Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

Formation of intermetallic structures at the interface of steel-to-aluminium explosive welds

Highlights: • The interface of Fe-Al explosive welds was characterised by SEM/EDS and EBSD. • The intermetallics formed at the weld interface are rich in Al (Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}). • The presence of intermetallic phases on the interface deeply affects the weldability. • Al-rich intermetallics increase the solidification time of the weld interface. - Abstract: The formation of intermetallic structures at the interface of carbon steel to 6082 aluminium alloy explosive welds and their influence on the weldability of these two materials were studied. The morphology, the microstructure, the chemical and phase compositions of the welds were characterised by several types of microscopy techniques. The interface characterisation proved that explosive mixtures with a lower detonation velocity were revealed as being more suitable for achieving consistent welds since jet entrapment was prevented and continuous molten layers were not formed at the weld interface. It was also found that the physical properties of the intermetallic phases generated at the weld interface have a strong influence on the weldability of steel-to-aluminium explosive welds. Specifically, it was shown that the formation of aluminium-rich intermetallic phases at the weld interface increases the solidification time of the interfacial molten material, decreasing the weldability of these two materials. The formation of these intermetallic compounds should be avoided by reducing the interaction between the flyer and the baseplate as well as by avoiding excessive molten layers.

36 MATERIALS SCIENCE↗

Microstructural evolution of rapidly solidified hypoeutectic Al 10Cu alloy during non-isothermal annealing transients induced by nano-second laser pulses

The evolution of characteristic nonequilibrium features presenting in morphologically distinct regions of rapid solidification (RS) microstructures in a hypoeutectic Al—10Cu (atomic %) in response to non-isothermal annealing transients has been studied by transmission electron microscopy (TEM). The capabilities of the Movie-Mode Dynamic TEM (MM-DTEM) instrument were used to expose select regions of the RS microstructure to sequences of rapid heating and cooling transients induced by nanosecond laser pulses while permitting in-situ observation. Partial melting, microstructural scale coarsening, morphological changes of the nonequilibrium features in the multi-phase RS microstructure, and solid-state phase transformation were observed. Heterogeneous nucleation of nanoscale θ-Al 2 Cu phase involved metastable supersaturated α-Al and the θ'-Al 2 Cu phases, establishing different sets of orientation relationships for the stable θ-Al 2 Cu and α-Al phases. Replacement of banded morphology grains that formed under conditions driven farthest from equilibrium by an equiaxed nanocrystalline structure comprised of α-Al phase, the primary solidification product, and an intergranular network of Al 2 Cu crystals has been attributed to local remelting. Here the experimental approach explored, permitted discovery of mechanistic details of location-specific transformation pathways activated in the multi-phase RS microstructure of hypoeutectic Al—Cu during subsequent nonisothermal transients.

36 MATERIALS SCIENCE↗

Microstructure and mechanical behavior of laser remelted amorphous Al-Ni-La welds

To explore the feasibility of using laser powder bed fusion systems to print bulk amorphous Al alloys, a single autogenous weld produced by laser remelting on a cast Al-5La-9Ni (at.%) alloy was studied for its microstructure and mechanical behavior. The solidification rates experienced by material within the welds were high enough to produce entirely amorphous regions within the welds. Welds were characterized using SEM, STEM, and APT and were found to contain Ni-rich amorphous clusters. Micropillar compression tests were used to assess mechanical properties of the welds and found that all of the amorphous regions exhibited yield strengths around 1 GPa. In conclusion, these results are discussed in the context of diffusivity of Ni and rare earth elements in liquid, glass forming ability, thermodynamic driving force for phase formation during solidification, free volume concentrations in bulk metallic glasses, and cluster-related softening.

APT↗

Cooling dynamics of two titanium alloys during laser powder bed fusion probed with in situ X-ray imaging and diffraction

Metal parts produced by laser powder bed fusion (LPBF) additive manufacturing exhibit characteristic microstructures comparable to those observed in laser welding. The primary cause of this characteristic microstructure is rapid, localized heating and cooling cycles, which result in extreme thermal gradients where material solidification is followed by fast cooling in the solid state. The final microstructure and mechanical performance are also influenced by pore formation caused by melt pool fluid dynamics. Here, we use high speed, in situ X-ray diffraction to probe the kinetics of cooling and solid-solid phase transitions after laser melting in two aerospace titanium alloys: Ti-6Al-4V, an α + β alloy; and Ti-5Al-5V-5Mo-3Cr, a near-β alloy. We complement these diffraction studies with in situ X-ray imaging to probe melt pool dynamics and pore formation. From these two complementary probes, we quantify pore formation during melting and the subsequent microstructural evolution as the material rapidly cools after solidification. These results are critical for understanding defect formation and residual stress development in different titanium alloys under LPBF conditions and can help inform process models to predict final part performance.

36 MATERIALS SCIENCE↗

Disorder trapping and formation of antiphase nanodomains in Ni 3 Sn: in situ observation and high resolution characterization

Rapid solidification of the intermetallic Ni 3 Sn compound from an undercooled liquid was investigated using time-resolved synchrotron X-ray diffraction. Primary growth of an ordered and a disordered cubic solid was observed in situ at a low and a high undercooling, respectively. The disordered cubic solid was reordered after rapid solidification and experienced a solid-state transformation in cooling. A HRTEM study revealed high density of crystal defects and nanodomains in the transformed matrix. A HAADFSTEM study determined that the nanodomains are antiphase domains with chemical disorder. These observations indicated a possibility of online control of mechanical properties in additively manufactured intermetallics.

36 MATERIALS SCIENCE↗

In situ study on the effect of thermomigration on intermetallic compounds growth in liquid-solid interfacial reaction

Synchrotron radiation real-time imaging technology was carried out in situ to observe and characterize the effect of thermomigration on the growth behavior of interfacial intermetallic compounds (IMCs) in Cu/Sn/Cu solder joint during soldering. The thermomigration resulted in asymmetrical formation and growth of the interfacial IMCs. Cu{sub 6}Sn{sub 5} and Cu{sub 3}Sn IMCs formed at the cold end and grew rapidly during the whole soldering process. However, only Cu{sub 6}Sn{sub 5} IMC formed at the hot end and remained relatively thin until solidification. The IMCs at the cold end were nearly seven times thicker than that at the hot end after solidification. The Cu dissolution at the cold end was significantly restrained, while that at the hot end was promoted, which supplied Cu atoms to diffuse toward the cold end under thermomigration to feed the rapid IMC growth. Moreover, the thermomigration also caused asymmetrical morphology of the interfacial IMCs at the cooling stage, i.e., the Cu{sub 6}Sn{sub 5} IMC at the cold end transformed into facet structure, while that at the hot end remained scallop-type. The asymmetrical growth behavior of the interfacial IMCs was analyzed from the view point of kinetics.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Evolution of magnetic properties and microstructure of Hf{sub 2}Co{sub 11}B alloys

Amorphous Hf{sub 2}Co{sub 11}B alloys produced by melt-spinning have been crystallized by annealing at 500–800 °C, and the products have been investigated using magnetization measurements, x-ray diffraction, and scanning electron microscopy. The results reveal the evolution of the phase fractions, microstructure, and magnetic properties with both annealing temperature and time. Crystallization of the phase denoted HfCo{sub 7}, which is associated with the development of coercivity, occurs slowly at 500 °C. Annealing at intermediate temperatures produces mixed phase samples containing some of the HfCo{sub 7} phase with the highest values of remanent magnetization and coercivity. The equilibrium structure at 800 °C contains HfCo{sub 3}B{sub 2}, Hf{sub 6}Co{sub 23}, and Co, and displays soft ferromagnetism. Maximum values for the remanent magnetization, intrinsic coercivity, and magnetic energy product among the samples are approximately 5.2 kG, 2.0 kOe, and 3.1 MGOe, respectively, which indicates that the significantly higher values observed in crystalline, melt-spun Hf{sub 2}Co{sub 11}B ribbons are a consequence of the non-equilibrium solidification during the melt-spinning process. Application of high magnetic fields during annealing is observed to strongly affect the microstructural evolution, which may provide access to higher performance materials in Zr/Hf-Co hard ferromagnets. The crystal structure of HfCo{sub 7} and the related Zr analogues is unknown, and without knowledge of atomic positions powder diffraction cannot distinguish among proposed unit cells and symmetries found in the literature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Radiopure ZnMoO{sub 4} scintillating bolometers for the LUMINEU double-beta experiment

The results of R&D of radiopure zinc molybdate (ZnMoO{sub 4}) based scintillating bolometers for the LUMINEU (Luminescent Underground Molybdenum Investigation for NEUtrino mass and nature) double-beta decay experiment are presented. A dedicated two-stage molybdenum purification technique (sublimation in vacuum and recrystallization from aqueous solutions) and an advanced directional solidification method (the low-thermal-gradient Czochralski technique) were utilized to produce high optical quality large mass (∼1 kg) ZnMoO{sub 4} crystal boules and first {sup 100}Mo (99.5%) enriched Zn{sup 100}MoO{sub 4} crystal scintillator (mass of ∼0.2 kg). Scintillating bolometers based on ZnMoO{sub 4} (≈ 0.33 kg) and Zn{sup 100}MoO{sub 4} (≈ 0.06 kg) scintillation elements and high purity Ge wafers were tested in the EDELWEISS set-up at the Modane Underground Laboratory (France). Long term low temperature tests demonstrate excellent detectors’ performance and effectiveness of the purification and solidification procedures for the achievement of high radiopurity of the material, in particular with a bulk activity of {sup 228}Th and {sup 226}Ra below 4 µBq/kg. The adopted protocol was used to produce for the first time a large volume Zn{sup 100}MoO{sub 4} crystal scintillator (mass of ∼1.4 kg, {sup 100}Mo enrichment is 99.5%) to search for neutrinoless double-beta decay of {sup 100}Mo in the framework of the LUMINEU project.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Molecular dynamics simulation of phase competition in terbium

The competition among multiple solid phases determines the final microstructures of a material. Such competition can originate at the very beginning of the solidification process. We report the results of molecular dynamics simulation of the phase competition between the hexagonal close-packed (hcp), face-centered cubic (fcc), and body-centered cubic (bcc) phases during the solidification of pure Tb. We found that the liquid supercooled below the hcp melting temperature has both bcc and hcp/fcc nuclei, but only the bcc nuclei grow such that the liquid always solidifies into the bcc phase, even at temperatures where the hcp phase is more stable. The hcp phase can only form in the last liquid droplet or at the bcc grain boundaries. Depending on the bcc grain orientations, the hcp phase jammed between the bcc grains either completely disappears or slowly grows via a solid-state massive transformation mechanism. Once the hcp phase becomes large enough, the stresses associated with its appearance can trigger a martensitic transformation. Yet, not the entire bcc phase is consumed by the martensitic transformation and the remaining bcc phase is transformed into the hcp phase via the solid-state massive transformation mechanism. If the supercooling is too large, the nucleation becomes almost barrier free and the liquid solidifies into a structure consisting of ultra-fine hcp and bcc grains after which the bcc phase quickly disappears.

36 MATERIALS SCIENCE↗

Interpreting dynamic-compression experiments to uncover the time dependence of freezing: Application to gallium

Using pulsed-power magnetic field sources to compress gallium to gigapascal pressures on nanosecond timescales, we report here experiments on shockless dynamic compression of a liquid metal. Time-resolved velocimetry data reveal signatures of rapid freezing from a metastable liquid state, and we demonstrate that the kinetics of this nonequilibrium solidification can be accurately simulated with a computational modeling framework we have developed in previous studies, where classical nucleation theory is coupled with hydrodynamics. Notably, velocity traces in some of our experiments show evidence of a phase transition, while others do not, even though other types of evidence suggest that solidification may be occurring in all of them. We explain how predictions made by our models regarding the presence or absence of these phase-transition signatures motivated additional experiments that later confirmed the theoretical predictions. Our analysis shows that due to the rapid, quasi-isentropic nature of the loading path, our experiments were able to compress liquid gallium to metastable states that are undercooled below the equilibrium melt temperature by more than 300 K and exhibit pressures that approach five times the equilibrium melt pressure. The understanding gained in this study should form the basis for future dynamic-compression experiments aimed at interrogating melt curves at high pressures.

gallium↗

Sparse thermal data for cellular automata modeling of grain structure in additive manufacturing

Grain growth in the wake of the melt pool formed during alloy-based additive manufacturing (AM) is complex and multifaceted, depending on parameters governing heat transport, fluid flow, and solidification itself. Cellular automata (CA) models have proven effective in providing computationally efficient and physically sound predictions of grain structure for several AM problems, but their efficiency is tied to the performance of heat transport models. CA models use only a small portion of the problem's temperature data (near the moving melt pool boundary), and much of the CA calculations do not affect the final result due to re-melting of material. Coupling of and communication between heat transport and solidification models, and eliminating operations irrelevant towards final grain structure prediction, will be necessary for using these methods for efficient simulation of large parts. In this work, we introduce a procedure of decoupling the CA from temperature field simulation, using files of relevant temperature data written by the heat transport model. This approach is validated against the standard coupling approach using data obtained through the computational fluid dynamics software OpenFOAM. Negligible differences are seen in grain size, volume, and texture distributions for multilayer simulation of test problems, while the quantity of temperature data for these test problems was reduced by four orders of magnitude (from 100s of GB to 10s of MB) and the code performance sped up by a factor of around 50. Furthermore, variability in microstructure as a function of cell size, substrate, time step, and nucleation parameters is studied, and it is found that cell sizes less than or equal to 1.67 μm and sufficiently small time steps yield Αstatistically equivalent microstructures. Finally, a potential use case for this CA approach—the layer-wise convergence in grain structure starting from extremes in initial grain size—is examined. This approach's ability to simulate expected trends in nucleation and epitaxial grain growth for large regions of microstructure, simulated independently of heat transport models themselves, should prove useful for investigation of various microstructure uncertainties and prediction of part-scale experimental results.

36 MATERIALS SCIENCE↗

The Effect of Vanadium on Morphology and Chemical Composition of Carbides in High Alloyed Chromium–Molybdenum Steels

Despite of the permanent progress of technique and finding of the new, modern materials that successfully replace metals, steel continues to play an important role in the technical practice. The tendency is to discover the new alloys with better mechanical and technological characteristics, compared to conventional and standard types of steels. High-alloyed Cr–Mo steel, with a high content of Vanadium is the new type of wear resistant material, with high hardness and satisfactory impact and fracture toughness. During the solidification process Vanadium, as a strong carbide forming element, creates a network of M{sub 7}C{sub 3} type carbide grains around the metal matrix, while in the matrix, the finely dispersed V{sub 6}C{sub 5} type carbides are formed. In this paper, the chemical composition and morphology have been studied of carbides and the other phases present in the metal matrix in 1.4 wt % C, 12 wt % Cr, 1.0 wt % Mo steels with additions up to 3.0 wt % V. Experimental results indicate that Vanadium affects the solidification process in high Chromium steel. Vanadium is distributed between eutectic M{sub 7}C{sub 3} carbide and the matrix, but its content in carbides is considerably higher. Vanadium changed the microstructure parameters of phases present in the structure of alloys, including volume fraction, size and morphology.

36 MATERIALS SCIENCE↗

Crack-Free 30% Chromium-Nickel Alloy Welding Products for Nuclear Service

We report prior research in the development of 30% chromium-nickel alloy nuclear welding wires has resulted in the resolution of primary water stress corrosion cracking (PWSCC) and ductility dip cracking (DDC) as well as improvement in solidification cracking (SC) resistance. The resolution of DDC exhibits some Laves phase, which has a negative effect on SC resistance. In this study, the use of an alternate carbide former, tantalum (Ta), in combination with niobium (Nb) was researched. Three heats of recently designed Filler Metal 52MSS-Ta (i.e., HV1648, HV1673A, and VX131WXW) were melted, fabricated, and systematically studied. DDC and SC were evaluated with thermodynamic modeling using the Scheil solidification simulation model, two types of varestraint tests, and strain-to-fracture (STF) testing. The varestraint and STF test results showed an improved SC resistance with reduced Laves phase and concurrent excellent DDC resistance. Optimized compositions with low Laves phase also exhibited high threshold strain values (TSVs) in the STF test. VX131WXW — which contains 2.81 wt-% Ta, 0.6 wt-% Nb, and 6 wt-% iron (Fe) - exhibited a TSV of 24%. Thermo-Calc computed the Laves phase to be 0.24% for VX131WXW compared to 0.06% in HV1673A. This difference in Laves phase resulted in the lower SC resistance of VX131WXW compared to HV1673A when measured with longitudinal varestraint testing. The maximum crack distance for HV1673A was about 0.6 mm while that of heat VX131WXW was about 1.0 mm. The typical diluted weld deposit made with VX131WXW was also resistant to PWSCC due to the chromium content exceeding 24%. These simultaneous results mark progress toward crack-free welds and provide direction for further optimization of Ta-containing filler metals.

30% chromium-nickel alloy↗

Radiation and Thermal Stability of Solid Radwaste After Immobilization in Polymer Matrix - 13504

The paper will illustrate results of the various experiments on radiation and thermal stability of polymer matrixes after solutions solidification including aqueous and organic solutions and mixed waste. It was shown that- after irradiation the specimen and after solidification the mixture with oil and TBP hydrogen has been observed (less 1%) and some others gases have been detected. Results of the performed experiments and the radiation stability data of the polymer compositions allow the conclusion that the technological process of immobilizing the above mentioned aqueous solutions and solutions with organic products into polymers at room temperature is the explosion- and flameproof as well as the storage thereof. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Preparation, Performance and Mechanism of Tc and I Getters in Cementitious Waste Forms - 17124

Cementitious waste forms offer a low temperature, cost effective technology for the solidification of liquid wastes. At the Department of Energy Hanford Site, 99-Tc and 129-I are radionuclides contained within low activity waste (LAW) which contribute significantly to environmental impacts associated with clean-up of the site. Cast Stone, a cementitious waste form comprised of 47 wt% blast furnace slag, 45 wt% fly ash and 8 wt% ordinary Portland cement, has undergone investigation as a possible candidate technology for the solidification of LAW. In screening tests using EPA Method 1315 leach testing of various mixes of Cast Stone with simulated LAW, Tc observed effective diffusivities (Dobs) had an average of 5.3 x 10-11 cm{sup 2}/s and I Dobs had an average of 5.7 x 10-9 cm{sup 2}/s. From these measurements, an opportunity exists to improve retention of Tc and I by Cast Stone. One approach to accomplish this is through the incorporation of Tc and I getters to selectively sequester Tc and I in the waste stream and eventual waste form. Initial testing conducted at PNNL identified potassium metal sulfide (KMS-2) and Sn(II)-apatite (Sn-A) as the strongest performing Tc getters and silver exchanged zeolite (Ag-Z) as the top performing I getter. This research also demonstrated that the Tc and I getters, when added to solution simultaneously, can have deleterious interactions with one another and lower the Tc and I removal levels. However, these interactions can be overcome through sequential treatment of solution with the getters. Cast Stone samples were fabricated using a 6.5 M Na average LAW simulant spiked with Tc and I with the addition of various combinations of Tc and I getters. Through EPA Method 1315 and Method 1313 testing it was found that the KMS-2 Tc getter was most successful at lowering Tc Dobs. The I getters were not effective, as apparent interference from sulfide components of the waste form may have led to dissociation of the AgI formed by the Ag-Z getter in sequestering the I from solution. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Immobilization of Organic Liquid Radioactive Waste (LWR) in a Sulfur Composite Matrix at the BN-350 Fast Neutron Reactor Site, Kazakhstan - 18031

The immobilization treatment and final disposition of all forms of organic radioactive liquids, such as pump oil, spent solvent, tri-butyl-phosphate (TBP) and scintillation fluids, remain a significant challenge for nuclear waste generators and national regulators. The majority of nuclear nations have instituted regulations that require some form of encapsulation of treated organic liquid, notwithstanding LLW organic liquids that can be safely incinerated. In most cases cement is the designated material for encapsulation; however, cement can pose certain problems with the containment of treated organic liquids. In 2013, with funding from the U.S. Department of Energy - National Nuclear Security Administration through its Global Initiative for Proliferation Prevention Program (GIPP), a proven U.S. technology for the treatment of radioactive organic liquids was introduced at the BN-350 fast neutron reactor facility in Aktau, Kazakhstan. As the facility was undergoing full decommissioning, one hundred and sixty cubic meters of contaminated pump oil (including Cs-137, Sr-90 and U-235/238) contained in large above ground tanks had to be treated for final disposal. As a result of the research conducted over a two-year period, a new 2-step treatment process was invented by combining the U.S. solidification technology with a newly developed inorganic filler and molecular sulfur, referred to as radiation-resistant composite (RRC) to fully encapsulate the waste oil. The outcome of extensive test program indicates that the final form can reach up to 60 wt.% with a compressive strength of about 100 kg/cm{sup 2}. Preliminary conclusions indicate that RRC outperforms cement as an encapsulation form for final waste treatment which meets U.S. Nuclear Regulatory requirements for final disposal. This paper examines the preliminary experimental work that was conducted in Kazakhstan with the U.S. polymer technology and radioactive pump oil, and the subsequent secondary process of combining the solidified material into a homogeneous final form utilizing RRC. Topics covered in the paper include: - Kazakhstan's regulatory requirements for attaining an achievable waste form for acceptance, which led to the RRC invention; - Technical objectives for the application of polymer technology and RRC materials to radioactive liquid waste; - Polymer solidification with radioactive oil and the result; step one of the RRC process; - Description of RRC materials, their origin and chemical characteristics; - Process of combining the solidified polymer mass with RRC materials into a solid, homogeneous matrix; step two of the RRC process; - Experimental results including leaching data, waste loading estimates and heat process calculations to create the matrix; - Cost advantages of the RRC process over cementation; - Limitations of the RRC process; - Next steps to verify conformance of the RRC technology to the U.S. requirements. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Hydraulic Properties of Grout Monoliths Containing Organic Ion Exchange Resin - 18369

The Waste Treatment and Immobilization Plant (WTP) at Hanford is being constructed to treat 56 million gallons of radioactive waste currently stored in underground tanks at the Hanford site. Operation of the WTP will generate several solid secondary waste (SSW) streams including spent spherical resorcinol formaldehyde cation exchange resin (IXr). The current plan for safe disposal of IXr is solidification in cementitious material (CM) typically comprised of cement, fly ash and blast furnace slag. Three CM formulations were tested to stabilize IXr for long-term land disposal. Two IXr loading rates, 0.1 and 0.3 v/v IXr:grout were used with the three CM formulations to prepare simulated waste form monoliths for hydraulic property testing. Following curing, the monoliths were removed from molds and tested to determine saturated hydraulic conductivity (K{sub sat}) and water retention properties. K{sub sat} was measured using a standard flexible permeameter method ASTM D-5084-10. A constant vapor pressure (CVP) method was used to determine van Genuchten parameters for desorption moisture retention curves for each of the SSW grout formulations. For the CVP method, vacuum saturated, intact wafers approximately 1.25 cm thick were placed above a saturated salt solution inside a sealed container for equilibration. Each saturated salt solution has an associated vapor pressure related to relative humidity in the container. Visual examination and three-dimensional x-ray micro computed tomography (μCT) indicated that the IXr was uniformly distributed in the cured waste form. Saturated hydraulic conductivity was within the range previously reported by Flach et al. in a study of the hydraulic properties of 98 pastes and grouts. The solidification of IXr in CM resulted in a waste form with water retention properties similar to cementitious pastes. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Study on Application of Geopolymer to the Retrieval of Fuel Debris in Fukushima Dai-ichi NPP

In order to retrieve fuel debris in Fukushima Dai-ichi NPP, many retrieval methods are proposed. Geopolymer is the candidate material applied for an alternative retrieval method. In this concept, Geopolymer can be used to stabilize fuel debris and suppress the diffusion of radioactive materials. Objective: Evaluation of geopolymer applied for retrieving fuel debris. Slump Flow Test: Slump flow values decreased as the test temperature increased. In air condition, water molecules evaporated from geopolymer and the viscosity of geopolymer increased. In water condition, the same trends as in air condition were observed. Slump flow values of geopolymer also depended on the elapsed time after mixing. By adding water, the slump flow values of geopolymer became higher (Even at 80 deg. C). It is possible to adjust the solidification time (Setting time) of geopolymer. Solidification Process of Geopolymer: After the first layer solidified, the second layer was injected. At 300 deg. C, porous structure was observed in the first layer, while the second layer structure was intact. In the actual application, multilayered geopolymer may be used to stabilize fuel debris. Conclusion: Fluidity of geopolymer decreased with raising temperature. Setting time can be adjusted by adding water. Geopolymer may be applied by injecting multiple times on high temperature materials above 100 deg. C.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗