Highly mobile segments in crystalline poly(ethylene oxide){sub 8}:NaPF{sub 6} electrolytes studied by solid-state NMR spectroscopy
Two types of high-crystallinity poly(ethylene oxide)/NaPF{sub 6} electrolytes with ethylene oxide (EO)/Na molar ratios of 8:1 and 6:1, termed as PEO{sub 8}:NaPF{sub 6} and PEO{sub 6}:NaPF{sub 6} with M{sub w} = 6000 g mol{sup −1} were prepared, and their ionic conductivity, structure, and segmental motions were investigated and compared. PEO{sub 8}:NaPF{sub 6} polymer electrolyte exhibits the room-temperature ionic conductivity 7.7 × 10{sup −7} S cm{sup −1} which is about five times higher than the PEO{sub 6}:NaPF{sub 6}. By variable-temperature measurements of static powder spectra and {sup 1}H spin-lattice relaxation time in rotation frame ({sup 1}H T{sub 1ρ}), we demonstrate that crystalline segments are more highly mobile in the crystalline PEO{sub 8}:NaPF{sub 6} with higher ionic conductivity than in the PEO{sub 6}:NaPF{sub 6} with lower ionic conductivity. The large-angle reorientation motion of polymer segments in the PEO{sub 8}:NaPF{sub 6} onsets at lower temperature (∼233 K) with a low activation energy 0.31 eV that is comparable with that of the pure PEO crystal. Whereas, the large-angle reorientation motion of polymer segments in the PEO{sub 6}:NaPF{sub 6} starts around 313 K with a high activation energy of 0.91 eV. As a result of the temperature-enhanced large-angle reorientations, the {sup 13}C static powder lineshape changes markedly from a low-temperature wide pattern with apparent principal values of chemical shift δ{sub 33} < δ{sub 22} < δ{sub 11} to a high-temperature narrow pattern of uniaxial chemical shift anisotropy δ{sub 33} > δ{sub 22} (δ{sub 11}). It is suggested that the segmental motion in crystalline PEO-salt complex promotes ionic conductivity.