Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “titanium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

Subcritical crack growth in two titanium alloys.

Measurement of subcritical crack growth during static loading of precracked titanium alloys in salt water using samples too thin for plane strain loading to predominate was examined as a method for determining the critical stress intensity for crack propagation in salt water. Significant internal crack growth followed by arrest was found at quite low stress intensities, but crack growth rates were relatively low. Assuming these techniques provided a reliable measurement of the critical stress intensity, the value for annealed Ti-4Al-1.5Mo-0.5V alloy was apparently about 35 ksi-in. to the 1/2 power, while that for annealed Ti-4Al-3Mo-1V was below 45 ksi-in. to the 1/2 power. Crack growth was also observed in tests conducted in both alloys in an air environment. At 65 ksi-in. to the 1/2 power, the extent of crack growth was greater in air than in salt water. Ti-4Al-3Mo-1V showed arrested crack growth in air at a stress intensity of 45 ksi-in. to the 1/2 power.

Williams, D. N.↗

Study of fretting wear in titanium, Monel-400, and cobalt-25 percent molybdenum using scanning electron microscopy.

Damage scar volume measurements taken from like metal fretting pairs, combined with scanning electron microscopy observations, showed that three sequentially operating mechanisms result in the fretting of titanium, Monel-400, and cobalt-25% molybdenum. Initially, adhesion and plastic deformation on the surface played an important role. This was followed after a few hundred cycles by a fatigue mechanism, producing spall-like pits in the damage scar. Finally, an oxidation-related mechanism became most significant. Damage scar measurements made on several elemental metals after 600,000 fretting cycles suggested that the ratio of oxide hardness to metal hardness was a measure of the susceptibility of a metal to progressive damage by fretting.

Bill, R. C.↗

Development and fracture mechanics data for 6Al-6V-2 Sn titanium alloy

Fracture mechanics properties of 6Al-6V-2Sn titanium in the annealed, solution-treated, and aged condition are presented. Tensile, fracture toughness, cyclic flaw growth, and sustained-load threshold tests were conducted. Both surface flaw and compact tension-specimen geometries were employed. Temperatures and/or environments used were -65 F (220 K) air, ambient, 300 F (422 K) air, and room-temperature air containing 10 and 100% relative humidity.

Fiftal, C. F.↗

Technique for direct measurement of magnetic entropy of solids: Results for dysprosium titanium oxide

A measurement technique was devised which permits direct observation of the magnetic entropy of solids as a function of applied magnetic field. Measurements were made of the magnetic entropy, in the temperature range 2 to 20 K, of polycrystalline samples of dysprosium titanium oxide (Dy2Ti2O7) to determine its suitability for use as the working substance of a magnetic refrigerator. Magnetization measurements were also made at 4.2 K and below to provide additional information on the nature of the compound. The measurements indicated that crystalline electric fields perturbed the ground state of the dysprosium ions, removed the 16-fold degeneracy predicted by Hund's rules, and left only a twofold degeneracy in its place. A positive, temperature independent contribution to the magnetization was observed in the saturation region, which indicated that the doublet ground-state wave function was perturbed by a nearby unpopulated upper energy level.

Flood, D. J.↗

Effect of outdoor exposure at ambient and elevated temperatures on fatigue life of Ti-6Al-4V titanium alloy sheet in the annealed and the solution treated and aged condition

Specimens of Ti-6Al-4V titanium alloy sheet in the annealed and the solution-treated and aged heat-treatment condition were exposed outdoors at ambient and 560 K (550 F) temperatures to determine the effect of outdoor exposure on fatigue life. Effects of exposure were determined by comparing fatigue lives of exposed specimens to those of unexpected specimens. Two procedures for fatigue testing the exposed specimens were evaluated: (1) fatigue tests conducted outdoors by applying 1200 load cycles per week until failure occurred and (2) conventional fatigue tests (continuous cycling until failure occurred) conducted indoors after outdoor exposure under static load. The exposure period ranged from 9 to 28 months for the outdoor fatigue-test group and was 24 months for the static-load group. All fatigue tests were constant-amplitude bending of specimens containing a drilled hole (stress concentration factor of 1.6). The results of the tests indicate that the fatigue lives of solution-treated and aged specimens were significantly reduced by the outdoor exposure at 560 K but not by the exposure at ambient temperature. Fatigue lives of the annealed specimens were essentially unaffected by the outdoor exposure at either temperature. The two test procedures - outdoor fatigue test and indoor fatigue test after outdoor exposure - led to the same conclusions about exposure effects.

Phillips, E. P.↗

Polyimide weld bonding for titanium alloy joints

Two weld bonding processes were developed for joining titanium alloy; one process utilizes a weld-through technique and the other a capillary-flow technique. The adhesive used for the weld-through process is similar to the P4/A5F system. A new polyimide laminating resin, BFBI/BMPM, was used in the capillary-flow process. Static property information was generated for weld-bonded joints over the temperature range of 219 K (-65 F) to 561 K (+550 F) and fatigue strength information was generated at room temperature. Significant improvement in fatigue strength was demonstrated for weld-bonded joints over spot-welded joints. A demonstration was made of the applicability of the weld-through weld-bonding process for fabricating stringer stiffened skin panels.

Vaughan, R. W.↗

Titanium honeycomb structure

A brazed titanium honeycomb sandwich system for supersonic transport wing cover panels provides the most efficient structure spanwise, chordwise, and loadwise. Flutter testing shows that high wing stiffness is most efficient in a sandwich structure. This structure also provides good thermal insulation if liquid fuel is carried in direct contact with the wing structure in integral fuel tanks.

Davis, R. A.↗

Development of the weldbond process for joining titanium

High quality resistance spot welds were produced by welding through epoxy adhesive on titanium alloys. Weldbond joints were consistently stronger than those of either mechanical fasteners, structural adhesive bonds, or mechanical fasteners with adhesive at the joint interface. Weldbond joints and/or spot weld joints showed superior strength at all temperature ranges as compared to other joints tested.

Fields, D.↗

Weld-brazing of titanium

A joining process, designated weld-brazing, which combines resistance spot-welding and brazing has been developed at the NASA Langley Research Center. Resistance spot-welding is employed to position and aline the parts and to establish a suitable faying surface gap for brazing and contributes to the integrity of the joint. Brazing enhances the properties of the joint and reduces the stress concentrations normally associated with spotwelds. Ti-6Al-4V titanium alloy joints have been fabricated using 3003 aluminum braze both in a vaccum furnace and in a retort containing an inert gas environment.

Bales, T. T.↗

Weld-brazing of titanium

A joining process, designated weld-brazing, which combines resistance spotwelding and brazing has been developed at the NASA Langley Research Center. Resistance spot-welding is employed to position and align the parts and to establish a suitable faying surface gap for brazing; it contributes to the integrity of the joint. Brazing enhances the properties of the joint and reduces the stress concentrations normally associated with spotwelds. Ti-6Al-4V titanium alloy joints have been fabricated using 3003 aluminum braze both in a vacuum furnace and in a retort containing an inert gas environment.

Bales, T. T.↗

Time-resolved spectra of bulk titanium combustion

Some preliminary spectroscopic results of an investigation of the radiation from bulk specimens of burning titanium are presented. The use of larger stationary specimens is shown to have considerably eased some of the experimental difficulties associated with metal combustion research and to approximate more closely the conditions prevailing in large-scale accidental metal fires.

Runyan, C. C.↗

A film-rupture model of hydrogen-induced, slow crack growth in alpha-beta titanium

The appearance of the terrace like fracture morphology of gaseous hydrogen induced crack growth in acicular alpha-beta titanium alloys is discussed as a function of specimen configuration, magnitude of applied stress intensity, test temperature, and hydrogen pressure. Although the overall appearance of the terrace structure remained essentially unchanged, a distinguishable variation is found in the size of the individual terrace steps, and step size is found to be inversely dependent upon the rate of hydrogen induced slow crack growth. Additionally, this inverse relationship is independent of all the variables investigated. These observations are quantitatively discussed in terms of the formation and growth of a thin hydride film along the alpha-beta boundaries and a qualitative model for hydrogen induced slow crack growth is presented, based on the film-rupture model of stress corrosion cracking.

Nelson, H. G.↗

Weld bonding of titanium with polyimide adhesives

A conductive adhesive primer and a capillary flow adhesive were developed for weld bonding titanium alloy joints. Both formulations contained ingredients considered to be non-carcinogenic. Lap-shear joint test specimens and stringer-stiffened panels were weld bonded using a capillary flow process to apply the adhesive. Static property information was generated for weld bonded joints over the temperature range of 219K (-65 F) to 561K (550 F). The capillary flow process was demonstrated to produce weld bonded joints of equal strength to the weld through weld bonding process developed previously.

Vaughan, R. W.↗

Crack-closure and crack-growth measurements in surface-flawed titanium alloy Ti6Al-4V

The crack-closure and crack-growth characteristics of the titanium alloy Ti-6Al-4V were determined experimentally on surface-flawed plate specimens. Under cyclic loading from zero to tension, cracks deeper than 1 mm opened at approximately 50 percent of the maximum load. Cracks shallower than 1 mm opened at higher loads. The correlation between crack-growth rate and the total stress-intensity range showed a lower threshold behavior. This behavior was attributed to the high crack-opening loads at short cracks because the lower threshold was much less evident in correlations between the crack-growth rates and the effective stress-intensity range.

Elber, W.↗

The surface structure of titanium and its interaction with bromine and chlorine

The surface structure and composition of titanium have been studied by electron diffraction and Auger electron spectroscopy in the temperature range 25 to 850 C. Atomically clean, well-defined Ti surfaces were obtained by a combination of argon ion sputtering and thermal treatment at 700 to 800 C. A series of surface superstructures was observed as the crystal temperature was gradually decreased. The development of the superstructures is best explained as due to surface reconstruction as a result of surface relaxation. The interaction of bromine and chlorine vapors with clean Ti surfaces was investigated in the temperature range 25 to 500 C. Bromine exposure at room temperature gave rise to an amorphous surface layer, which on annealing transformed into an epitaxial TiBr2 structure. Chlorine interaction resulted in the formation of an epitaxial TiCl3 on both cold and hot Ti surfaces. Surface impurities inhibited the chemical interaction process on the Ti surface.

Khan, I. H.↗

Combustion of bulk titanium in oxygen

The combustion of bulk titanium in one atmosphere oxygen is studied using laser ignition and several analytical techniques. These were high-speed color cinematography, time and space resolved spectra in the visible region, metallography (including SEM) of specimens quenched in argon gas, X-ray and chemical product analyses, and a new optical technique, the Hilbert transform method. The cinematographic application of this technique for visualizing phase objects in the combustion zone is described. The results indicate an initial vapor phase reaction immediately adjacent to the molten surface but as the oxygen uptake progresses the evaporation approaches the point of congruency and a much reduced evaporation rate. This and the accumulation of the various soluble oxides soon drive the reaction zone below the surface where gas formation causes boiling and ejection of particles. The buildup of rutile cuts off the oxygen supply and the reaction ceases.

Clark, A. F.↗

Friction differences between aliphatic and aromatic structures in lubrication of titanium

Sliding friction experiments were conducted with a titanium (0001) single crystal surface with various adsorbed aliphatic and aromatic compounds containing the same number of carbon atoms. An Auger emission spectroscopy analysis was used to monitor the presence of the organic lubricating compounds. Results of the investigation indicate that hexane and benzene give the same friction coefficients over a range of loads. At light loads the friction decreased with an increase in the halogen atom size where the halogens chlorine, bromine, and iodine are incorporated into the benzene molecular structure. The aliphatic compounds chlorohexane and bromohexane exhibited lower friction coefficients than the aromatic structures chlorobenzene and bromobenzene.

Buckley, D. H.↗

Retort braze bonding of borsic/aluminum composite sheet to titanium

Braze bonding studies between Borsic/aluminum composite and titanium sheet were conducted to establish acceptable brazing techniques and to assess potential joint efficiencies. Excellent braze joints were produced which exhibited joint strengths exceeding 117 MPa (17,000 psi) and which retained up to 2/3 of this strength at 589 K (600 F). Noticeable composite strength degradation resulting from the required high temperature braze cycle was found to be a problem.

Webb, B. A.↗