Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Lithiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Toward quantifying capacity losses due to solid electrolyte interphase evolution in silicon thin film batteries

To understand the origins of failure and limited cycle life in lithium-ion batteries (LIBs), it is imperative to quantitatively link capacity-fading mechanisms to electrochemical and chemical processes. This is extremely challenging in real systems where capacity is lost during each cycle to both active material loss and solid electrolyte interphase (SEI) evolution, two indistinguishable contributions in traditional electrochemical measurements. Here, we have used a model system in combination with (1) precision measurements of the overall Coulombic efficiency via electrochemical experiments and (2) x-ray reflectivity measurements of the active material losses. The model system consisted of a 515 Å thick amorphous silicon (a-Si) thin film on silicon carbide in half-cell geometry using a carbonate electrolyte with LiPF6 salt. This approach allowed us to quantify the capacity lost during each cycle due to SEI evolution. Combined with electrochemical analysis, we identify SEI growth as the major contribution to capacity fading. Specifically, the continued SEI growth results in increasing overpotentials due to increased SEI resistance, and this leads to lower extent of lithiation when the cutoff voltage is reached during lithiation. Our results suggest that SEI grows more with increased time spent at low voltages where electrolyte decomposition is favored. Finally, we extracted a proportionality constant for SEI growth following a parabolic growth law. Our methodology allows for the quantitative determination of lithium-ion loss mechanisms in LIBs by separately tracking lithium ions within the active materials and the SEI and offers a powerful method of quantitatively understanding LIB loss mechanisms.

25 ENERGY STORAGE↗

Redox oscillations in 18650-type lithium-ion cell revealed by in operando Compton scattering imaging

Compton scattering imaging using high-energy synchrotron x rays allows the visualization of the spatiotemporal lithiation state in lithium-ion batteries probed in operando. Here, we apply this imaging technique to the commercial 18650-type cylindrical lithium-ion battery. Our analysis of the line shapes of the Compton scattering spectra taken from different electrode layers reveals the emergence of inhomogeneous lithiation patterns during the charge-discharge cycles. Moreover, these patterns exhibit oscillations in time where the dominant period corresponds to the timescale of the charging curve.

42 ENGINEERING↗

Experimental considerations and applications for time-resolved impedance on silicon-anode battery systems

Dynamic electrochemical impedance spectroscopy (dEIS) utilizes a superimposed multi-sinusoidal waveform and enables temporally resolved investigations on various electrochemical processes; however, the signal-to-noise ratio must be maximized while retaining linearity and stationarity within the system. In the present work, we probe the impact of the waveform’s total amplitude as well as the waveform and phase profiles. The equal amplitude multi-sinusoidal waveform with 35 mV total amplitude (<1 mV per frequency) and random phase profile exhibits the lowest impedance noise. This input signal is sufficient in avoiding the high frequency signal attenuation from the potentiostat’s low-pass filter. Additionally, we demonstrate the optimized dEIS waveform’s utility in investigating surface passivation within thin-film and composite silicon (Si) anodes. Within a two-electrode Si-lithium metal coin cell, the charge transfer resistance (RCT) associated with alloying kinetics dominates the overall impedance. RCT increases with state of charge indicating a kinetic bottleneck at higher lithiation states. To explore this further, we utilize a three-electrode Si-LiNi0.8Mn0.1Co0.1O2 pouch cell to deconvolute the Si impedance contributions. The evolution of the solid electrolyte interphase (SEI) and charge transfer resistances correlate to specific Li–Si alloy phases. We attribute this to the influence of Si particle volume expansion on SEI instabilities and a kinetic bottleneck at higher lithiation states.

Lam, Steven [ORNL]↗

Operando pair distribution function analysis of nanocrystalline functional materials: the case of TiO 2 -bronze nanocrystals in Li-ion battery electrodes

Structural modelling of operando pair distribution function (PDF) data of complex functional materials can be highly challenging. To aid the understanding of complex operando PDF data, this article demonstrates a toolbox for PDF analysis. The tools include denoising using principal component analysis together with the structureMining , similarityMapping and nmfMapping apps available through the online service `PDF in the cloud' ( PDFitc , https://pdfitc.org/). The toolbox is used for both ex situ and operando PDF data for 3 nm TiO 2 -bronze nanocrystals, which function as the active electrode material in a Li-ion battery. The tools enable structural modelling of the ex situ and operando PDF data, revealing two pristine TiO 2 phases (bronze and anatase) and two lithiated Li x TiO 2 phases (lithiated versions of bronze and anatase), and the phase evolution during galvanostatic cycling is characterized.

Chemistry↗

Lithium difluoro(oxalato)borate as additive to Improve the thermal stability of llithiated graphite.

The reaction of lithiated graphite with a nonaqueous electrolyte of 1.2 M LiPF{sub 6} in ethylene carbonate/ethyl methyl carbonate (3:7 by weight) was investigated using differential scanning calorimetry. The decomposition of the solid electrolyte interphase (SEI) took place at about 100 C and was followed by a continuous formation/decomposition of the SEI up to 250 C. Another two peaks were observed at temperatures above 250 C. These peaks were attributed to the major reaction of lithiated graphite with the nonaqueous electrolyte. With the addition of lithium difluoro(oxalato)borate as an electrolyte additive, the onset temperatures of the three peaks were pushed higher, as confirmed by the activation energies obtained.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding the Degredation of Silicion Electrodes for Lithium Ion Batteries Using Acoustic Emission

Silicon is a promising anode material for lithium ion battery application due to its high specific capacity, low cost, and abundance. However, when silicon is lithiated at room temperature it can undergo a volume expansion in excess of 280% which leads to extensive fracturing. This is thought to be a primary cause of the rapid decay in cell capacity routinely observed. Acoustic emission (AE) was employed to monitor activity in composite silicon electrodes while cycling in lithium ion half-cells using a constant current-constant voltage procedure. The major source of AE was identified as the brittle fracture of silicon particles resulting from the alloying reaction that gives rise to LixSi phases. The largest number of emissions occurred on the first lithiation corresponding to surface fracture of the silicon particles, followed by distinct emission bursts on subsequent charge and discharge steps. Furthermore, a difference in the average parameters describing emission during charge and discharge steps was observed. Potential diagnostic and materials development applications of the presented AE techniques are discussed.

74 ATOMIC AND MOLECULAR PHYSICS↗

In Operando XANES Imaging of High Capacity Intermetallic Anodes for Lithium Ion Batteries

In operando 2D X-ray absorption near edge structure (XANES) imaging was performed near the Cu K-edge during cycling of Cu 6 Sn 5 composite anodes for lithium ion batteries. Galvanostatic lithiation and delithiation with intermittent constant voltage holds near reaction plateaus show evolution of absorption spectra for active material particles. XANES spectra obtained from images taken during cycling were compared to standard spectra for Cu, Cu 6 Sn 5 , and Li 2 CuSn. Chemical composition was assessed for Cu-containing phases. Distinct Cu, Cu 6 Sn 5 , and Li 2 CuSn regions were identified for each voltage plateau. Mechanical degradation, electrode particle fracture and expansion were observed during delithiation. Furthermore, movement of particles during cycling suggests that expansion also impacts the supporting secondary phases and the transport networks therein. These results demonstrate that spectroscopic X-ray imaging methods can clearly distinguish chemically distinct phases in alloy electrodes and have the versatility to observe the evolution of these phases during lithiation and delithiation.

25 ENERGY STORAGE↗

Design Principles to Govern Electrode Fabrication for the Lithium Trivanadate Cathode

A full depth of discharge mathematical model for the lithium trivanadate cathode, considering lithiation of the layered α-phase, phase change, and lithiation of the rock-salt like β-phase at lower potentials, is developed. The coupled electrode-scale and crystal-scale model is fit to electrochemical data, and additionally validated with operando EDXRD. There is good agreement between the simulated and measured spatial variation of the volume fraction of the β-phase. This mathematical model is used to guide electrode fabrication, accounting for both ionic and electronic transport effects. Values of three design parameters—electrode thickness, porosity, and volume fraction of conductor—are identified, and the sensitivity of the energy density to these design parameters is quantified. The model is also used to investigate electrode design to create electrodes that deliver the maximum achievable energy density under the constraint that the α to β-phase transition is avoided, since phase change has been demonstrated to reduce cycle life. The energy density sacrificed to avoid phase change decreases at higher discharge rates, but the target values for electrode fabrication remain the same as those when optimizing the electrode for the full depth of discharge.

25 ENERGY STORAGE↗

Benefits of Fast Battery Formation in a Model System

Lithium-ion battery formation affects battery cost, energy density, and lifetime. An improved understanding of the first cycle of solid-electrolyte interphase (SEI) growth on carbonaceous negative electrodes could aid in the design of optimized formation protocols. In this work, we systematically study SEI growth during the formation of carbon black negative electrodes in a standard carbonate electrolyte. We show that the initial ethylene carbonate (EC) reduction reaction occurs at ~0.5-1.2 V during the first lithiation, except under fast lithiation rates (≥10C). The products of this EC reduction reaction do not passivate the electrode; only the SEI formed at lower potentials affects the second-cycle Coulombic efficiency. Thus, cycling quickly through the voltage regime of this reaction can decrease both formation time and first-cycle capacity loss, without an increase in subsequent-cycle capacity loss. We also show that the capacity consumed by this reaction is minimized at low temperatures and low salt concentrations. Finally, we discuss the mechanism behind our experimental results. This work reveals the fundamental processes underlying initial SEI growth on carbonaceous negative electrodes and provides insights for both optimizing the battery formation process and enabling novel electrolytes.

25 ENERGY STORAGE↗

Potassium-Containing α-MnO 2 Nanotubes: The Impact of Hollow Regions on Electrochemistry

α-MnO 2 type materials have been studied as electrode materials in rechargeable batteries and electrocatalysts due to their 2 × 2 tunneled crystal structures capable of accommodating cations and their tunable physiochemical properties. In this study, we deliberately synthesized K + containing α-MnO 2 (K 0.9 Mn 8 O 16 ) hollow nanotubes varying the dimensions of the hollow regions and level of surface defects. The K 0.9 Mn 8 O 16 nanotube material samples have similar crystallinity, thermal stability, and average Mn oxidation state. Oxygen surface defects in the hollow regions were revealed through detailed studies using electron energy loss spectroscopy. The impact of the hollow regions and associated surface defects on the electrochemistry of K x Mn 8 O 16 were investigated using cyclic voltammetry, galvanostatic intermittent titration technique, and galvanostatic cycling. The K 0.9 Mn 8 O 16 nanotubes with a large hollow region (~30 nm) and higher level of surface defects show higher apparent lithium ion diffusion coefficients and lower polarization compared to the nanotubes with a small hollow region (~10 nm). In-situ lithiation demonstrated that the dimensions of the nanotube walls expanded, but the hollow region did not change in size as result of lithiation. Furthermore, this research demonstrates that tuning particle architecture and surface defects can positively impact functional behavior of electrochemical storage materials.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Pathways Toward High-energy Li-sulfur Batteries, Identified via Multi-reaction Chemical Modeling

Here we present a 1D model of a Li-Sulfur battery with physically derived geometric parameters and thermodynamically consistent electrochemical kinetics. The approach enables straightforward comparison of proposed Li-S mechanisms and provides insights into the influence of polysulfide intermediates on battery discharge. Comparing predictions from multiple mechanisms demonstrates the need for both lithiated and non-lithiated polysulfide species, and highlights the challenge of developing parameter estimates for complex electrochemical mechanisms. The model is also used to explore cathode design strategies. Discharge performance and polysulfide concentrations for electrolyte/sulfur ratios in the range 2–4 μ L mg −1 identifies trade-offs that limit battery energy and power density, and highlights the risk of polysulfide precipitation. New cathode and electrolyte approaches must limit polysulfide concentrations in the electrolyte, both to unlock better rate capabilities in Li-S technology and to prevent capacity fade due to polysulfide precipitation.

25 ENERGY STORAGE↗

Electrochemical Formation of Li-M-(M')-Si Phases Using Multivalent Electrolyte Salt Additives

Lithium-rich silicides (Li 15 Si 4 ), formed during the electrochemical lithiation of silicon, show high reactivity with electrolyte components that contribute to capacity decay, formal lithium loss, and low coulombic efficiency. Recently, the reactivity of lithium silicides was found to be suppressed by substituting a multivalent cation (i.e. Mg, Ca) for lithium that results in the room temperature formation of a ternary Li-M-Si phase. In this study, we explored a range of multivalent electrolyte salt additives (M = Ni, Cu, La, Ce, Sr, Ba, and Ca-Mg mixed salt) in a lithium-ion cell configuration and identified a room temperature electrochemical route to the formation of new ternary and quaternary lithium silicides. Using this method, both nickel and copper salts were found to plate onto the silicon electrode surface upon lithiation. Further, based on refined synchrotron XRD data, multivalent cations with an ionic radius similar to Na (~1.03 Å) or smaller can be inserted electrochemically into a formally cation-deficient Li 15 Si 4 host lattice to form new ternary (or quartenary) phases. The electrochemical synthesis of a new quaternary Li-M-M’-Si phase represents a facile route to preparing and scaling materials isostructural to the Heusler phase and electron-precise Li 14 MgSi 4 phase that results in enhanced cycling and calendar life performance.

25 ENERGY STORAGE↗

Trimer Quinoxalines as Organic Cathode Materials for Lithium-Ion Batteries

Due to synthetic ease, high redox potentials, low solubility in polar electrolytes, and good electric conductivity of their semiconducting crystals, discotic quinoxaline trimers (3Q) have been considered as possible candidates for 4 V organic cathodes in lithium-ion batteries. To assess their feasibility as such materials, several 3Q derivatives have been synthesized and tested in half-cells. In voltage limited cycling tests at 1.2–3.9 V vs Li/Li + , the specific discharge capacities of 40–180 mAh g -1 were obtained at a rate of 1 C, and multiple lithiation of 3Q and its derivatives was observed during discharge. However, the obtained discharge capacity was only a fraction of the theoretical capacity expected for reversible six-electron reduction; there was also rapid capacity fade. Our spectroscopic studies indicate the reversible three-electron lithiation at 2 V vs Li/Li + , but suggest instability of more highly discharged states. Finally, our conclusion is that while the 3Q derivatives combine several traits that are desirable in an organic cathode material (including negligible solubility, capacity for multiple charging, and near-100% coulombic efficiency), these materials are still impractical to use.

25 ENERGY STORAGE↗

Electrochemical Charge Transfer Reaction Kinetics at the Silicon-Liquid Electrolyte Interface

Since the gravimetric lithiation capacity of silicon is roughly ten times that of graphite, while their mass densities are comparable, for the same particle size the current density required to cycle a silicon electrode at a given C-rate is about ten times greater than that of graphite. Depending on the magnitude of the corresponding Butler-Volmer exchange current density, j o , such high current densities may cause the charge transfer kinetics at the silicon-electrolyte interface to become rate limiting. Previously reported values of j o for Si differ by about 10 orders of magnitude. Here we report j o measurements using electrochemical impedance spectroscopy (EIS) for single crystal electronically conductive silicon wafers with well-defined (100) and (111) orientations and active surface areas. The electrochemical cycling regime was designed to avoid artifacts due to stress-induced surface cracking of Si upon lithiation. The exchange current density of the silicon-electrolyte interface is found to be 0.1 ± 0.01 mA/cm 2 when using electrolyte consisting of 1 M LiPF 6 in EC/DMC (1/1 by wt) + FEC (10 wt%) + VC (2 wt%). Furthermore, these results are then used to illustrate the dependence of kinetic overpotential on particle size and C-rate for silicon compared to lower volumetric capacity compounds such as graphite.

25 ENERGY STORAGE↗

Stress Evolution in Composite Silicon Electrodes during Lithiation/Delithiation

We report real-time average stress measurements on composite silicon electrodes made with two different binders – viz. Carboxymethyl cellulose (CMC) and Polyvinylidene fluoride (PVDF) – during electrochemical lithiation and delithiation. During galvanostatic lithiation at very slow rates, the stress in a CMC-based electrode becomes compressive and increases to 70 MPa, where it reaches a plateau and increases slowly thereafter with capacity. The PVDF-based electrode exhibits similar behavior, although with lower peak compressive stress of about 12 MPa. These initial experiments indicate that the stress evolution in a Si composite electrode depends strongly on the mechanical properties of the binder. Stress data obtained from a series of lithiation/delithiation cycles suggests plasticity induced irreversible shape changes in contacting Si particles, and as a result, the stress response of the system during any given lithiation/delithiation cycle depends on the cycling history of the electrode. While these results constitute the first in situ stress measurements on composite Si electrodes during electrochemical cycling, the diagnostic technique described herein can be used to assess the mechanical response of a composite electrode made with other active material/binder combinations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Energy Dispersive X-ray Diffraction (EDXRD) of Li1.1V3O8 Electrochemical Cell

ABSTRACT In this study, we conducted the first energy dispersive x-ray diffraction (EDXRD) experiments on Li/Li 1.1 V 3 O 8 coin cells discharged to different lithiation levels in order to investigate the phase transitions upon electrochemical reduction. The phase transformation from layered Li-poor α to Li-rich α to defect rock-salt β phase was confirmed with cells of different lithiation stages. No spatial localization of phase formation was observed throughout the cathodes under the conditions of this measurement.

Zhang, Qing↗

Electrochemically Induced Phase Evolution of Lithium Vanadium Oxide: Complementary Insights Gained via Ex-Situ, In-Situ, and Operando Experiments and Density Functional Theory

ABSTRACT Understanding the structural evolution of electrode material during electrochemical activity is important to elucidate the mechanism of (de)lithiation, and improve the electrochemical function based on the material properties. In this study, lithium vanadium oxide (LVO, LiV 3 O 8 ) was investigated using ex-situ, in-situ, and operando experiments. Via a combination of in-situ X-ray diffraction (XRD) and density functional theory results, a reversible structural evolution during lithiation was revealed: from Li poor α phase (LiV 3 O 8 ) to Li rich α phase (Li 2.5 V 3 O 8 ) and finally β phase (Li 4 V 3 O 8 ). In-situ and operando energy dispersive X-ray diffraction (EDXRD) provided tomographic information to visualize the spatial location of the phase evolution within the LVO electrode while inside a sealed lithium ion battery.

energy storage (including batteries and capacitors↗