Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Mechanical properties of fusion welded ceramics in the $\mathrm{SiC-ZrB}$ 2 and $\mathrm{SiC-ZrB}$ 2 -$\mathrm{ZrC}$ systems

Mechanical properties of welded SiC-ZrB 2 and SiC-ZrB 2 -ZrC ceramics were measured up to 1700 °C. Commercial powders were hot pressed, machined into coupons, and preheated to 1600 °C before joining the ceramics using either tungsten inert gas welding or plasma arc welding. Toughness of the parent materials was 3–4 MPa*m 1/2 which decreased after welding to 2–2.5 MPa*m 1/2 . Strength of the SiC-ZrB 2 -ZrC parent material was ~700 MPa at 25 °C, ~300 MPa at 1700 °C, and retained 40–60% of this strength once welded. Strength of the SiC-ZrB2 parent material was ~600 MPa at 25 °C and 1700 °C and retained 20–30% of this strength once welded. Griffith analysis indicated that the strength in the parent materials was controlled by the size of SiC clusters while strength of welds was controlled by the size of pores in fusion zones. Therefore, removal of pores in produced fusion zones should be investigated to improve strength of future ceramic welds.

36 MATERIALS SCIENCE↗

Spatial mapping of the localized corrosion behavior of a magnesium alloy AZ31B tungsten inert gas weld

Sections of a magnesium alloy, AZ31B, joined with tungsten inert gas (TIG) welding, were examined with scanning electrochemical microscopy (SECM) and scanning Kelvin probe force microscopy (SKPFM) to investigate corrosion mechanisms by correlating observed corrosion behavior with weld-affected microstructural variations. Insight into the changing nature of the galvanic couples between weld zones and at localized microgalvanic sites were investigated using SECM and SKPFM to map both electrochemically active regions and Volta potential differences across the weld-affected zones. The formation of an Al-Zn solidification network in the fusion zone (FZ) at and near the TIG weld epicenter differs from the outer heat-affected zone (HAZ), where intermetallic particles (IMPs) are the notable secondary phase from the magnesium matrix. These microstructures were mapped with SKPFM before and after brief exposure to a salt solution, revealing micro-galvanic couples as the main driving force to corrosion initiation and propagation within each zone. The IMPs and Al-Zn solidification network act as strong cathodes and govern the corrosion processes. The galvanic coupling and evolution of the intrinsic corrosion behavior between the weld zones is explained by monitoring the hydrogen evolution reaction (HER) with SECM over time. Anodically induced cathodic activation is confirmed for this welded material, as micro-galvanic couples between microstructural features are found to transition over time to broad electrochemically active areas within the weld-affected zones, resulting in polarity reversal as time of exposure proceeds.

Anodically induced cathodic activation↗

Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel

Highlights: • The fresh martensite formed in P92-sided CGHAZ during PWHT due to high Ni content. • Transition from type I to type IV cracking was observed with increasing temperature. • Creep damaged area changed depending on the dominant creep mechanism. • The transition value of Larson-Miller parameter would be within 25,063–26,168. - Abstract: Characterization of microstructures and creep fracture characteristics of dissimilar welds between Ni-based Inconel 740H superalloy and ferritic/martensitic P92 steel has been investigated. The welds were produced by shielded metal arc (SMA) welding process with the AWS A5.11 Class ENiCrFe-3 filler metal, commonly known as Inconel 182 superalloy. Postweld heat treatment (PWHT) at 760 °C for 4 h was conducted to temper the martensite in heat-affected zone (HAZ) of P92 and to form γ′ strengthener in Inconel 740H. The deposited Inconel 182 austenitic weld metal had a columnar microstructure, and grew epitaxially from the Inconel 740H base metal. The weld interface between P92 and weld metal was characterized by the discrete line with a minimal inter-diffusion, where the fresh untempered martensite was found to be formed during PWHT due to higher Ni contents diffused from Inconel 182 into P92. The P92 base metal and Inconel 182 weld metal displayed low hardness values (~240 Hv), and the sharp hardness increase was detected at coarse-grained HAZ of P92 while the hardness minimum occurred at the fine-grained HAZ (FGHAZ). Fracture location after creep was found to shift from the P92-sided fusion line to the FGHAZ of P92 with increasing creep temperature. The carbon migration from the P92 into the weld metal was not significant at lower creep temperature (600 °C), where the crack initiation at the P92-sided fusion line appeared to be related with a significant strain incompatibility across the fusion line. At both 650 °C and 700 °C where diffusion-controlled creep was more pronounced, the type IV cracking was observed. This may be attributed to the strain localization at the weak grain boundaries of FGHAZ due to the smaller grain size as well as the lack of grain boundary strengthening by carbides.

36 MATERIALS SCIENCE↗

Ultrasonic inspection of austenitic stainless steel welds with artificially produced stress corrosion cracks

Austenitic stainless steel welds and nickel alloy welds, which are widely used in nuclear power plants, present major challenges for ultrasonic inspection due to the grain structure in the weld. Large grains in combination with the elastic anisotropy of the material lead to increased scattering and affect sound wave propagation in the weld. This results in a reduced signal-to-noise ratio, and complicates the interpretation of signals and the localization of defects. Mechanized ultrasonic inspection was applied to study austenitic stainless steel test blocks with different types of flaws, including inter-granular stress corrosion cracks (IGSCC). The results show that cracks located in the heat affected zone of the weld are easily detected when inspection from both sides of the weld is possible. In cases of limited accessibility, when ultrasonic inspection can be carried out only from one side of a weld, it may be difficult to distinguish between signals from scattering in the weld and signals from cracks.

42 ENGINEERING↗

Measured Biaxial Residual Stress Maps in a Stainless Steel Weld

Here, this paper describes a sequence of residual stress measurements made to determine a two-dimensional map of biaxial residual stress in a stainless steel weld. A long stainless steel (316L) plate with an eight-pass groove weld (308L filler) was used. The biaxial stress measurements follow a recently developed approach, comprising a combination of contour method and slitting measurements, with a computation to determine the effects of out-of-plane stress on a thin slice. The measured longitudinal stress is highly tensile in the weld- and heat-affected zone, with a maximum around 450 MPa, and compressive stress toward the transverse edges around ₋250 MPa. The total transverse stress has a banded profile in the weld with highly tensile stress at the bottom of the plate (y = 0) of 400 MPa, rapidly changing to compressive stress (at y = 5 mm) of ₋200 MPa, then tensile stress at the weld root (y = 17 mm) and in the weld around 200 MPa, followed by compressive stress at the top of the weld at around ₋150 MPa. Finally, the results of the biaxial map compare well with the results of neutron diffraction measurements and output from a computational weld simulation.

36 MATERIALS SCIENCE↗

3013 DE Inner Container Closure Weld Corrosion Evaluation

Destructive evaluation (DE) of 3013 containers is one part of the U. S. Department of Energy Integrated Surveillance Program. During standard DE of 3013 containers, visual examinations for pitting and stress corrosion cracking (SCC) are performed on the accessible surfaces of the outer, inner, and convenience containers, which make up the 3013 container. As a result of 3013 DE additional analysis, the area near the inner container closure weld has been identified as being a region of increased corrosion susceptibility, which may provide a pathway for corrosive gases to the outer container. This area has a higher residual stress, an altered microstructure, and less corrosion resistant weld oxides as a result of the welding process as well as a lower temperature than other areas of the container, which may increase the absorption of moisture on the surface. The deposition of moisture in this stressed region could lead to pitting and stress corrosion cracking. During FY2013, the inner container closure weld area was more closely evaluated on several archived samples from DE containers. These containers included FY09 DE2, FY12 DE4, FY12 DE6 and FY12 DE7 and the Hanford High Moisture Container. The additional examinations included visual observations with a stereomicroscope, scanning electron microscopy along with energy dispersive spectroscopy for chemical analysis, and serial metallography of the sidewall and lid that are part of the inner container closure weld region. Pitting was observed in all the samples taken from the closure weld regions of the examined inner containers. This pitting was generally less 20 µm with most less than 5µm. These pits were similar in depth to those observed in the vapor exposed surfaces of teardrops in the shelf life corrosion testing. Cracking was not observed on either the vapor-exposed surfaces of the teardrop coupons or the inner container closure weld region. Further testing is necessary to determine if the conditions in the welded inner container could support SCC during the 50 year life time for the 3013 container.

36 MATERIALS SCIENCE↗

Nanoindentation Characterization of FeCrAl C26M Welds

The present report summarizes the initial mechanical characterization of a welded FeCrAl alloy, C26M, with comparison to two other welded specimens, C35M and C37M. The welded C26M showed a larger fusion and heat-affected zone than either the C35M or C37M welds. Nanoindentation hardness measurements using a Berkovich tip showed no major changes in the hardness and modulus between the fusion zone, heat-affected zone, and unaffected C26M tube. Nanoindentation strain-rate sensitivity tests were also performed and showed no changes between each of the regions in the C26M weld. Spherical nanoindentation tests were carried out to evaluate the nanoindentation modulus and nanoindentation yield strength in each of the regions of the C26M weld sample. No significant changes in strength from welding were observed with an average nanoindentation yield strength of ~1 GPa and nanoindentation modulus of ~220 GPa. Nanoindentation tests all show that the C26M does not change significantly after welding and that further characterization with some form of tensile loading is necessary to determine if any significant change has occurred.

36 MATERIALS SCIENCE↗

Microstructure and strength of a thick-section gas-tungsten arc weld in cast Haynes® 282® alloy

A 50-mm deep gas tungsten arc weld was made with matching filler metal in cast Haynes 282 alloy. The narrow gap joint was filled with 104 weld beads. The weld deposit was of high quality with no visible indications of physical defects. The weld heat-affected zone was characterized by microcracking and localized recrystallization. Hardness testing showed that a softened region in the as-welded heat-affected zone was nearly eliminated by post-weld heat treatment. Tensile testing up to 816°C showed that cross-weld specimen strengths were about 80% of the yield strength of the original cast base metal. The rupture strengths of cross-weld specimens are within 20% of wrought base metal reference data.

36 MATERIALS SCIENCE↗

Hardness Prediction by Incorporating Heat Transfer and Molten Pool Fluid Flow in a Multi-pass, Multi-layer Weld for Onsite Repair of Grade 91 steel

Introduction: In the current fleet of fossil-fired power plants, creep strength enhanced ferritic steels (CSEF) are used to sustain the harsh service conditions. Enhanced properties of Grade 91 steel result from tempered martensite with a fine distribution of MX and M23C6 carbides. Grade 91 steel is subjected to onsite welding repair to remedy their degradation due to extreme service condition. Knowledge of weld repairability of these steels, such as as-welded hardness distribution, is essential to establishing sound repair procedures. Experimental trial and error tests can consume a lot of time as many welding variables need to be studied. For numerical modelling, most of the multi-pass multi-layer models are based on finite element method, which are limited to solve the heat conduction equation and ignore convective heat transfer due to melt flow. Moreover, the mesh has to be pre-built based on a known or assumed weld cross-section geometry. These finite element based models thus have limited predictive capability as defects are not considered and nugget size are pre-assumed. This research aims at developing a thermal and microstructure evolution model incorporating molten pool dynamics in a multi-pass multi-layer material deposition to predict the as-welded hardness distribution. Technical Approach: All the thermal, physical, and metallurgical properties of Grade 91 as a function of temperature are collected from the literature and inputted into the thermo-fluid model based on Flow-3D, a computational fluid dynamics software. A multi-pass, multi-layer material deposition is simulated where the melting of filler wire into the molten pool is directly considered based on the volume of fluid (VOF) method. The flow behaviour of the molten pool is used to understand the formation of deposition geometry and defects. The temperature profiles during the multi-pass, multi-layer welding are calculated. The results computed using the new model are compared against the experimental data of fusion zone geometry and thermal cycles. Hardness prediction in the heat-affected zone (HAZ) are made using Johnson-Mehl-Avrami (JMA) equation for solid-state phase transformation kinetics. The JMA parameters are extracted from the experimental data available in the literature. For comparison, a standard finite element heat conduction model is also developed to predict the thermal cycles and hardness distribution in the multi-pass, multi-layer weld. Expected Result: Results obtained using the molten pool dynamic simulation versus the finite element heat conduction model are compared. Specifically, the effects of convective heat transfer on the accuracy of the calculated thermal history, bead shape and size, and HAZ hardness distribution are examined.

Modeling, Grade 91 steel, Multi-pass multi-layer d↗

Study program of NASA/GSFC weld quality monitor system

The Weld Quality Monitor has provided online control through the application of linear transducers. The electronic systems must be upgraded to increase confidence level required in production. The Weld Quality Monitor has been used with a recent model solid state power supply to evaluate ability to differentiate between sound and defective weld joints. The Weld Quality Monitor has been evaluated on Dumet and Kovar to interconnect materials Nickel and Alloy 180 in weld joints used on microelectronic module fabrication. Distinct separation was achieved between low strength welds and sound welds by the Quality Monitor. Evaluation performed indicates a drift level at less than 2 percent on a series of 50 consecutive welds. Operation under shop conditions identified need for controlled electrode impact. This was achieved with pneumatic actuation.

Hutchinson, W. R.↗

Study of gas tungsten arc welding procedures for tantalum alloy T-111 (Ta-8 W-2Hf) plate

Methods of eliminating or reducing underbread cracking in multipass GTA welds in thick T-111 plate were studied. Single V butt welds prepared using experimental filler metal compositions and standard weld procedures resulted in only moderate success in reducing underbread cracking. Subsequent procedural changes incorporating manual welding, slower weld speeds, and three or fewer fill passes resulted in crack-free single V welds only when the filler metal was free of hafnium. The double V joint design with successive fill passes on opposite sides of the joint produced excellent welds. The quality of each weld was determined metallographically since the cracking, when present, was very slight and undetectable using standard NDT techniques. Tensile and bend tests were performed on selected weldments. The inherent filler metal strength and the joint geometry determined the strength of the weldment. Hardness and electron beam microprobe traverses were made on selected specimens with the result that significant filler metal-base metal dilution as well as hafnium segregation was detected. A tentative explanation of T-111 plate underbread cracking is presented based on the intrinsic effects of hafnium in the weldment.

Gold, R. E.↗

Polyimide weld bonding for titanium alloy joints

Two weld bonding processes were developed for joining titanium alloy; one process utilizes a weld-through technique and the other a capillary-flow technique. The adhesive used for the weld-through process is similar to the P4/A5F system. A new polyimide laminating resin, BFBI/BMPM, was used in the capillary-flow process. Static property information was generated for weld-bonded joints over the temperature range of 219 K (-65 F) to 561 K (+550 F) and fatigue strength information was generated at room temperature. Significant improvement in fatigue strength was demonstrated for weld-bonded joints over spot-welded joints. A demonstration was made of the applicability of the weld-through weld-bonding process for fabricating stringer stiffened skin panels.

Vaughan, R. W.↗

Linear dimension establishes weld integrity

Study finds that when automatic in-place tube-welding head is used to butt-weld two stainless-steel tubes together, welding process can be made so reliable that when weld exceeds a certain minimum dimension, penetration of weld can be assumed to be complete. Detailed procedure for tube welding considers effects of arc gap, shielding gas, welding speed, and other parameters related to weld reliability.

Lewis, J. C.↗

Welding Research

Welding fabrication and welding processes were studied. The following research projects are reported: (1) welding fabrication; (2) residual stresses and distortion in structural weldments in high strength steels; (3) improvement of reliability of welding by in process sensing and control (development of smart welding machines for girth welding of pipes); (4) development of fully automated and integrated welding systems for marine applications; (5) advancement of welding technology; (6) research on metal working by high power laser (7) flux development; (8) heat and fluid flow; (9) mechanical properties developments.

Source record↗

Evaluation of electrode shape and nondestructive evaluation method for welded solar cell interconnects

Resistance welds of solar cell interconnect tabs were evaluated. Both copper-silver and silver-silver welds were made with various heat inputs and weld durations. Parallel gap and annular gap weld electrode designs were used. The welds were analyzed by light microscope, electron microprobe and scanning laser acoustic microscope. These analyses showed the size and shape of the weld, the relationship between the acoustic micrographs, the visible electrode footprint, and the effect of electrode misalignment. The effect of weld heat input on weld microstructure was also shown.

Baraona, C. R.↗

NASA welding assessment program

A program was conducted to demonstrate the cycle life capability of welded solar cell modules relative to a soldered solar cell module in a simulated low earth orbit thermal environment. A total of five 18-cell welded (parallel gap resistance welding) modules, three 18-cell soldered modules, and eighteen single cell samples were fabricated using 2 x 4 cm silicon solar cells from ASEC, fused silica cover glass from OCLI, silver plated Invar interconnectors, DC 93-500 adhesive, and Kapton-Kevlar-Kapton flexible substrate material. Zero degree pull strength ranged from 2.4 to 5.7 lbs for front welded contacts (40 samples), and 3.5 to 6.2 lbs for back welded contacts (40 samples). Solar cell cross sections show solid state welding on both front and rear contacts. The 18-cell welded modules have a specific power of 124 W/kg and an area power density of 142 W/sq m (both at 28 C). Three welded and one soldered module were thermal cycle tested in a thermal vacuum chamber simulating a low earth orbit thermal environment.

Patterson, R. E.↗

Signal Analysis of Gas Tungsten Arc Welds

Gas tungsten arc welding is a process in which the input parameters such as current, voltage and travel speed, can be easily controlled and/or monitored. However, weld quality is not solely a function of these parameters. An adaptive method of observing weld quality is desired to improve weld quality assurance. The use of dynamic electrical properties of the welding arc as a weld quality monitor was studied. The electrical properties of the arc are characterized by the current voltage transfer function. The hardware and software necessary to collect the data at a maximum rate of 45 kHz and to allow the off-line processing of this data are tested. The optimum input current waveform is determined. Bead-on-plate welds to observe such characteristics of the weld as the fundamental frequency of the puddle are studied. Future work is planned to observe changes of the arc response with changes in joint geometry, base metal chemistry, and shielding gas composition are discussed.

Eagar, T. W.↗

On the determination of the origin of linear anomaly in the macrostructure of VPPA welded 2219-T87 aluminum alloy: Preliminary report

The cause and significance of the weld radiograph enigma, which is a linear anomaly in the features of the X-ray film is examined. By observing features on available radiographs and in studying published reports of similar features, it was possible to conclude that there are many manifestations of the enigma, and that they are all specific features of fine structure in radiographs due to natural processes connected with welding and to specific X-ray absorption and diffraction phenomena. These processes include the thermal distribution and liquid metal flow in welding, the development of microstructure, morphology, second phase particles and porosity due to the solidification process, and to the pattern of residual stresses after the weld metal has cooled to the ambient temperature. Microdensitometer traces were made across weld radiographs of standard enigmatic types. Similar patterns were produced by computer simulation. These show that the enigma is a relatively low contrast feature compared to real weld defects, such as undercuts or centerline cracks. The enigma can be distinguished from weld defects by these microdensitometer traces. The enigma effect on weld properties is not known but is expected to be minor.

Jemian, W. A.↗