Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STACKING FAULTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

Surface effects on the radiation response of nanoporous Au foams

We report on an experimental and simulation campaign aimed at exploring the radiation response of nanoporous Au (np-Au) foams. We find different defect accumulation behavior by varying radiation dose-rate in ion-irradiated np-Au foams. Stacking fault tetrahedra are formed when np-Au foams are irradiated at high dose-rate, but they do not seem to be formed in np-Au at low dose-rate irradiation. A model is proposed to explain the dose-rate dependent defect accumulation based on these results.

36 MATERIALS SCIENCE↗

Properties of the main Mg-related acceptors in GaN from optical and structural studies

The luminescent properties of Mg-doped GaN have recently received particular attention, e.g., in the light of new theoretical calculations, where the deep 2.9 eV luminescence band was suggested to be the main optical signature of the substitutional Mg{sub Ga} acceptor, thus, having a rather large binding energy and a strong phonon coupling in optical transitions. We present new experimental data on homoepitaxial Mg-doped layers, which together with the previous collection of data give an improved experimental picture of the various luminescence features in Mg-doped GaN. In n-type GaN with moderate Mg doping (<10{sup 18} cm{sup −3}), the 3.466 eV ABE1 acceptor bound exciton and the associated 3.27 eV donor-acceptor pair (DAP) band are the only strong photoluminescence (PL) signals at 2 K, and are identified as related to the substitutional Mg acceptor with a binding energy of 0.225 ± 0.005 eV, and with a moderate phonon coupling strength. Interaction between basal plane stacking faults (BSFs) and Mg acceptors is suggested to give rise to a second deeper Mg acceptor species, with optical signatures ABE2 at 3.455 eV and a corresponding weak and broad DAP peak at about 3.15 eV. The 2.9 eV PL band has been ascribed to many different processes in the literature. It might be correlated with another deep level having a low concentration, only prominent at high Mg doping in material grown by the Metal Organic Chemical Vapor Deposition technique. The origin of the low temperature metastability of the Mg-related luminescence observed by many authors is here reinterpreted and explained as related to a separate non-radiative metastable deep level defect, i.e., not the Mg{sub Ga} acceptor.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of hot-pressed short ZrO{sub 2} fiber toughened ZrB{sub 2}-based ultra-high temperature ceramics

Two different ZrB{sub 2}-based ultra-high temperature ceramics were produced by hot pressing: ZrB{sub 2} + 20 vol.% SiC particle + 15 vol.% ZrO{sub 2} fiber and ZrB{sub 2} + 20 vol.% SiC whisker + 15 vol.% ZrO{sub 2} fiber. The microstructures were analyzed by using transmission electron microscopy and high-resolution transmission electron microscopy. It was shown that a clean interface without any impurities was identified in ZrB{sub 2}-based hybrid ceramics with SiC whiskers and ZrO{sub 2} fibers, which would significantly improve the toughening mechanism. The results of high-resolution transmission electron microscopy showed that stacking faults in SiC whiskers resulted from an insertion of a (111) layer, which would be one of the main reasons for material anisotropy. However, the interface between the SiC particle and ZrO{sub 2} fiber was found to be ambiguous in ZrB{sub 2}-based hybrid ceramics with SiC particles and ZrO{sub 2} fibers due to the slight reaction. The orientation relationship between t-ZrO{sub 2} and m-ZrO{sub 2} phases obeyed the classical correspondence: (100){sub m}//(100){sub t} and [001]{sub m}//〈001〉{sub t}, which further verified the feasibility of phase transformation toughening mechanism. - Highlights: • ZrB{sub 2}-based ceramics toughened by short ZrO{sub 2} fiber are characterized by TEM and HRTEM. • The orientation relationship of t- and m-ZrO{sub 2} are (100){sub m}//(100){sub t}, [001]{sub m}//〈001〉{sub t} • The clean interface without any impurities leads to improve the toughening mechanism.

36 MATERIALS SCIENCE↗

Microstructure characterization of SiC nanowires as reinforcements in composites

SiC nanowires have been rarely investigated or explored along their axial direction by transmission electron microscopy (TEM). Here we report the investigation of the cross-section microstructure of SiC nanowires by embedding them into Al matrix. Morphology of SiC nanowires was cylindrical with smooth surface or bamboo shape. Cubic (3C-SiC) and hexagonal structure (2H-SiC) phases were detected by X-ray diffraction (XRD) analysis. High density stacking faults were observed in both the cylindrical and bamboo shaped nanowires which were perpendicular to their axial direction. Selected area electron diffraction (SAED) patterns of the cylindrical and bamboo shaped SiC nanowires both in the perpendicular and parallel direction to the axial direction were equivalent in the structure. After calculation and remodeling, it has been found that the SAED patterns were composed of two sets of diffraction patterns, corresponding to 2H-SiC and 3C-SiC, respectively. Therefore, it could be concluded that the SiC nanowires are composed of a large number of small fragments that are formed by hybrid 3C-SiC and 2H-SiC structures. - Graphical abstract: Display Omitted - Highlights: • Cross-section microstructure of SiC nanowires was observed in Al composite. • Cylindrical with smooth surface or bamboo shape SiC nanowires were found. • The cylindrical and bamboo shaped SiC nanowires were equivalent in structure. • Structure of SiC nanowires was remodeled. • SiC nanowires are composed of hybrid 3C-SiC and 2H-SiC structures.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Development of a semi-empirical potential for simulation of Ni solute segregation into grain boundaries in Ag

An Ag–Ni semi-empirical potential was developed to simulate the segregation of Ni solutes at Ag grain boundaries (GBs). The potential combines a new Ag potential fitted to correctly reproduce the stable and unstable stacking fault energies in this metal and the existing Ni potential from Mendelev et al (2012 Phil. Mag. 92 4454–69). The Ag–Ni cross potential functions were fitted to ab initio data on the liquid structure of the Ag 80 Ni 20 alloy to properly incorporate the Ag–Ni interaction at small atomic separations, and to the Ni segregation energies at different sites within a high-energy Σ9 (221) symmetric tilt GB. By deploying this potential with hybrid Monte Carlo/molecular dynamics simulations, it was found that heterogeneous segregation and clustering of Ni atoms at GBs and twin boundary defects occur at low Ni concentrations, 1 and 2 at%. This behavior is profoundly different from the homogeneous interfacial dispersion generally observed for the Cu segregation in Ag. A GB transformation to amorphous intergranular films was found to prevail at higher Ni concentrations (10 at%). In conclusion, the developed potential opens new opportunities for studying the selective segregation behavior of Ni solutes in interface-hardened Ag metals and its effect on plasticity.

36 MATERIALS SCIENCE↗

< c+a > dislocations in {101 - 2} twins in Mg: A kinematic and energetic requirement

Consideration of published TEM and molecular dynamics studies of interactions between matrix dislocations and {101¯2} twin boundaries (TB) in hexagonal close packed metals inspires a hypothesis regarding the formation of dislocations with < c+a > Burgers vectors inside the twins. It was previously reported that when basal < a > dislocations from the matrix are swept by an advancing TB, they are converted into partial dislocations bounding basal I 1 stacking faults (SFs) within the twin. In the present work, we show that this dislocation configuration near TB renders it energetically favorable for a pair of partial dislocations to constrict into a dislocation within the twin. New in situ TEM observations confirm this hypothesis by revealing long < c+a > dislocation dipoles terminated by the TB at one end and by I1 SFs within the twin at the other end. Finally, the resulting near-screw < c+a > dislocation dipoles are observed to be glissile, enabling self-annihilation in some circumstances. Thus, rather than requiring a high energy dislocation pile-up to press two < a > dislocations through a TB into a single < c+a > dislocation, it is demonstrated that < c+a > dislocations naturally form, within {101¯2} twins in Mg, as TB migrates into a matrix, which inevitably contains dislocations with < a > Burgers vectors. Furthermore, these observations help to explain how the twins themselves may subsequently deform and why they may be particularly vulnerable to plastic, shear localization.

36 MATERIALS SCIENCE↗

Effect of Mn addition on deformation behaviour of 23% Cr low nickel duplex stainless steel

Highlights: • Increasing Mn content obviously affects dynamic softening behaviour of flow curves. • More complete austenite DRX occurred with middle Mn addition of 10.3% at 1 s{sup −1}. • The constitutive equations for different Mn addition alloys are developed. • The values of activation energy and Z parameter are lowest with middle Mn addition. • Different Mn addition processing maps with increasing strain were established. - Abstract: Isothermal compression testing of 23% Cr low nickel duplex stainless steels, with different Mn concentrations, was investigated in the temperature range of 1173–1423 K, the strain rate range of 0.01–10 s{sup −1} and with a height reduction of 70%. Increasing the Mn content from 6.3 to 14.1% affected the deformation dynamic softening behaviour of flow curves at lower temperature and higher strain rate. It was also observed that increasing the deformation stain rate contributed to flow softening, and was caused by dynamic recrystallization (DRX) as a function of Mn addition. Deformation microstructure analysis demonstrated that more complete austenite phase DRX occurred with 10.3% Mn addition than that with 6.3% Mn addition at 1 s{sup −1}, but an excessive Mn content of 14.1% was unfavourable due to the increase of austenite fraction and stacking fault energy enhancement. Increasing the strain rate to 10 s{sup −1} promoted austenite phase DRX at 1323 K with the Mn addition under large strain. Meanwhile, the ferrite phase DRX occurred at 1173 K/1–10 s{sup −1} with 6.3% Mn, and was weakened with higher Mn addition. Compared to the 6.3% and 14.1% Mn, continuous DRX occurred at 1323 K/1 s{sup −1} with 10.3% Mn, due to the larger fraction of high angle misorientations. The values for the activation energy and Zener–Hollomon parameter decreased with Mn addition from 6.3 to 10.3%, and then increased with a higher Mn addition of 14.1%, indicating that a proper content of Mn addition can reduce the thermal deformation resistance and promote DRX. The constitutive equations for different Mn addition alloys were developed using a hyperbolic sine equation. Processing maps with different Mn addition for the strains of 0.3, 0.6 and 1.2 were established. The 10.3% Mn content sample corresponded to the lowest instability region, implying that the workability was improved with the middle Mn addition.

36 MATERIALS SCIENCE↗

Suppression of vacancy cluster growth in concentrated solid solution alloys

Large vacancy clusters, such as stacking-fault tetrahedra, are detrimental vacancy-type defects in ion-irradiated structural alloys. Suppression of vacancy cluster formation and growth is highly desirable to improve the irradiation tolerance of these materials. In this paper, we demonstrate that vacancy cluster growth can be inhibited in concentrated solid solution alloys by modifying cluster migration pathways and diffusion kinetics. The alloying effects of Fe and Cr on the migration of vacancy clusters in Ni concentrated alloys are investigated by molecular dynamics simulations and ion irradiation experiment. While the diffusion coefficients of small vacancy clusters in Ni-based binary and ternary solid solution alloys are higher than in pure Ni, they become lower for large clusters. This observation suggests that large clusters can easily migrate and grow to very large sizes in pure Ni. In contrast, cluster growth is suppressed in solid solution alloys owing to the limited mobility of large vacancy clusters. Finally, the differences in cluster sizes and mobilities in Ni and in solid solution alloys are consistent with the results from ion irradiation experiments.

36 MATERIALS SCIENCE↗

A Study of Tensile Flow and Work-Hardening Behavior of Alloy 617

The simple power relationship σ = Κε{sub p}{sup n} satisfactorily expresses the tensile flow behavior of many metals and alloys in their uniform plastic strain regime. However, many FCC materials with low stacking fault energy have opposed such power law relationship. Alloy 617, an age-hardenable Ni-based superalloy is also observed not to obey the simple power law relationship neither in its solution-treated nor in its aged conditions. Various flow relationships were used to obtain the best fit for the tensile data, and different relationships were identified for the different aged conditions. The work-hardening rate (θ) demonstrates three distinct regions for all aged conditions, and there is an obvious change in the trend of θ versus σ. In the initial portion, θ decreases rapidly followed by a gradual increase in the second stage and again a decrease in its third stage is perceived in the Alloy 617. These three-stage characteristics are attributed to a commonly known precipitate, γ′: Ni{sub 3}(Ti, Al) which evolves during aging treatment and well recognized under transmission electron microscopy (TEM) observation. TEM results also reveal a slight degree of coarsening in γ′ over aging. The tensile flow and the work-hardening behavior are well correlated with other microstructural evolution during the aging treatments.

36 MATERIALS SCIENCE↗

Polarized photoluminescence excitation spectroscopy of a-plane InGaN/GaN multiple quantum wells grown on r-plane sapphire

We have performed a detailed study of the impact of basal plane stacking faults (BSFs) on the optical properties of both a-plane InGaN/GaN quantum wells (QWs) and GaN template samples grown on r-sapphire. In particular, we have used polarised photoluminescence excitation spectroscopy (P-PLE) to investigate the nature of the low temperature recombination as well as extracting information on the valence band (VB) polarisation anisotropy. Our low temperature P-PLE results revealed not only excitons associated with intersubband quantum well transitions and the GaN barrier material but also a transition associated with creation of excitons in BSFs. The strength of this BSF transition varied with detection energy across the quantum well emission suggesting that there is a significant contribution to the emission line width from changes in the local electronic environment of the QWs due to interactions with BSFs. Furthermore, we observed a corresponding progressive increase in the VB splitting of the QWs as the detection energy was varied across the quantum well emission spectrum.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructural Engineering of Mn-Alloyed Austenitic Steel for Hydrogen Storage and Delivery

Austenitic stainless steels are commonly used for hydrogen storage and transportation. These alloys have a high nickel (Ni) content, which increases alloy cost. In this study, high manganese (Mn) austenitic alloys were evaluated as potential lower cost alternatives. Two heats of high Mn alloys with different stacking fault energies (SFE) of ~29 mJ·m -2 and 49 mJ·m -2 were acquired. Additionally, a new vanadium (V)-microalloyed high Mn alloy was designed to achieve a SFE of 47 mJ·m -2 to minimize planar slip deformation mechanisms. Post-processing via cold working in conjunction with aging was also performed on the V-microalloyed high Mn steel. Hydrogen embrittlement sensitivity was investigated using circumferential notch tensile specimens cathodically charged with hydrogen in a 0.05M NaOH electrolytic solution. The alloys were compared to a cold-worked 316L stainless steel, which exhibited no strength loss due to hydrogen. The high Mn alloys with SFE of ~29 mJ·m 2 and 49 mJ·m -2 had notch strength losses of 11 and 6 pct, respectively. The V-microalloyed high Mn steel in the as-hot-rolled condition had a notch strength loss of 17 pct. Furthermore, the V-microalloyed high Mn steel in the cold worked and aged condition indicated no notch strength loss in hydrogen, which was comparable to the performance of the 316L stainless steel.

36 MATERIALS SCIENCE↗

Mechanical behavior of a composite interface: Calcium-silicate-hydrates

The generalized stacking fault (GSF) is a conceptual procedure historically used to assess shear behavior of defect-free crystalline structures through molecular dynamics or density functional theory simulations. We apply the GSF technique to the spatially and chemically complex quasi-layered structure of calcium-silicate-hydrates (C-S-H), the fundamental nanoscale binder within cementitious materials. A failure plane is enforced to calculate the shear traction-displacement response along a composite interface containing highly confined water molecules, hydroxyl groups, and calcium ions. GSF simulations are compared with affine (homogeneous) shear simulations, which allow strain to localize naturally in response to the local atomic environment. Comparison of strength and deformation behavior for the two loading methods shows the composite interface controls bulk shear deformation. Both models indicate the maximum shear strength of C-S-H exhibits a normal-stress dependency typical of cohesive-frictional materials. These findings suggest the applicability of GSF techniques to inhomogeneous structures and bonding environments, including other layered systems such as biological materials containing organic and inorganic interfaces.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Bamboo-like 3C-SiC nanowires with periodical fluctuating diameter: Homogeneous synthesis, synergistic growth mechanism, and their luminescence properties

Herein, bamboo-like 3C-SiC nanowires have been successfully fabricated on homogeneous 6H-SiC substrate by a simple chemical vapor reaction (CVR) approach. The obtained 3C-SiC nanostructure with periodical fluctuating diameter, is composed of two alternating structure units, the typical normal-sized stem segment with perfect crystallinity and obvious projecting nodes segment having high-density stacking faults. The formation of the interesting morphology is significantly subjected to the peculiar growth condition provided by the homogeneous substrate as well as the varying growth elastic energy. Furthermore, the photoluminescence (PL) performance measured on the bamboo-like SiC nanowire shows an intensive emission peaks centered at 451 nm and 467 nm, which has been expected to make a positive progress toward the optical application of the SiC-based one-dimensional (1D) nanostructures, such as light emission diode (LED). - Graphical abstract: Based on the synergistic growth mechanism from homogeneous substrate and elastic energy, bamboo-like 3C-SiC nanowires with periodically fluctuating diameter have been synthesized on 6H-SiC. The blue-violet light emission properties of the bamboo-like nanowires have also been investigated for exploring their peculiar optical application. - Highlights: • Bamboo-like 3C-SiC nanowires with periodically fluctuating diameter have been synthesized on 6H-SiC. • A synergistic growth mechanism from homogeneous substrate and elastic energy has been proposed firstly. • The blue-violet light emission properties of the products displayed peculiar optical application.

36 MATERIALS SCIENCE↗

Characterization of Metamorphic GaAsP/Si Materials and Devices for Photovoltaic Applications

GaAsyP{sub 1-y} anion-sublattice compositionally graded buffers and device structures were grown directly on Si(100) substrates by way of a high-quality GaP integration layer, yielding GaAsP target layers having band gaps of photovoltaic interest (1.65-1.8 eV), free of antiphase domains/borders, stacking faults, and microtwins. GaAsyP{sub 1-y} growths on both Si and GaP substrates were compared via high-resolution X-ray diffractometry of the metamorphic buffers and deep-level transient spectroscopy (DLTS) of p{sup +}-n diodes that are lattice matched to the final buffer layer. Structural analysis indicates highly efficient epitaxial relaxation throughout the entire growth structure for both types of samples and suggests no significant difference in physical behavior between the two types of samples. DLTS measurements performed on GaAsP diodes fabricated on both Si and GaP substrates reveal the existence of identical sets of traps residing in the n-type GaAsP layers in both types of samples: a single majority carrier (electron) trap, which is located at EC - 0.18&nbsp;eV, and a single minority carrier (hole) trap, which is located at EV + 0.71&nbsp;eV. Prototype 1.75-eV GaAsP solar cell test devices grown on GaAsyP{sub 1-y}/Si buffers show good preliminary performance characteristics and offer great promise for future high-efficiency III-V photovoltaics integrated with Si substrates and devices.

14 SOLAR ENERGY↗

The influence of temperature on the strain-hardening behavior of Fe-22/25/28Mn-3Al-3Si TRIP/TWIP steels

In this work, the influence of temperature and stacking fault energy (SFE) on the strain-hardening behavior and critical resolved shear stress for twinning was investigated for three Fe–22/25/28Mn–3Al–3Si wt.% transformation- and twinning-induced plasticity (TRIP/TWIP) steels. The SFEs were calculated by two different methods, density functional theory and statistical thermodynamic modeling. The dislocation structure, observed at low levels of plastic deformation, transitions from “planar” to “wavy” dislocation glide with an increase in temperature, Mn content, and/or SFE. The change in dislocation glide mechanisms from planar to wavy reduces the strain hardening rate, in part due to fewer planar obstacles and greater cross slip activity. Additionally, the alloys exhibit a large decrease in strength and ductility with increasing temperature from 25 to 200 °C, attributed to a substantial reduction in the thermally activated component of the flow stress, predominate suppression of TRIP and TWIP, and a significant increase in the critical resolved shear stress for mechanical twinning. Interestingly, the increase in SFE with temperature had a rather minor influence on the critical resolved shear stress for mechanical twinning, and other temperature dependent factors which likely play a more dominant role are discussed.

36 MATERIALS SCIENCE↗

Effect of short-range order on microstructure, texture and strain hardening of cold drawn Cu-10 at.%Mn alloy

Highlights: • Excluding the effect of stacking fault energy, short-range order effect is discussed solely. • Short-range order is beneficial for twinning and slip planarity. • Short-range order promotes the formation of <111> fiber texture. • Strain hardening improving by short-range order. - Abstract: The aim of the present study is to investigate the effect of short-range order (SRO) on the microstructural evolution and mechanical property of Cu-10 at.%Mn alloy during cold drawing deformation. Characterization of the cold drawn Cu-10 at.%Mn alloy samples were performed using transmission electron microscope (TEM) and electron back scattering diffraction (EBSD), and their hardness were also tested. The results show that SRO is beneficial for both twinning and the transition of dislocation glide from wavy slip to planar slip at the low strains. At the high strains, the wavy slip generates due to the destruction of SRO. SRO increases the volume fraction of <111> texture component and the critical strain threshold. Moreover, the presence of SRO significantly improves strain hardening by combining the effects of dislocation, deformation twinning and texture hardening, which results in a significant increase of hardness.

36 MATERIALS SCIENCE↗

Formation of deformation textures in face-centered-cubic materials studied by in-situ high-energy x-ray diffraction and self-consistent model.

The evolution of deformation textures in copper and a brass that are representative of fcc metals with different stacking fault energies (SFEs) during cold rolling is predicted using a self-consistent (SC) model. The material parameters used for describing the micromechanical behavior of each metal are determined from the high-energy X-ray (HEXRD) diffraction data. At small reductions, a reliable prediction of the evolution of the grain orientation distribution that is represented as the continuous increase of the copper and brass components is achieved for both metals when compared with the experimental textures. With increasing deformation, the model could characterize the textures of copper, i.e., the strengthening of the copper component, when dislocation slip is still the dominant mechanism. For a brass at moderate and large reductions, a reliable prediction of its unique feature of texture evolution, i.e., the weakening of the copper component and the strengthening of the brass component, could only be achieved when proper boundary conditions together with some specified slip/twin systems are considered in the continuum micromechanics mainly containing twinning and shear banding. The present investigation suggests that for fcc metals with a low SFE, the mechanism of shear banding is the dominant contribution to the texture development at large deformations.

36 MATERIALS SCIENCE↗

Understanding the deformation behavior of the γ rich transformative Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 complex concentrated alloy using in situ synchrotron diffraction

In situ tensile testing coupled with synchrotron x-ray diffraction was used to study the deformation behavior of metastability-engineered Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 complex concentrated alloy. Monitoring the evolution of phase fraction and strain hardening response allowed the determination of true critical stress for the onset of the transformation-induced plasticity (TRIP) to be ∼375 MPa, preceded by slip starting at ∼255 MPa. In situ EBSD was used to validate the critical stress for transformation at the microstructure level and observe slip traces to confirm prior slip activity before the transformation. Further, a modeling framework based on stacking fault energy (SFE) was developed to predict the critical stress for transformation. Modeling suggested the SFE of the alloy to fall nearly 15 mJ/m 2 , which agrees well with SFE values calculated using synchrotron peak shifting (12 mJ/m 2 ) and thermodynamic calculation (11 mJ/m 2 ). As a result of γ-fcc to ε-hcp phase transformation, new {0002} ε planes emerged parallel to unaligned {111} γ planes with the tensile loading following S-N orientation relationship. Such selective emergence of new diffraction rings corresponding to ε phase is understood based on the reorientation of γ crystals with reference to tensile axis. In conclusion, this approach can be extended to effectively design alloys based on critical stress required for activating different deformation mechanisms to further push the limits of the strength-ductility envelope.

Complex concentrated alloy↗