At least 487 records · Page 27

Epitaxial growth of nickel on Si(100) by dc magnetron sputtering

The influence of the substrate temperature on the growth of highly textured Ni(111) and epitaxial Ni(200) with the relationships Ni[100] parallel Si[110] and Ni(001) parallel Si(001) on hydrogen terminated Si(100) wafer substrates by means of direct current magnetron sputtering is reported. In order to minimize crystal defect formation and to achieve a high quality epitaxial growth of Ni on Si, a two step deposition process was developed whereby different deposition conditions were used for an initial nickel seed layer and the remaining nickel film. The in-plane and out-of-plane structural properties of the films were investigated using x-ray scattering techniques, whereas magneto-optical Kerr effect and neutron reflectometry were used to confirm the magnetic nature of the epitaxially deposited nickel films.

36 MATERIALS SCIENCE↗

Effect of Bi{sub 2}O{sub 3} seed layer on crystalline orientation and ferroelectric properties of Bi{sub 3.25}La{sub 0.75}Ti{sub 3}O{sub 12} thin films prepared by rf-magnetron sputtering method

Bi{sub 3.25}La{sub 0.75}Ti{sub 3}O{sub 12} (BLT) thin films with Bi{sub 2}O{sub 3} seed layers were prepared on Pt(111)/Ti/SiO{sub 2}/Si substrate by rf-magnetron sputtering method. The effect of annealing procedure, thickness, and position of Bi{sub 2}O{sub 3} seed layer on the structural and electrical properties of BLT thin film was investigated. When using a two-step annealing procedure, the x-ray diffraction pattern indicated that BLT thin film with a Bi{sub 2}O{sub 3} seed layer showed c-axis preference orientation. Compared with Pt/BLT/Bi{sub 2}O{sub 3}/Pt structure film, the Pt/Bi{sub 2}O{sub 3}/BLT/Bi{sub 2}O{sub 3}/Pt structure film showed higher oriented to c direction. The ferroelectric property of BLT thin film improved remarkably with the incorporation of Bi{sub 2}O{sub 3} seed layer. Under the applied voltage of 14 V, the remnant polarization and coercive voltage of the Bi{sub 2}O{sub 3}/BLT/Bi{sub 2}O{sub 3} capacitor with 18-nm-thick Bi{sub 2}O{sub 3} seed layer were 45.2 {mu}C/cm{sup 2} and 9.2 V, respectively. Moreover, the Pt/Bi{sub 2}O{sub 3}/BLT/Bi{sub 2}O{sub 3}/Pt film with 18-nm-thick Bi{sub 2}O{sub 3} seed layers exhibited good fatigue endurance even after 6x10{sup 9} switching cycles, which was attributed to the double-sided Bi{sub 2}O{sub 3} layer. They decreased the grain boundary density by enhancing the grain size of BLT film and enhanced the c-axis preferential orientation. Compared with BLT film deposited directly on Pt, double-sided Bi{sub 2}O{sub 3} layer would greatly enhance the leakage current resistance of the BLT film.

36 MATERIALS SCIENCE↗

Achieving high free electron mobility in ZnO:Al thin films grown by reactive pulsed magnetron sputtering

The study is focused on the improvement of the free electron mobility in Al-doped ZnO films grown by reactive pulsed magnetron sputtering. At optimum growth conditions low-absorbing films are obtained with a Hall mobility of 46 cm{sup 2} V{sup -1} s{sup -1}, a free electron density of 6.0x10{sup 20} cm{sup -3}, and an electrical resistivity of 2.26x10{sup -4} {omega} cm. The relation between the mobility and free electron density for different growth conditions is discussed in terms of ionized impurity scattering, impurity clustering, and grain boundary limited transport.

36 MATERIALS SCIENCE↗

Highly phosphorus-doped crystalline Si layers grown by pulse-magnetron sputter deposition

The electrical properties of highly phosphorus-doped crystalline silicon films deposited by pulse-magnetron sputtering were studied. The films were grown, 450 nm thick, on Si(100) and Si(111) wafers at low substrate temperatures T{sub s} of 450-550 deg. C and post-treated by rapid thermal annealing (RTA) and plasma hydrogenation (PH). In the case of films grown on Si(100), at all values of T{sub s} postgrowth treatment by RTA resulted in an increase in the dopant activation up to 100% and of the Hall mobility to about bulklike values of 50 cm{sup 2} V{sup -1} s{sup -1}. This result suggests high structural quality of the films on Si(100). The Si(111) films, which are typically more defective, exhibit a completely different behavior with a strong dependence of the electrical dopant activation and the Hall mobility on T{sub s}. By post-treatment a maximum P donor activation level of 22% could be obtained. The variation in the post-treatment procedure (RTA+PH and PH+RTA) for the films deposited at high T{sub s} showed that PH results only in minor changes in the film properties. The different influence of RTA and PH is discussed in terms of the different defect structure of the films. These investigations reveal that high T{sub s} and after-treatment by RTA are the main preconditions for optimal electrical film properties.

36 MATERIALS SCIENCE↗

High Temperature Thermal Stability and Oxidation Resistance of Magnetron-sputtered Homogeneous CrAlON Coatings on 430 Steel

The requirements of low cost and high-temperature corrosion resistance for bipolar interconnect plates in solid oxide fuel cell stacks has directed attention to the use of metal plates with oxidation resistant coatings. We have investigated the performance of steel plates with homogenous coatings of CrAlON (oxynitrides). The coatings were deposited using RF magnetron sputtering, with Ar as a sputtering gas. Oxygen in these coatings was not intentionally added. Oxygen might have come through contaminated nitrogen gas bottle, leak in the chamber or from the partial pressure of water vapors. Nitrogen was added during the growth process to get oxynitride coating. The Cr/Al composition ratio in the coatings was varied in a combinatorial approach. The coatings were subsequently annealed in air for up to 25 hours at 800 deg. C. The composition of the coated plates and the rate of oxidation were characterized using Rutherford backscattering (RBS) and nuclear reaction analysis (NRA). From our results, we conclude that Al rich coatings are more susceptible to oxidation than Cr rich coatings.

36 MATERIALS SCIENCE↗

Evolution of the plasma composition of a high power impulse magnetron sputtering system studied with a time-of-flight spectrometer

The plasma of a high power impulse magnetron sputtering system has been investigated using a time-of-flight spectrometer. The target materials included high sputter yield materials (Cu, Ag), transition metals (Nb, Cr, Ti), and carbon (graphite); the sputtering gases were argon, krypton, and nitrogen, and two different target thicknesses were selected to consider the role of the magnetic field strength. Measurements for selected combinations of those parameters give quantitative information on the transition from gas-dominated to metal-dominated (self-sputtering) plasma, on the fractions of ion charge states, and in the case of molecular gases, on the fraction of atomic and molecular ions.

36 MATERIALS SCIENCE↗

Effect of high-energy electron beam irradiation on the properties of ZnO thin films prepared by magnetron sputtering

In this work we demonstrate that high-energy electron beam irradiation (HEEBI) performed in air at room temperature affects remarkably the electrical, optical, and structural properties of undoped ZnO films prepared on SiO{sub 2} substrates by magnetron sputtering techniques. Hall and photoluminescence measurements revealed that the p-type conductivity was realized in HEEBI treated films with low dose of 10{sup 14} electrons/cm{sup 2} and converted to n-type conductivity with further increase in the amount of dose. X-ray photoelectron spectroscopy showed that indiffusion of Si from the substrate as well as N from the ambient into the films took place as a result of HEEBI treatment at high and low doses, respectively. X-ray diffraction analysis indicated that all as-grown films were found to have compressive stress, which was relieved to some extent by HEEBI treatment with high dose of 10{sup 16} electrons/cm{sup 2}. It was also found that better crystallinity with a bigger grain size was observed in HEEBI treated ZnO films with a higher dose. Field emission scanning electron microscope showed that HEEBI treated films with low dose had surface morphologies with big rodlike shapes. The major acceptorlike defects were determined to be oxygen interstitial and zinc vacancy. A model was proposed in terms of O, Zn, N, and Si diffusion to explain the observed results.

36 MATERIALS SCIENCE↗

Effects of low-temperature-buffer, rf-power, and annealing on structural and optical properties of ZnO/Al{sub 2}O{sub 3}(0001) thin films grown by rf-magnetron sputtering

ZnO thin films were epitaxially grown on Al{sub 2}O{sub 3} (0001) substrates in a radio-frequency (rf) magnetron sputtering chamber. The surface morphology of ZnO was remarkably affected by the incorporation of a low-temperature grown ZnO buffer as well as the changes in rf-power. X-ray diffractions, combined with the surface micropits, revealed strain relaxations in the ZnO epilayers grown with higher rf-powers, which in turn caused a redshift to the intrinsic exciton absorption peak. Strain relaxations were also observed in the ZnO epilayers upon thermal annealing, which led to a redshift in the E{sub 2}{sup high} Raman mode. A factor of approx0.7 cm{sup -1} GPa{sup -1}, i.e., a biaxial stress of 1 GPa can shift the E{sub 2}{sup high} mode by 0.7 cm{sup -1}, was obtained. The point defects related absorptions and the exciton localizations were suppressed by annealing, which, in conjunction with the strain-relaxation induced redshift in the intrinsic-exciton absorptions, steepened the absorption edge and increased the optical bandgap energy of the ZnO epilayer.

36 MATERIALS SCIENCE↗

Properties of silicon homojunctions with pulse-magnetron sputtered crystalline n{sup +}-emitter layers

Highly phosphorus doped crystalline silicon films were grown by pulse-magnetron sputter deposition on (100) and (111) oriented silicon wafer substrates at low temperatures of 450-550 deg. C. Rapid thermal annealing (RTA) and plasma hydrogenation (PH) were applied as postgrowth treatments. To explore the nature of the junction transport processes the I-V characteristics were studied in different device geometries as a function of temperature. The analysis suggests that depending on the substrate orientation (hkl) both postgrowth treatments influence the bulk-related current component J{sub 0b}{sup (hkl)} of the saturation current density in different manners and introduce additional conduction paths at the perimeter of the measured diode structures. For diodes grown on Si(100) postgrowth treatment by RTA results in a decrease in J{sub 0b}{sup (100)} to respectable 4x10{sup -11} A cm{sup -2}, whereas no major influence of RTA for the Si(111) based junctions could be obtained. They prove to be sensitive to PH post-treatment, which resulted in a reduction in J{sub 0b}{sup (111)} to 8x10{sup -11} A cm{sup -2}. The perimeter induced excess current is most strongly pronounced for the hydrogenated diodes on Si(111) and much less relevant for the RTA treated Si(100) structures.

36 MATERIALS SCIENCE↗

Arsenic doped p-type zinc oxide films grown by radio frequency magnetron sputtering

As-doped ZnO films were grown by the radio frequency magnetron sputtering method. As the substrate temperature during growth was raised above approx400 deg. C, the films changed from n type to p type. Hole concentration and mobility of approx6x10{sup 17} cm{sup -3} and approx6 cm{sup 2} V{sup -1} s{sup -1} were achieved. The ZnO films were studied by secondary ion mass spectroscopy, x-ray photoelectron spectroscopy (XPS), low temperature photoluminescence (PL), and positron annihilation spectroscopy (PAS). The results were consistent with the As{sub Zn}-2V{sub Zn} shallow acceptor model proposed by Limpijumnong et al. [Phys. Rev. Lett. 92, 155504 (2004)]. The results of the XPS, PL, PAS, and thermal studies lead us to suggest a comprehensive picture of the As-related shallow acceptor formation.

36 MATERIALS SCIENCE↗

Microstructure and tribological properties of Ti-contained amorphous carbon film deposited by DC magnetron sputtering

Pure amorphous carbon (a-C) film and that with a small amount of Ti were deposited on high speed steel (W18Cr4V) substrates by means of dc closed field unbalanced magnetron sputtering. The chemical composition and microstructure of the a-C films were performed using x-ray photoelectron spectroscopy, x-ray diffraction, Raman spectra, and transmission electron microscopy. The mechanical and tribological properties were evaluated using a nanoindentor, Rockwell and scratch tests, and a conventional ball-on-disk tribometer, respectively. The pure a-C film showed the high hardness (53 GPa), elastic modulus (289 GPa), but the poor adhesive strength. When adding a small amount of Ti to the a-C film, both the adhesive strength and the tribological properties were improved. The Ti contained a-C film had the low wear rate (1.9x10{sup -17} m{sup 3} N{sup -1} m{sup -1}) and friction coefficient in humid air.

36 MATERIALS SCIENCE↗

Reactive dc magnetron sputtering of (GeO{sub x}-SiO{sub 2}) superlattices for Ge nanocrystal formation

The motivation of this work is the tailored growth of Ge nanocrystals for photovoltaic applications. The use of superlattices provides a reliable method to control the Ge nanocrystal size after phase separation. In this paper, we report on the deposition of (GeO{sub x}-SiO{sub 2}) superlattices via reactive dc magnetron sputtering and the self-ordered Ge nanocrystal formation during subsequent annealing. Attention is directed mainly to define proper deposition conditions for tuning the GeO{sub x} composition between elemental Ge (x=0) and GeO{sub 2} (x=2) by the variation in the deposition temperature and the oxygen partial pressure. A convenient process window has been found which allows sequential GeO{sub x}-SiO{sub 2} deposition without changing the oxygen partial pressure during deposition. The phase separation and Ge nanocrystal formation after subsequent annealing were investigated with in situ x-ray scattering, Raman spectroscopy, and electron microscopy. By these methods the existence of 2-5 nm Ge nanocrystals at annealing temperatures of 600-750 deg. C has been confirmed which is within the superlattice stability range. The technique used allows the fabrication of superlattice stacks with very smooth interfaces (roughness<1 nm); thus the Ge nanocrystal layers could be separated by very thin SiO{sub 2} films (d<3 nm) which offers interesting possibilities for charge transport via direct tunneling.

36 MATERIALS SCIENCE↗

Fabrication of size-selected Pd nanoclusters using a magnetron plasma sputtering source

We report on the fabrication of palladium (Pd) nanoclusters using a dc magnetron sputtering source. Plasma sputtering vaporizes the target's material forming nanoclusters by inert gas condensation. The sputtering source produces ionized nanoclusters that enable the study of the nanoclusters' size distribution using a quadrupole mass filter. In this work, the dependence of Pd nanoclusters' size distribution on various source parameters, such as the sputtering discharge power, inert gas flow rate, and aggregation length have been investigated. This work demonstrates the ability of tuning the palladium nanoclusters' size by proper optimization of the source operation conditions. The experimental nanocluster sizes are compared with a theoretical model that reveals the growth of large nanoclusters from 'embryos' by a two-body collision. The model is valid for a specific range of deposition parameters (low inert gas flow rates and aggregation lengths equal or below 70 mm).

77 NANOSCIENCE AND NANOTECHNOLOGY↗

High-frequency magnetic properties of Zn ferrite films deposited by magnetron sputtering

The effect of thermal annealing on structural and magnetic properties has been investigated for Zn ferrite films deposited on Si (111) substrates using radio frequency magnetron sputtering. The saturation magnetization at room temperature was enhanced upto 303 emu/cm{sup 3} by annealing at relatively low temperature of 200 deg. C and decreased at higher temperatures. The complex permeability {mu}={mu}{sup '}-i{mu}{sup ''} values of the ferrite films as-deposited and annealed at 200 and 400 deg. C were measured at frequency upto 5 GHz. These films exhibited better high-frequency properties, especially, the film annealed at 200 deg. C had a large {mu}{sup '} of 19.5 and high resonance frequency f{sub r} of 1.61 GHz. And the reason was investigated preliminarily based on the bianisotropy model.

36 MATERIALS SCIENCE↗

Structural and magnetic properties of magnetron sputtered Ni-Mn-Sn ferromagnetic shape memory alloy thin films

In the present study, structural and magnetic properties of Mn-rich, off-stoichiometric, nanocrystalline Ni-Mn-Sn ferromagnetic shape memory alloy thin films, grown on Si (100) substrates at 550 deg. C by dc magnetron sputtering have been systematically investigated. The crystallization, surface morphology, and structural features were studied using x-ray diffraction, atomic force microscopy, and field emission scanning electron microscopy. The structural transition from austenite to martensite was observed with an increase of Mn content. Austenitic phase with mixed L2{sub 1}/A2+B2 structure has been observed at room temperature in Ni{sub 52.6}Mn{sub 23.7}Sn{sub 23.6} (S{sub 1}) and Ni{sub 51.5}Mn{sub 26.1}Sn{sub 22.2} (S{sub 2}) films, while those with composition of Ni{sub 58.9}Mn{sub 28.0}Sn{sub 13.0} (S{sub 3}) and Ni{sub 58.3}Mn{sub 29.0}Sn{sub 12.6} (S{sub 4}) show martensitic phase with 14M modulated monoclinic structures. Field induced martensite-austenite transformation has been observed in magnetization studies using superconducting quantum interference device magnetometer. Temperature dependent magnetization measurements demonstrate the influence of magnetic field on the structural phase transition temperature. The investigations reveal an increase of martensitic transformation temperature (T{sub M}) with corresponding increase in substitution of Mn. The films exhibit ferromagnetic behavior at low temperatures below Curie temperature (T{sub C}). The decrease in saturation moment with increasing Mn content, indicates the existence of antiferromagnetic correlations within ferromagnetic matrix.

36 MATERIALS SCIENCE↗

Ion-enhanced oxidation of aluminum as a fundamental surface process during target poisoning in reactive magnetron sputtering

Plasma deposition of aluminum oxide by reactive magnetron sputtering (RMS) using an aluminum target and argon and oxygen as working gases is an important technological process. The undesired oxidation of the target itself, however, causes the so-called target poisoning, which leads to strong hysteresis effects during RMS operation. The oxidation occurs by chemisorption of oxygen atoms and molecules with a simultaneous ion bombardment being present. This heterogenous surface reaction is studied in a quantified particle beam experiment employing beams of oxygen molecules and argon ions impinging onto an aluminum-coated quartz microbalance. The oxidation and/or sputtering rates are measured with this microbalance and the resulting oxide layers are analyzed by x-ray photoelectron spectroscopy. The sticking coefficient of oxygen molecules is determined to 0.015 in the zero coverage limit. The sputtering yields of pure aluminum by argon ions are determined to 0.4, 0.62, and 0.8 at 200, 300, and 400 eV. The variation in the effective sticking coefficient and sputtering yield during the combined impact of argon ions and oxygen molecules is modeled with a set of rate equations. A good agreement is achieved if one postulates an ion-induced surface activation process, which facilitates oxygen chemisorption. This process may be identified with knock-on implantation of surface-bonded oxygen, with an electric-field-driven in-diffusion of oxygen or with an ion-enhanced surface activation process. Based on these fundamental processes, a robust set of balance equations is proposed to describe target poisoning effects in RMS.

36 MATERIALS SCIENCE↗

Wurtzite structure Sc{sub 1-x}Al{sub x}N solid solution films grown by reactive magnetron sputter epitaxy: Structural characterization and first-principles calculations

AlN(0001) was alloyed with ScN with molar fractions up to {approx}22%, while retaining a single-crystal wurtzite (w-) structure and with lattice parameters matching calculated values. Material synthesis was realized by magnetron sputter epitaxy of thin films starting from optimal conditions for the formation of w-AlN onto lattice-matched w-AlN seed layers on Al{sub 2}O{sub 3}(0001) and MgO(111) substrates. Films with ScN contents between 23% and {approx}50% exhibit phase separation into nanocrystalline ScN and AlN, while ScN-rich growth conditions yield a transformation to rocksalt structure Sc{sub 1-x}Al{sub x}N(111) films. The experimental results are analyzed with ion beam analysis, x-ray diffraction, and transmission electron microscopy, together with ab initio calculations of mixing enthalpies and lattice parameters of solid solutions in wurtzite, rocksalt, and layered hexagonal phases.

36 MATERIALS SCIENCE↗

Role of oxygen atoms in the growth of magnetron sputter-deposited ZnO films

The role of oxygen atoms in the growth of magnetron sputter-deposited ZnO films was studied by alternating the deposition of a several-nanometer-thick ZnO layer and the O{sub 2}/Ar mixture plasma exposure, i.e., layer-by-layer technique. The film crystallization promoted with suppressing the oxygen vacancy and interstitial defects by adjusting the exposure condition of O{sub 2}/Ar plasma. These findings suggest that the chemical potential of oxygen atom determine the film crystallization as well as the electronic state. The diffusion and effusion of oxygen atoms at the growing surface play a role of thermal annealing, promoted the film crystallization as well as the creation and the annihilation of oxygen and zinc related defects. The role of oxygen atoms reaching at the film-growing surface is discussed in term of chemical annealing. The possible oxygen diffusion mechanism is proposed.

36 MATERIALS SCIENCE↗