brittle material and 1 the most ductile one). Plasticity index reduced by 51% and 2% for PI and TiNT/PI, respectively after 3 h UV irradiation, indicating that TiNT can protect underlying PI from further damage. The hardness of neat PI decreased whereas, for TiNT/PI, it increased under UV, suggesting crosslinking of broken polymer chains with nanotubes. Graphical Abstract: Photodegradation of a titanate nanotubes/polyimide composite can lead to cross-linking of broken polymer chains by nanostructured material, resulting in increased hardness. .

36 MATERIALS SCIENCE↗

Friction stir welding joint of dissimilar materials between AZ31B magnesium and 6061 aluminum alloys: Microstructure studies and mechanical characterizations

Friction stir welding is an efficient manufacturing method for joining dissimilar alloys, which can dramatically reduce grain sizes and offer high mechanical joint efficiency. Lap FSW joints between dissimilar AZ31B and Al 6061 alloy sheets were made at various tool rotation and travel speeds. Rotation and travel speeds varied between 560–1400 r/min and 16–40 mm/min respectively, where the ratio between these parameters was such that nearly constant pitch distances were applied during welding. X-ray diffraction pattern (XRD), optical microscopy images (OM), electron probe microanalysis (EPMA) and scanning electron microscopy equipped with an energy-dispersive X-ray spectroscopy (SEM-EDS) were used to investigate the microstructures of the joints welded. Intermetallic phases including Al{sub 12}Mg{sub 17} (γ) and Al{sub 3}Mg{sub 2} (β) were detected in the weld zone (WZ). For different tool rotation speeds, the morphology of the microstructure in the stir zone changed significantly with travel speed. Lap shear tensile test results indicated that by simultaneously increasing the tool rotation and travel speeds to 1400 r/min and 40 mm/min, the joint tensile strength and ductility reached a maximum. Microhardness measurements and tensile stress–strain curves indicated that mechanical properties were affected by FSW parameters and mainly depended on the formation of intermetallic compounds in the weld zone. In addition, a debonding failure mode in the Al/Mg dissimilar weld nugget was investigated by SEM and surface fracture studies indicated that the presence of intermetallic compounds in the weld zone controlled the failure mode. XRD analysis of the fracture surface indicated the presence of brittle intermetallic compounds including Al{sub 12}Mg{sub 17} (γ) and Al{sub 3}Mg{sub 2} (β). - Highlights: • Dissimilar Al/Mg joint was obtained by lap friction stir welding technique. • Effect of rotation and travel speeds on the formation of intermetallic compounds • Microstructure and chemical studies including metallography, XRD, SEM-EDS, and EPMA • Mechanical property tests such as stress–strain curves, failure load and hardness • IMCs as Al{sub 3}Mg{sub 2} and Al{sub 12}Mg{sub 17} were identified in weld nugget and at Al/Mg interface.

36 MATERIALS SCIENCE↗

Prospects for sub-nanometer scale imaging of optical phenomena using electron microscopy

Imaging of optical phenomena at the sub-nanometer scale can offer fundamental insights into the electronic or vibrational states in atomic-scale defects, molecules, and nanoparticles, which are important in quantum information, heterogeneous catalysis, optoelectronics, and structural biology. Several techniques have surpassed the traditional Abbe diffraction limit and attained spatial resolutions down to a few nanometers, but sub-nanometer scale optics has remained elusive. Here, we propose an approach that combines spectrally specific photoabsorption with sub-nanometer scale resolution transmission electron microscopy (TEM) of photoexcited electrons. We first estimate the signal level and conditions required for imaging nanoscale optical phenomena in core-shell quantum dots (QDs) like CdS/CdTe. Furthermore, we show the possibility of imaging photoexcited states of atomic-scale defects in a monolayer hexagonal boron nitride (h-BN) using ab initio and high resolution (HR)TEM simulations. The ability to directly visualize photoexcited states at the sub-nanometer scale opens opportunities to study properties of individual quantum dots and atomic defects.

74 ATOMIC AND MOLECULAR PHYSICS↗