Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Titanium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Chemical, Morphological, Structural, Optical, and Magnetic Properties of Transition Metal Titanium (Ti)-Doped LaFeO{sub 3} Nanoparticles

In the present work, pure and transition metal titanium (Ti)-doped LaFe{sub 1−x}Ti{sub x}O{sub 3}(x = 0.0, 0.2, 0.4, and 0.6) nanoparticles have been successfully synthesized by hydrothermal synthesis technique for various molar ratios of 0.2, 0.4, and 0.6. The prepared samples were grinned and annealed in furnace at 600 {sup ∘}C/4 h. The X-ray diffraction (XRD) analysis confirms the phase orthorhombic formation of LaFeO{sub 3} and Ti-doped LaFeO{sub 3}. The stoichiometric analysis was performed through energy-dispersive X-ray studies (EDX). The micro-structural features of surface morphology were examined by field emission scanning electron microscopy (FESEM). Further, surface nanocrystalline of the titanium (Ti)-doped LaFe{sub 1−x}Ti{sub x}O{sub 3} was also investigated through high-resolution transmission electron microscopic (TEM) analysis. The enhancement of room temperature magnetization value has been observed from the M–H curve which is measured using vibrating sample magnetometer (VSM).The weak ferromagnetic behavior was observed from hysteresis loop. From hysteresis loop, saturation takes place when the applied magnetic field intensity is 15 kO{sub e}.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Regularities of Plasma-Immersion Formation of Long-Pulse High-Intensity Titanium Ion Beams

The results of experimental investigations on plasma-immersion formation of ballistically focused beams of low-energy titanium ions with the pulse duration up to 30 μs are presented. The processes of neutralization of the space charge of high-intensity beams upon increasing the ion-current density by a few orders of magnitude during their focusing are addressed. The conditions of preliminary injection of the metal plasma, its parameters, the formation of the beam plasma during residual-gas ionization and secondary and thermionic emissions are shown to be of critical importance for an effective transport of these beams in the equi-potential drift space. It is demonstrated that the use of a disc electrode, preventing the macroparticles from penetrating the region of the ballistic beam focusing, increases the efficiency of long-pulse titanium ion beam transport and simultaneously reduces the probability of instability development.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Inductive System for Reliable Magnesium Level Detection in a Titanium Reduction Reactor

The determination of the Magnesium level in a Titanium reduction retort by inductive methods is often hampered by the formation of Titanium sponge rings which disturb the propagation of electromagnetic signals between excitation and receiver coils. We present a new method for the reliable identification of the Magnesium level which explicitly takes into account the presence of sponge rings with unknown geometry and conductivity. The inverse problem is solved by a look-up-table method, based on the solution of the inductive forward problems for several tens of thousands parameter combinations.

36 MATERIALS SCIENCE↗

Titanium Alloys Thin Sheet Welding with the Use of Concentrated Solar Energy

The present study deals with the welding of titanium alloys thin sheets 1.3 mm thick, with the use of concentrated solar energy. The experimental part of the work took place at a medium size solar furnace at the installation of the Centre National de la Recherche Scientifique, at Odeillo, in Southern France, where similar and dissimilar defect-free welds of titanium Grades 4 and 6 were achieved, in the butt joint configuration. After the determination of the appropriate welding conditions, the optimum welded structures were examined and characterized microstructurally, by means of light optical microscopy, scanning electron microscopy, and microhardness testing. In addition, test pieces extracted from the weldments were tested under uniaxial tensile loading aiming to the estimation of the strength and the ductility of the joint. The analysis of the experimental results and the recorded data led to the basic concluding remarks which demonstrate increased hardness distribution inside the fusion area and severe loss of ductility, but adequate yield and tensile strength of the welds.

36 MATERIALS SCIENCE↗

High Cycle Fatigue Performance in Laser Shock Peened TC4 Titanium Alloys Subjected to Foreign Object Damage

During their service, titanium alloys are likely to suffer from the foreign object damage (FOD), resulting in a decrease in their fatigue strength. Laser shock peening (LSP) has been proved to effectively increase the damage tolerance of military engine components by introducing a magnitude compressive residual stress in the near-surface layer of alloys. In this paper, smooth specimens of a TC4 titanium alloy were used and treated by LSP and subsequently exposed to FOD, which was simulated by firing a steel sphere with a nominal velocity of 300 m/s, at 90° with the leading edge of the LSP-treated region using a light gas gun. All impacted specimens were then subjected to fatigue loading. The results showed that LSP could effectively improve the fatigue strength of the damaged specimens. The effect of LSP on the fatigue strength was assessed through fracture observations, microhardness tests and residual stress analyses. The residual stresses due to the plastic deformation caused by LSP and the FOD impact, which were found to play a crucial role on the fatigue strength, were determined using the commercial software ABAQUS.

36 MATERIALS SCIENCE↗

Electrochemical Behavior of Biomedical Titanium Alloys Coated with Diamond Carbon in Hanks’ Solution

Biomedical implants in the knee and hip are frequent failures because of corrosion and stress on the joints. To solve this important problem, metal implants can be coated with diamond carbon, and this coating plays a critical role in providing an increased resistance to implants toward corrosion. In this study, we have employed diamond carbon coating over Ti-6Al-4V and Ti-13Nb-13Zr alloys using hot filament chemical vapor deposition method which is well-established coating process that significantly improves the resistance toward corrosion, wears and hardness. The diamond carbon-coated Ti-13Nb-13Zr alloy showed an increased microhardness in the range of 850 HV. Electrochemical impedance spectroscopy and polarization studies in SBF solution (simulated body fluid solution) were carried out to understand the in vitro behavior of uncoated as well as coated titanium alloys. The experimental results showed that the corrosion resistance of Ti-13Nb-13Zr alloy is relatively higher when compared with diamond carbon-coated Ti-6Al-4V alloys due to the presence of β phase in the Ti-13Nb-13Zr alloy. Electrochemical impedance results showed that the diamond carbon-coated alloys behave as an ideal capacitor in the body fluid solution. Moreover, the stability in mechanical properties during the corrosion process was maintained for diamond carbon-coated titanium alloys.

36 MATERIALS SCIENCE↗

Tribological Performance of Duplex-Annealed Ti-6Al-2Sn-4Zr-2Mo Titanium Alloy at Elevated Temperatures Under Dry Sliding Condition

Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2) is a typical near-α titanium alloy developed for high-temperature applications. It offers numerous enhanced properties like an outstanding strength-to-weight ratio, a low Young’s modulus and exceptional creep and corrosion resistance. On the other hand, titanium alloys are known for their weak resistance to wear. Ti-6-2-4-2 is mainly applied in aero engine component parts, which are exposed to temperatures up to 565 °C. Through an increasing demand on efficiency, engine components are exposed to higher combustion pressures and temperatures. Elevated temperature tribology tests were conducted on a pin-on-disk tribometer equipped with a heating chamber. The tests were carried out under dry conditions with a constant sliding distance of 600 m with a speed of 0.16 m/s at the ball point. The sliding partner was AISI E52100 steel ball with the hardness of 58HRC. The varied input variables are normal load and temperature. It can be concluded that the coefficient of friction (CoF) increases with increasing temperature, while the wear rate decreases to its minimum at 600 °C due to increasing adhesion and oxidation mechanisms. Wear track observations using a scanning electron microscope (SEM) including energy-dispersive x-ray spectroscopy (EDS) were used to determine the occurring wear mechanisms.

36 MATERIALS SCIENCE↗

Influence of Annealing on the Properties of Explosively Welded Titanium Grade 1—AW7075 Aluminum Alloy Bimetals

Explosive welding of titanium Grade 1 to AW7075 aluminum alloy arranged in parallel setup was performed. The annealing of produced bimetals at the temperatures of 450, 500 and 550 °C for times ranging from 20 to 100 h was carried out after explosive welding. The produced bimetal was characteristic by its wavy interface typical for that bonding process. Increase in the microhardness at the interface was recorded due to work hardening. Delamination of titanium Grade 1 flyer sheet was firstly observed when annealing temperature of 500 °C for 40 h was carried out. Annealing at 550 °C also resulted in delamination of upper sheet. The intermetallic compound (IMC) layer was observed at the interface after annealing of bimetals. The higher the annealing temperature and time, the higher the thickness of continuous IMC layer. The maximum measured thickness of IMC layer averaged 13 µm. Energy dispersive x-ray spectroscopy (EDS) and x-ray diffraction (XRD) analyses revealed that the interface layer is consisted of Al{sub 18}Ti{sub 2}Mg{sub 3} IMC. Microhardness at the interface increased dramatically up to 439 HV0.1 after annealing of bimetal due to the presence of above-mentioned IMC.

36 MATERIALS SCIENCE↗

Effect of Orientation of Weld Line on Formability of Electron Beam-Welded Dissimilar Thickness Titanium Sheets

Recently, manufacturing industries are looking forward to get insight into the influence of weld orientation on formability of tailor-welded blanks (TWBs) of titanium sheets for design and fabrication of lightweight components. Hence, commercially pure titanium (CP Ti) sheets of 1.0 and 1.2 mm thickness were joined together by electron beam welding process using accelerating voltage of 55 kV, beam current of 14.9 mA and welding speed of 865 mm/min. Two different types of TWBs with weld line perpendicular to the rolling direction (WL ⊥ RD) and weld line parallel to the rolling direction (WL || RD) were fabricated, and subsequently, the tensile test, microstructure and microhardness characterizations were conducted to ensure quality of weld. The limiting dome height (LDH) tests were carried out using laboratory-scale setup to evaluate forming behavior of both the above TWBs in terms of FLD, strain distribution, weld line movement and failure location. It was found that the tensile stress–strain response and formability performance of TWBs were significantly influenced by weld line orientation with lower ductility, ultimate tensile strength and LDH in TWB of WL || RD. Moreover, significant weld line movement and non-uniform strain distribution with necking and subsequently fracture were observed away from the weld line in thinner 1.0 mm CP Ti sheets depending on both sample geometry and weld line orientation.

36 MATERIALS SCIENCE↗

Effect of Zinc Interlayer in Microstructure Evolution and Mechanical Properties in Dissimilar Friction Stir Welding of Aluminum to Titanium

The welding of aluminum (Al) and titanium (Ti) is difficult and challenging due to the differences in their chemical and physical properties, and the formation of brittle intermetallic phases. In the present experiment, a zinc (Zn) interlayer was used during friction stir welding of Al to Ti. The weld was characterized in detail to understand the mechanisms associated with microstructural evolution and improvement in mechanical properties of the weld. X-ray computed tomography results reveal three-dimensional distribution of particles and flakes of titanium in the weld nugget. It was also observed that Ti particles are inhomogeneously distributed in the weld and the distribution depends on their morphology. Such a distribution of Ti was informative in understanding material flow. In addition, the consolidation of Zn in the Al matrix reveals the nature of material flow in the weld nugget as well. The importance of the Zn interlayer and mechanism of phase formation was explored in this study. It was characterized that the mechanical mixing of Zn with Al and Ti alters phase evolution and restricts the formation of conventional Al{sub 3}Ti intermetallic phase. The presence of zinc homogenizes elemental distribution and inhibits the formation of brittle intermetallic phases, which leads to a substantial improvement in mechanical properties of the weld.

36 MATERIALS SCIENCE↗

Improved Electrochemical Performance of Plasma Electrolytic Oxidation Coating on Titanium in Simulated Body Fluid

The effect of plasma electrolytic oxidation (PEO) pre-treatments on corrosion behavior of titanium in simulated body fluid (SBF) is investigated. Three pre-treatments are compared, using silicate, calcium phosphate and mixed silicate and calcium phosphate (1:1) electrolytes, respectively. The resultant coatings in different compositions and morphologies were examined by high-resolution field emission scanning electron microscopy equipped with energy-dispersive spectrometer and x-ray diffraction. The PEO-treated specimens revealed distribution of coating species, mainly the titanium-rich inner coating region. However, findings show highly localized variations in composition within their crystalline structures, due to the melting and rapid solidification of the coating material in three different electrolytes. Corrosion behavior of the coatings was also examined in SBF at 37 °C by potentiodynamic polarization, revealing an improvement in corrosion resistance for mixed electrolyte compared to silicate and calcium phosphate electrolytes.

36 MATERIALS SCIENCE↗

Experimental Study on Microstructure and Hardness of Pure Titanium Subjected to Torsion Deformation at Different Temperatures

The studies of mechanical property, microstructure evolution and fracture analysis in pure titanium processed by torsion deformation at 298, 673 and 1073 K are conducted systematically. The variations of mechanical property of deformed pure titanium are shown through Vickers hardness evaluation. During torsion at 298 K, the grains are refined and elongated, but the α phase with different shapes precipitates for twisted samples at 673 and 1073 K. The fracture appearance indicates that the elongated dimples occur on fracture surface at 298 K. Besides, a large number of shear facets are arranged. However, typical intergranular fracture appearance with lots of blocks in polyhedral shape covers the fracture surface at 673 and 1073 K, respectively.

36 MATERIALS SCIENCE↗

Low-Pressure Diffusion Bonding of Vanadium to Commercially Pure Titanium and Ti-6Al-4V

Modern technology increasingly requires components to be made from specific high-performance materials. To support complex multi-metal structures, a variety of techniques are required to join dissimilar metal parts with precise shapes. This study evaluates vacuum diffusion bonding as a method for joining titanium and vanadium, focusing on both pure titanium and the common alloy Ti-6Al-4V. We employ modest pressure provided by a weight and simple surface preparation to simulate the most commercially applicable process. Here, we show that Ti-6Al-4V alloy bonds readily to V, forming a continuous, clearly defined interdiffusion layer with predictable kinetics. Conversely, commercially pure Ti forms a crack-prone bond with V that fails to improve at higher bonding temperatures or longer times. We attribute this failure to the concentration of stress caused by the ß-to-α phase transformation in Ti. The contrasting bonding efficacy between pure Ti and the alloy provides insight into the crystallographic interactions that occur at the interface during bonding and cooling. These results provide surprising insight into a new method for bonding Ti alloys to V and possibly other metals that share the body-centered cubic crystal structure.

36 MATERIALS SCIENCE↗

Shock and Microstructural Characterization of the α-ω Phase Transition in Titanium Crystals

In this paper, a multicrystal comprised of a small number of large crystals of high-purity titanium and a [ 0001 ] oriented high-purity single crystal titanium sample were shock loaded using gas gun plate impact experiments. Tests were performed at stresses above the &#x03B1;<!-- α --> &#x2212;<!-- - --> &#x03C9;<!-- ω --> phase transition stress (for high-purity polycrystalline specimens) to observe the behavior of oriented crystals under similar conditions. Post-mortem characterization of the shocked microstructure was conducted on the single crystal sample to measure textures, and quantify phases and twinning. The apparent activation of plastic and transformation mechanisms was dependent upon crystal orientation. Specifically, the [ 0001 ] crystal showed a higher Hugoniot elastic limit than the [ 10 1 &#x00AF;<!-- ¯ --> 0 ] or [ 3 1 &#x00AF;<!-- ¯ --> 4 &#x00AF;<!-- ¯ --> 4 ] orientations. The slope of velocity as a function of time was lower in the [ 0001 ] orientation than the other orientations during plastic deformation, indicating sluggish transformation kinetics for the α to ω phase transition for the [ 0001 ] oriented crystal. Finally, microtexture measurements of a recovered [ 0001 ] oriented single crystal revealed the presence of retained ω phase after unloading, with orientations of the constituent phase fractions indicative of the forward α→ω transition, rather than the reverse ω→α transition, suggesting that the material never achieved a state of 100% ω phase.

36 MATERIALS SCIENCE↗

Skeletal stem cell and bone implant interactions are enhanced by LASER titanium modification

Purpose: To evaluate the osteo-regenerative potential of Titanium (Ti) modified by Light Amplification by Stimulated Emission of Radiation (LASER) beam (Yb-YAG) upon culture with human Skeletal Stem Cells (hSSCs{sup 1}). Methods: Human skeletal cell populations were isolated from the bone marrow of haematologically normal patients undergoing primary total hip replacement following appropriate consent. STRO-1{sup +} hSSC{sup 1} function was examined for 10 days across four groups using Ti discs: i) machined Ti surface group in basal media (Mb{sup 2}), ii) machined Ti surface group in osteogenic media (Mo{sup 3}), iii) LASER-modified Ti group in basal media (Lb{sup 4}) and, iv) LASER-modified Ti group in osteogenic media (Lo{sup 5}). Molecular analysis and qRT-PCR as well as functional analysis including biochemistry (DNA, Alkaline Phosphatase (ALP{sup 6}) specific activity), live/dead immunostaining (Cell Tracker Green (CTG{sup 7})/Ethidium Homodimer-1 (EH-1{sup 8})), and fluorescence staining (for vinculin and phalloidin) were undertaken. Inverted, confocal and Scanning Electron Microscopy (SEM) approaches were used to characterise cell adherence, proliferation, and phenotype. Results: Enhanced cell spreading and morphological rearrangement, including focal adhesions were observed following culture of hSSCs{sup 1} on LASER surfaces in both basal and osteogenic conditions. Biochemical analysis demonstrated enhanced ALP{sup 6} specific activity on the hSSCs{sup 1}-seeded on LASER-modified surface in basal culture media. Molecular analysis demonstrated enhanced ALP{sup 6} and osteopontin expression on titanium LASER treated surfaces in basal conditions. SEM, inverted microscopy and confocal laser scanning microscopy confirmed extensive proliferation and migration of human bone marrow stromal cells on all surfaces evaluated. Conclusions: LASER-modified Ti surfaces modify the behaviour of hSSCs.{sup 1} In particular, SSC{sup 1} adhesion, osteogenic gene expression, cell morphology and cytoskeleton structure were affected. The current studies show Ti LASER modification can enhance the osseointegration between Ti and skeletal cells, with important implications for orthopaedic application. - Highlights: • Bone stem cells on LASER Ti surface display enhanced cell growth and viability. • Bone stem cells on LASER Ti surface exhibit marked biocompatibility. • Human bone stem cells on LASER Ti surface exhibit altered morphology. • LASER Ti enhance osteogenic differentiation of human bone skeletal stem cells. • LASER Ti provides a unique approach to enhance osseointegration with the material.

60 APPLIED LIFE SCIENCES↗

Titanium dioxide nanoparticles induce an adaptive inflammatory response and invasion and proliferation of lung epithelial cells in chorioallantoic membrane

Titanium dioxide nanoparticles (TiO{sub 2} NPs) studies have been performed using relatively high NPs concentration under acute exposure and limited studies have compared shape effects. We hypothesized that midterm exposure to low TiO{sub 2} NPs concentration in lung epithelial cells induces carcinogenic characteristics modulated partially by NPs shape. To test our hypothesis we synthesized NPs shaped as belts (TiO{sub 2}-B) using TiO{sub 2} spheres (TiO{sub 2}-SP) purchased from Sigma Aldrich Co. Then, lung epithelial A549 cells were low-exposed (10 µg/cm{sup 2}) to both shapes during 7 days and internalization, cytokine release and invasive potential were determined. Results showed greater TiO{sub 2}-B effect on agglomerates size, cell size and granularity than TiO{sub 2}-SP. Agglomerates size in cell culture medium was 310 nm and 454 nm for TiO{sub 2}-SP and TiO{sub 2}-B, respectively; TiO{sub 2}-SP and TiO{sub 2}-B induced 23% and 70% cell size decrease, respectively, whilst TiO{sub 2}-SP and TiO{sub 2}-B induced 7 and 14-fold of granularity increase. NO{sub x} production was down-regulated (31%) by TiO{sub 2}-SP and up-regulated (70%) by TiO{sub 2}-B. Both NPs induced a transient cytokine release (IL-2, IL-6, IL-8, IL-4, IFN-γ, and TNF-α) after 4 days, but cytokines returned to basal levels in TiO{sub 2}-SP exposed cells while TiO{sub 2}-B induced a down-regulation after 7 days. Midterm exposure to both shapes of NPs induced capability to degrade cellular extracellular matrix components from chorioallantoic membrane and Ki-67 marker showed that TiO{sub 2}-B had higher proliferative potential than TiO{sub 2}-SP. We conclude that midterm exposure to low NPs concentration of NPs has an impact in the acquisition of new characteristics of exposed cells and NPs shape influences cellular outcome. - Graphical abstract: (A) Lung epithelial cells were low exposed (below 10 µg/cm{sup 2}) to titanium dioxide nanoparticles (TiO{sub 2}-NPs) shaped as spheres (TiO{sub 2}-SP) and belts (TiO{sub 2}-B) for midterm (7 continuous days) separately. (B) Then, cells from each cell culture were harvested and seeded on the top of the chorioallantoic membrane (CAM) for 5 days and (C) invasion and proliferation of cells were analyzed in CAM sections. - Highlights: • Hydrodynamic size of TiO2- SP was smaller than TiO2-B in cell culture media • TiO2- SP induced higher decrease in cell size than TiO2-B • TiO2-SP induced a transient cytokine release and TiO2-B a downregulation • TiO2-B caused higher proliferative capability than TiO2-SP.

54 ENVIRONMENTAL SCIENCES↗

Deformation behavior of CP-titanium under strain path changes: Experiment and crystal plasticity modeling

The deformation behavior of commercially pure rolled titanium subjected to strain path changes is studied using experiments and a crystal plasticity model. Four different loading combinations are performed at room temperature to study the activation of slip, twinning, de-twinning and double-twinning in hexagonal closed packed titanium. The strain paths considered are: rolling direction compression (RDC) followed by normal direction compression (NDC), RDC followed by transverse direction compression (TDC), NDC followed by RDC, and NDC followed by TDC. An EBSD-based analysis of the distribution of boundary misorientation angles before and after reload was developed to analyze the evolution of {$10\bar{1}2$} tensile and {$11\bar{2}2$} compression twins. This analysis supports the model results concerning the treatment of twin reorientation. A de-twinning and double-twinning model accounting for back stress effects, an important feature of strain path changes, is implemented within the framework of the visco-plastic self-consistent (VPSC) model along with a dislocation density (DD) based hardening scheme. In the model, plasticity is accommodated by prismatic $\langle$a$\rangle$, basal $\langle$a$\rangle$ and pyramidal $\langle$c+a$\rangle$ slip modes, and {$10\bar{1}2$} tensile and {$11\bar{2}2$} compression twinning modes. The VPSC model predicts the evolution of twinning, de-twinning and double-twinning processes for both tensile and compression twinning modes under strain path change. The model predicts macroscopic stress-strain response, texture evolution, and twin volume fraction that are in agreement with experimental observations. The evolution of texture is investigated in detail by separately analyzing the twinned domains, rather than the evolution of the global texture.

36 MATERIALS SCIENCE↗

Crystallographic stability of the BCC phase during quenching of metastable beta titanium alloy Ti-5553 and comparison of structural criteria for the predictive capability of α” martensite

This work evaluates the compositional standard currently developed for Ti-5553 powder and explores the metastable β region for sensitivity to martensitic formation during rapid quenching from the melt. Ti-5553 is a beta-stabilized titanium alloy that is increasingly being used in additive manufacturing applications. A series of alloys within the Ti-5553 compositional space was processed using two-piston spat quenching to perform rapid solidification and quenching for each of these alloy compositions. Typical empirical models such as molybdenum equivalency are not able to fully separate the retained BCC and martensitic compositions. Further, the use of thermodynamic data to estimate the transformation energy needed to form martensite can differentiate the alloys and provide a metric to further develop compositional limits for metastable beta titanium alloy development.

36 MATERIALS SCIENCE↗