At least 523 records · Page 29

Mapping ice formation to mineral-surface topography using a micro mixing chamber with video and atomic-force microscopy

We developed a method for examining ice formation on solid materials under cloud-like conditions. Our experimental approach couples video-rate optical microscopy of ice formation with high-resolution atomic force microscopy (AFM) of the initial mineral surface. We demonstrate how colocating stitched AFM images with video microscopy can be used to relate the likelihood of ice formation to nanoscale properties of a mineral substrate, e.g., the abundance of surface steps of a certain height. We also discuss the potential of this setup for future iterative investigations of the properties of ice nucleation sites on materials.

54 ENVIRONMENTAL SCIENCES↗

Applications of Subsurface Microscopy

Exploring the interior of a cell is of tremendous importance in order to assess the effects of nanomaterials on biological systems. Outside of a controlled laboratory environment, nanomaterials will most likely not be conveniently labeled or tagged so that their translocation within a biological system cannot be easily identified and quantified. Ideally, the characterization of nanomaterials within a cell requires a nondestructive, label-free, and subsurface approach. Subsurface nanoscale imaging represents a real challenge for instrumentation. Indeed the tools available for high resolution characterization, including optical, electron or scanning probe microscopies, mainly provide topography images or require tagants that fluoresce. Although the intercellular environment holds a great deal of information, subsurface visualization remains a poorly explored area. Recently, it was discovered that by mechanically perturbing a sample, it was possible to observe its response in time with nanoscale resolution by probing the surface with a micro-resonator such as a microcantilever probe (Figure 1). Microcantilevers are used as the force-sensing probes in Atomic Force Microscopy (AFM), where the nanometer-scale probe tip on the microcantilever interacts with the sample in a highly controlled manner to produce high-resolution raster-scanned information of the sample surface. Taking advantage of the existing capabilities of AFM, we present a novel technique, Mode Synthesizing Atomic Force Microscopy (MSAFM) (Figure 1), which has the ability to probe subsurface structures such as non-labeled nanoparticles embedded in a cell. In MSAFM mechanical actuators (PZTs) excite the probe and the sample at different frequencies as depicted in Figure 1. The nonlinear nature of the tip-sample interaction, at the point of contact of the probe and the surface of the sample, in the contact mode AFM configuration permits the mixing of the elastic waves. The new dynamic system comprises new synthesized imaging modes, resulting from sum- and difference-frequency generation of the driving frequencies. The specific electronics of MSAFM allows the selection of individual modes and the monitoring of their amplitude and phase. From these quantities of various synthesized modes a series of images can be acquired. The new images contain subsurface information, thus revealing the presence of nanoparticles inside the cells.

Tetard, Laurene↗

Stable support films for electron microscopy

This disclosure provides systems, methods, and apparatus related to arrangements including electron microscopy grids. In one aspect an arrangement includes an electron microscopy grid. The electron microscopy grid comprises a first surface and a second surface, with the first surface having a holey carbon film disposed thereon. A plurality of lipid molecules are disposed in a hole in the holey carbon film. Each lipid molecule of the plurality of lipid molecules has a hydrophilic head and a hydrophobic tail. A biotin-binding protein is attached to the hydrophilic heads of the plurality of lipid molecules. The biotin-binding protein is crystalline.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Super resolution for magneto-optical microscopy

Sub-diffraction limited magneto-optical microscopy, such as Kerr or Faraday effect microscopy, provide many advantages to fields of science and technology for measuring, or imaging, the magnetization structures and magnetization domains of materials. Disclosed is a method and system for performing sub-diffraction limited magneto-optic microscopy. The method includes positioning a microlens or microlens layer relative to a surface of a sample to image the surface of the sample, forming a photonic nanojet to probe the surface of the sample, and receiving light reflected by the surface of the sample or transmitted through the sample at an imaging sensor. The methods and associated systems and devices enable sub-diffraction limited imaging of magnetic domains at resolutions 2 to 8 times the classical diffraction limit.

te Velthuis, Suzanne Gabriëlle Everdine↗

Hollow Ptychography: Toward Simultaneous 4D Scanning Transmission Electron Microscopy and Electron Energy Loss Spectroscopy

With the recent development of high-acquisition-speed pixelated detectors, 4D scanning transmission electron microscopy (4D-STEM) is becoming routinely available in high-resolution electron microscopy. 4D-STEM acts as a “universal” method that provides local information on materials that is challenging to extract from bulk techniques. It extends conventional STEM imaging to include super-resolution techniques and to provide quantitative phase-based information, such as differential phase contrast, ptychography, or Bloch wave phase retrieval. However, an important missing factor is the chemical and bonding information provided by electron energy loss spectroscopy (EELS). 4D-STEM and EELS cannot currently be acquired simultaneously due to the overlapping geometry of the detectors. Here, the feasibility of modifying the detector geometry to overcome this challenge for bulk specimens is demonstrated, and the use of a partial or defective detector for ptycholgaphic structural imaging is explored. Here, results show that structural information beyond the diffraction-limit and chemical information from the material can be extracted together, resulting in simultaneous multi-modal measurements, adding the additional dimensions of spectral information to 4D datasets.

4D-scanning transmitting electron microscopy (STEM↗

Carbonation dynamics of hydrated alite revealed by electron microscopy

CO 2 sequestration in concrete is crucial to relieve the environmental burden, while the carbonation mechanisms remain unclear. Here, we explored the carbonation dynamics of alite hydrates through electron microscopy. We discovered that calcite is the main phase of carbonate crystals throughout the entire carbonation period in the alite system. Further, the shape evolution of calcite crystals was captured: spindle carbonates initially formed on C-S-H substrate and then transformed into rhombohedrons; Intermediate states such as polyhedral particles and layered rhomboids were also observed. Based on our quantitative calculations, the growth rate of calcite particles was determined approximately 0.2 μm/day, which may be affected by the relative concentration between calcium ions and CO 2 source. A direct relation between the microstructure and mechanical properties of calcite was uncovered using atomic force microscopy. Furthermore, we found that the morphology development of calcite crystals during carbonation may be explained by the surface energy variation of different facets. This work suggests a unique approach to track carbonation kinetics and provides new opportunities to unveil underlying carbonation mechanisms at the nanoscale.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Combined electron microscopy and spectroscopy characterization of as-received, acid purified, and oxidized HiPCO single-wall carbon nanotubes

Single-wall carbon nanotubes (SWCNTs) are very important materials due to their combination of unique structure, dimension, strength, chemical stability, and electronic properties. Nevertheless, SWCNTs from commercial sources usually contain several impurities, which are usually removed by a purification process that includes reflux in acids and strong oxidation. This strong chemical procedure may alter the nanotube properties and it is thus important to control the extent of functionalization and oxidation during the purification procedure. In this report, we provide a comprehensive study of the structure and physical composition of SWCNTs during each step of the purification process. Techniques such as Raman spectroscopy, transmission electron microscopy, scanning electron microscopy, thermogravimetric analysis, X-ray photoelectron spectroscopy and Infrared spectroscopy were used to track the SWCNTs structure, in terms of length and diameter distribution, and surface chemical modifications during each purification stage.

36 MATERIALS SCIENCE↗

Electron microscopy study of direct laser deposited IN718

The microstructure of direct laser deposited (DLD) IN718 has been investigated in detail using scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results confirm that the dendrite core microstructure can be linked to the cooling rate experienced during the deposition. A ~ 100 μm wide δ partially dissolved region in the IN718 substrate was observed close to the substrate/deposit boundary. In the deposited IN718, γ/Laves eutectic constituent is the predominant minor microconstituent. Irregular and regular (small) (Nb,Ti)C carbides and a mixture of the carbides and Laves were observed. Most M{sub 3}B{sub 2} borides were nucleated around a (Nb,Ti)C carbide. Needles of δ phase precipitated from the Laves phase were also observed. A complex constituent (of Laves, δ, α-Cr, γ″, and γ matrix) is reported in IN718 for the first time. The formation of α-Cr particles could be related to Cr rejection during the formation and growth of Cr-depleted δ phase. - Highlights: • Secondary phases in IN718 deposits were identified using electron diffraction and EDS. • MC, M{sub 3}B{sub 2}, γ/Laves eutectic and γ/NbC/Laves eutectic were observed. • Needle-like δ phases were precipitated from the Laves phase. • A complex constituent (Laves, δ, α-Cr, γ″ and γ) was reported for the first time.

36 MATERIALS SCIENCE↗

In-situ investigation of incipient melting in a 319 type Al alloy using laser scanning confocal microscopy

Highlights: • In-situ analysis of incipient melting of ternary eutectic in Al alloy. • Incipient melting occurred in three distinct stages in the eutectic. • Increased heating rate increase rate of liquid film propagation. • Incipient melting transformed initial eutectic structure and caused oxidation. • Study determined incipient melting mechanism for eutectic structures. - Abstract: The modified 319 Al alloy system has been used extensively in precision sand casting of automotive powertrain applications such as engine blocks and cylinder heads, with significant improvement in vehicle fuel efficiency. However, a concern in elevated temperature processing of Al alloys, such as heat treatment and hot working processes, is incipient melting of secondary phases, which is deleterious to mechanical properties. In this study, the laser scanning confocal microscopy (LSCM) technique was used in the analysis of in-situ changes in microstructure as a result of incipient melting. Microstructural analysis was carried out prior to and following elevated temperature exposure in the LSCM using optical microscopy, SEM and EDX. The results suggest that incipient melting of the Al-Al{sub 2}Cu-Al{sub 5}Mg{sub 8}Cu{sub 2}Si{sub 6} ternary eutectic clusters was initiated by the formation of a liquid film which propagated rapidly from the eutectic clusters, coating the Al dendrites in regions adjacent to the eutectic clusters. Following film formation, the ternary eutectic clusters melted completely. Incipient melting also resulted in a localized change in composition in the interdendritic channels as supported by a change in cluster morphology from eutectic to a combination of coarse blocky Al-Cu-Ni and Si particles, and ultra-fine eutectic.

36 MATERIALS SCIENCE↗

Imaging hole-density inhomogeneity in arsenic-doped CdTe thin films by scanning capacitance microscopy

We report nanometer-scale hole-density imaging in As-doped CdTe films by scanning capacitance microscopy (SCM). The hole-density profiling is validated by contrasting a CdTe cross-section sample made by molecular-beam epitaxy with systematically increased As doping in a staircase pattern over the range of 10 15 -10 18 /cm 3 within a single film. In polycrystalline films, the carrier distribution is significantly nonuniform, with inhomogeneity ranging from several hundred nm to several um and hole density varying by one order of magnitude (low 10^16 to low 10 17 /cm 3 ). This nonuniformity is distributed randomly, independent of the grain structure and grain boundaries (GBs). Kelvin probe force microscopy (KPFM) maps the surface potential and is correlated to cathodoluminescence (CL) and SCM by imaging over identical areas. Higher potential and lower CL intensity are found on GBs but not by SCM contrast; this indicates positive GB charging and recombination, but not GB-specific hole-density changes. The overall KPFM potential image is in rough agreement with the SCM carrier distribution and indicates band-edge potential fluctuations. Nonuniform carrier concentration, potential fluctuations, and defect recombination can all cause voltage and performance loss in As-doped CdTe solar technology.

14 SOLAR ENERGY↗

Decoupling Mesoscale Functional Response in PLZT across the Ferroelectric–Relaxor Phase Transition with Contact Kelvin Probe Force Microscopy and Machine Learning

Relaxor ferroelectrics exhibit a range of interesting material behavior, including high electromechanical response, polarization rotations, as well as temperature and electric field-driven phase transitions. The origin of this unusual functional behavior remains elusive due to limited knowledge on polarization dynamics at the nanoscale. Piezoresponse force microscopy and associated switching spectroscopy provide access to local electromechanical properties on the micro- and nanoscale, which can help to address some of these gaps in our knowledge. However, these techniques are inherently prone to artefacts caused by signal contributions emanating from electrostatic interactions between tip and sample. Understanding functional behavior of complex, disordered systems like relaxor materials with unknown electromechanical properties therefore requires a technique that allows distinguishing between electromechanical and electrostatic response. Here, contact Kelvin probe force microscopy (cKPFM) is used to gain insight into the evolution of local electromechanical and capacitive properties of a representative relaxor material lead lanthanum zirconate across the phase transition from a ferroelectric to relaxor state. The obtained multidimensional data set was processed using an unsupervised machine learning algorithm to detect variations in functional response across the probed area and temperature range. Further analysis showed the formation of two separate cKPFM response bands below 50 °C, providing evidence for polarization switching. At higher temperatures only one band is observed, indicating an electrostatic origin of the measured response. In addition, the junction potential difference, which was extracted from the cKPFM data, becomes independent of the temperature in the relaxor state. As a result, the combination of this multidimensional voltage spectroscopy technique and machine learning allows to identify the origin of the measured functional response and to decouple ferroelectric from electrostatic phenomena necessary to understand the functional behavior of complex, disordered systems like relaxor materials.

36 MATERIALS SCIENCE↗

Unveiling Spatial and Temporal Dynamics of Plasmon-Enhanced Localized Fields in Metallic Nanoframes through Ultrafast Electron Microscopy

Plasmonic nanomaterials, particularly noble metal nanoframes (NFs), are important for applications such as catalysis, biosensing, and energy harvesting due to their ability to enhance localized electric fields and atomic efficiency via localized surface plasmon resonance (LSPR). Yet the fundamental structure-function relationships and plasmonic dynamics of the NFS are difficult to study experimentally and thus far rely predominately on computational methodologies, limiting their utilization. This study leverages the capabilities of ultrafast electron microscopy (UEM), specifically photon-induced near-field electron microscopy (PINEM), to probe the light-matter interactions within plasmonic NF structures. Here, the effects of shape, size, and plasmonic coupling of Pt@Au core-shell NFs on spatial and temporal characteristics of plasmon-enhanced localized electric fields are explored. Importantly, time-resolved PINEM analysis reveals that the plasmonic fields around hexagonal NF prisms exhibit a spatially dependent excitation and decay rate, indicating a nuanced interplay between the spatial geometry of the NF and the temporal evolution of the localized electric field. These results and observations uncover nanophotonic energy transfer dynamics in NFs and highlight their potential for applications in biosensing and photocatalysis.

Plasmonics↗

Nanostructural and Electrochemical Evolution of the Solid-Electrolyte Interphase on CuO Nanowires Revealed by Cryogenic-Electron Microscopy and Impedance Spectroscopy

Battery performance is critically dependent on the nanostructure and electrochemical properties of the solid-electrolyte interphase (SEI)—a passivation film that exists on most lithium-battery anodes. However, knowledge of how the SEI nanostructure forms and its impact on ionic transport remains limited due to its sensitivity to transmission electron microscopy and difficulty in accurately probing the SEI impedance. Here, we track the voltage-dependent, stepwise evolution of the nanostructure and impedance of the SEI on CuO nanowires using cryogenic-electron microscopy (cryo-EM) and electrochemical impedance spectroscopy (EIS). In carbonate electrolyte, the SEI forms at 1.0 V vs Li/Li + as a 3 nm thick amorphous SEI and grows to 4 nm at 0.5 V; as the potential approaches 0.0 V vs Li/Li + , the SEI on the CuO nanowires forms an 8 nm thick inverted multilayered nanostructure in ethylene carbonate/diethyl carbonate (EC/DEC) electrolyte with 10 vol % fluoroethylene carbonate (FEC) and a mosaic nanostructure in EC/DEC electrolyte. Upon Li deposition, the total SEI thickness grows to 16 nm, and significant growth of the inner amorphous layer takes place in the inverted multilayered nanostructure, indicating that electrolyte permeates the SEI. Using a refined EIS methodology, we isolate the SEI impedance on Cu and find that the SEI nanostructure directly correlates to macroscopic Li-ion transport through the SEI. The inverted layered nanostructure decreases the interfacial impedance upon formation, whereas the mosaic nanostructure continually increases the interfacial impedance during growth. Furthermore these structural and electrochemical findings illustrate a more complete portrait of SEI formation and guide further improvements in engineered SEI.

25 ENERGY STORAGE↗

Comparative study on the growth of silver nanoplates on GaAs substrates by electron microscopy, synchrotron x-ray diffraction and optical spectroscopy.

We have recently developed a simple and efficient approach involving the galvanic reaction between a pure aqueous solution of AgNO{sub 3} and GaAs wafers to directly grow high-quality Ag nanoplates with chemical clean surfaces on the GaAs wafers [Chem. Mater. 2007, 19, 5845; Small 2007, 3, 1964]. The capability to finely control the dimensions (i.e., size and thickness) of the Ag nanoplates and the time-dependent characterizations have not been explored yet. In this article, time-dependent evolutions of the Ag nanostructures grown on highly doped n-type GaAs wafers through the reactions with AgNO{sub 3} solutions, which have concentrations varying in the range of 1-10 M, for different times have been systematically investigated by employing various powerful techniques including electron microscopy, synchrotron X-ray diffraction, and optical microscopy. The results indicate that the sizes of Ag nanoplates can be tuned in the range from tens of nanometers to half a micrometer and their thicknesses can be varied from -20 to -160 nm by simultaneously controlling the concentration of AgNO{sub 3} solution and the growth time. The as-grown Ag nanoplates exhibit tunable strong extinction peaks in the ultraviolet-visible-near-infrared spectral regimes, where the GaAs substrates intensively interact with the light.

43 PARTICLE ACCELERATORS↗

A New Geometric Method Based on Two-Dimensional Transmission Electron Microscopy for Analysis of Interior versus Exterior Pd Loading on Hollow Carbon Nanofibers

Hallow carbon nanofibers (CNFs) are being explored as catalyst supports because of their unique properties; catalytic activities with both interior and exterior metal loadings are being evaluated. Electron tomography (3D transmission electron microscopy, 3D TEM) has been used to estimate internal versus external loading of metal nanoclusters. However, this method is time consuming and requires a specialized TEM. We prepared three hollow CNF supported Pd samples with various Pd localizations, and developed a geometric analysis method based on 2D TEM images to estimate Pd internal versus external loading percentages. Results show the similar localization for the same sample in terms of the number, surface area, and mass of Pd nanoclusters but distinct values for different samples. To test our method, we compare results for one segment of a CNF using both 3D scanning transmission electron microscopy (3D TEM) and our new 2D geometic analysis method. Agreement is within 15.1%. Our results also agree with 3D TEM results from the literature for similarly prepared Pd on CNFs (within 5.6%). Our geometric analysis method is proposed as a more straightforward and fast way to evaluate metal nanocluster localizations on tubular supports.

2D↗

Correlative fluorescence microscopy and liquid STEM of proteins labeled with quantum dots on intact cells.

Liquid scanning transmission electron microscopy (liquid STEM) was used to image individual quantum dots bound to receptors in COS7 cells. The same regions on intact fixed cells were imaged both with fluorescence microscopy and liquid STEM. The obtained spatial resolution on was 3 nm. The resolution was sufficient to discriminate between quantum dots and gold nanoparticles for double labeling applications.

59 BASIC BIOLOGICAL SCIENCES↗

Single-step electrochemical method for producing very sharp Au scanning tunneling microscopy tips

A single-step electrochemical method for making sharp gold scanning tunneling microscopy tips is described. 3.0M NaCl in 1% perchloric acid is compared to several previously reported etchants. The addition of perchloric acid to sodium chloride solutions drastically shortens etching times and is shown by transmission electron microscopy to produce very sharp tips with a mean radius of curvature of 15 nm.

36 MATERIALS SCIENCE↗

Dislocation network at InN/GaN interface revealed by scanning tunneling microscopy

For heteroepitaxy of InN on GaN(0001) by molecular-beam epitaxy, the lattice misfit strain is relieved by misfit dislocations (MDs) formed at the interface between InN and GaN. Imaging by scanning tunneling microscopy (STM) of the surfaces of thin InN epifilms reveals line feature parallel to <1120>. Their contrast becomes less apparent for thicker epifilms. From the interline spacing as well as a comparison with transmission electron microscopy studies, it is suggested that they correspond to the MDs beneath the surface. The STM contrast originates from both the surface distortion caused by the local strain at MDs and the electronic states of the defects.

36 MATERIALS SCIENCE↗