Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Thermal Stability and Lattice Strain Evolution of High-Nb-Containing TiAl Alloy under Low-Cycle-Fatigue Loading

The micromechanical behavior and the effect of temperature on the micromechanical mechanism of high-Nb-containing TiAl alloy during low-cycle fatigue still remain uncertain. Herein, in situ and ex situ synchrotron-based high-energy X-ray (HEXRD) experiment results reveal that the gamma and omega(o) phases suffer compressive lattice strains but the lattice strain in the alpha(2) phase evolves from tensile to compressive during low-cycle fatigue at 900 degrees C. In addition, the three phases suffer compressive lattice strains during cooling to room temperature, which could result in larger compressive lattice strains in gamma and omega(o) phases and the change of the lattice strain state in the alpha(2) phase. The peak-broadening results show gamma recrystallization is dominant in the interrupted low-cycle-fatigue samples, whereas inhomogeneous deformation occurs in the failed low-cycle-fatigue samples. The performed synchrotron diffraction experiments offer a deeper insight into the phase transformations and micromechanism of TiAl alloy during low-cycle fatigue.

cyclic stress-strain behavior↗

Comparison of the Thermal Stability in Equal‐Channel‐Angular‐Pressed and High‐Pressure‐Torsion‐Processed Fe–21Cr–5Al Alloy

Nanostructured steels are expected to have enhanced irradiation tolerance and improved strength. However, they suffer from poor microstructural stability at elevated temperatures. In this study, Fe–21Cr–5Al–0.026C (wt%) Kanthal D (KD) alloy belonging to a class of (FeCrAl) alloys considered for accident‐tolerant fuel cladding in light‐water reactors is nanostructured using two severe plastic deformation techniques of equal‐channel angular pressing (ECAP) and high‐pressure torsion (HPT), and their thermal stability between 500–700 °C is studied and compared. ECAP KD is found to be thermally stable up to 500 °C, whereas HPT KD is unstable at 500 °C. Microstructural characterization reveals that ECAP KD undergoes recovery at 550 °C and recrystallization above 600 °C, while HPT KD shows continuous grain growth after annealing above 500 °C. Enhanced thermal stability of ECAP KD is from significant fraction (>50%) of low‐angle grain boundaries (GBs) (misorientation angle 2–15°) stabilizing the microstructure due to their low mobility. Small grain sizes, a high fraction (>80%) of high‐angle GBs (misorientation angle >15°) and accordingly a large amount of stored GB energy, serve as the driving force for HPT KD to undergo grain growth instead of recrystallization driven by excess stored strain energy.

Arivu, Maalavan↗

Water-Mediated Surface Diffusion Mechanism Enables the Cold Sintering Process: A Combined Computational and Experimental Study

The cold sintering process (CSP) densifies ceramics at much lower temperatures than conventional sintering processes. Several ceramics and composite systems have been successfully densified under cold sintering. For the grain growth kinetics of zinc oxide, reduced activation energies are shown, and yet the mechanism behind this growth is unknown. In this work, we investigate these mechanisms in more detail with experiments and ReaxFF molecular dynamics simulations. We investigated the recrystallization of zinc cations under various acidic conditions and found that their adsorption to the surface can be a rate-limiting factor for cold sintering. In conclusion, our studies show that surface hydroxylation in CSP does not inhibit crystallization; in contrast, by creating a surface complex, it creates an orders of magnitude acceleration in surface diffusion, and in turn, accelerates recrystallization.

36 MATERIALS SCIENCE↗

The melt memory effects in polymer crystallization

This paper presents a systematic review of the literature on the melt memory effects observed in polymers, an area that has engendered considerable debate for over 50 years. Recent advances in experimental techniques have provided fresh insights into how a polymer's thermal history influences its recrystallization behavior. It has been observed that given other conditions unchanged, the crystallization temperature during recrystallization decreases with an increase in the melt temperature T s above the melting point T m until a critical melt temperature is attained. This phenomenon also extends to the half-time of crystallization and the secondary structures, such as lamellar thickness, of semi-crystalline polymers. Despite these findings, a comprehensive constitutive model that encapsulates polymer melt memory effects remains elusive. Cutting-edge instrumentation, including in situ small and wide-angle X-ray scattering, temperature-controlled Fourier transform infrared spectroscopy, and flash differential scanning calorimetry, have posed significant challenges to the traditional nucleation and growth models established in the 1970s. These models are foundational to our understanding of polymer crystallization, which is an integral part of polymer processing and production. In this review, the historical contours of this discourse are traced, with an examination of both the recent experimental breakthroughs and theoretical advancements pertinent to polymer melt memory effects. In conclusion, this paper delves into the prevailing theories of polymer nucleation and crystallization and engages with theoretical discussions and numerical simulations that attempt to elucidate and rationalize these melt memory phenomena.

36 MATERIALS SCIENCE↗

The Effect of Homogenization Heat Treatment on the Texture Evolution in U-10Mo Alloy

Uranium alloyed with 10 wt% Mo (U-10Mo) undergoes discontinuous precipitation (DP) when subjected to sub-eutectoid heat-treatment. It is hypothesized that the crystallographic texture of the U-10Mo can be modified to minimize the degree of DP, however the evolution of texture throughout the manufacturing process is not well understood. Crystallographic textures of two U-10Mo samples homogenized at 900°C and 1000°C were studied after uniaxial rolling and annealing. A total of 6 samples were analyzed upon rolling using a combination of hot and cold rolling conditions to strains of 83%, 90% and 97% and subsequently annealed at 700°C for one hour. Microstructures and textures were analyzed via electron backscatter diffraction (EBSD) for each homogenization, strain and post-annealed states. Results show that the U-10Mo exhibits typical rolling textures seen in body-centered cubic materials with increasing intensities of both a- and ?-fibers with increasing strain. After recrystallization, the texture appeared to be effectively randomized in all samples. Homogenization temperature showed no effect on the rolling and recrystallization behavior. Potential factors leading to the randomization of texture are discussed along with the implications of textures on the minimization of DP.

nuclear fuel, texture, rolling↗

Microstructural Evolution of Tantalum During Deformation and Subsequent Annealing

Microstructure-aware models are necessary to predict the behavior of material based on process knowledge or to extrapolate mechanical properties of materials to environmental conditions which are not easily reproduced in the laboratory, e.g., nuclear reactor environments. Elemental Ta provides a relatively simple BCC system in which to develop a microstructural understanding of deformation processes which can then be applied to more complicated BCC alloys. In situ neutron diffraction during compressive deformation and subsequent heat treatment have been used to monitor the evolution of microstructural features in Ta throughout simulated processing steps. Crystallographic texture and dislocation density are determined as a function of first plastic strain, then temperature. Lattice strains are determined and attributed to stresses at macroscopic, grain and dislocation length scales. The increase of the dislocation density through deformation and subsequent recovery during heat treatment is monitored through the changing diffraction line profile. Also, randomization of the texture is used as a signature of recrystallization. The recovery of dislocations through annihilation is not observed to depend on the initial dislocation density in the range studied here. In contrast, recrystallization is observed to depend strongly on the initially dislocation density.

36 MATERIALS SCIENCE↗

Microstructure and Sn crystal orientation evolution in Sn-3.5Ag lead-free solders in high temperature packaging applications

Understanding the reliability of eutectic Sn-3.5Ag lead-free solders in high temperature packaging applications is of significant interest in power electronics for the next generation electric grid. Large area (2.5mm 2.5mm) Sn-3.5Ag solder joints between silicon dies and direct bonded copper substrates were thermally cycled between 5 C and 200 C. Sn crystal orientation and microstructure evolution during thermal cycling were characterized by electron backscatter diffraction (EBSD) in scanning electron microscope (SEM). Comparisons are made between observed initial texture and microstructure and its evolution during thermal cycling. Gradual lattice rotation and grain boundary misorientation evolution suggested the continuous recrystallization mechanism. Recrystallization behavior was correlated with dislocation slip activities.

high temperature packaging↗

Formation of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) Nano-composites via Mechanical Alloying and Friction Stir Processing

Combination of mechanical alloying and friction stir processing was used for the fabrication of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) nano-composites. Pre-milled hematite + Al powder mixture was introduced into the stir zone generated on 1050 aluminum alloy sheet by friction stir processing. Uniform and active milled powder mixture reacted with plasticized aluminum to produced Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles. Al{sub 13}Fe{sub 4} intermetallic showed elliptical shape with a typical size of ~ 100 nm, while nano-sized Al{sub 2}O{sub 3} exhibited irregular floc-shaped particles that formed clusters with the remnant of iron oxide particles in the fine recrystallized aluminum matrix. As the milling time (1-3 h) of the introduced powder mixture increased, the volume fraction of Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles increased in the fabricated composite. The hardness and ultimate tensile strength of the fabricated nano-composites varied from 54.5 to 75 HV and 139 to 159 MPa, respectively; these are much higher than those of the friction stir processed base alloy (33 HV and 97 UTS). The highest hardness and strength were achieved for the nano-composite fabricated using the 3-h milled powder mixture; hard nano-sized reaction products and fine recrystallized grains of Al matrix had major and minor roles on enhancing these properties, respectively.

36 MATERIALS SCIENCE↗

Microstructure and Electromagnetic Shielding Properties of Mg-Zn-Ce-Y-Zr Alloys

Microstructure and electromagnetic interference shielding properties of extruded Mg-Zn-Ce-Y-Zr alloys were systematically investigated. A bimodal grain structure of fine recrystallized grains and deformed grains was observed in the alloys. Yttrium (Y) and cerium (Ce) refined the recrystallized grains. Mg-Zn-Ce phase, Mg{sub 3}Zn{sub 3}Y{sub 2} phase and a few precipitates containing Zn and Zr were observed. Y and Ce additions changed the texture of the alloys. When the total rare earth content reached 4 wt.%, the texture was remarkably weaker than other studied alloys. The shielding capacity increased first and then decreased with Y contents. The value of shielding effectiveness for the extruded Mg-5Zn-1Ce-2Y-0.6Zr alloys reached 79-118 dB in the frequency range of 30 MHz-1.5 GHz, which was significantly higher than that of some aluminum alloys. The addition of Y and Ce is effective in improving the shielding capacity in Mg alloys. The electrical conductivity and second phases in the alloys were important in enhancing shielding effectiveness. The texture and precipitation exerted significant effect on electrical conductivity. In addition, subsequently aging treatment evidently improved shielding effectiveness.

36 MATERIALS SCIENCE↗

On the Hot Deformation Behavior of a Ni-Free Austenitic Stainless Steel Interstitially Alloyed with Low Nitrogen Content

Hot deformation behavior of a Ni-free, Fe-17Cr-12Mn-0.28N-0.06C (wt.%) austenitic stainless steel, hereinafter coded as FeCrMnN, was investigated using hot compression tests conducted under different deformation conditions comprising temperature and strain rate ranges of 800-1200 °C and 0.01-10 s{sup −1}, respectively. While the hot deformation at high strain rate and low temperatures (e.g., 10 s{sup −1} and 800 or 900 °C) showed essentially dynamic recovery, resulting in a pancake-shaped microstructure, most of the other conditions exhibited occurrence of dynamic recrystallization (DRX). Increasing deformation temperature and decreasing strain rate showed a decrease in the critical stress and strain for initiating DRX. In general, DRX resulted in extensive microstructural reconstitution and grain refinement. For instance, hot deformation at 1000 °C/0.01 s{sup −1} resulted in a fully recrystallized fine-grained microstructure with an average grain size of about 15 μm in comparison with the initial grain size of 60 µm. Increasing the temperature enhanced grain growth, but an increase in strain rate resulted in a finer grain structure. The amount of delta ferrite in the present steel varied under different conditions of deformation such that the lowest amount of delta ferrite (about 4.5%) was observed at 1000 °C. The activation energy of deformation (Q{sub def}) for the present FeCrMnN steel with the initial grain size of 60 µm was estimated to be about 502 kJ/mol, which is higher than that of the conventional austenitic stainless steels.

36 MATERIALS SCIENCE↗

EBSD Study on Processing Domain Parameters of Oxide Dispersion Strengthened 18Cr Ferritic Steel

This paper presents the results of an experimental study aimed to identify hot working domains in oxide dispersion strengthened (ODS) 18Cr ferritic steel over a wide range of temperatures (1323-1473 K) and strain rates (0.01-10 s{sup −1}). The experimental data were obtained by uniaxial compression test using the Gleeble-1500D simulator in this range of temperature and strain rate. An inverse relationship with temperature and positive strain rate sensitivity associated with dynamic recovery and recrystallization, which is influenced by temperature and strain rate, was derived from the flow stress. Based on the processing map generated at 0.5 true strain, using rate dynamic material model (DMM) approach and the calculated instability parameter (ξ(ϵ́))>0, the optimum processing domain has been determined for this steel. The most favorable processing parameters are found in the temperature ranges of 1350-1450 K with a strain rate of 0.01 s{sup −1} and 1473 K with a strain rate 0.1 s{sup −1} with peak efficiency of 30 and 35%, respectively. The material flow behavior was studied using scanning electron microscopy (SEM)-based EBSD microstructural characterization. The steel subjected to 1323 K at high strain rate 10 s{sup −1} in the low-efficiency workability region showed low aspect ratio as compared to the elongated bamboo-like initial microstructure; however, minimum strain rate (0.01 s{sup −1}) showing that localized slip/shearing is the key mechanism and fiber texture studied from the intensity distribution of inverse pole figure showed the presence of significant amount of θ-fibers. In contrast, dynamic recrystallization dominated at higher efficiency region in the safe domain of processing map and γ-fiber texture was evident in the specimen deformed at 1373 and 1473 K with strain rate of 0.01 and 0.1 s{sup −1}, respectively, which is responsible for the change in the initial 〈1 1 0〉//ED α-fiber texture.

36 MATERIALS SCIENCE↗

Effects of Solution Treatment on Microstructure Transformation, Tensile and Exfoliation Corrosion Properties of 7136 Aluminum Alloy

The effects of solution treatment on microstructure transformation and tensile properties of 7136 aluminum alloys were investigated by means of scanning electron microscopy, electron backscatter diffraction, differential scanning calorimeter, x-ray diffraction and tensile test, electrochemical evaluations, exfoliation corrosion tests, respectively. The results indicate that solution treatment had a significant effect on the microstructure transformation and tensile properties. Soluble constituents of 7136 aluminum alloys were more likely to form the η(MgZn{sub 2}) phase rather than the S(Al{sub 2}CuMg) phase. With increasing the solution temperature, the η phase was re-dissolved into the α(Al) matrix gradually. After solution treatment of 475 °C/1 h, the η phase was completely dissolved into the matrix, with insoluble Fe-rich phases remained. The dissolution of η phase would increase the strength and the corrosion resistance of the alloys. When continuing to increase the solution temperature, the recrystallized fraction increased obviously, resulting in the decrease in the strength and the corrosion resistance. Consequently, the strength and the corrosion resistance of the alloys increased firstly and then decreased with the increase in solution temperature. After solution treatment of 475 °C/1 h, the tensile strength and yield strength of the aged alloy reached their peaks, 738 and 715 MPa, respectively. The elongation of the alloy solution treated at 475 °C/1 h reached 11.2%, and its exfoliation corrosion rating got EB level. Furthermore, after the double-stage solution treatment of 450 °C/1 h + 475 °C/1 h, the recrystallized fraction decreased, resulting in a slight increase to 12.6% of the elongation, a slight increase in the corrosion resistance and a slight decrease in the strength.

36 MATERIALS SCIENCE↗

A Comparative Study of Constitutive Characteristics and Microstructure Evolution between Uniaxial and Plane Strain Compression of an AA6061 Alloy

The hot deformation behavior of an AA6061 alloy was comparatively studied by uniaxial compression (UC) and plane strain compression (PSC) in the temperature range of 300-450 °C and strain rate range of 0.01-5 s{sup −1}. The processing maps were constructed based on a dynamic materials model, and the associated microstructures were observed. Under the same deformation conditions, the flow stress of the AA6061 alloy during PSC is higher than that during UC, which can be characterized by the Zener–Hollomon (Z) parameter in a hyperbolic sine-type equation with an activation energy Q of 175.2 kJ mol{sup −1} and 201.9 kJ mol{sup −1}, respectively. In addition, the instability domain is narrower under PSC compared to that under UC. The observed microstructures also indicate that as the Z value decreases, the tendency of dynamic recrystallization increases during PSC. The softening mechanisms in the AA6061 alloy after PSC and UC mainly consist of the dynamic recovery that is accompanied by a slight dynamic recrystallization. The optimum parameters are in the temperature range of 360-450 °C and strain rate range of 0.03-0.3 s{sup −1} for UC, and for PSC, the optimum parameters are in the temperature range of 320-400 °C and strain rate range of 0.01-0.05 s{sup −1}.

36 MATERIALS SCIENCE↗

Origin of the {111}〈112〉 Cold Rolling Texture Development in a Soft Magnetic Fe-27%Co Alloy

Plastic deformation of Fe-27%Co alloy at room temperature was investigated. The present alloy, usually delivered with a low-texture component for the magnetic core in rotating machines, develops a rather high intensity of Goss texture after recrystallization, when a suitable manufacturing process is applied. Thanks to this texture and its magnetic properties, this material can replace the grain-oriented Fe-3%Si alloy in electric transformer application. The intensity of the recrystallization Goss component depends directly on the sharpness of the {111}〈112〉 orientation developed during cold rolling. Thus, the origin of this {111}〈112〉 deformation texture has been studied using visco-plastic self-consistent (VPSC) simulations. This model showed that only the {110}〈111〉 slip systems allow developing the {111}〈112〉 texture. The predominance of this slip system has been effectively identified from slip markings on the deformed sample by EBSD. More, this simulation has shown that a Goss texture at the hot-rolled state favors the {111}〈112〉 development during cold rolling, as observed experimentally.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure Evolution and Mechanical Properties of Selective Laser Melted Inconel 718 Alloy

The microstructure characteristics of the selective laser melted Inconel 718 alloy under as-deposited, homogenization + solution + aging (HSA) and solution + aging (SA) conditions were studied. The anisotropy and heterogeneity of mechanical properties under different conditions were also investigated. Under the as-deposited condition, the morphology and size of the grains are heterogeneous. The dendrite structures which grow nearly perpendicular to the molten pool traces, accompanying interdendritic Laves phase, can be observed within the grains. The dendrite structure completely disappeared, and the Laves phases embedded in the interdendritic regions also dissolved into the matrix to precipitate γ′ and γ″ phases after heat treatments. Fully recrystallized grains were obtained under the HSA condition, while only incomplete recrystallized grains were obtained under the SA condition. However, the characteristics of γ′ and γ″ phases are very similar under the HSA and SA conditions. Significant improvement in strength after heat treatments was due to the dissolution of undesirable Laves phase and the precipitation of γ′ and γ″ phases. For all the three conditions, different tensile properties were observed depending on the orientation of the specimens. The scatter of mechanical properties is notable, and heat treatments increased the scatter of mechanical properties.

36 MATERIALS SCIENCE↗

Thermomechanical Behavior of Biocompatible Austenitic Stainless Steels during Simulated Torsion Tests

The thermomechanical behavior and the microstructural evolution during the hot deformation are important aspects of metal alloys during hot forging and rolling processes. Here, the correlation between dynamically recrystallized grain size (d{sub DRX}), steady-state stress (σ{sub ss}) and Zener–Hollomon (Z) parameter is investigated according to the Universal Derby–Ashby relationship. Specimens of a UNS S 31673 and a UNS S 31675 steels, used in the manufacture of orthopedic implants, were subjected to continuous isothermal torsion tests. A strain of 3.0 and strain rates of 0.01, 0.1, 1.0 and 10 s{sup −1} at temperatures of 1000, 1100 and 1200 °C, were employed. The results showed that the competition between the hardening and dynamic softening (i.e., recovery and recrystallization) mechanisms, as depicted by the flow curves, agreed with the Derby relation. This observation is also a consequence of the variation in the stacking fault energy (SFE) with the applied strain. Additionally, the influence of the hot deformation parameters on the shape of the curves and the grain refinement is governed by the balance between these thermally activated mechanisms.

36 MATERIALS SCIENCE↗

Cryogenic Treatment of CoCrFeMnNi(NbC) High-Entropy Alloys

The effect of cryogenic treatment on the microstructure and mechanical properties of CoCrFeMnNi and CoCrFeMnNi(NbC) high-entropy alloys was investigated during annealing. The heat-treated samples were characterized by optical microscopy, scanning electron microscopy–wavelength-dispersive x-ray spectroscopy, x-ray diffraction technique, differential scanning calorimetry, Vickers hardness testing and tensile testing. The results showed a single-phase FCC crystal structure matrix in both alloys during cryogenic treatment and annealing. Cryogenic treatment altered the recrystallization behavior of CoCrFeMnNi high-entropy alloy, while it did not influence the recrystallization of CoCrFeMnNi(NbC) high-entropy alloy. It was also found that cryogenic treatment changed the precipitation behavior of CoCrFeMnNi(NbC) high-entropy alloy during annealing. In both studied high-entropy alloys, the mechanical testing indicated that the cryogenic treatment can effectively reduce the yield strength of cold-rolled samples after annealing. This was primarily attributed to the effect of cryogenic treatment in enhancing crystalline defects annihilation. Furthermore, the cryogenic treatment increased the ultimate tensile strength of CoCrFeMnNi(NbC). A lager plastic deformation and precipitates were considered as the main reasons for the higher ultimate tensile strength.

36 MATERIALS SCIENCE↗