A Stress-State Modified Strain Based on FAilure Criterion for Evaluating the Structural Integrity of an Inner Eutectic Barrier.
Abstract not provided.
Anodization Compatibility of Eutectic Aluminum-Cerium Alloys
Explore the source record for details and available documents.
Continuous in situ Measurements of Lead Bismuth Eutectic Corrosion under Proton Irradiation
Explore the source record for details and available documents.
One-group fission cross sections for plutonium and minor actinides inserted in calculated neutron spectra of fast reactor cooled with lead-208 or lead-bismuth eutectic
The paper is dedicated to one-group fission cross sections of Pu and MA in LFRs spectra with the aim to increase these values by choosing a coolant which hardens neutron spectra. It is shown that replacement of coolant from Pb-Bi with Pb-208 in the fast reactor RBEC-M, designed in Russia, leads to increasing the core mean neutron energy. As concerns fuel Pu isotopes, their one-group fission cross sections become slightly changed, while more dramatically Am-241 one-group fission cross section is changed. Another situation occurs in the lateral blanket containing small quantities of minor actinides. It is shown that as a result of lateral blanket mean neutron energy hardening the one-group fission cross sections of Np-237, Am-241 and Am-243 increases up to 8-11%. This result allows reducing the time of minor actinides burning in FRs. (authors)
Corrosion of Wrought and LPBF 316H in Molten Eutectic Na-Mg Chloride Salt
This presentation shows experimental work at INL evaluating the corrosion behavior of wrought and laser powder bed fusion (LPBF) 316H stainless steel (SS) in chloride molten salt systems. This evaluation focuses on understanding the relationship between the material’s as-built characteristics and its corrosion performance, the effects of acid cleaning and descaling before corrosion.
Characterization of weld metal microstructure in a Ni-30Cr alloy with additions of niobium and molybdenum
Additions of niobium (Nb) and molybdenum (Mo) were made to an Alloy 690 base alloy in order to investigate the formation of a eutectic constituent at the end of solidification and to evaluate the effect of the eutectic liquid on backfilling (or healing) of solidification cracks. Solidification cracking was induced using the cast pin tear test (CPTT) and regions of backfilling were located and characterized via optical and electron microscopy. Computational predictions of fraction eutectic and composition of the eutectic constituent were compared to experimental findings and were found to correlate well in both cases. The extent of crack backfilling increased significantly with increasing Nb content, but the addition of Mo did not seem to influence the amount of eutectic constituent or the degree of backfilling. SEM/EDS analysis confirmed that the eutectic composition is constant and that increasing Nb above 4 wt% has little effect on expanding the solidification temperature range, but has a beneficial effect on mitigating solidification cracking by a crack healing effect. - Highlights: • Increasing fraction eutectic as a function of Nb, as predicted by ThermoCalc™, is consistent with image analysis results. • Nb, unlike Mo, had a significant effect on the fraction eutectic formed. • Both influence the composition of the eutectic. • Thermocalc™ predictions regarding Nb content in eutectic are consistent with EDS results, but are high for the Mo content. • Increased levels of niobium resulted in a higher degree of crack backfilling and leads to a lower cracking susceptibility. • Mo may influence the eutectic liquid along solidification grain boundaries, improving backfill and thus cracking resistance.
In-situ investigation of incipient melting in a 319 type Al alloy using laser scanning confocal microscopy
Highlights: • In-situ analysis of incipient melting of ternary eutectic in Al alloy. • Incipient melting occurred in three distinct stages in the eutectic. • Increased heating rate increase rate of liquid film propagation. • Incipient melting transformed initial eutectic structure and caused oxidation. • Study determined incipient melting mechanism for eutectic structures. - Abstract: The modified 319 Al alloy system has been used extensively in precision sand casting of automotive powertrain applications such as engine blocks and cylinder heads, with significant improvement in vehicle fuel efficiency. However, a concern in elevated temperature processing of Al alloys, such as heat treatment and hot working processes, is incipient melting of secondary phases, which is deleterious to mechanical properties. In this study, the laser scanning confocal microscopy (LSCM) technique was used in the analysis of in-situ changes in microstructure as a result of incipient melting. Microstructural analysis was carried out prior to and following elevated temperature exposure in the LSCM using optical microscopy, SEM and EDX. The results suggest that incipient melting of the Al-Al{sub 2}Cu-Al{sub 5}Mg{sub 8}Cu{sub 2}Si{sub 6} ternary eutectic clusters was initiated by the formation of a liquid film which propagated rapidly from the eutectic clusters, coating the Al dendrites in regions adjacent to the eutectic clusters. Following film formation, the ternary eutectic clusters melted completely. Incipient melting also resulted in a localized change in composition in the interdendritic channels as supported by a change in cluster morphology from eutectic to a combination of coarse blocky Al-Cu-Ni and Si particles, and ultra-fine eutectic.
Evolution of Fe-Rich Intermetallics in Al-Si-Cu 319 Cast Alloy with Various Fe, Mo, and Mn Contents
In the present work, the precipitation and preferential selection of Fe-rich intermetallics in Al-Si-Cu 319 cast alloys with two Fe contents (0.3 and 0.7 wt pct) and various Mo contents (0 to 0.4 wt pct) were investigated. The results showed that two types of platelet β-Fe (defined as eutectic β-Fe and pre-eutectic β-Fe) and α-Fe can precipitate depending on the alloy compositions, such as the Fe and Mo contents. Generally, the addition of Mo promotes the formation of α-Fe instead of β-Fe. However, its effect on the phase competition between β-Fe and α-Fe is greatly related to the Fe content. In alloys with low Fe content (0.3 pct), an addition of 0.37 pct Mo can promote the complete precipitation of α-Fe and suppress the formation of eutectic β-Fe. However, in alloys with high Fe content (0.7 pct), only the pre-eutectic β-Fe amount decreases with increasing Mo addition, leaving the eutectic β-Fe almost unchanged, while both pre-eutectic β-Fe and eutectic β-Fe can be fully suppressed with a combined addition of Mn (0.24 pct) and Mo (0.4 pct). Compared with Mn, Mo exhibits a stronger effect on the promotion of α-Fe. The combined addition of Mn and Mo can achieve better modifications of both pre-eutectic and eutectic β-Fe in 319 alloys with high Fe content.
Characterization on carbide of a novel steel for cold work roll during solidification process
A novel steel for cold work roll was developed in this work. Its phase structures were determined by X-ray diffraction, and phase transformation temperatures during the cooling process were measured by Differential Scanning Calorimeter. The Fe–C isopleths of the steel were calculated by Thermo-Calc to preliminarily determine the characteristic temperatures of the different phases. Then the specimens were quenched at these characteristic temperatures. The typical microstructures were observed by Optical Microscopy and Field Emission Scanning Electron Microscopy with Energy Disperse Spectroscopy. The results show that α-Fe, MC, M{sub 2}C and M{sub 7}C{sub 3} precipitate when the specimen is cooled slowly to room temperature. According to the DSC curve and the Fe–C isopleths, the characteristic temperatures of the phase transformation and carbide precipitation are chosen as 1380 °C, 1240 °C, 1200 °C and 1150 °C respectively. Primary austenite precipitates at 1380 °C, then eutectic reaction occurs in residual liquid after quenching and the eutectic microstructures distribute along the crystal grain boundary. The eutectic MC is leaf-like and eutectic M{sub 2}C is fibrous-like. Both of them precipitate in ternary eutectic reaction simultaneously at 1240 °C, grow together in the form of dendrite along the crystal grain boundary. Secondary MC precipitates from the austenitic matrix at 1200 °C and nucleates at the position where eutectic MC located accompanied by the dissolving of eutectic carbides. The mixed secondary M{sub 2}C and M{sub 7}C{sub 3} precipitate at 1150 °C. The secondary M{sub 2}C is strip-like and honeycomb-like, while the M{sub 7}C{sub 3} is chrysanthemum-like and maze-like. - Highlights: • The solidification process was analyzed by Thermo-Calc, DSC, XRD and SEM observation. • Primary and secondary carbides precipitated during solidification were determined. • The three dimensional morphologies of all carbides was observed. • The eutectic MC exhibits the dendritical structure which was not observed before.
Melting and thermal expansion in the Fe-FeO system at high pressure
Melting in the Fe–FeO system was investigated at pressures up to 93 GPa using synchrotron X-ray diffraction (XRD) and a laser heated diamond anvil cell (DAC). The criteria for melting were the disappearance of reflections associated with one of the end-member phases upon raising the temperature above the eutectic and the reappearance of those reflections on dropping the temperature below the eutectic. The Fe–FeO system is a simple eutectic at 50 GPa and remains eutectic to at least 93 GPa. The eutectic temperature was bound at several pressure points between 19 and 93 GPa, and in some cases the liquidus temperature was also determined. The eutectic temperature rises rapidly with pressure closely following the melting curve of pure Fe. A detailed phase diagram at 50 GPa is presented; the eutectic temperature is 2500 ± 150 K and the eutectic composition is bound between 7.6 ± 1.0 and 9.5 ± 1.0 wt.% O. The coefficient of thermal expansion of FeO is a strong function of volume and decreases with pressure according to a simple power law.
Laboratory micro- and nanoscale X-ray tomographic investigation of Al–7 at.%Cu solidification structures
X-ray computed tomography across multiple length scales provides an opportunity to non-destructively visualize and quantify the micro- to nano-scale microstructural features of solidification structures in three dimensions. Aluminum–7 at.%copper samples were directionally solidified at three cooling rates (0.44, 0.67, and 1.33 °C/s), resulting in systematic changes in the as-solidified microstructure, which are difficult to quantify using traditional microscopic techniques. The cooling rate of a material affects its ultimate microstructure, and characterizing that microstructure is key to predicting and understanding its bulk properties. Here, two different laboratory X-ray computed tomography instruments were used to characterize as-solidified microstructures, including micro-scale computed tomography with approximately 1 mm field-of-view, ∼ 1.7 μm resolution, and nano-scale X-ray computed tomography ∼ 65 μm FOV, 150 nm resolution. Micro-scale X-ray radiography and computed tomography enabled a quantitative investigation of changes in the primary dendritic solidification structure with increasing cooling rate. Nano-scale absorption contrast X-ray computed tomography resolved the distinct phases of the lamellar eutectic structure and three dimensional measurements of the ∼ 1 μm interlamellar spacing. It is found that the lamella eutectic structure thickness is inversely proportional to the cooling rate. Nano-scale Zernike phase contrast was also used to image voids at eutectic colony boundaries. The application and resolution of these two instruments are discussed with respect to the resolvable features of the solidification structures. - Highlights: • Al–Cu eutectic is a model system for studying solidification microstructure. • X-ray computed tomography provides a 3D picture of these complex structures. • Micro-scale tomography images the primary and secondary dendritic structures. • Nano-scale tomography images the eutectic lamella and measures its thickness. • The ∼ 1 micrometer thickness of the eutectic lamella correlates to the cooling rate.
Technetium Waste Form Development - Progress Report
Analytical electron microscopy using SEM and TEM has been used to analyze a ~5 g. ingot with composition 71.3 wt% 316SS-5.3 wt% Zr-13.2 wt% Mo-4.0 wt% Rh-6.2 wt% Re prepared at the Idaho National Laboratory. Four phase fields have been identified two of which are lamellar eutectics, with a fifth possibly present. A Zr rich phase was found distributed as fine precipitate, ~10µm in diameter, often coating large cavities. A Mo-Fe-Re-Cr lamellar eutectic phase field appears as blocky regions ~30µm in diameter, surrounded by a Fe-Mo-Cr lamellar eutectic phase field, and that in turn is surrounded by a Zr-Fe-Rh-Mo-Ni phase field. The eutectic phase separation reactions are different. The Mo-Fe-Re-Cr lamellar eutectic appears a result of austenitic steel forming at lower volume fraction within an Mo-Fe-Re intermetallic phase, whereas the Fe-Mo-Cr lamellar eutectic may be a result of the same intermetallic phase forming within a ferritic steel phase. Cavitation may have arisen either as a result of bubbles, or from loss of equiaxed particles during specimen preparation.
Transmission electron microscopy of the rapid solidification microstructure evolution and solidification interface velocity determination in hypereutectic Al-20at.%Cu after laser melting
The evolution of rapid solidification (RS) microstructure and solidification interface velocity has been studied experimentally by in-situ transmission electron microscopy and postmortem characterization for hypereutectic Al-20at.%Cu (37 wt.%Cu) after laser melting. Four morphologically distinct regions formed via growth modes changing from θ-Al 2 Cu phase dendrites to eutectic cell growth, possibly α-Al dendrite growth (α-cell), banded growth, and α-Al plane front growth. Tendency for faceting and low capacity for solute trapping limited the θ-phase dendrite growth to solidification interface velocity v < 0.07 m/s. Consequently, formation of pro-eutectic micro-constituent was suppressed, and RS microstructure formation was dominated by eutectic, α-cell, and banded morphology grains for the Al-20at.%Cu alloy. Eutectic growth operated for interface velocity of 0.1 m/s ≤ v < 0.3 m/s, with a transition from regular lamellar, 2-λ and 1-λ mode to a dense irregular morphology dominated by α-phase at v = 0.3 m/s. Interface temperature calculations indicated feasibility of α-cell growth mode for 0.3 m/s ≤ v < 0.7 m/s. Banded growth occurred for 0.7 m/s ≤ v < 1.3 m/s. Plane front α-phase growth was evident for interface velocities v ≥ 1.3 m/s. Previous work on rapid solidification microstructure development in hypereutectic Al-Cu alloys reported a regime of α-cell growth subsequently to eutectic and prior to transition to banded growth for Al-19at.%Cu (36 wt.%Cu), while for Al-22at.%Cu (40 wt.%Cu) eutectic growth transitioned directly to α-plane front growth without emergence of a banded regime. Finally, based on the current study the disappearance of the banded growth regime occurs for a composition larger than 20at.%Cu.
Microstructure and mechanical properties of hypoeutectic Al–6Ce–3Ni-0.7Fe (wt.%) alloy
Here, a hypoeutectic, Fe-modified Al–Ce–Ni alloy (Al–6Ce–3Ni-0.7Fe, wt.%) is studied in terms of microstructure, thermal stability, ambient temperature strengthening, and creep resistance. The as-cast microstructure consists of primary Al dendrites and interdendritic binary eutectic regions (Al–Al11Ce3 and/or Al–Al9(Fe,Ni)2), with micron/submicron lamellar spacing, depending on the location along the height of the ingot. The cast alloy exhibits excellent coarsening resistance at 400 °C, with mostly unchanged microstructure and microhardness after 6 weeks of aging, indicating good thermal stability of Al11Ce3 and Al9(Fe,Ni)2. Orowan strengthening and load transfer are identified as strengthening mechanisms at ambient and elevated temperature. A high volume fraction of the intermetallic phases (providing load transfer) and relatively coarse eutectic spacing (for modest Orowan strengthening) result in a moderate as-cast microhardness of 566 ± 32 MPa. Creep resistance at 300 and 350 °C is similar to a binary Al-12.5Ce eutectic alloy (with twice the Ce content) because of two countering effects: Al–6Ce–3Ni-0.7Fe shows a higher volume fraction of strengthening intermetallic phases, but it also exhibits a large fraction of primary Al dendrites which weaken the alloy. By contrast, the alloy, when laser-remelted at the surface, has a fully eutectic microstructure without primary aluminum dendrites achieved by high undercooling on solidification, with a refined network of eutectic phases that doubles the microhardness as compared to the cast alloy. Whereas coarsening is faster due to the shorter diffusion distances between the eutectic phases, hardness remains ~30% higher than the as-cast alloy after ~6 weeks aging at 400 °C.
Coordination and thermophysical properties of select trivalent lanthanides in LiCl–KCl
The coordination chemistry of various fission and decay products, such as actinides and lanthanides, are crucial to the commercial deployment of molten salt reactors as they can affect the thermophysical properties. In this report we examined the structure, coordination environment, and physical properties such as the density and the vibrational density of states for three lanthanide species, namely Ce, Eu, and Sm in the LiCl–KCl eutectic system using a combination of quantum mechanics simulations and spectroscopic experiments. Quantum mechanics molecular dynamics (QM-MD) modelling was employed to determine the physical properties of each system resulting in accurate local coordination of each species. Then, the vibrational density of states (DOS) was determined using a two-phase thermodynamic modelling which was then compared to the experimentally obtained Raman spectra of the species in molten LiCl–KCl having the eutectic composition. We find that Ce 3+ , Eu 3+ and Sm 3+ all adopt octahedral local coordination environments in the eutectic salt composition in good agreement with experimental results. Ce3+ is found to fluctuate between an octahedral six-coordinated and a seven-coordinated structure due to the increased local proximity of Cl in the eutectic salt, resulting in a lower fluidicity/diffusivity than the other trivalent lanthanides studied. The thermophysical properties of the eutectic composition with trivalent lanthanides were not significantly different from the pure eutectic salt composition, but several changes were noted.