Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SiC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

SiC Optically Modulated Field-Effect Transistor

An optically modulated field-effect transistor (OFET) based on a silicon carbide junction field-effect transistor (JFET) is under study as, potentially, a prototype of devices that could be useful for detecting ultraviolet light. The SiC OFET is an experimental device that is one of several devices, including commercial and experimental photodiodes, that were initially evaluated as detectors of ultraviolet light from combustion and that could be incorporated into SiC integrated circuits to be designed to function as combustion sensors. The ultraviolet-detection sensitivity of the photodiodes was found to be less than desired, such that it would be necessary to process their outputs using high-gain amplification circuitry. On the other hand, in principle, the function of the OFET could be characterized as a combination of detection and amplification. In effect, its sensitivity could be considerably greater than that of a photodiode, such that the need for amplification external to the photodetector could be reduced or eliminated. The experimental SiC OFET was made by processes similar to JFET-fabrication processes developed at Glenn Research Center. The gate of the OFET is very long, wide, and thin, relative to the gates of typical prior SiC JFETs. Unlike in prior SiC FETs, the gate is almost completely transparent to near-ultraviolet and visible light. More specifically: The OFET includes a p+ gate layer less than 1/4 m thick, through which photons can be transported efficiently to the p+/p body interface. The gate is relatively long and wide (about 0.5 by 0.5 mm), such that holes generated at the body interface form a depletion layer that modulates the conductivity of the channel between the drain and the source. The exact physical mechanism of modulation of conductivity is a subject of continuing research. It is known that injection of minority charge carriers (in this case, holes) at the interface exerts a strong effect on the channel, resulting in amplification of the photon-detection signal. A family of operating curves characterizing the OFET can be generated in a series of measurements performed at different intensities of incident ultraviolet light.

Tabib-Azar, Massood↗

Active Oxidation of SiC

The high temperature oxidation of silicon carbide occurs in either a passive or active mode, depending on temperature and oxygen potential. Passive oxidation forms a protective oxide film which limits attack of the SiC:SiC(s) + 3/2 O2(g) = SiO2(s) + CO(g.) Active oxidation forms a volatile oxide and leads to extensive attack of the SiC: SiC(s) + O2(g) = SiO(g) + CO(g). The transition points and rates of active oxidation are a major issue. Previous studies are reviewed and the leading theories of passive/active transitions summarized. Comparisons are made to the active/passive transitions in pure Si, which are relatively well-understood. Critical questions remain about the difference between the active-to-passive transition and passive-to-active transition. For Si, Wagner [2] points out that the active-to-passive transition is governed by the criterion for a stable Si/SiO2 equilibria and the passive-to-active transition is governed by the decomposition of the SiO2 film. This suggests a significant oxygen potential difference between these two transitions and our experiments confirm this. For Si, the initial stages of active oxidation are characterized by the formation of SiO(g) and further oxidation to SiO2(s) as micron-sized rods, with a distinctive morphology. SiC shows significant differences. The active-to-passive and the passive-to-active transitions are close. The SiO2 rods only appear as the passive film breaks down. These differences are explained in terms of the reactions at the SiC/SiO2 interface. In order to understand the breakdown of the passive film, pre-oxidation experiments are conducted. These involve forming dense protective scales of 0.5, 1, and 2 microns and then subjecting the samples with these scales to a known active oxidation environment. Microstructural studies show that SiC/SiO2 interfacial reactions lead to a breakdown of the scale with a distinct morphology.

Jacobson, Nathan S.↗

SiC-Based Miniature High-Temperature Cantilever Anemometer

The figure depicts a miniature cantilever-type anemometer that has been developed as a prototype of compact, relatively nonintrusive anemometers that can function at temperatures up to 600 C and that can be expected to be commercially mass-producible at low cost. The design of this anemometer, and especially the packaging aspect of the design, is intended to enable measurement of turbulence in the high-temperature, high-vibration environment of a turbine engine or in any similar environment. The main structural components of the anemometer include a single-crystal SiC cantilever and two polycrystalline SiC clamping plates, all made from chemical-vapor-deposited silicon carbide. Fabrication of these components from the same basic material eliminates thermal-expansion mismatch, which has introduced spurious thermomechanical stresses in cantilever-type anemometers of prior design. The clamping plates are heavily oxidized to improve electrical insulation at high temperature. A cavity that serves as a receptacle for the clamped end of the cantilever is etched into one end of one clamping plate. Trenches that collectively constitute a socket for a multipin electrical plug (for connection to external electronic circuitry) are etched into the opposite end of this clamping plate. Metal strips for electrical contact are deposited on one face of the other clamping plate. Piezoresistive single-crystal SiC thin-film strain gauges are etched in the n-type SiC epilayer in a Wheatstone-bridge configuration. Metal contact pads on the cantilever that extend into the clamping-receptacle area, are obtained by deposition and patterning using standard semiconductor photolithography and etching methods. The cantilever and the two clamping plates are assembled into a sandwich structure that is then clamped in a stainless-steel housing. The Wheatstone- bridge carrying SiC cantilever with the metal contact pads on the piezoresistors is slid into the receptacle in the bottom clamping plate. The top clamping plate is brought into contact with the bottom plate so that the narrow section of the metal strips on the top clamp plate aligns with the metal contact pads on the cantilever. When the parts are clamped together, the metal strips provide electrical connections between the Wheatstone-bridge contact points and the sides the trenches that constitute the socket for the multipin electrical plug. Hence, to connect the Wheatstone bridge to external circuitry for processing of the anemometer readout, one need only insert the plug in the socket. In operation, the cantilever end of the stainless-steel housing is mounted flush with an engine wall and the unclamped portion of the cantilever is exposed into the flow. The cantilever is deflected in direct proportion to the force induced by component of flow parallel to the engine wall and perpendicular to the broad exposed face of the cantilever. The maximum strain on the cantilever occurs at the clamped edge and is measured by the piezoresistors, which are located there. The corresponding changes in resistance manifest themselves in the output of the Wheatstone bridge.

Okojie, Robert S.↗

Structural Characterization of Lateral-grown 6H-SiC am-plane Seed Crystals by Hot Wall CVD Epitaxy

The performance of commercially available silicon carbide (SiC) power devices is limited due to inherently high density of screw dislocations (SD), which are necessary for maintaining polytype during boule growth and commercially viable growth rates. The NASA Glenn Research Center (GRC) has recently proposed a new bulk growth process based on axial fiber growth (parallel to the c-axis) followed by lateral expansion (perpendicular to the c-axis) for producing multi-faceted m-plane SiC boules that can potentially produce wafers with as few as one SD per wafer. In order to implement this novel growth technique, the lateral homoepitaxial growth expansion of a SiC fiber without introducing a significant number of additional defects is critical. Lateral expansion is being investigated by hot wall chemical vapor deposition (HWCVD) growth of 6H-SiC am-plane seed crystals (0.8mm x 0.5mm x 15mm) designed to replicate axially grown SiC single crystal fibers. The post-growth crystals exhibit hexagonal morphology with approximately 1500 m (1.5 mm) of total lateral expansion. Preliminary analysis by synchrotron white beam x-ray topography (SWBXT) confirms that the growth was homoepitaxial, matching the polytype of the respective underlying region of the seed crystal. Axial and transverse sections from the as grown crystal samples were characterized in detail by a combination of SWBXT, transmission electron microscopy (TEM) and Raman spectroscopy to map defect types and distribution. X-ray diffraction analysis indicates the seed crystal contained stacking disorders and this appears to have been reproduced in the lateral growth sections. Analysis of the relative intensity for folded transverse acoustic (FTA) and optical (FTO) modes on the Raman spectra indicate the existence of stacking faults. Further, the density of stacking faults is higher in the seed than in the grown crystal. Bundles of dislocations are observed propagating from the seed in m-axis lateral directions. Contrast extinction analysis of these dislocation lines reveals they are edge type basal plane dislocations that track the growth direction. Polytype phase transition and stacking faults were observed by high-resolution TEM (HRTEM), in agreement with SWBXT and Raman scattering.

Single Crystal↗

Development of SiC Large Tapered Crystal Growth

Majority of very large potential benefits of wide band gap semiconductor power electronics have NOT been realized due in large part to high cost and high defect density of commercial wafers. Despite 20 years of development, present SiC wafer growth approach is yet to deliver majority of SiC's inherent performance and cost benefits to power systems. Commercial SiC power devices are significantly de-rated in order to function reliably due to the adverse effects of SiC crystal dislocation defects (thousands per sq cm) in the SiC wafer.

Neudeck, Phil↗

Step Free Surface Heteroepitaxy of 3C-SiC Layers on Patterned 4H/6H-SiC Mesas and Cantilevers

The off-axis approach to SiC epitaxial growth has not prevented many substrate crystal defects from propagating into SiC epilayers, and does not permit the realization of SiC heteropolytype devices. This paper reviews recent advancements in SiC epitaxial growth that begin to overcome the above shortcomings for arrays of device-sized mesas patterned into on-axis 4H/6HSiC wafers. These on-axis mesa growth techniques have produced 4H/6H-SiC homoepilayers and 3C-SiC heteroepilayers with substantially lower dislocation densities. The results should enable improved homojunction and heterojunction silicon carbide prototype devices.

Neudeck, P. G.↗

A wide bandgap silicon carbide (SiC) gate driver for high-temperature and high-voltage applications

Limitations of silicon (Si) based power electronic devices can be overcome with Silicon Carbide (SiC) because of its remarkable material properties. SiC is a wide bandgap semiconductor material with larger bandgap, lower leakage currents, higher breakdown electric field, and higher thermal conductivity, which promotes higher switching frequencies for high power applications, higher temperature operation, and results in higher power density devices relative to Si [1]. The proposed work is focused on design of a SiC gate driver to drive a SiC power MOSFET, on a Cree SiC process, with rise/fall times (less than 100 ns) suitable for 500 kHz to 1 MHz switching frequency applications. A process optimized gate driver topology design which is significantly different from generic Si circuit design is proposed. The ultimate goal of the project is to integrate this gate driver into a Toyota Prius plug-in hybrid electric vehicle (PHEV) charger module. The application of this high frequency charger will result in lighter, smaller, cheaper, and a more efficient power electronics system.

Lamichhane, Ranjan↗

Effect of Neutron Irradiation Damage on Fission Product Transport in the SiC Layer of TRISO Fuel Particles (HTR2018)

Abstract – Metallic fission products are found to transport through the SiC layer of the tristructural isotropic (TRISO) fuel particle and various studies has been undertaken to understand the transport behavior. It has been recently discovered that the precipitation of intragranular palladium containing fission products in SiC layer of neutron-irradiated TRISO fuel particles occurs via a novel dual-step nucleation mechanism. Direct observations of Pd silicide imprinting into morphological templates of a-SiC precipitates in neutron irradiated SiC layer of TRISO fuel will be discussed with examples from selected particles from both the Advanced Gas Reactor (AGR)-1 (fabricated laboratory-scale at Oak Ridge National Laboratory) and AGR-2 (fabricated at pilot scale by an industrial vendor) experiments. As neutron irradiation damage structures are expected to accelerate the intragranular diffusion kinetics of fission products, their size, shape, density and distribution patterns across the radial thickness of the SiC layer can be directly correlated with the nature of intragranular transport pathways of fission products. In this work, the distinction of neutron irradiation damage structures as a function of fuel type, burnup level and fabrication histories of TRISO coated particles from the AGR-1 and AGR-2 experiments has been studied. The five particles investigated, three AGR-1 and two AGR-2 particles, represent irradiation histories of four fuel types with burnup levels varying from 12.55 to 17.4 % fissions per initial metal atom.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Oxidation of SiC cladding under Loss of Coolant Accident (LOCA) conditions in LWRs

An experimental assessment of Silicon Carbide (SiC) cladding oxidation rate in steam under conditions representative of Loss of Coolant Accidents (LOCA) in light water reactors (LWRs) was conducted. SiC oxidation tests were performed with monolithic alpha phase tubular samples in a vertical quartz tube at a steam temperature of 1140 deg. C and steam velocity range of 1 to 10 m/sec, at atmospheric pressure. Linear weight loss of SiC samples due to boundary layer controlled reaction of silica scale (SiO{sub 2} volatilization) was experimentally observed. The weight loss rate increased with increasing steam flow rate. Over the range of test conditions, SiC oxidation rates were shown to be about 3 orders of magnitude lower than the oxidation rates of zircaloy 4. A SiC volatilization correlation for developing laminar flow in a vertical channel is formulated. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Development of joining technology using local heating for SiC fuel cladding

Silicon carbide (SiC) is an attractive material for an accident-tolerant fuel in light water reactors because of its lower hydrogen-generation rate and lower heat of reaction than conventional Zircaloy. On the other hand, practical application of SiC fuel cladding faces a lot of critical issues, one of which is end-plug joining. The objective of this study is to clarify the feasibility of end-plug joining by silicon brazing using local heating by evaluating the shear strength of joint specimens and producing a circumferential joint experimentally. Silicon is thought to be a compatible joining material with SiC because as well as being a constituent of SiC, its thermal-expansion coefficient is close to that of SiC. Local heating using processes such as laser irradiation and a resistance-heating element needs to be applied for end-plug joining. Brazing is expected to seal a cladding with an end plug by using brief heating without a strong compression force. Shear strength was evaluated using specimens with silicon-brazing joints processed using laser irradiation. The joint sections without defects showed shear strengths higher than or equal to 59 MPa at temperatures from normal room temperature to 1473 K. The average shear strength of the joint (99 MPa) is comparable to that of a diffusion-bonding joint using titanium or molybdenum foil. A tube and a plug were circumferentially joined with silicon brazing using laser irradiation or a graphite heating element. A defocused laser beam was effective for joining without cracking during laser irradiation. Although local heating using a resistance-heating element can more easily control the temperature of the joint, it took longer processing time than that using laser irradiation due to limited temperature-increase rate in order to avoid thermal shock damage. (authors)

36 MATERIALS SCIENCE↗

Chromium-Based Mitigation Coatings on SiC Materials for Fuel Cladding

SiC composites are undergoing assessment under the Advanced Fuels Campaign for Light Water Reactors (LWR) as an Accident Tolerant Fuel (ATF) cladding. As noted, the main concern has been the hydrothermal corrosion of SiC under all LWR chemistries, resulting in cladding oxidation and recession unacceptable for the duration of burn-up. Improvements in future fuel burn-up further increase recession mitigation requirements. Hermeticity of ceramic cladding may also be a concern in terms of quality control. Coatings are being investigated as a practical solution to address concerns regarding SiC cladding for both accident conditions and normal operations. SiC materials were coated by various technologies to produce Cr-based mitigation coatings as a corrosion barrier in LWR water chemistry. In all cases, deposition of Cr compounds requires that SiC behave as a cathode during processing, which requires surface electrical conductivity. Morphology and phase analysis of the coatings are still undergoing investigation, mainly for predicting differential swelling, thermal expansion and microcracking. Autoclave corrosion and in-pile irradiation in a PWR water loop will follow in mid-2016. (authors)

36 MATERIALS SCIENCE↗

Corrosion test of HTGR graphite with SIC coating - 18671

The application of SiC composite as a corrosion-resistive coating of graphite remains an important task for HTGR. Different methods and technologies have been developed for SiC-coatings of fuel and graphite frames to reduce their chemical corrosion/spraying and sorption capacity with respect to hydrogen. The use of such a coating would lead to some stabilization of the structure of carbon formations and their properties, which are changing in almost all HTGR operational regimes. This paper presents a study of the chemical interaction of the SiC gradient coating of the high-density IG-110 graphite with H{sub 2}O, O{sub 2}, CH{sub 4}, H{sub 2}, at pressures 1 and 100 Pa in a temperature range up to 1400 deg. C. The experiments at 100 Pa were conducted using mass spectrometry registration of time dependencies of partial pressure changes of the gas mixture, keeping the sample at a constant temperature (integral mode). Similar registrations at 1 Pa of moisture were made in differential mode (under continuous pump out) with 10 deg. C/min heating/cooling rate. The experimental results and microstructural study made it possible to get the parameters and peculiarities of the passive and the active corrosions of SiC and draw some conclusions about the level of the reduction of gas interaction with the bulk graphite due to SiC coating (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Post Irradiation Examination of SiC Tube Subjected to Simultaneous Irradiation and Radial High Heat Flux

Silicon carbide (SiC) based composite is considered among leading candidate materials for accident tolerant fuel (ATF) cladding in light water reactors (LWRs) because of its outstanding irradiation and oxidation resistance, as well as low neutron absorption. Under normal operation conditions, the synergism between neutron irradiation and a high radial heat flux though the cladding thickness is expected to produce significant stress. This stress is attributed to a significant through-thickness temperature gradient and the resulting differential swelling strain due the highly temperature-dependent point-defect swelling of SiC. Although modeling of the in-pile stress state of SiC cladding has been conducted using finite element analysis, the analysis is challenging because of the complex stress state that depends upon swelling, irradiation creep, and thermal conductivity, all of which are both temperature and dose-dependent. These integral models have not yet been verified by experiments. In order to experimentally validate the multi-physics thermo-mechanical models of ATF SiC cladding during operation, SiC tube specimens have been irradiated under a high radial heat flux. This paper reports preliminary results from the post-irradiation examination (PIE) in on-going project supported by the U.S. Department of Energy's Nuclear Science User Facility program. The objectives of the PIE are (1) determination of the irradiation temperature distribution within the tube specimens, and (2) evaluation of the state and magnitude of the stress within the tube specimens arising from the temperature gradient. This paper mainly presents findings for objective (1)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Engineering Epitaxial Gamma-Al-2O-3 Gate Dielectric Films on 4H-SiC

The formation of epitaxial {gamma}-Al{sub 2}O{sub 3} thin films on 4H-SiC was found to be strongly dependent on the film thickness. An abrupt interface was observed in films up to 200 {angstrom} thick with an epitaxial relationship of {gamma}-Al{sub 2}O{sub 3}(111) {parallel} 4H-SiC(0001) and {gamma}-Al{sub 2}O{sub 3}(4{bar 4}0) {parallel} 4H-SiC(11{bar 2}0). The in-plane alignment between the film and the substrate is nearly complete for {gamma}-Al{sub 2}O{sub 3} films up to 115 {angstrom} thick, but quickly diminishes in thicker films. The films are found to be slightly strained laterally in tension; the strain increases with thickness and then decreases in films thicker than 200 {angstrom}, indicating strain relaxation which is accompanied by increased misorientation. By controlling the structure of ultrathin Al{sub 2}O{sub 3} films, metal-oxide-semiconductor capacitors with Al{sub 2}O{sub 3} gate dielectrics on 4H-SiC were found to have a very low leakage current density, suggesting suitability of Al{sub 2}O{sub 3} for SiC device integration.

36 MATERIALS SCIENCE↗

Characterization of 4H-SiC Low Gain Avalanche Detectors (LGADs)

4H-SiC Low Gain Avalanche Detectors (LGADs) have been fabricated and characterized. The devices employ a circular mesa design with low-resistivity contacts and an SiO 2 passivation layer. The I–V and C–V characteristics of the 4H-SiC LGADs are compared with complementary 4H-SiC PiN diodes to confirm a high breakdown voltage and low leakage current. Both LGADs and PiN diodes were irradiated with alpha particles from a $^{210}_{84}$Po source. The charge collected by each device was compared, and it was observed that low-gain charge carrier multiplication is achieved in the 4H-SiC LGAD.

43 PARTICLE ACCELERATORS↗

Synthesis of One-Dimensional SiC Nanostructures from a Glassy Buckypaper

A simple and scalable synthetic strategy was developed for the fabrication of one-dimensional SiC nanostructures - nanorods and nanowires. Thin sheets of single-walled carbon nanotubes (SWNTs) were prepared by vacuum filtration and were washed repeatedly with sodium silicate (Na₂SiO₃) solution. The resulting “glassy buckypaper” was heated at 1300 - 1500 °C under Ar/H₂ to allow a solid state reaction between C and Si precursors to form a variety of SiC nanostructures. The morphology and crystal structures of SiC nanorods and nanowires were characterized using scanning electron microscopy (SEM), high-resolution transmission electron microscopy (HR-TEM), energy dispersive xray spectroscopy (EDX), electron diffraction (ED) and x-ray diffraction (XRD) techniques. Furthermore, electrical conductance measurements were performed on SiC nanorods, demonstrating their potential applications in high-temperature sensors and control systems.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

High temperature oxidation behaviors of bulk SiC with low partial pressures of air and water vapor in argon

Oxidation behaviors of bulk SiC at 1000–1400 °C in Ar-20 vol% H 2 O-10 vol% air were investigated. The thickness of the passivation oxide layer showed a parabolic increase with time. Dense and uniform layers formed below 1200 °C, whereas pores and cracks were observed at higher temperatures. An analytical model was proposed to estimate the oxide layer growth and SiC mass loss rate. The SiC layer should be effective in retaining the fission products after oxidation by excessive water and air. This work is the first detailed study of SiC layer oxidation during loss of coolant accidents (LOCA) for HTGRs.

36 MATERIALS SCIENCE↗

Compatibility of SiC with ODS FeCrAl in flowing Pb-Li at 600° - 700°C

To establish the maximum operating temperature for the dual coolant lead lithium (DCLL) blanket concept, thermal convection loop (TCL) experiments were conducted for 1000 h with a peak temperature of 700 °C to determine compatibility with commercial eutectic Pb~17at.%Li. Two TCLs were fabricated from alloy APMT (FeCrAlMo) and the baseline TCL experiment contained only APMT specimens. The second TCL experiment exposed more fusion relevant CVD SiC and ODS Fe-10Cr-6Al specimens in the hot and cold legs. In the second experiment, the mass losses were much larger for the ODS FeCrAl specimens and most of the CVD SiC specimens experienced a mass gain as SiC reacted to form an Fe- and Cr-rich carbide reaction product. Dissolved Fe and Cr reacted with the SiC and removing Fe and Cr from the liquid appeared to increase ODS FeCrAl dissolution. Such a dissimilar material interaction appears consistent with thermodynamic calculations. Significant attack at the top of the hot leg in both experiments suggests that the Pb-Li compatibility of FeCrAl alloys is inadequate at 700 °C in a flowing environment and the maximum PbLi temperature is < 675 °C.

36 MATERIALS SCIENCE↗