Three-dimensional measurements of fatigue crack closure
Three dimensional fatigue crack opening profiles in transparent polymer test specimens were determined. The load required to separate crack faces was measured along the crack profile at various positions through the specimens thickness. Crack opening loads at the specimen surface (under plane stress conditions) were compared with measurements made under plane strain conditions the specimen interior. The fatigue crack opening load was correlated with fatigue crack retardation behavior caused by peak overloads, and the results discussed in terms of three dimensional aspects of the fatigue crack closure mechanism for fatigue crack retardation.