SEARCH · Engineering Papers
Results for “magnetic diffraction”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Optimizing a low-energy electron diffraction spin-polarization analyzer for imaging of magnetic surface structures
A newly designed scanning electron microscope with polarization analysis (SEMPA or spin-SEM) for the acquisition of magnetic images is presented. Core component is the spin detector, based on the scattering of low-energy electrons at a W(100) surface in ultrahigh vacuum. The instrument has been optimized with respect to ease of handling and efficiency. The operation and performance of a general low-energy electron diffraction (LEED) detector for SEMPA have been modeled in order to find the optimum operating parameters and to predict the obtainable image asymmetry. Based on the energy dependence of the secondary electron polarization and intensity, the detector output is simulated. For our instrument with optimized performance we demonstrate experimentally 8.6% polarization asymmetry in the domain structure of an iron whisker. This corresponds to 17.2% image contrast, in excellent agreement with the predicted simulated value. A contrast to noise ratio of 27 is achieved at 5 ms acquisition time per pixel.
Spatially limited antiferromagnetic order in a cluster glass compound Tb2Ni0.90Si2.94
In the present study, the synthesis of a new ternary intermetallic compound Tb2Ni0:90Si2:94 has been reported. The detailed studies on structure, static and dynamical magnetic properties of the compound have been investigated by means of powder x-ray diffraction, compositional analysis, dc & ac magnetization, non-equilibrium dynamics, heat capacity and neutron diffraction measurements. The dc & ac magnetic susceptibility reveal that the compound undergoes spin cluster-glass behaviour below 9.9 K. The frequency dependence of the freezing temperature have been analyzed on the basis of dynamic scaling laws such as power-law divergence and Vogel-Fulcher law, which further con rm the cluster-glass state formation for the compound. A detailed study on non-equilibrium dynamical behaviour associated with cluster-glass state has been carried out through magnetic relaxation behaviour along with magnetic memory effect in zero-field-cooled (ZFC) as well as field-cooled (FC) conditions and associated aging effect. The zero-field neutron diffraction study reveals the presence of a spatially limited antiferromagnetic phase in addition to the magnetically frustrated cluster-glass state. This result has also been supported through zero-field heat capacity studies. The variation in local electronic environment among the magnetic rare- earth ions caused by the structural disorder associated with Ni/Si ions have been argued to be responsible for the coexistence of different magnetic phases.
Determination of magnetic parameters in La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/SrTiO{sub 3} thin films using EMCD
It is well known that the magnetic state of the La{sub 0.7}Sr{sub 0.3}MnO{sub 3} (LSMO) thin-film heterostructure is strongly correlated with the lattice, spin, orbital, and charge states, since these influence the electric and magnetic transport properties even on the unit-cell level. Therefore, understanding the material's magnetic properties on the nanoscale is important for the development of novel applications. The recently developed electron magnetic-circular dichroism (EMCD) technique allows the determination of atomic site-specific magnetic information via the use of transmitted electrons; however, its sensitivity is not high enough to quantitatively acquire magnetic information in many weak magnetism systems. Here, we utilized a dynamical diffraction-effect assisted EMCD technique to quantitatively determine the spin and orbital magnetic moment of LSMO/SrTiO{sub 3} thin films on the nanometer scale using a transmission electron microscope. Further, data processing was optimized to enhance the intensity of the EMCD signals for manganese, which have very weak magnetism at room temperature. High signal-to-noise ratio and accurate quantitative magnetic measurement are eventually achieved. Finally, the spin magnetic moments (0.73 ± 0.26 μ{sub B}) are derived, and we also limited the ratio of the orbital to spin magnetic moment within an interval of (−0.03, 0.01). Our results not only present the nanoscale magnetic parameters of LSMO/SrTiO{sub 3}, but also demonstrate how the measurement limit of the spin (or orbital) magnetic moment can be achieved, which is via the developed dynamical diffraction effect assisted EMCD technique.
Effect of oxygen non-stoichiometry on the structural and magnetotransport properties of LaMn{sub 0.85}Cr{sub 0.15}O{sub 3+{delta}}
Thermogravimetry, X-ray diffraction (XRD), d.c. magnetization, high-temperature susceptibility and electrical resistivity measurements were performed for LaMn{sub 0.85}Cr{sub 0.15}O{sub 3+{delta}} perovskites with accurate control of the oxygen content (0{<=}{delta}{<=}0.11). For 0{<=}{delta}<0.09, three orthorhombic structures (Pnma) are found: for 0{<=}{delta}<0.045, the O' phase (b/{radical}2<c<a), for 0.045{<=}{delta}<0.06, the O'' (b/{radical}2<a<c) and for 0.06{<=}{delta}<0.09, the O{sup '''} (a<b/{radical}2<c). For 0.09{<=}{delta}{<=}0.11, a rhombohedral symmetry (R3{sup -}barc) coexists with O{sup '''} in a biphasic field. Magnetic measurements revealed the ferromagnetic interactions (FM) character of the Mn{sup 3+}-O-Cr{sup 3+} interaction, but also the intricate magnetic phase diagram due to the presence of multiple interactions (Mn{sup 3+,4+}-O-Mn{sup 3+,4+}, Cr{sup 3+}-O-Mn{sup 3+}, etc.). The comparison of the results for LaMn{sub 0.85}Cr{sub 0.15}O{sub 3+{delta}} with those of LaMn{sub 0.9}Cr{sub 0.1}O{sub 3+{delta}} allows discuss the role of Cr{sup 3+} on the structural, magnetic and magnetotransport properties of the LaMn{sub 1-x}Cr{sub x}O{sub 3+{delta}} perovskites. - Graphical abstract: The variation of the critical transition temperature T{sub N},{sub C} as a function of the tilt angle '{phi}' for La Mn{sub 0.9}Cr{sub 0.1}O{sub 3+{delta}} and LaMn{sub 0.9}Cr{sub 0.1}O{sub 3+{delta}} compounds with 3.00{<=}3+{approx_equal}{<=}3.07 is shown. It can be observed that the LaMn{sub 0.85}Cr{sub 0.15}O{sub 3+{approx_equal}} does not present the typical minimum associated with the competition between antiferromagnetic (AFM) and ferromagnetic (FM) interactions.
Identifying the Critical Role of Li Substitution in P2-Na x [Li y Ni z Mn 1-y-z ]O 2 (0 < x, y, z < 1) Intercalation Cathode Materials for High-Energy Na-Ion Batteries
Li-substituted layered P2–Na 0.80 [Li 0.12 Ni 0.22 Mn 0.66 ]O 2 is investigated as an advanced cathode material for Na-ion batteries. Both neutron diffraction and nuclear magnetic resonance (NMR) spectroscopy are used to elucidate the local structure, and they reveal that most of the Li ions are located in transition metal (TM) sites, preferably surrounded by Mn ions. To characterize structural changes occurring upon electrochemical cycling, in situ synchrotron X-ray diffraction is conducted. It is clearly demonstrated that no significant phase transformation is observed up to 4.4 V charge for this material, unlike Li-free P2-type Na cathodes. The presence of monovalent Li ions in the TM layers allows more Na ions to reside in the prismatic sites, stabilizing the overall charge balance of the compound. Consequently, more Na ions remain in the compound upon charge, the P2 structure is retained in the high voltage region, and the phase transformation is delayed. Ex situ NMR is conducted on samples at different states of charge/discharge to track Li-ion site occupation changes. Surprisingly, Li is found to be mobile, some Li ions migrate from the TM layer to the Na layer at high voltage, and yet this process is highly reversible. Novel design principles for Na cathode materials are proposed on the basis of an atomistic level understanding of the underlying electrochemical processes. These principles enable us to devise an optimized, high capacity, and structurally stable compound as a potential cathode material for high-energy Na-ion batteries.
Structural Characterization and Magnetic Properties of SrCo{sub 2}Fe{sub 16}O{sub 27} Hexaferrite Synthesized by Citric Acid Sol-Gel Method
The W -type SrCo{sub 2}Fe{sub 16}O{sub 27} (SCFO) hexagonal ferrite samples were prepared by the sol-gel method using metal nitrate as raw material, citric acid as complexing agent, and water as solvent. The effects of different sintering temperatures and holding times on the phase composition and morphology properties were explored in detail by using the X-ray diffractometer and field emission scanning electron microscope. The X-ray diffraction, microstructure, and magnetic performance of most optimum sintering temperature and holding time of preparing single-phase SCFO hexagonal ferrite were investigated. The experimental results indicate that the best optimum sintering temperature and holding time of SCFO hexagonal ferrite are 1280 °C and 4 h, respectively. Field emission scanning electron microscopy results indicate that the size of the particles is about 5–10 μ m. The result of magnetic measurement shows that SCFO hexagonal ferrite exhibits the soft magnetic property and the Curie temperature (T{sub C}) is ∼ 850 K. Furthermore, by analyzing the Arrott plot, the phase transition near the T{sub C} is a secondary phase transition.
Srystal structure and physical properties of the new ternary antimonides Ln{sub 3}Pd{sub 8}Sb{sub 4} (Ln=Y, Gd, Tb, Dy, Ho, Er, Tm)
The ternary antimonides Ln{sub 3}Pd{sub 8}Sb{sub 4} (Ln=Y, Gd, Tb, Dy, Ho, Er, Tm) have been synthesized for the first time. The crystal structure of Er{sub 3}Pd{sub 8}Sb{sub 4} has been solved from the X-ray single crystal data: own type structure, space group Fm3-bar m, a=1.3050(1) nm, R{sub F}=0.0484, R{sub W}=0.0524 for 17 free parameters and 401 reflections with F(hkl)>4{sigma}(F). The structure of Er{sub 3}Pd{sub 8}Sb{sub 4} can be viewed as a ternary ordered version of the Sc{sub 11}Ir{sub 4}-type. The lattice parameters of the isotypic compounds Ln{sub 3}Pd{sub 8}Sb{sub 4} (Ln=Y, Gd, Tb, Dy, Ho, Tm) have been refined from the X-ray powder diffraction data. The magnetic and electrical properties of the compounds Ln{sub 3}Pd{sub 8}Sb{sub 4} (Ln=Tb, Ho, Er) have been studied down to 1.75 K. The Ho- and Er-based phases have been found to order antiferromagnetically at 2.5 and 2.0 K, respectively. For all three compounds, the magnetic susceptibility follows in the paramagnetic region the Curie-Weiss behavior with the effective magnetic moments close to the respective free trivalent ion values. All three antimonides studied exhibit metallic character of the electrical conductivity. - Graphical abstract: Projection of the crystal structure of Er{sub 3}Pd{sub 8}Sb{sub 4} onto XY plane and the coordination polyhedra of all the atoms.
Influence of Zn on magnetocaloric effect in (0.95)La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/Ni{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} ceramic composites
Highlights: • Synthesis of magnetic ceramic composites. • Magnetization of dual phase ceramics. • Magnetic entropy change in (0.95)La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/(0.05)Ni{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} solid solution. - Abstract: We report the magnetic and magnetocaloric properties of (0.95)La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/(0.05)Ni{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} (x = 0.0, 0.1, 0.3, and 0.5) ceramic composites. The composite samples with nominal compositions were prepared using the conventional solid-state reaction method. The phase purity and structure were confirmed by using X-ray diffraction. Temperature dependent magnetization measurements and Arrott analysis reveal second order of magnetic phase transition in the composite samples. A maximum in magnetic entropy change of ∼0.75 J/kg K at 1 T has been observed in (0.95)La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/(0.05)NiFe{sub 2}O{sub 4} sample. The values of magnetic entropy change of these composites make them attractive for potential applications. These composite samples may consider as potential material for magnetic refrigeration near room temperature.
Persistent short-range spin fluctuation in rare-earth substituted square lattice Sr 2 Ir 0.89 Tb 0.11 O 4
Sr 2 IrO 4 , a prototypical 𝐽 eff = 1/2 square lattice system, is widely studied for novel physics. While transition metal substitution effects are well explored, rare-earth doping at the Ir 4+ site is less explored. Here we present a detailed magnetization and neutron diffraction study on Sr 2 Ir 1−𝑥 Tb 𝑥 O 4 (𝑥 = 0.11). The system tends to adopt an in-plane antiferromagnetic configuration with a “++++” stacking sequence. Strong spin fluctuations persist down to the lowest measured temperature, consistent with the concave shape order parameter. A pronounced magnetic diffuse scattering rod develops along the 𝐿 direction at low temperature, indicating the formation of short-range magnetic correlations with a characteristic length of ∼ 24(2) Å. In conclusion, this work provides a new pathway to exotic quantum phases in the strongly spin-orbit-coupled iridates.
Synthesis, structure, and magnetic properties of a Yb{sup III} complex with the iminopyridine radical-anionic ligand
The reaction of equimolar amounts of ytterbocene (C{sub 5}Me{sub 4}H){sub 2}Yb(THF){sub 2} and iminopyridine 2,6-Pr{sup i}{sub 2}C{sub 6}H{sub 3}N=CH(C{sub 5}H{sub 4}N) accompanied by the one-electron oxidation of the ytterbium ion produced the unique lanthanide complex (C{sub 5}Me{sub 4}H){sub 2}Yb{sup III}[2,6-Pr{sup i}{sub 2}-C{sub 6}H{sub 3}NCH(C{sub 5}H{sub 4}N)]–• with the iminopyridine radical-anionic ligand. The structure of the complex in the crystalline state was established by X-ray diffraction and its magnetic properties were studied in the temperature range of 1.8—300 K.
Crystal fields, disorder, and antiferromagnetic short-range order in Yb 0.24 Sn 0.76 Ru
Not Available
New complex bismuth oxides in the Bi{sub 2}O{sub 3}–NiO–Sb{sub 2}O{sub 5} system and their properties
Phase equilibria in the Bi{sub 2}O{sub 3}–NiO–Sb{sub 2}O{sub 5} system have been investigated. The isothermal section of the system (650°) has been constructed. For the first time the existence of the pyrochlore structure solid solution, (Bi{sub 2−x}Ni{sub x})Ni{sub 2/3−y}Sb{sub 4/3+y}O{sub 7±δ}, x=0.1−0.35, y=0−0.1, and a new compound Bi{sub 3}Ni{sub 2/3}Sb{sub 7/3}O{sub 11} of KSbO{sub 3} structure type have been discovered. The structures and properties of these compounds were studied by XRD, XAFS, diffuse reflection spectroscopy and magnetic methods. Rietveld refinement of synchrotron radiation-based powder XRD data for pyrochlore sample of 38.43Bi{sub 2}O{sub 3}–33.0NiO–28.57Sb{sub 2}O{sub 5} composition and Bi{sub 3}Ni{sub 2/3}Sb{sub 7/3}O{sub 11} compound was performed. The best possible refinement of the positional parameters for both pyrochlore and Bi{sub 3}Ni{sub 2/3}Sb{sub 7/3}O{sub 11} structures was achieved for disordered models. Magnetic, diffuse reflection and an X-ray absorption spectroscopy study confirmed that in both compounds nickel ions are mainly in a 2+ oxidation state. According to magnetic data, Bi{sub 1.84}Ni{sub 0.16}(Ni{sub 0.63}Sb{sub 1.37})O{sub 7} pyrochlore and Bi{sub 3}Ni{sub 2/3}Sb{sub 7/3}O{sub 11} are overall paramagnetic in nature. - Graphical abstract: Isothermal section of the Bi{sub 2}O{sub 3}–NiO–Sb{sub 2}O{sub 5} system at 650 °C in air and variation of magnetic susceptibility and inverse susceptibility with temperature for Bi{sub 1.84}Ni{sub 0.79}Sb{sub 1.37}O{sub 7} pyrochlore. - Highlights: • We have constructed the isothermal section of the system Bi{sub 2}O{sub 3}–NiO–Sb{sub 2}O{sub 5}. • The boundaries of pyrochlore structure solid solution have been determined. • New Bi{sub 3}Ni{sub 2/3}Sb{sub 7/3}O{sub 11} compound of KSbO{sub 3} structure type have been discovered. • The structures were studied by means of synchrotron X-ray diffraction and XAFS. • Magnetic measurements revealed that both compounds are paramagnetic at 2–350 K.
Magnetic Tunability in RE-DOBDC MOFs via NO x Acid Gas Adsorption
The magnetic susceptibility of NO x -loaded RE-DOBDC (rare earth (RE): Y, Eu, Tb, Yb; DOBDC: 2,5-dihydroxyterephthalic acid) metal–organic frameworks (MOFs) is unique to the MOF metal center. RE-DOBDC samples were synthesized, activated, and subsequently exposed to humid NO x . Each NO x -loaded MOF was characterized by powder X-ray diffraction, and the magnetic characteristics were probed by using a VersaLab vibrating sample magnetometer (VSM). Lanthanide-containing RE-DOBDC (Eu, Tb, Yb) are paramagnetic with a reduction in paramagnetism upon adsorption of NO x . Y-DOBDC has a diamagnetic moment with a slight reduction upon adsorption of NO x . The magnetic susceptibility of the MOF is determined by the magnetism imparted by the framework metal center. The electronic population of orbitals contributes to determining the extent of magnetism and change with NO x (electron acceptor) adsorption. Eu-DOBDC results in the largest mass magnetization change upon adsorption of NO x due to more available unpaired f electrons. Experimental changes in magnetic moment were supported by density functional theory (DFT) simulations of NO x adsorbed in lanthanide Eu-DOBDC and transition metal Y-DOBDC MOFs.
Thermal low spin-high spin equilibrium of Fe(II) in thiospinels CuFe{sub 0.5}(Sn{sub (1-x)}Ti{sub x}){sub 1.5}S{sub 4} (0{<=}x{<=}1)
A series of spinel compounds with composition CuFe{sub 0.5}(Sn{sub (1-x)}Ti{sub x}){sub 1.5}S{sub 4} (0{<=}x{<=}1) is analysed by X-ray diffraction, measurements of magnetic susceptibilities and {sup 57}Fe Moessbauer spectroscopy. All samples show a temperature-dependent equilibrium between an electronic low spin 3d(t{sub 2g}){sup 6}(e{sub g}){sup 0} and a high spin 3d(t{sub 2g}){sup 4}(e{sub g}){sup 2} state of the Fe(II) ions. The spin crossover is of the continuous type and extends over several hundred degrees in all samples. The Sn/Ti ratio influences the thermal equilibrium between the two spin states. Substitution of Sn(IV) by the smaller Ti(IV) ions leads to a more compact crystal lattice, which, in contrast to many metal-organic Fe(II) complexes, does not stabilise the low spin state, but increases the residual high spin fraction for T{yields}0 K. The role played by antiferromagnetic spin coupling in the stabilisation of the high spin state is discussed. The results are compared with model calculations treating the effect of magnetic interactions on spin state equilibria. -- Graphical Abstract: Comparison of fractions of high spin Fe(II) from Moessbauer spectra (circles) with plots of {chi}{sub m}T (dots) versus T. Discrepancies between both methods indicate anti-ferromagnetic spin coupling. Display Omitted Research highlights: {yields} Many Fe(II) complexes show thermally induced high spin-low spin crossover. {yields} Spin crossover in spinel compounds is extremely scarce. {yields} Usually, lattice contraction favours the low spin state in Fe(II) complexes. {yields} In these spinels, lattice contraction favours the high spin state. {yields} The stabilisation of the high spin state is explained by spin-spin interactions.
Flat-band tuning and emergent itinerant magnetism in Sr(Co 1− x Pd x ) 2 As 2
The interplay between magnetism and flat-band (FB) instability is a central theme in quantum materials research. A striking example is the emergence of magnetic order in a nominally nonmagnetic compound when a flat band is tuned near the Fermi energy (E F ). Here, in this study, we investigate this phenomenon in the Pauli paramagnet SrCo 2 As 2 , where an FB associated with Co e g orbitals lies close to E F . Remarkably, a minute substitution of the nonmagnetic element Pd onto the Co site (~2%) induces antiferromagnetic order with a transition temperature as high as T N = 25 K. Temperature- and magnetic-field-dependent magnetic and transport measurements, complemented by zero-field neutron diffraction, reveal a helical magnetic order for x ≤ 0.10 in Sr(Co 1−x Pd x ) 2 As 2 , transitioning to a complex ferromagnetic state at higher Pd concentrations. Spectroscopic evidence and theoretical band structure calculations demonstrate that electron doping shifts the flat band closer to E F , significantly enhancing the Stoner parameter. This enhancement drives a strong ferromagnetic instability, leading to helical magnetic ordering dominated by in-plane ferromagnetic interactions. The emergence of robust magnetic ordering through substitution with nonmagnetic elements is a unique phenomenon that underscores the pivotal role of flat-band instability in tuning magnetism in itinerant systems.
4 d element induced improvement of structural disorder and development of weakly reentrant spin-glass behavior in NiRuMnSn
The pursuit of efficient spin polarization in quaternary Heusler alloys with the general formula XX'YZ (where X, X', and Y are transition metals and Z is a p-block element) has been a subject of significant scientific interest. While previous studies showed that isoelectronic substitution of a 4d element in place of a 3d element in quaternary Heusler alloys improves the half-metallic ferromagnetic characteristics, our research here, on the quaternary Heusler alloy NiRuMnSn, reveals a strikingly different scenario. In this study, we present a detailed structural analysis of the material using x-ray absorption fine structure and neutron diffraction techniques which confirms the formation of a single-phase compound with 50:50 site disorder between Ni and Ru atoms at 4c and 4d sites. Contrary to expectations, our density functional theory calculations suggest a considerable decrease in spin polarization even in the ordered structure. Additionally, we report on the compound's exceptional behavior, displaying a rare reentrant spin-glass property below ~ 60 K, a unique and intriguing feature for quaternary Heusler-type compounds.