Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “degradeable”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

Electrolyte Reactivity at the Charged Ni-Rich Cathode Interface and Degradation in Li-Ion Batteries

The chemical and electrochemical reactions at the positive electrode–electrolyte interface in Li-ion batteries are hugely influential on cycle life and safety. Ni-rich layered transition metal oxides exhibit higher interfacial reactivity than their lower Ni-content analogues, reacting via mechanisms that are poorly understood. Here, we study the pivotal role of the electrolyte solvent, specifically cyclic ethylene carbonate (EC) and linear ethyl methyl carbonate (EMC), in determining the interfacial reactivity at charged LiNi 0.33 Mn 0.33 Co 0.33 O 2 (NMC111) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes by using both single-solvent model electrolytes and the mixed solvents used in commercial cells. While NMC111 exhibits similar parasitic currents with EC-containing and EC-free electrolytes during high voltage holds in NMC/Li 4 Ti 5 O 12 (LTO) cells, this is not the case for NMC811. Online gas analysis reveals that the solvent-dependent reactivity for Ni-rich cathodes is related to the extent of lattice oxygen release and accompanying electrolyte decomposition, which is higher for EC-containing than EC-free electrolytes. Combined findings from electrochemical impedance spectroscopy (EIS), TEM, solution NMR, ICP, and XPS reveal that the electrolyte solvent has a profound impact on the degradation of the Ni-rich cathode and the electrolyte. Higher lattice oxygen release with EC-containing electrolytes is coupled with higher cathode interfacial impedance, a thicker oxygen-deficient rock-salt surface reconstruction layer, more electrolyte solvent and salt breakdown, and higher amounts of transition metal dissolution. These processes are suppressed in the EC-free electrolyte, highlighting the incompatibility between Ni-rich cathodes and conventional electrolyte solvents. Finally, new mechanistic insights into the chemical oxidation pathways of electrolyte solvents and, critically, the knock-on chemical and electrochemical reactions that further degrade the electrolyte and electrodes curtailing battery lifetime are provided.

25 ENERGY STORAGE↗

Degradation and Self-Healing in Perovskite Solar Cells

Organic–inorganic halide perovskites are well-known for their unique self-healing ability. In the presence of strong external stimuli, such as light, temperature, and moisture, high-energy defects are created which can be healed by removing the perovskite from the degradation source. Furthermore, this self-healing ability has been showcased in devices with recoverable performance and day-and-night cycling operation to dramatically extend the device lifetime and even mechanical durability. However, to date, the mechanistic details and theory around this captivating trait are sparse and convoluted by the complex nature of perovskites. With a clear understanding of the intrinsic self-healing property, perovskite solar cells with extended lifetimes and durability can be designed to realize the large-scale commercialization of perovskite solar cells. Here, we spotlight the relevant degradation and self-healing literature and then propose design strategies to help conceptualize future research.

14 SOLAR ENERGY↗

Altered Stability and Degradation Pathway of CH 3 NH 3 PbI 3 in Contact with Metal Oxide

Degradation in CH 3 NH 3 PbI 3 (MAPbI 3 ), when in contact with commonly used metal oxide transport layer materials in optoelectronic devices, is explored experimentally and theoretically. On the basis of the decomposition temperature, the interfacial stability decreases in the following order: MAPbI 3 + TiO 2 ~ MAPbI 3 alone > MAPbI 3 + SnO 2 > MAPbI 3 + NiO, consistent with thermodynamic data. When MAPbI 3 contacts NiO or SnO 2 , experimental results unequivocally show interfacial decomposition occurs at a lower temperature than bulk decomposition and produces different degradation products. Density functional theory calculations reveal an altered reaction pathway on oxide surfaces and elucidate the difference between NiO and TiO 2 . Furthermore, these results pinpoint the importance of understanding the interaction between halide perovskite and other materials used in a device to achieve intrinsically stable devices.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Overcoming Degradation Pathways to Achieve Stable Blue Perovskite Light-Emitting Diodes

Mixed halide (Br/Cl) perovskite nanocrystals (NCs) that represent an advanced blue emitter commonly suffer from spectral instability and poor lifespan; notably, the lack of understanding of the failure mechanisms of these devices has restricted the future progress. Here, we determine that the degradation of CsPbBr x Cl 3– x NCs containing blue light-emitting diodes (LEDs) is due to the combination of two effects. Cl – drift among adjoining NCs under an electric field is found to induce a Cl-deficient material region in multiple NC layers, which dominates the unstable electroluminescence and causes fast degradation in the corresponding devices. In comparison, the monolayer NC devices that feature restricted anion drift pathways exhibit better operational stability; however, excess hole injection is demonstrated to induce irreversible chlorine loss in NCs. Such a process that largely arises from electrochemical oxidation of Cl – initiates a mild device failure in operation of tens of minutes. Through revealing these mechanisms, we modulate the devices’ construction and operational conditions to achieve a longer lifespan.

14 SOLAR ENERGY↗

Revisiting the activity of two poly(vinyl chloride)- and polyethylene-degrading enzymes

Biocatalytic degradation of non-hydrolyzable plastics is a rapidly growing field of research, driven by the global accumulation of waste. Enzymes capable of cleaving the carbon-carbon bonds in synthetic polymers are highly sought-after as they may provide tools for environmentally friendly plastic recycling. Despite some reports of oxidative enzymes acting on non-hydrolyzable plastics, including polyethylene or poly(vinyl chloride), the notion that these materials are susceptible to efficient enzymatic degradation remains controversial, partly driven by a general lack of studies independently reproducing previous observations. Here, we attempt to replicate two recent studies reporting that deconstruction of polyethylene and poly(vinyl chloride) can be achieved using an insect hexamerin from Galleria mellonella (so-called “Ceres”) or a bacterial catalase-peroxidase from Klebsiella sp., respectively. Reproducing previously described experiments, we do not observe any activity on plastics using multiple reaction conditions and multiple substrate types. Digging deeper into the discrepancies between the previous data and our observations, we show how and why the original experimental results may have been misinterpreted.

36 MATERIALS SCIENCE↗

Reactive transport modeling of organic carbon degradation in marine methane hydrate systems

Abstract Natural methane hydrate has often been observed in sand layers that contain no particulate organic carbon (POC), but are surrounded by organic-rich, fine-grained marine muds. In this paper, we develop a reactive transport model (RTM) of a microbially-mediated set of POC degradation reactions, including hydrolysis of POC driven by extracellular enzymes, fermentation of the resulting high-molecular weight dissolved organic carbon (HMW-DOC), and methanogenesis that consumes low-molecular weight dissolved organic carbon (LMW-DOC). These processes are mediated by two groups of microbes, fermenters and methanogens that are heterogeneously distributed in different lithologies, with the largest numbers of microbes in the large pores of coarse-grained layers. We find that the RTM can reproduce methane hydrate occurrences observed in two different geological environments, at Walker Ridge Site 313-H (Gulf of Mexico) and IODP Site U1325 (Cascadia Margin). We also find that microbes can degrade POC even if they are physically separated, as extracellular enzymes and DOC can diffuse away from where they are produced by microbes. Microbial activity is highest at relatively early times after burial at shallow depths and near lithological boundaries, where concentration gradients transport solutes to intervals that contain the most microbes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atomic structure of light-induced efficiency-degrading defects in boron-doped Czochralski silicon solar cells

Boron-doped Czochralski (Cz) Si is the most commonly used semiconductor in the fabrication of solar cells. The minority carrier lifetime of boron-doped Cz Si decreases upon exposure to light due to B–O-related defects, which reduce the performance of ~10 9 solar modules worldwide. Using electron paramagnetic resonance (EPR), we have identified the spin-active paramagnetic signatures of this phenomenon and gained insights into its microscopic mechanism. We found a distinct defect signature, which diminished when the degraded sample was annealed. The second signature, a broad magnetic field spectrum, due to the unionized B acceptors, was present in the annealed state but vanished upon light exposure. These observations show that, on degradation, nearly all the ~10 16 cm –3 B atoms in Cz Si complexed with interstitial O atoms, whereas only ~10 12 cm –3 of these complexes created defects that were recombination-active. The formation rate of these recombination-active defects correlated with the decay of the minority carrier lifetime. Furthermore, the line shape parameters linked these defects to both B and O impurities in Cz Si.

14 SOLAR ENERGY↗

Analysis of thermochemical energy storage in metal carbonates: characterizing cycling-induced degradation

A solid–gas reaction rate modeling framework is applied to characterize degradation in thermochemical materials induced by thermal cycling. Time constants and a kinetic conversion ratio are established for a representative carbonation-calcination reaction, which provides insight into degradation mechanisms and reveals a mitigation strategy by tuning reaction duration.

25 ENERGY STORAGE↗

Degradation of Monocrystalline Silicon Photovoltaic Modules From a 10-Year-Old Rooftop System in Florida

A system of 180 monocrystalline aluminum back-surface field modules were installed in Cocoa, Florida, for 10 years. In total, 156 modules are characterized and compared to 3 controls. Power degradation rates vary between – 0.14% to – 3.22% per year, with median and average rates of –0.92% and –1.05% per year, respectively. The losses are primarily resistive with minor optical and recombination loss contributions. Electroluminescence imaging shows a characteristic pattern, which is shown to be resistive in nature when compared to photoluminescence. Resistive losses are due to corrosion of the rear contact Ag/solder interface and, to a much lesser degree, gridline Ag oxidation. Moisture ingress through the backsheet is likely responsible for mediating corrosion. Optical losses are due mostly to a combination of antireflection coating degradation, minor encapsulant browning, and delamination. Minor front contact corrosion may contribute to recombination. Furthermore, this study expands upon previous work on this vintage of the module by examining a large sample set, comprehensive characterization including techniques not previously used on these modules, and a comparison between two other systems of different climates.

14 SOLAR ENERGY↗

The Economic Impact of Battery Degradation Modelling Uncertainty

Battery energy storage systems (BESS) are used for a variety of applications, with their economic benefit often being the decisive factor for deployment. A multitude of physico-chemical aging mechanisms lead to capacity fade over a BESS life cycle. The models that are used to describe this capacity fade are prone to inherent model errors. Through a holistic techno-economic modelling approach, we investigate the impact of battery degradation modelling uncertainty on the economic benefit of representative BESS applications. Here, it is shown how improved parameter fit quality can reduce the resulting economic uncertainty. Furthermore, we highlight that the consideration of degradation modelling uncertainty is especially crucial when: (i) the cash flow highly depends on the available battery capacity, (ii) a fixed, e.g. warranty mandated, state of health limit acts as the threshold for battery end-of-life, (iii) long evaluation periods and low discount rates are the focus of economic evaluation.

aging↗

Activation Energy for Solder Bond Degradation: Thermal Cycling of Field-aged Modules at Multiple Upper Temperatures

The reliability of solder joints in the solar cell metallization-interconnect system influences the lifetime of photovoltaic modules. Two field-aged modules-one with Sn 62 Pb 36 Ag 2 solder at the solder joints (Solarex MSX 60), and the other with the standard Sn 60 Pb 40 solder (Siemens M55)-were subjected to a modified thermal cycling (TC) test of IEC 61215. Three sections in each module were maintained at 85 degrees C, 95 degrees C, and 105 degrees C during the 15-minute high temperature dwell time. Current equivalent to the module short-circuit current was injected through the module when the chamber temperature was above 25 degrees C to simulate regular field operation. This novel approach aims to induce thermomechanical fatigue (TMF) at the solder joints and intermetallic compound (IMC) formation at the metal/solder interfaces. The activation energy (E a ) for solder bond degradation was calculated based on the series resistance (R s ) increase in TC testing rather than power drop to avoid the effect of confounding variables. Module-level R s increase in MSX 60 module after TC800 cycles and in M55 module after TC400 cycles was 1.22% and 183.7%, respectively. The E a determined for the module with 2wt% Ag is 0.24 eV and for that with the standard solder is 0.27 eV. The solder bond degradation seems to have been driven by TMF rather than IMC formation for both modules.

14 SOLAR ENERGY↗

Spectral Rear Irradiance Testing and Modeling for Degradation and Performance of Solar Fields

This work investigates how the spectrum of irradiance incident on the rear of solar modules impacts the degradation and performance of backsheets. We model the spectral irradiance incident on the rear of modules through raytrace simulations and validate with measured field data collected from a 75kW single axis-tracked bifacial test site. A generic equation to estimate relative degradation is proposed, and we show that current acceleration factors for UV damage in chambers can be sub-estimate up to 4.5% absolute from the usually assumed 10% dosage on the rear surfaces.

bifacial performance↗

Near-Busbar Degradation of Screen-Printed Metallization in Silicon Photovoltaic Modules

We study photovoltaic (PV) module degradation after extended accelerated stress testing including 2000 hours of damp heat followed by a current-injection procedure meant to stabilize defects linked to light-induced degradation. In addition to de-stabilization/recovery of light-induced defects, we observe severe series resistance due to loss of contact between the Si cell and near-busbar screen-printed metallization (i.e. grid finger delamination). Using scanning electron microscopy and energy dispersive x-ray spectroscopy on cell fragments cored from the module, we show poor contact is caused by a gap between the screen-printed Ag metallization and Si due to missing glass frit.

degradation↗

Identification and widespread environmental distribution of a gene cassette implicated in anaerobic dichloromethane degradation

Anthropogenic activities and natural processes release dichloromethane (DCM, methylene chloride), a toxic chemical with substantial ozone-depleting capacity. Specialized anaerobic bacteria metabolize DCM; however, the genetic basis for this process has remained elusive. Comparative genomics of the three known anaerobic DCM-degrading bacterial species revealed a homologous gene cluster, designated the methylene chloride catabolism (mec) gene cassette, comprising 8–10 genes encoding proteins with 79.6%–99.7% amino acid identities. Functional annotation identified genes encoding a corrinoid-dependent methyltransferase system, and shotgun proteomics applied to two DCM-catabolizing cultures revealed high expression of proteins encoded on the mec gene cluster during anaerobic growth with DCM. In a DCM-contaminated groundwater plume, the abundance of mec genes strongly correlated with DCM concentrations (R 2 = 0.71–0.85) indicating their potential value as process-specific bioremediation biomarkers. mec gene clusters were identified in metagenomes representing peat bogs, the deep subsurface, and marine ecosystems including oxygen minimum zones (OMZs), suggesting a capacity for DCM degradation in diverse habitats. Here, the broad distribution of anaerobic DCM catabolic potential infers a role for DCM as an energy source in various environmental systems, and implies that the global DCM flux (i.e., the rate of formation minus the rate of consumption) might be greater than emission measurements suggest.

59 BASIC BIOLOGICAL SCIENCES↗

Characterizing degraded visual environments with scanning lenses to improve contrast recovery

Atmospheric aerosols, such as fog and smoke, degrade optical signals via the scattering and absorption of light, making it difficult to recover information from the surrounding environment. Here, we present a technique that measures the angular distribution of light in scattering environments to help recover these degraded optical signals. This is done by passing a collimated beam through the aerosol environment and collecting the scattered and unscattered light with an f-theta scan lens. The lens transforms the angular distribution of the scattered light into the linear domain, mapping the collected light onto a detector. The measured angular scattering distribution is then used to estimate the point spread function of the environment at an arbitrary stand-off distance. This point spread function can be used to deconvolve images blurred by the aerosol environment in which the angular scattering distribution was initially measured. With this approach, we demonstrate improvements in the effective resolution of deblurred images up to 26% over a 120-cm stand-off distance. Experimentation was performed in the Sandia National Laboratories tabletop fog chamber, a platform that generates aerosol environments analogous to real-world fogs. We intend to leverage this technique in future work to develop a low-SWaP system for the in situ characterization of aerosol environments.

Aerosols↗

Strong-Bonding Hole-Transport Layers Reduce Ultraviolet Degradation of Perovskite Solar Cells

The light-emitting diodes (LEDs) used in indoor testing of perovskite solar cells do not expose them to the levels of ultraviolet (UV) radiation that they would receive in actual outdoor use. We report degradation mechanisms of p-i-n-structured perovskite solar cells under unfiltered sunlight and with LEDs. Weak chemical bonding between perovskites and polymer hole-transporting materials (HTMs) and transparent conducting oxides (TCOs) dominate the accelerated A-site cation migration, rather than direct degradation of HTMs. An aromatic phosphonic acid, [2-(9-ethyl-9H-carbazol-3-yl)ethyl]phosphonic acid (EtCz3EPA), enhanced bonding at the perovskite/HTM/TCO region with a phosphonic acid group bonded to TCOs and a nitrogen group interacting with lead in perovskites. A hybrid HTM of EtCz3EPA with strong hole-extraction polymers retained high efficiency and improved the UV stability of perovskite devices, and a champion perovskite minimodule-independently measured by the Perovskite PV Accelerator for Commercializing Technologies (PACT) center-retained operational efficiency of >16% after 29 weeks of outdoor testing.

14 SOLAR ENERGY↗

Long-term impact of light- and elevated temperature-induced degradation on photovoltaic arrays

Low levelized cost of electricity (LCOE) has been identified as critical for widespread adoption of photovoltaics (PV) without subsidies. Maintaining decades-long high-energy production is often an under-recognized opportunity in meeting cost goals because component lifetimes are not fully quantified at the time of manufacture. Whereas certain standardized tests minimize risk of early failure, there is little guidance to quantitatively predict degradation (or lack thereof) over decades, based on accelerated tests. In this article, we move toward bridging the understanding between indoor accelerated tests and outdoor performance data, with the goal of predicting energy yield with enough accuracy to inform financial decisions. Light- and elevated temperature-induced degradation (LETID) in p-type Si modules is analyzed in terms of impact on long-term module performance and thus LCOE. A method to predict the progression of LETID, using fixed kinetic constants and a numerical solution to the basic reaction rate equations, is detailed. Predictions are compared against both published data and that new to this study. These data include both indoor accelerated tests and fielded modules. We use the results in financial models to derive LCOE of modules in different climates with varying amounts of LETID, including uncertainty. Cost models based on the predictions indicate that LETID has a significant and climate-dependent impact on LCOE. Finally, we show that - even given the uncertainties identified in the study - these financial calculations can provide useful guidance to quantify risk based on accelerated test results. The analysis serves as an example of developing a predictive approach to PV reliability using physics of failure.

14 SOLAR ENERGY↗

Excess carrier concentration in silicon devices and wafers: How bulk properties are expected to accelerate light and elevated temperature degradation

Light and elevated temperature induced degradation (LeTID) is accelerated nearly linearly by the presence of excess carriers. It is therefore important to understand how excess carrier concentration (Δn) changes as a function of exposure conditions, materials properties, and sample structure. We simulate Δn as a function of wafer thickness and bulk minority carrier lifetime (τ) in solar cells and wafers using SCAPS and Quokka3. We also derive closed-form analytic expressions. For wafers, there is a near-linear relationship between Δn and τ or thickness, whereas for solar cells, Δn in the bulk may become limited by rear surface recombination. Thus, LeTID may progress more quickly in wafers than in cells, with a stronger dependence on τ. When comparing experiments, observed degradation rates must be corrected between samples or conditions to account for differences in Δn. This study demonstrates three tools to estimate the magnitude of such corrections, which can aid in the quantitative interpretation of LeTID data and performance predictions. Finally, while each tool yields similar results, there are advantages to each approach that must be weighed in terms of simplicity of inputs versus sophistication of treatment. Incomplete specification of back contact characteristics in commercial products is identified as an important contributor to uncertainty in expected LeTID rates.

36 MATERIALS SCIENCE↗