Effect of sample size on the maximum value distribution of fatigue driving forces in metals and alloys

An analytical framework is presented to predict the effects of sample size on the maximum value distribution (MVD) of the driving forces for fatigue crack formation in metals and alloys. The distribution of the maximum driving force for fatigue crack formation over the domain follows the generalized extreme value theory in the limit as the domain size increases to infinity. Here, a simulation-based analysis of microstructure influences on fatigue resistance for polycrystalline metals and alloys is very costly, and reaching those limits is intractable. This work models the MVD of Fatigue Indicator Parameters (FIPs), which serve as surrogate measures for the driving force for fatigue crack formation, at finite sample sizes prior to their convergence to a limiting extreme value distribution. Large-scale crystal plasticity finite element (CPFE) simulations of FCC Al 7075-T6 with microstructure realizations of various sizes are incorporated to calibrate and evaluate the developed framework, and a total of ∼6.5 million grains of Al 7075-T6 are examined. The calibrated analytical solution agrees well with the brute force Monte Carlo simulation results extracted from the CPFE simulations. Furthermore, the developed formulation can predict the MVD of FIPs for different sample sizes using a size-dependent parameter, and it is capable of accurately extrapolating the MVD of FIPs for much larger microstructure sample sizes than the size used for its calibration.

Crystal plasticity↗

Tensile and Fatigue Testing and Material Hardening Model Development for 508 LAS Base Metal and 316 SS Similar Metal Weld under In-air and PWR Primary Loop Water Conditions

This report provides an update on an assessment of environmentally assisted fatigue for light water reactor components under extended service conditions. This report is a deliverable in September 2015 under the work package for environmentally assisted fatigue under DOE’s Light Water Reactor Sustainability program. In an April 2015 report we presented a baseline mechanistic finite element model of a two-loop pressurized water reactor (PWR) for systemlevel heat transfer analysis and subsequent thermal-mechanical stress analysis and fatigue life estimation under reactor thermal-mechanical cycles. In the present report, we provide tensile and fatigue test data for 508 low-alloy steel (LAS) base metal, 508 LAS heat-affected zone metal in 508 LAS–316 stainless steel (SS) dissimilar metal welds, and 316 SS-316 SS similar metal welds. The test was conducted under different conditions such as in air at room temperature, in air at 300 oC, and under PWR primary loop water conditions. Data are provided on materials properties related to time-independent tensile tests and time-dependent cyclic tests, such as elastic modulus, elastic and offset strain yield limit stress, and linear and nonlinear kinematic hardening model parameters. The overall objective of this report is to provide guidance to estimate tensile/fatigue hardening parameters from test data. Also, the material models and parameters reported here can directly be used in commercially available finite element codes for fatigue and ratcheting evaluation of reactor components under in-air and PWR water conditions.

316 Stainless Steel↗

Progress Report on Long Hold Time Creep Fatigue of Alloy 617 at 850°C

Alloy 617 is the leading candidate material for an intermediate heat exchanger for the very high temperature reactor. To evaluate the behavior of this material in the expected service conditions, strain-controlled cyclic tests that include long hold times up to 240 minutes at maximum tensile strain were conducted at 850°C. In terms of the total number of cycles to failure, the fatigue resistance decreased when a hold time was added at peak tensile strain. Increases in the tensile hold duration degraded the creep-fatigue resistance, at least to the investigated strain controlled hold time of up to 60 minutes at the 0.3% strain range and 240 minutes at the 1.0% strain range. The creep-fatigue deformation mode is considered relative to the lack of saturation, or continually decreasing number of cycles to failure with increasing hold times. Additionally, preliminary values from the 850°C creep-fatigue data are calculated for the creep-fatigue damage diagram and have higher values of creep damage than those from tests at 950°C.

36 MATERIALS SCIENCE↗

Novel Experiments to Characterize Creep-Fatigue Degradation in VHTR Alloys

It is well known in energy systems that the creep lifetime of high temperature alloys is significantly degraded when a cyclic load is superimposed on components operating in the creep regime. A test method has been developed in an attempt to characterize creep-fatigue behavior of alloys at high temperature. The test imposes a hold time during the tensile phase of a fully reversed strain-controlled low cycle fatigue test. Stress relaxation occurs during the strain-controlled hold period. This type of fatigue stress relaxation test tends to emphasize the fatigue portion of the total damage and does not necessarily represent the behavior of a component in-service well. Several different approaches to laboratory testing of creep-fatigue at 950°C have been investigated for Alloy 617, the primary candidate for application in VHTR heat exchangers. The potential for mode switching in a cyclic test from strain control to load control, to allow specimen extension by creep, has been investigated to further emphasize the creep damage. In addition, tests with a lower strain rate during loading have been conducted to examine the influence of creep damage occurring during loading. Very short constant strain hold time tests have also been conducted to examine the influence of the rapid stress relaxation that occurs at the beginning of strain holds.

36 MATERIALS SCIENCE↗

Fatigue-Crack-Growth Behavior of Two Pipeline Steels

This paper focuses on studying the fatigue-crack-growth behavior of two types of pipeline steels, and investigating their microstructural differences, which could influence the fatigue behavior. For fatigue experiments, compact-tension (CT) specimens are employed. These two kinds of base pipeline steels are Alloy B [Fe-0.05C-1.52Mn-0.12Si-0.092Nb, weight percent (wt.%)] and Alloy C [(Fe- 0.04C-1.61Mn-0.14Si-0.096Nb, wt.%)]. They have been tested at various frequencies (10 Hz, 1 Hz, and 0.1 Hz) and different R ratios (0.1 and 0.5, R = P min. /P max. where P min. is the minimum applied load, and P max. is the maximum applied load) in air. The effects of frequencies and R ratios on crackpropagation behavior are compared. The microstructures of fracture surfaces are investigated, using both scanning-electron microscopy (SEM) and transmission-electron microscopy (TEM). It is concluded that higher R ratios lead to faster crack-growth rates, while frequency does not have much influence on the fatigue-crack-growth rates. Moreover, Alloy B (Fe-0.05C-1.52Mn-0.12Si-0.092Nb, wt.%) tends to have better fatigue resistance than Alloy C (Fe-0.04C-1.61Mn-0.14Si-0.096Nb, wt.%) under various test conditions in air.

36 MATERIALS SCIENCE↗

Fatigue Life Behaviour of Glass/Kenaf Woven-Ply Polymer Hybrid Biocomposites

Investigation on the fatigue life of hybrid composites is critical to extend their applications and acceptance among industries; however, there is a lack of research focus on fatigue performance of the hybrid composite. In this study, the fatigue life of glass/kenaf woven-ply hybrid composite with thermoplastic and thermoset polymer matrix was investigated. Hybrid composites consist of two different fibre configurations: kenaf/glass/kenaf and glass/kenaf/glass. Thermoplastic hybrid composites were manufactured through the hot press moulding compression method, while thermoset hybrid composites were fabricated through the vacuum-assisted resin infusion method. The tensile strength and fatigue strengths of the kenaf/glass/kenaf composite have been identified to be significantly lower than those of the glass/kenaf/glass composite regardless of the types of matrix used. However, thermoplastic-based kenaf/glass/kenaf composites are less fatigue sensitive compared to glass/kenaf/glass composites; however, this phenomenon is vice versa for thermoset composites due to the epoxy matrix, which limits the stiffening effect in natural fibres.

36 MATERIALS SCIENCE↗

Effect of Deoxidation Process on Inclusion and Fatigue Performance of Spring Steel for Automobile Suspension

55SiCrA spring steel was smelted in a vacuum induction levitation furnace. The liquid steel was treated by Si deoxidation, Al modification with Ca treatment and Al modification, and the steel samples were obtained with deformable Al 2 O 3 -SiO 2 -CaO-MgO inclusions closely contacted with steel matrix, Al 2 O 3 -CaO-CaS-SiO 2 -MgO inclusions surrounded by small voids or Al 2 O 3 (> 80 pct)-SiO 2 -CaO-MgO inclusions surrounded by big voids, respectively. Effect of three types of inclusions on steel fatigue cracks was studied. The perpendicular and transverse fatigue cracks around the three types of inclusions leading to fracture were found to vary in behavior. Under the applied stress amplitude of 775 MPa, the fatigue lives of the three spring steels decreased from 4.0 × 10 7 to 3.8 × 10 7 , and to 3.1 × 10 7 cycles. For the applied stress amplitude of 750 MPa, the fatigue lives of the three spring steels decreased from 5.2 × 10 7 to 4.1 × 10 7 , and to 3.4 × 10 7 cycles. Based on the voids around inclusions, the equivalent size of initial fatigue crack has been newly defined as √(((area inclusion )/((1-CC)))), where the contraction coefficient CC of inclusion was introduced. A reliable forecast model of the critical size of inclusion leading to fracture was established by the incorporation of actual width b inclusion or diameter d inclusion of internal inclusion; the model prediction was found to be in agreement with experimental results.

36 MATERIALS SCIENCE↗

High Cycle Fatigue Performance in Laser Shock Peened TC4 Titanium Alloys Subjected to Foreign Object Damage

During their service, titanium alloys are likely to suffer from the foreign object damage (FOD), resulting in a decrease in their fatigue strength. Laser shock peening (LSP) has been proved to effectively increase the damage tolerance of military engine components by introducing a magnitude compressive residual stress in the near-surface layer of alloys. In this paper, smooth specimens of a TC4 titanium alloy were used and treated by LSP and subsequently exposed to FOD, which was simulated by firing a steel sphere with a nominal velocity of 300 m/s, at 90° with the leading edge of the LSP-treated region using a light gas gun. All impacted specimens were then subjected to fatigue loading. The results showed that LSP could effectively improve the fatigue strength of the damaged specimens. The effect of LSP on the fatigue strength was assessed through fracture observations, microhardness tests and residual stress analyses. The residual stresses due to the plastic deformation caused by LSP and the FOD impact, which were found to play a crucial role on the fatigue strength, were determined using the commercial software ABAQUS.

36 MATERIALS SCIENCE↗

Effect of Localized Corrosion on Fatigue–Crack Growth in 2524-T3 and 2198-T851 Aluminum Alloys Used as Aircraft Materials

Corrosion and fatigue of aluminum alloys are major issues for the in-service life assessment of aircraft structures and for the management of aging air fleets. The aim of this work was to evaluate the effect of localized corrosion on fatigue crack growth (FCG) resistance of the AA2198-T851 Al-Li alloy (Solution Heat Treated, Cold Worked, and Artificially Aged), comparing it with the FCG resistance of AA2524-T3 (Solution Heat Treated and Cold Worked), considering the effect of seawater fog environment. Before fatigue tests, the corrosion behavior of 2198-T851 and 2524-T3 aluminum alloys was verified using open circuit potential and potentiodynamic polarization techniques. Fatigue in air and corrosion fatigue tests were performed applying a stress ratio (R) of 0.1, 15 Hz (air) and 0.1 Hz (seawater fog) frequencies, using a sinusoidal waveform in all cases. The results showed that the localized characteristics of the 2198-T851 and 2524-T3 aluminum alloys are essentially related to the existence of intermetallic compounds, which, due to their different nature, may be cathodic or anodic in relation to the aluminum matrix. The corrosive medium has affected the FCG rate of both aluminum alloys, in a quite similar way. Graphical Abstract: .

36 MATERIALS SCIENCE↗

Effects of Mg Content on the Fatigue Strength and Fracture Behavior of Al-Si-Mg Casting Alloys

In order to investigate the influence of Mg content on the fatigue properties in Al-Si-Mg alloy, uniaxial tensile tests and rotating bending fatigue tests were conducted on two Al-7Si-Mg casting alloys, with different Mg contents of 0.3 and 0.6 wt.%. The fracture surfaces of the specimens were observed by scanning electron microscopy, and the fatigue crack growth process was obtained by the replica method. The results indicate that the increase in Mg content enhances the yield strength and tensile strength of the alloy, whereas it reduces its elongation. There is an obvious knee point in the S–N curves of Al-7Si-0.6Mg alloy while that of Al-7Si-0.3Mg alloy shows continuous decrease. The fatigue strength at 5 × 10{sup 5} cycles is 60 MPa for Al-7Si-0.3Mg alloy and 80 MPa for Al-7Si-0.6Mg alloy. For the two types of specimens, the fatigue failure can initiate from crystal slip and casting defects. The replica results suggest that cracks in Al-7Si-0.6Mg alloy grow more slowly than that in Al-7Si-0.3Mg alloy.

36 MATERIALS SCIENCE↗

Hydrogen Effect on the Fatigue Crack Growth in Austenitic Stainless Steel Investigated by a New Method Based on Nanohardness Distribution

A new method of nanohardness distribution for investigating the hydrogen effect on the fatigue crack in austenitic stainless steels was developed. The nanohardness distribution around the fatigue crack tip is dependent on the plastic zone and different microstructures in materials. Nanoindentation could provide a possibility to quantitatively estimate the size of the plastic zone and to expressly identify the strain-induced α′ martensitic transformation around the fatigue crack tip. The results of measured nanohardness distribution reveal that hydrogen reduces the size of the estimated plastic zone around the fatigue crack tip, especially in the specimen tested in hydrogen gas environment, which is attributed to hydrogen-enhanced localized plasticity. Both hydrogen and α′ martensite greatly influence the nanohardness and the gradient of hydrogen concentration near the crack tip, which will have a significant effect on the fatigue crack growth.

36 MATERIALS SCIENCE↗

Tailoring the Properties of a Ni-Based Superalloy via Modification of the Forging Process: an ICME Approach to Fatigue Performance

Traditionally, material design and property modifications are usually associated with compositional changes. However, subtle changes in the manufacturing process parameters can also have a dramatic effect on the resulting material properties. In this work, an integrated computational materials engineering (ICME) framework is adopted to tailor the fatigue performance of a Ni-based superalloy, RR1000. An existing fatigue model is used to identify microstructural features that promote enhanced fatigue life, namely a uniform, fine grain size distribution, random orientation, a distinct grain boundary distribution (specifically high twin boundary density and limited low-angle grain boundaries). A deformation mechanism map and process models for grain boundary engineering of RR1000 are used to identify the optimal thermo-mechanical processing parameters to realize these desirable microstructural features. For validation, small-scale forgings of RR1000 were produced and heat-treated to attain fine grain and coarse grain microstructures that represent the conventionally processed and grain boundary engineered (GBE) conditions, respectively. For each of the four microstructural variants of RR1000, the twin density and grain size were characterized and were in agreement with the desired microstructural attributes. In order to validate the deformation mechanisms and fatigue behavior of the material, high-resolution digital image correlation was performed to generate strain maps relative to the microstructural features. The high density of twin boundaries was confirmed to inhibit the length of slip bands, which is directly attributed to extended fatigue life. Thus, this study demonstrated the successful role of models, both process and performance, in the design and manufacture of Ni-based superalloy disk forgings.

36 MATERIALS SCIENCE↗

Multiscale mechanical fatigue damage of stainless steel investigated by neutron diffraction and X-ray microdiffraction

Mechanical fatigue behavior of AL6XN stainless steel as a typical type of planar slip alloy was investigated by in situ neutron diffraction and synchrotron-based X-ray microdiffraction methods. Under cyclic loading at a high strain amplitude (+/- 0.8%), the fatigue damage originated mainly from the accumulation of statistical stored dislocations, as clearly evidenced from a continuous increase in diffraction peak width with increasing the number of load cycles. However, under cyclic loading at a low strain amplitude (+/- 0.3%), the density of statistical stored dislocations became saturated just after a hundred loading cycles and the fatigue damage was mainly dominated by the accumulation of persistent [Alders bands (PLBs) and the complex interactions among various PLBs as evidenced through X-ray microdiffraction measurements. It was further found that there exists obvious grain-orientation-dependent local damage in the low-strain-amplitude fatigued sample. In particular, fatigued grains orientated with [001] paralleling the loading direction are subjected to compressive stress and contain a large number of broad PLBs in boundaries arraying the edge dislocation pile-ups, which generate a large stress gradient leading to local plastic instability. As a result, the highly localized stress field at PLBs in the cyclically-deformed sample at a low strain amplitude may explain the obvious cyclic stress softening.

36 MATERIALS SCIENCE↗

Micromechanical and fatigue in situ synchrotron characterization of an additively manufactured superalloy with porosity

Additive manufacturing (AM) has the potential to transform component production, but its widespread adoption is constrained by defects, such as pores, that compromise structural integrity. Here, this study investigates the influence of porosity on the micromechanical and fatigue response of AM Inconel 718 (IN718), a widely used aerospace superalloy. One baseline specimen with minimal stochastic porosity and another intentionally seeded with lack of fusion (LOF) pores were examined using high-energy X-ray diffraction microscopy (HEDM) and micro-computed tomography during cyclic loading. Fatigue cracks in the LOF specimen initiated more frequently and at lower cycle counts than in the baseline specimen. The number fraction of fatigue cracks that grew was comparatively higher in the LOF specimen. Grain-level metrics, including stress and diffraction spot widths, were quantified using far-field HEDM. Across the thousands of grains detected in both specimens, the pores in the LOF specimen increased the variability of stress and spot width evolution in the azimuthal direction, the latter serving as a surrogate measure of plastic deformation. However, no correlations emerged between these metrics and grain proximity to fatigue crack initiation sites or pores, underscoring the limitations of grain-averaged metrics for predicting fatigue. Nonetheless, the rich dataset reported here provides a foundation for future modeling efforts.

High-energy X-ray diffraction microscopy↗

Examining infrared thermography based approaches to rapid fatigue characterization of additively manufactured compression molded short fiber thermoplastic composites

A novel additive manufacturing (AM) methodology combined with a compression molding (CM) process has been developed to optimize the microstructure of short fiber thermoplastic composites (SFTs)with higher fiber alignment and lower porosity, yielding superior stiffness, strength, and structural integrity. Here, the current work examines the efficacy of the ‘passive’ infrared thermography (IRT) techniques for rapid fatigue characterization of SFTs that use the surface temperature evolution during cyclic loading due to self-heating as a fatigue indicator. A comparison of fatigue limits obtained from traditional stress-life (SN) (≈53.1%σ uts ) and IRT (≈54.1%σ uts ) shows a close match. However, the SN curve required 18 specimens and two weeks of continuous cyclic testing, while IRT used three specimens with 5 hours of testing. Thus, the IRT approach provides an accelerated testing framework for rapidly estimating the fatigue limit. Additionally, existing phenomenological approaches to IRT fatigue characterization have been examined.

42 ENGINEERING↗

Slip delocalization and diffusion mediated carbide formation during fatigue of a nickel-base superalloy

Fatigue crack initiation at high temperatures occurs at microscopic fatigue shear bands that form near twin boundaries in polycrystalline nickel-base superalloys that contain minimal metallurgical defects. The associated dislocation sub-structure is complex and dependent on thermal and mechanical conditions. Here we show the formation of fine-scale carbide precipitates along these fatigue shear bands in a nickel-base superalloy during fatigue above 650 °C. The formation of carbide precipitates is studied using calculations of bulk and pipe diffusion. The contribution of pipe diffusion is observed to be critical in the formation of fine-scale carbides and occurs coincident with the delocalization of slip during fatigue.

36 MATERIALS SCIENCE↗

Fatigue-crack propagation behavior in a high-carbon chromium SUJ2 bearing steel: Role of microstructure

High-carbon chromium martensite steels are commonly selected for bearing components in the power generation, automotive and aerospace industries where fatigue failure is a major concern. Accordingly, it is of importance to elucidate the structure-property relationships governing the fatigue properties of such bearing steels. Here, the role of microstructure in influencing the fatigue-crack propagation behavior of a high-carbon chromium SUJ2 bearing steel is examined with emphasis on three martensitic structures: (i) a fine-grained (~10 μm) structure with intragranular (but no intergranular) carbides, (ii) a coarser-grained (~25 μm) structure with discontinuous grain-boundary carbides primarily near triple junctions, and (iii) a coarse-grained (~31 μm) structure with continuous grain-boundary carbides. Although growth rates were fairly similar above ~10 -8 m/cycle, significant differences in behavior were observed at lower, near-threshold growth rates; specifically at a load ratio of 0.1, the ΔKth fatigue threshold was increased from 3.8 MPa m ½ in the fine-grained structure to 5.9 to 6.3 MPa m ½ in the two coarser-grained structures. The dominant factor governing such near-threshold behavior was found to be crack-tip shielding from roughness-induced crack closure, which was most pronounced in the coarser-grained structures; additionally, shielding from crack deflection and branching was apparent in these structures as the crack propagated through the network of intersecting martensite lamellae within the coarse grains. Compared to high-strength stainless steels and low-strength carbon steels, the fine-grained SUJ2 steel displays an exceptional combination of high strength and fatigue-crack growth resistance and is considered to be a superior structural alloy for bearing applications.

36 MATERIALS SCIENCE↗

Hydrogen accelerated fatigue crack growth of friction stir welded X52 steel pipe

Friction stir welded steel pipelines were tested in high pressure hydrogen gas to examine the effects of hydrogen accelerated fatigue crack growth. Fatigue crack growth rate (da/dN) vs. stress-intensity factor range (ΔK) relationships were measured for an X52 friction stir welded pipe tested in 21 MPa hydrogen gas at a frequency of 1 Hz and R = 0.5. Tests were performed on three regions: base metal (BM), center of friction stir weld (FSW), and 15 mm off-center of the weld. For all three material regions, tests in hydrogen exhibited accelerated fatigue crack growth rates that exceeded an order of magnitude compared to companion tests in air. Among tests in hydrogen, fatigue crack growth rates were modestly higher in the FSW than the BM and 15 mm off-center tests. Select regions of the fracture surfaces associated with specified ΔK levels were examined which revealed intergranular fracture in the BM and 15 mm off-center specimens but an absence of intergranular features in the FSW specimens. In conclusion, the X52 friction stir weld and base metal tested in hydrogen exhibited fatigue crack growth rate relationships that are comparable to those for conventional arc welded steel pipeline of similar strength found in the literature.

08 HYDROGEN↗