At least 505 records · Page 28

Definition and effect of chemical properties of surfaces in friction, wear, and lubrication

Much of the data relative to the properties of surfaces that have been used in the past in analyzing, interpreting and predicting adhesion, friction and wear behavior for solid surfaces is now suspect. With the advent of analytical surface tools, careful and complete characterization of surfaces indicate that very frequently the outermost layers of solid surfaces are markedly different in chemistry than had been previously thought. These layers, as will be shown, are extremely important in adhesion, friction and wear behavior. Some of the properties to be discussed in the paper relative to their role in adhesion, friction, wear and lubrication will include: (1) adsorption, both physical and chemical; (2) orientation of the solid as well as the lubricant; (3) surface energy; (4) surface segregation; (5) surface versus bulk metallurgical effects; (6) electronic nature of the surface; and (7) bonding mechanisms.

Buckley, D. H.↗

Lubrication and failure mechanisms of molybdenum disulfide films. 1: Effect of atmosphere

Friction, wear, and wear lives of rubbed molybdenum disulfide (MoS2 films applied to sanded 440C HT steel surfaces were evaluated in moist air, dry air, and dry argon. Optical microscope observations were made as a function of sliding distance to determine the effect of moisture and oxygen on the lubricating and failure mechanisms of MoS2 films. In general, the lubrication process consisted of the formation of a thin, metallic colored, coalesced film of MoS2 that flowed between the surfaces in relative motion. In air, failure was due to the transformation of the metallic colored, coalesced films to a black, powdery material. Water in the air appeared to accelerate the transformation rate. In argon, no transformation of MoS2 was observed with the microscope, but cracking and spalling of the coalesced film occurred and resulted in the gradual depletion of the film.

Fusaro, R. L.↗

Lubrication and failure mechanisms of molybdenum disulfide films. 2: Effect of substrate roughness

An optical microscope was used to study the lubrication and failure mechanisms of rubbed MoS2 films applied to three substrate surface finishes; polished, sanded, and sandblasted as a function of sliding distance. The lubrication mechanism was the plastic flow of thin films of MoS2 between flat plateaus on the rider and on the metallic substrate. If the substrate was rough, flat plateaus were created during run-in and the MoS2 flowed across them. Wear life was extended by increasing surface roughness since valleys in the roughened substrate served as reservoirs for MoS2 and as deposit sites for wear debris. In moist air the failure mechanism was the transformation of metallic colored MoS2 films to a black, powdery material that was found by X-ray diffraction to be alpha iron, MoO3, and possibly FeMoO3. In dry argon the failure mechanism was the gradual depletion of MoS2 from the contact region by transverse flow, and the wear debris on the track at failure was alpha iron, residual MoS2, and possibly FeS.

Fusaro, R. L.↗

Boundary lubrication, thermal and oxidative stability of a fluorinated polyether and a perfluoropolyether triazine

Boundary lubricating characteristics, thermal stability, and oxidation-corrosion stability were determined for a fluorinated polyether and a perfluoropolyether triazine. A ball-on-disk apparatus, a tensimeter, and oxidation-corrosion apparatus were used. Results were compared to data for a polyphenyl ether and a C-ether. The polyether and triazine yielded better boundary lubricating characteristics than either the polyphenyl ether or C-ether. The polyphenyl ether had the greatest thermal stability (443 C) while the other fluids had stabilities in the range 389 to 397 C. Oxidation-corrosion results indicated the following order of stabilities: perfluoropolyether trizine greater than polyphenyl ether greater than C-ether greater than fluorinated polyether.

Jones, W. R., Jr.↗

Wear of aluminum and hypoeutectic aluminum-silicon alloys in boundary-lubricated pin-on disk sliding

The friction and wear of pure aluminum and a number of hypoeutectic aluminum-silicon alloys (with 3 to 12 wt %Si) were studied with a pin-on-disk apparatus. The contacts were lubricated with mineral oil and sliding was in the boundary-lubrication regime at 2.6 cm/sec. Surfaces were analyzed with photomicrographs, scanning electron microscopy, X-ray dispersive analysis, and diamond pyramid hardness measurements. There were two wear regimes for the alloys - high and low - whereas pure aluminum exhibited a high wear rate throughout the test period. Wear rate decreased and the transition stress from high to low wear increased with increasing hardness. There was no correlation between friction coefficient and hardness. A least squares curve fit indicated a wear-rate dependence greater than the inverse first power of hardness. The lower wear rates of the alloys may be due to the composites of silicon platelets in aluminum resulting in increased hardness and thus impairing the shear of the aluminum.

Ferrante, J.↗

Positive commandable oiler for satellite bearing lubrication

The results of a feasibility study showed that on-orbit commandable lubrication of ball bearings can be accomplished by direct oil application to the moving ball surfaces. Test results for the lubricant applicator portion of the system are presented, in conjunction with a design approach for the reservoir and metering components.

James, G. E.↗

Auger spectroscopy analysis of lubrication with zinc dialkyldithiophosphate of several metal combinations in sliding contact

Sliding friction experiments were conducted with aluminum and other riders rubbing on disks of various elemental metals in the presence of a thin film of zinc dialkyldithiophosphate (ZDP). Auger emission spectroscopy was used to in situ monitor the changes in surface chemistry with rubbing under various loads. The metal disks examined included iron, titanium, rhodium, tungsten, molybdenum, and copper. For equivalent films of ZDP the film is a more effective lubricant for some metals than it is for others. The important active element in the compound varies with the metal lubricated and is a function of metal chemistry. The zinc in the ZDP is susceptible to electron beam induced desorption.

Buckley, D. H.↗

An evaluation of grease type ball bearing lubricants operating in various environments

Grease type lubricants in bearings were evaluated in five different adverse environments for a one year period. Four repetitions of each test were made to provide statistical samples. These tests were then used to select four lubricants for five year tests in selected environments with five repetitions of each test for statistical samples. Three five year tests were started in (1) continuous operation; (2) start-stop operation, with both in vacuum at ambient temperatures; and (3) continuous operation at 93.3 C. To date, in the one year tests, the best results in all environments were obtained with a high viscosity index perfluoroalkylpolyether grease.

Mcmurtrey, E. L.↗

Sputtering technology in solid film lubrication

Current and potential sputtering technology is reviewed as it applies primarily to the deposition of MoS2, though such lubricants as WS2 and PTFE are also considered. It is shown by electron microscopy and surface sensitive analytical techniques that the lubricating properties of sputtered MoS2 films are directly influenced by the sputtering parameters selected (i.e., power density, pressure, sputter etching, dc-biasing, etc.), substrate temperature, chemistry, topography, and environmental conditions during the friction test. Electron micrographs and diffractograms of sputtered MoS2 films clearly show the resultant changes in film morphology which affect film adherence and frictional properties.

Spalvins, T.↗

Shear strength measurements of lubricants at high pressure

Measurements of lubricant shear rheological behavior in the amorphous solid region and near the liquid-solid transition are reported on three lubricants under pressure. Elastic, plastic and viscous behavior was observed. The maximum yield shear stress (limiting shear stress) is a function of temperature and pressure and is believed to be the property which determines the maximum traction in elastohydrodynamic contacts such as traction drives.

Bair, S.↗

Lubrication handbook

Handbook is divided into two major parts: solid lubricants and liquid lubricants used in aerospace industry. Listed materials cover broad application spectrum from manufacturing and ground support to missile and spacecraft hardware. Handbook can serve as ready reference in design and maintenance service of industrial equipment.

Source record↗

Thermal elastohydrodynamic lubrication of spur gears

An analysis and computer program called TELSGE were developed to predict the variations of dynamic load, surface temperature, and lubricant film thickness along the contacting path during the engagement of a pair of involute spur gears. The analysis of dynamic load includes the effect of gear inertia, the effect of load sharing of adjacent teeth, and the effect of variable tooth stiffness which are obtained by a finite-element method. Results obtained from TELSGE for the dynamic load distributions along the contacting path for various speeds of a pair of test gears show patterns similar to that observed experimentally. Effects of damping ratio, contact ratio, tip relief, and tooth error on the dynamic load were examined. In addition, two dimensionless charts are included for predicting the maximum equilibrium surface temperature, which can be used to estimate directly the lubricant film thickness based on well established EHD analysis.

Wang, K. L.↗

Effects of supply conditions on film thickness in lubricated Hertzian contacts

A generalization of the hydrodynamic expression for Hertzian contacts is described and various methods for calculating the thickness of the oil film winter steady-state, isothermal conditions are given. This is important for engineering applications such as gears and bearings because these results are closer to real operating conditions. Theories of lubrication are discussed, and the mathematics involved are presented using approximately 30 equations and 13 figures. For lubricated, linear, elliptical or point Hertzian contacts it is demonstrated how to calculate the thickness of the oil film at the center of the contact for steady-state isothermal conditions.

Dalmaz, G.↗

Lubrication of optimized-design tapered-roller bearings to 2.4 million DN

The performance of 120.65 mm (4.75 in.) bore high speed design, tapered roller bearings was investigated at shaft speeds to 20,000 rpm (2.4 million DN) under combined thrust and radial load. The test bearing design was computer optimized for high speed operation. Temperature distribution bearing heat generation were determined as a function of shaft speed, radial and thrust loads, lubricant flow rates, and lubricant inlet temperature. The high speed design, tapered roller bearing operated successfully at shaft speeds up to 20,000 rpm under heavy thrust and radial loads. Bearing temperatures and heat generation with the high speed design bearing were significantly less than those of a modified standard bearing tested previously. Cup cooling was effective in decreasing the high cup temperatures to levels equal to the cone temperature.

Parker, R. J.↗

Boundary lubrication, thermal and oxidative stability of a fluorinated polyether and a perfluoropolyether triazine

Boundary lubricating characteristics, thermal stability and oxidation-corrosion stability were determined for a fluorinated polyether and a perfluoropolyether triazine. A ball-on-disk apparatus, a tensimeter and oxidation-corrosion apparatus were used. Results were compared to data for a polyphenyl ether and a C-ether. The polyether and triazine yielded better boundary lubricating characteristics than either the polyphenyl ether or C-ether. The polyphenyl ether had the greatest thermal stability (443 C) while the other fluids had stabilities in the range 389 to 397 C. Oxidation-corrosion results indicated the following order of stabilities: perfluoropolyether triazine greater than polyphenylether greater than C-ether greater than fluorinated polyether.

Jones, W. R., Jr.↗

Effect of Substrate Surface Finish on the Lubrication and Failure Mechanisms of Molybdenum Disulfide Films

An optical microscope was used to study the lubrication and failure mechanisms of rubbed (burnished) MoS2 films applied to three substrate surface finishes - polished, sanded, and sandblasted - as a function of sliding distance. The lubrication mechanism was the plastic flow of thin films of MoS2 between flat plateaus on the rider and on the metallic substrate. If the substrates were rough, flat plateaus were created during 'run in' and the MoS2 flowed across them. Wear life was extended by increasing surface roughness since valleys in the roughened substrate served as reservoirs for MoS2 and a deposit site for wear debris. In moist air, the failure mechanism was the transformation of metallic colored MoS2 films to a black, powdery material that was found by X ray diffraction to consist primarily of alpha iron and MoO3 powders. In dry argon, the failure mechanism was the gradual depletion of the MoS2 film from the contact region by transverse flow. Analysis of the wear debris on the wear track at failure showed it consisted mainly of alpha iron and some residual MoS2. No molybdenum oxides were found.

Fusaro, R. L.↗

Dynamics of solid dispersions in oil during the lubrication of point of contacts. Part 2: Molybdenum disulfide

A Hertzian contact consisting of a steel ball in contact with a glass disk is lubricated with MoS2 dispersions and observed by optical microscopy at various slide/roll conditions. In general the behavior of MoS2 and graphite are similar. That is, the solids tend to enter the contact and form a film on the contacting surfaces whenever a rolling component of motion is used, but solid particles seldom enter the contact during pure sliding. The MoS2 has more pronounced plastic flow behavior than graphite. However, the polished steel ball is more readily scratched by MoS2 than by graphite. Under the conditions of these studies, lower friction and wear are observed with pure oil rather than with the dispersions. However under other conditions (such as different contact geometry or rougher surfaces) the solid lubricant dispersions might be beneficial.

Cusano, C.↗

Steady-state boundary lubrication with formulated C-ethers to 260 C

Steady state wear and friction studies were made at boundary lubrication conditions in a pin on disk (pure iron on rotating CVM M 50 steel) sliding friction apparatus with five C ether formulated fluids (modified polyphenyl ether containing phosphrous ester, organic acid, and other additives). Conditions included 20, 150, and 260 C disk temperatures, dry air test atmosphere, 1 kilogram load, 50 rpm disk speed, and test times to 130 minutes. Results were compared with those obtained with a formulated MIL L 27502 candidate ester and the C ether base fluid. Three of the C ether formulations gave better lubrication than both reference fluids under most conditions. The other two C ether formulations yielded higher wear rates and friction coefficients than the C ether base fluid for most of the temperature range. Only one C ether formulation showed consistently higher steady state wear rates than the ester.

Loomis, W. R.↗