Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “propylene”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

Nano-casted Metal Oxide Aerogels as Dual Purpose Structural Components for Space Exploration

NASA missions and space exploration rely on strong, ultra lightweight materials. Such materials are needed for building up past and present space vehicles such as the Sojourner Rover (1997) or the two MERs (2003), but also for a number of components and/or systems including thermal insulators, Solar Sails, Rigid Aeroshells, and Ballutes. The purpose of my internship here at Glenn Research Center is to make dual purpose materials; materials that in addition to being lightweight have electronic, photophysical and magnetic properties and, therefore, act as electronic components and sensors as well as structural components. One type of ultra lightweight material of great interest is aerogels, which have densities ranging from 0.003 g/cc to 0.8 g/cc . However, aerogels are extremely fragile and, as a result, have limited practical applications. Recently, Glenn Research Center has developed a process of nano-casting polymers onto the inorganic network of silica-based aerogels increasing the strength 300 fold while only increasing the density 3 fold. By combining the process of nano-casting polymers with inorganic oxide networks other than silica, we are actively pursuing lightweight dual purpose materials. To date, thirty different inorganic oxide aerogels have been prepared using either standard sol-gel chemistry or a non-alkoxide method involving metal chloride precursors and an epoxide; epichlorohydrin, propylene oxide or trimethylene oxide, as proton scavengers. More importantly, preliminary investigations show that the residual surface hydroxyl groups on each of these inorganic oxide aerogels can be successfully crosslinked with urethane. In addition to characterizing physical and mechanical properties such as density, strength and flexibility, each of these metal oxide aerogels are being characterized for thermal and electronic conductivity and magnetic and optical properties.

Vassilaras, Plousia E.↗

Thermal Control Replacement Materials Evaluated for Durability and Selected for the Hubble Space Telescope

During the Hubble Space Telescope (HST) second servicing mission, astronauts noticed that the outer layer of the multilayer insulation (MLI) was cracked in many locations around the telescope. The insulation s outer layer is composed of 5-mil (0.127 mm) Teflon FEP (DuPont; fluorinated ethylene propylene) with vapor-deposited aluminum (VDA) on the backside. The MLI blankets, which are used on over 80 percent of the external surface of the telescope, provide passive thermal control for equipment. Two large cracks were observed on the light shield directly above the high gain antenna. The upper light shield crack propagated from a cut placed in the blanket during installation around a handrail standoff. Two cracks propagated almost normal to each other, with the outer layer curling tightly as the cracks propagated. A second much larger vertical crack had started to curl and lift away from the telescope, as seen in the figure. MLI on the equipment bays was cracked extensively also, and in some areas it had pulled away from the bay. Continued degradation of the equipment bay insulation would potentially cause limited observations because of housekeeping boxes; for example, the data interface unit could overheat during some portions of the year, in certain sun angles.

deGroh, Kim K.↗

Synchrotron Vacuum Ultraviolet Light and Soft X-Ray Radiation Effects on Aluminized Teflon FEP Investigated

Since the Hubble Space Telescope (HST) was deployed in low Earth orbit in April 1990, two servicing missions have been conducted to upgrade its scientific capabilities. Minor cracking of second-surface metalized Teflon FEP (DuPont; fluorinated ethylene propylene) surfaces from multilayer insulation (MLI) was first observed upon close examination of samples with high solar exposure retrieved during the first servicing mission, which was conducted 3.6 years after deployment. During the second HST servicing mission, 6.8 years after deployment, astronaut observations and photographic documentation revealed significant cracks in the Teflon FEP layer of the MLI on both the solar- and anti-solar-facing surfaces of the telescope. NASA Goddard Space Flight Center directed the efforts of the Hubble Space Telescope MLI Failure Review Board, whose goals included identifying the low-Earth-orbit environmental constituent(s) responsible for the cracking and embrittling of Teflon FEP which was observed during the second servicing mission. The NASA Lewis Research Center provided significant support to this effort. Because soft x-ray radiation from solar flares had been considered as a possible cause for the degradation of the mechanical properties of Teflon FEP (ref. 1), the effects of soft xray radiation and vacuum ultraviolet light on Teflon FEP were investigated. In this Lewisled effort, samples of Teflon FEP with a 100-nm layer of vapor-deposited aluminum (VDA) on the backside were exposed to synchrotron radiation of various vacuum ultraviolet and soft x-ray wavelengths between 18 nm (69 eV) and 0.65 nm (1900 eV). Synchrotron radiation exposures were conducted using the National Synchrotron Light Source at Brookhaven National Laboratory. Samples of FEP/VDA were exposed with the FEP surface facing the synchrotron beam. Doses and fluences were compared with those estimated for the 20-yr Hubble Space Telescope mission.

Dever, Joyce A.↗

Teflon FEP Analyzed After Retrieval From the Hubble Space Telescope

During the Hubble Space Telescope (HST) Second Servicing Mission, 6.8 years after the telescope was deployed in low Earth orbit, degradation of unsupported Teflon FEP (DuPont; fluorinated ethylene propylene), used as the outer layer of the multilayer insulation (MLI) blankets, was evident as large cracks on the telescope light shield. A sample of the degraded outer layer (see the photograph) was retrieved during the second servicing mission and returned to Earth for ground testing and evaluation. Also retrieved was a Teflon FEP radiator surface from a cryogen vent cover that was exposed to the space environment on the aft bulkhead of the HST. NASA Goddard Space Flight Center directed the efforts of the Hubble Space Telescope MLI Failure Review Board, whose goals included determining the FEP degradation mechanisms. As part of the investigations into the degradation mechanisms, specimens retrieved from the first and second HST servicing missions, 3.6 and 6.8 years after launch, respectively, were characterized through exhaustive mechanical, optical, and chemical testing. Testing led by Goddard included scanning electron microscopy, optical microscopy, tensile testing, solar absorptance measurements, time-of-flight secondary ion mass spectroscopy (TOF-SIMS), Fourier transform infrared microscopy (m-FTIR), attenuated total reflectance infrared microscopy (ATR/FTIR), and x-ray diffraction (XRD). The NASA Lewis Research Center contributed significantly to the analysis of the retrieved HST materials by leading efforts and providing results of bend testing, surface microhardness measurements, x-ray photoelectron spectroscopy, solid-state nuclear magnetic resonance spectroscopy, and density measurements. Other testing was conducted by Nano Instruments, Inc., and the University of Akron.

Dever, Joyce A.↗

Effects of Various Wavelength Ranges of Vacuum Ultraviolet Radiation on Teflon FEP Film Investigated

Teflon Fluorinated Ethylene Propylene (FTP) films (DuPont) have been widely used for spacecraft thermal control and have been observed to become embrittled and cracked upon exposure to the space environment. This degradation has been attributed to a synergistic combination of radiation and thermal effects. A research study was undertaken at the NASA Glenn Research Center to examine the effects of different wavelength ranges of vacuum ultraviolet (VUV) radiation on the degradation of the mechanical properties of FEP. This will contribute to an overall understanding of space radiation effects on Teflon FEP, and will provide information necessary to determine appropriate techniques for using laboratory tests to estimate space VUV degradation. Research was conducted using inhouse facilities at Glenn and was carried out, in part, through a grant with the Cleveland State University. Samples of Teflon FEP film of 50.8 microns thickness were exposed to radiation from a VUV lamp from beneath different cover windows to provide different exposure wavelength ranges: MgF2 (115 to 400 nm), crystalline quartz (140 to 400 nm), and fused silica (FS, 155 to 400 nm). Following exposure, FEP film specimens were tensile tested to determine the ultimate tensile strength and elongation at failure as a function of the exposure duration for each wavelength range. The graphs show the effect of ultraviolet exposure on the mechanical properties of the FEP samples.

Dever, Joyce A.↗

Insights Developed Into the Damage Mechanism of Teflon FEP Thermal Control Material on the Hubble Space Telescope

Metalized Teflon FEP (DuPont; fluorinated ethylene propylene) thermal control material on the Hubble Space Telescope (HST) has been found to degrade in the space environment. Teflon FEP thermal control blankets retrieved during the first servicing mission were found to be embrittled on solar-facing surfaces and to contain microscopic cracks (the FEP surface is exposed to the space environment). During the second servicing mission, astronauts noticed that the FEP outer layer of the multilayer insulation blanketing covering the telescope was cracked in many locations. Large cracks were observed on the light shield, forward shell, and equipment bays. A tightly curled piece of cracked FEP from the light shield was retrieved during the second mission. This piece was severely embrittled, as witnessed by ground testing. A Failure Review Board was organized by NASA Goddard Space Flight Center to determine the mechanism causing the multilayer insulation degradation. This board included members of the Electro-Physics Branch of the NASA Glenn Research Center at Lewis Field. Density measurements of the retrieved materials obtained under the review board's investigations indicated that FEP from the first servicing mission was essentially unchanged from pristine FEP but that the second servicing mission FEP had increased in density in comparison to pristine FEP (ref. 1). The results were consistent with crystallinity measurements taken using x-ray diffraction and with results from solid-state nuclear magnetic resonance tests (see the table and ref. 1). Because the second servicing mission FEP was embrittled and its density and crystallinity had increased in comparison to pristine FEP, board researchers expected that the first servicing mission FEP, which was also embrittled, would also have increased in crystallinity and density, but it did not. Because the retrieved second servicing mission material curled while in space, it experienced a higher temperature extreme during thermal cycling (estimated at 200 C) than the first servicing mission material (estimated at 50 C). Therefore, Glenn initiated and conducted an investigation of the effects of heating pristine FEP and FEP that had been exposed on the Hubble Space Telescope. Samples of pristine and first and second servicing mission FEP were heated to 200 C and evaluated for changes in density and morphology. We hoped that the results would help explain why FEP degrades in the Hubble Space Telescope space environment.

deGroh, Kim K.↗

Environmental Exposure Conditions for Teflon FEP on the Hubble Space Telescope Investigated

The Hubble Space Telescope (HST) was launched into low Earth orbit on April 24,1990. During the first servicing mission in December 1993 (3.6 years after launch), multilayer insulation (MLI) blankets were retrieved from the two magnetic sensing systems located on the light shield. Retrieval of one of the solar arrays during this mission also provided MLI blanket material from the solar array drive arm. These MLI materials were analyzed in ground-based facilities, and results indicate that the space-facing outer layer of the MLI, aluminized Teflon FEP (DuPont; fluorinated ethylene propylene), was beginning to degrade. Close inspection of the FEP revealed through-the-thickness cracks in areas with the highest solar exposure and stress concentration. During the second servicing mission in February 1997 (6.8 years after launch), astronauts observed and documented severe cracking in the outer layer of the MLI blankets on both the solar-facing and anti-solar-facing surfaces. During this second mission, some material from the outer layer of the light shield MLI was retrieved and subsequently analyzed in ground-based facilities. After the second servicing mission, a Failure Review Board was convened by NASA Goddard Space Flight Center to address the MLI degradation problem on HST. Members of the Electro-Physics Branch of the NASA Glenn Research Center at Lewis Field participated on this board. To determine possible degradation mechanisms, board researchers needed to consider all environmental constituents to which the FEP MLI surfaces were exposed. On the basis of measurements, models, and predictions, environmental exposure conditions for FEP surfaces on HST were estimated for various time periods from launch in 1990 through 2010, the planned end-of-life for HST. The table summarizes these data including the number and temperature ranges of thermal cycles; equivalent Sun hours; fluence and absorbed radiation dose from solar event x rays; fluence and absorbed dose from solar wind protons and electrons trapped in Earth s magnetic field; fluence of plasma electrons and protons; and atomic oxygen fluence.

Dever, Joyce A.↗

Effect of Air and Vacuum Storage on the Degradation of X-Ray-Exposed Aluminized-Teflon Investigated

Metalized Teflon FEP (fluorinated ethylene propylene, DuPont), a common thermal control material, has been found to degrade in the low-Earth-orbit space environment. The aluminized-FEP (Al-FEP) exterior layer on the Hubble Space Telescope has become extremely embrittled, with extensive cracking occurring on all sides of the telescope. This embrittlement has been primarily attributed to radiation exposure (x-rays from solar flares, electron/proton radiation, and possibly near-ultraviolet radiation) combined with thermal cycling. Limited samples of FEP tested after long-term exposure to low Earth orbit on the Hubble Space Telescope and on the Long Duration Exposure Facility indicated that there might be continued degradation in tensile properties over time. An investigation was conducted at the NASA Glenn Research Center to evaluate the effect of air and vacuum storage on the mechanical properties of x-ray-exposed FEP. Aluminized-FEP (5-mil-thick) tensile samples were x-ray exposed with 15.3-kV copper xrays for 2 hr, reducing the percent elongation to failure by approximately 50 percent in comparison to that for pristine Al-FEP. X-ray-exposed samples were stored in air or under vacuum for various time periods to see the effect of storage on tensile properties. Tensile results indicated that samples stored in air had larger decreases in tensile properties than samples stored under vacuum had, as seen in the graph. Samples stored under vacuum (for up to 400 hr) showed no further decrease in tensile properties over time, whereas samples stored in air (for up to 900 hr) appeared to show decreases in tensile properties over time. X-ray-exposed samples stored in air developed a hazy appearance in the exposed area, as seen in the photographs. When the source of the haziness was evaluated using scanning electron microscopy and atomic force microscopy, it was found to reside at the Al/FEP interface as witnessed by an increased surface roughness of the aluminized side of the material and a dramatic decrease in the adhesion between the Al and FEP. Optical properties of air-stored irradiated samples showed an increase in the diffuse reflectance, which is consistent with observed roughening that was characterized by AFM. These findings indicate that air exposure helps degrade x-ray-irradiated FEP. These results indicate that proper sample handling and storage is necessary with space-retrieved materials and with those exposed to ground-based irradiation simulation exposures.

deGroh, Kim K.↗

Sensitive Technique Developed Using Atomic Force Microscopy to Measure the Low-Earth-Orbit Atomic Oxygen Erosion of Polymers

A recession measurement technique has been developed at the NASA Glenn Research Center to determine the atomic oxygen durability of polymers exposed to the space environment for short durations. Polymers such as polyimide Kapton and Teflon FEP (fluorinated ethylene propylene, DuPont) are commonly used in spacecraft because of their desirable properties, such as flexibility, low density, and in the case of FEP, low solar absorptance and high thermal emittance. Polymers on the exterior of spacecraft in the low- Earth-orbit environment are exposed to energetic atomic oxygen, resulting in erosion and potential structural loss. It is, therefore, important to understand the atomic oxygen erosion yield (E, the volume loss per incident oxygen atom) of polymers being considered in spacecraft design. Because long-term space exposure data are rare and very costly, short-term exposures, such as on the space shuttles, are often relied on for atomic oxygen erosion determination. The most common technique for determining E is through mass-loss measurements. For limited-duration exposure experiments, such as shuttle flight experiments, the atomic oxygen fluence is often so small that mass-loss measurements are not sensitive enough. Therefore, a recession measurement technique has been developed at Glenn to obtain accurate erosion yields of polymers exposed to low atomic oxygen fluences.

deGroh, Kim D.↗

MISSE PEACE Polymers: An International Space Station Environmental Exposure Experiment Being Conducted

As part of the Materials International Space Station Experiment (MISSE), 41 different polymers are being exposed for approximately 1 1/2 years to the low-Earth-orbit (LEO) environment on the exterior of the International Space Station. MISSE is a materials flight experiment sponsored by the Air Force Research Lab/Materials Lab and NASA, and is the first external experiment on the space station. A similar set of 41 polymers will be flown as part of the Polymer Erosion and Contamination Experiment (PEACE) a shuttle flight experiment that is being developed at the NASA Glenn Research Center collaboratively with the Hathaway Brown School for girls. Therefore, these 41 polymers are collectively called the MISSE PEACE Polymers. The purpose of the MISSE PEACE Polymers experiment is to determine how durable polymers are in the LEO space environment where spacecraft, such as the space station, orbit. Polymers are commonly used as spacecraft materials because of their desirable properties such as good flexibility, low density, and certain electrical properties or optical properties (such as a low solar absorptance and high thermal emittance). Two examples of the use of polymers on the exterior of spacecraft exposed to the space environment include metalized Teflon FEP (fluorinated ethylene propylene, DuPont) thermal control materials on the Hubble Space Telescope, and polyimide Kapton (DuPont) solar array blankets.

deGroh, Kim K.↗

Physical and Thermal Properties Evaluated of Teflon FEP Retrieved From the Hubble Space Telescope During Three Servicing Missions

Mechanical properties of aluminized Teflon fluorinated ethylene propylene (FEP) thermal control materials on the Hubble Space Telescope (HST) exposed to low Earth orbit for up to 9.7 years have significantly degraded, with extensive cracking occurring on orbit. The NASA Glenn Research Center and the NASA Goddard Space Flight Center have collaborated on analyzing the physical and thermal properties of aluminized FEP (FEP-Al, DuPont) materials retrieved in December 1999 during HST's third servicing mission (SM3A). Comparisons have been made to properties of FEP-Al retrieved during the first and second HST servicing missions, SM1 and SM2, in order to determine degradation processes for FEP on HST.

Dever, Joyce A.↗

Thermal Contributions to the Degradation of Ground-Laboratory- and Space-Irradiated Teflon Investigated

The Hubble Space Telescope (HST) is covered with two primary types of thermal control materials, radiators and multilayer insulation blankets, which passively control temperatures during orbit. Both of these thermal control materials utilize back-surface metalized Teflon FEP (DuPont, fluorinated ethylene propylene) as the exterior (spacefacing) layer because of its excellent optical properties (low solar absorptance and high thermal emittance). The aluminized-FEP (Al-FEP) outermost layer of the multilayer insulation blankets on the HST has become embrittled while in space, resulting in severe on-orbit cracking (see the photographs). During the second servicing mission, an extremely embrittled piece of Al-FEP was retrieved that had curled, exposing the backsurface aluminum to space (see the photograph on the right). Because the aluminum surface has a lower thermal emittance than the FEP, this curled piece reached 200 C during orbit, 150 C higher than the nominal temperature extreme. To better understand the effect of temperature on the rate of degradation, and on the mechanism of degradation, of this insulation material in the low-Earth-orbit environment, researchers at the NASA Glenn Research Center conducted experiments to determine the effect of heating on the degradation of FEP that has been irradiated in a ground laboratory facility or in space on the HST. For this study, Teflon FEP retrieved from the HST during the third servicing mission after 9.7 years of space exposure was provided to Glenn by the NASA Goddard Space Flight Center.

deGroh, Kim K.↗

New Active Optical Technique Developed for Measuring Low-Earth-Orbit Atomic Oxygen Erosion of Polymers

Polymers such as polyimide Kapton (DuPont) and Teflon FEP (DuPont, fluorinated ethylene propylene) are commonly used spacecraft materials because of desirable properties such as flexibility, low density, and in the case of FEP, a low solar absorptance and high thermal emittance. Polymers on the exterior of spacecraft in the low-Earth-orbit (LEO) environment are exposed to energetic atomic oxygen. Atomic oxygen reaction with polymers causes erosion, which is a threat to spacecraft performance and durability. It is, therefore, important to understand the atomic oxygen erosion yield E (the volume loss per incident oxygen atom) of polymers being considered in spacecraft design. The most common technique for determining E is a passive technique based on mass-loss measurements of samples exposed to LEO atomic oxygen during a space flight experiment. There are certain disadvantages to this technique. First, because it is passive, data are not obtained until after the flight is completed. Also, obtaining the preflight and postflight mass measurements is complicated by the fact that many polymers absorb water and, therefore, the mass change due to water absorption can affect the E data. This is particularly true for experiments that receive low atomic oxygen exposures or for samples that have a very low E. An active atomic oxygen erosion technique based on optical measurements has been developed that has certain advantages over the mass-loss technique. This in situ technique can simultaneously provide the erosion yield data on orbit and the atomic oxygen exposure fluence, which is needed for erosion yield determination. In the optical technique, either sunlight or artificial light can be used to measure the erosion of semitransparent or opaque polymers as a result of atomic oxygen attack. The technique is simple and adaptable to a rather wide range of polymers, providing that they have a sufficiently high optical absorption coefficient. If one covers a photodiode with a uniformly thick sheet of semitransparent polymer such as Kapton H polyimide, then as atomic oxygen erodes the polymer, the short-circuit current from the photodiode will increase in an exponential manner with fluence. This nonlinear response with fluence results in a lack of sensitivity for measuring low atomic oxygen fluences. However, if one uses a variable-thickness polymer or carbon sample, which is configured as shown in the preceding figure, then a linear response can be achieved for opaque materials using a parabolic well for a circular geometry detector or a V-shaped well for a rectangular-geometry detector. Variable-thickness samples can be fabricated using many thin polymer layers. For semitransparent polymers such as Kapton H polyimide, there is an initial short-circuit current that is greater than zero. This current has a slightly nonlinear dependence on atomic oxygen fluence in comparison to opaque materials such as black Kapton as shown in the graph. For this graph figure, the total thickness of Kapton H was assumed to be 0.03 cm. The photodiode short-circuit current shown in the graph was generated on the basis of preliminary measurements-a total reflectance rho of 0.0424 and an optical absorption coefficient a of 146.5 cm(sup -1). In addition to obtaining on-orbit data, the advantage of this active erosion and erosion yield measurement technique is its simplicity and reliance upon well-characterized fluence witness materials as well as a nearly linear photodiode short-circuit current dependence upon atomic oxygen fluence. The optical technique is useful for measuring either atomic oxygen fluence or erosion, depending on the information desired. To measure the atomic oxygen erosion yield of a test material, one would need to have two photodiode sensors, one for the test material and one that uses a known erosion yield material (such as Kapton) to measure the atomic oxygen fluence.

Banks, Bruce A.↗

A Theoretical Investigation of Oxidation Efficiency of a Volatile Removal Assembly Reactor Under Microgravity Conditions

Volatile Removal Assembly (VRA) is a subsystem of the Closed Environment Life Support System (CELSS) installed in the International Space Station. It is used for removing contaminants (volatile organics) in the wastewater produced by the space station crews. The major contaminants are formic acid, ethanol, and propylene glycol. The VRA contains a slim packbed reactor (3.5 cm diameter and four 28 cm long tubes in series) to perform catalyst oxidation of wastewater at elevated pressure and temperature under microgravity conditions. In the reactor, the contaminants are burned with oxygen gas (O2) to form water and carbon dioxide (CO2) that dissolves in the water stream. Optimal design of the reactor requires a thorough understanding about how the reactor performs under microgravity conditions. The objective of this study was to develop a mathematical model to interpret experimental data obtained from normal and microgravity conditions, and to predict the performance of VRA reactor under microgravity conditions. Catalyst oxidation kinetics and the total oxygen-water contact area control the efficiency of catalyst oxidation for mass transfer, which depends on oxygen gas holdup and distribution in the reactor. The process involves bubbly flow in porous media with chemical reactions in microgravity environment. This presents a unique problem in fluid dynamics that has not been studied. Guo et al. (2004) developed a mathematical model that predicts oxygen holdup in the VRA reactor. No mathematical model has been found in the literature that can be used to predict the efficiency of catalyst oxidation under microgravity conditions.

Guo, Boyun↗

Freeze Tolerant Radiator for an Advanced EMU

During an Extravehicular Activity (EVA), the astronaut s metabolic heat and the heat produced by the Portable Life Support Unit (PLSS) must be rejected. This heat load is currently rejected by a sublimator, which vents up to eight pounds of water each EVA. However, for advanced space missions of the future, water venting to space needs to be minimized because resupply impacts from earth will be prohibitive. If this heat load could be radiated to space from the PLSS, which has enough surface area to radiate most of the heat, the amount of water now vented could be greatly reduced. Unfortunately, a radiator rejects heat at a relatively constant rate, but the astronauts generate a variable heat load depending on how hard they are working. Without a way to vary the heat removal rate, the astronaut would experience cold discomfort or even frostbite. A proven method allowing a radiator to be turned-down is to sequentially allow tubes that carry the heat transfer fluid to the radiator to freeze. A drawback of current freezable radiators using this method is that they are far to heavy for use on a PLSS, because they use heavy construction to prevent the tubes from bursting as they freeze and thaw. This creates the need for a large radiator to reject most of the heat but with a lightweight tube that doesn t burst as it freezes and thaws. The new freezable radiator for the Extravehicular Mobility Unit (EMU) has features to accommodate the expansion of the radiator fluid when it freezes, and still have the high tube to fin conductance needed to minimize the number and weight of the tubes. Radiator fluid candidates are water and a propylene glycol-water mixture. This design maintains all materials within their elastic limits so that large volume changes can be achieved without breaking the tube. This concept couples this elastic expansion with an extremely lightweight, extremely high conductivity carbon fiber fin that can carry the heat needed to thaw a frozen tube. By using most of the exposed surface area of the PLSS as a radiator, the system can reject about 75% of the highest heat load, and reduce the loss of water through sublimation by a factor of four. The proposed radiator and a small water tank can be no heavier than the current system.

Copeland, Robert J.↗

Screening and Identification of Cryopreservative Agents for Human Cellular Biotechnology Experiments in Microgravity

Dimethyl sulfoxide (DMSO) has been used as a standard cryopreservative agent for mammalian cell culture; however, prolonged exposure of thawed cells to DMSO can alter cell growth. While DMSO is easily eliminated in ground-based experiments, removal of DMSO in flight-based experiments is more difficult due to various on-orbit constraints. Failure of cryopreservation is due to a number of factors, including intracellular ice formation, solute effect, and apoptotic cell death following thawing. One objective of this study is to identify and characterize an alternative cryopreservative that could be used on the International Space Station (ISS). We systematically screened for potential permeating and non-permeating agents using a human colorectal carcinoma cell line, MIP-101. Cells were suspended in cryopreservation solution and frozen either following a two-step procedure involving initial cooling at -1 C/min overnight followed by storage in liquid nitrogen (LN2) vapor, or by freezing cells directly in the LN2 vapor phase at -10 C/min. Ability to preserve cellular function after one cycle of freeze-thawing was assessed by the recovery of viable cells in short and long-term cell culture experiments. Results showed that permeating preservatives glycerol (G) and ethylene glycol (EG) had an efficacy (80-110%) comparable to, if not better than, 7.5% DMSO; but, propylene glycol (PG) had a somewhat lesser efficacy. Among the non-permeating preservatives, trehalose, raffinose, and dextran exhibited significant protective effect (50-80%) relative to that offered by 7.5% DMSO, but at -10 C and not at -1 C/min cooling rate. Preliminary data thus suggest that a combination of permeating and non-permeating agents may have improved efficacy as a cryoprotectant and serve as an alternate to DMSO for experimentation on ISS.

Love,J.↗

Solar Effects on Tensile and Optical Properties of Hubble Space Telescope Silver-Teflon(Registered Trademark) Insulation

A section of the retrieved Hubble Space Telescope (HST) solar array drive arm (SADA) multilayer insulation (MLI), which experienced 8.25 years of space exposure, was analyzed for environmental durability of the top layer of silver-Teflon (DuPont) fluorinated ethylene propylene (Ag-FEP). Because the SADA MLI had solar and anti-solar facing surfaces and was exposed to the space environment for a long duration, it provided a unique opportunity to study solar effects on the environmental degradation of Ag-FEP, a commonly used spacecraft thermal control material. Data obtained included tensile properties, solar absorptance, surface morphology and chemistry. The solar facing surface was found to be extremely embrittled and contained numerous through-thickness cracks. Tensile testing indicated that the solar facing surface lost 60% of its mechanical strength and 90% of its elasticity while the anti-solar facing surface had ductility similar to pristine FEP. The solar absorptance of both the solar facing surface (0.155 plus or minus 0.032) and the anti-solar facing surface (0.208 plus or minus 0.012) were found to be greater than pristine Ag-FEP (0.074). Solar facing and anti-solar facing surfaces were microscopically textured, and locations of isolated contamination were present on the anti-solar surface resulting in increased localized texturing. Yet, the overall texture was significantly more pronounced on the solar facing surface indicating a synergistic effect of combined solar exposure and increased heating with atomic oxygen erosion. The results indicate a very strong dependence of degradation, particularly embrittlement, upon solar exposure with orbital thermal cycling having a significant effect.

deGroh, Kim, K.↗

Preventing Ice Before it Forms

In the late 1990s, a team of engineers at Ames Research Center invented an anti-icing fluid to keep ice from building up on airplane wings. Ice on wings can be a serious safety hazard, especially during takeoff, when a sheet of ice the thickness of a compact disc can reduce lift by 25 percent or more. The typical approach to clearing off the ice is to use a deicing solution once the ice has built up. The fluid created by the Ames team, though, when applied to a dry surface, prevents the ice from even forming a surface bond, which saves deicing time and money, while also preventing excessive use of chemical solvents. If, however, the solution is not applied before ice forms, it also serves as a traditional deicing formula. The formula contains propylene glycol, which has a very low freezing point, and a thickener, which helps the fluid adhere to the surface. Ice gathers on top of the formula, and then it can be wiped off with little effort. This thickening agent, a pseudo-plastic, sprays on as a liquid, like lemonade, gels like a lemon sherbet, turns back to a liquid when wiped, and then gels again into its sherbet consistency when left to solidify. The sherbet-gel stage is especially important when the formula is sprayed onto a vertical or steeped surface, as it clings better than a liquid would.

Source record↗