Simulation of the Effect of Texture on Anisotropy in SLM-Produced IN 718 Microstructures
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
This study investigates the stability of Inconel–Cu Multimetallic Layered Composites (MMLCs) in nuclear reactor applications using Molecular Dynamics simulations. The focus is on understanding the underlying mechanisms governing the properties of MMLCs for advanced nuclear reactors, specifically, the mechanochemistry of the interface between Inconel and copper alloys. The selection of Inconel–Cu MMLCs is primarily due to copper’s superior thermal conductivity, enhancing heat management within reactors by preventing hotspots and ensuring uniform temperature distribution. This research examines Incoloy 800H and two Inconel variants (718 and 625), assessing their stability at 1000 K after exposure to 10 keV collision cascades up to 0.12 dpa. Notable findings include defect clustering on the {1 2 0} family of planes of Inconel and Cu, with Stacking Faults and Lomer–Cottrell locks on the Inconel side.
The microstructure of electro-spark deposited (ESD) superalloy IN718 was studied by the use of scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM) and X-ray photoelectron spectroscopy (XPS) techniques. In converse to general assumption, the extremely high cooling rate involved in the ESD process did not produce partitionless solidification that is devoid of second phase microconstituents in the material, nano-sized Laves phase and MC carbide particles were observed within the deposited layer. Notwithstanding the several thermal cycles involved in the process, the extremely low heat input of the process produced a deposited region that is free of the main strengthening phase of the alloy, γ″ phase precipitates, which is in contrast to what have been reported on laser deposition. Nevertheless, application of the standard full heat treatment of the alloy resulted in extensive formation of the γ″ phase precipitates and δ phase precipitates, the most stable secondary phase of the alloy, with nearly, if not complete, dissolution of the Laves phase particles. Furthermore, the XPS analysis done in the study revealed the formation of nano-oxides within the deposited layer, which increased the microhardness of the superalloy in the as-deposited condition and inhibited its grain growth during post-process heat treatment. The microstructure analysis done in this work is crucial to the understanding of properties of the superalloy processed by the ESD technique. - Highlights: •Electron microscopy analyses of electro-spark deposited IN 718 superalloy were performed. •Nano-sized secondary phase particles were observed within the deposited layer. •The study shows that the ESD did not produce partitionless solidification of the alloy.
This paper investigates the residual stress distributions from shot peening of Nickel Alloy 718 fuel assembly hold down spring material of PWR. Precision X-Ray Diffraction (XRD) testing has been performed to quantify residual stress versus depth on shot peened Nickel Alloy 718 samples that have been plastically deformed to different levels of stress. The results from these XRD tests have been used to benchmark a finite element model (FEM) that includes the effects of the residual compressive stress layer from shot peening. The benchmarked method of applying shot peening residual stresses can be applied to FEMs of Nickel Alloy 718 fuel assembly hold down springs to investigate the stress distributions in the springs at different loading conditions. XRD test results with a comparison to the benchmarked FEM are presented. (authors)
Powder bed fusion Direct Metal Laser Melting (DMLM) is an evolving additive manufacturing (AM) fabrication technology that is providing high performance parts to many industries. This technology has significant promise for use in building components for nuclear power plants. Implementation of materials produced using this and similar processes offer a potential step change in efficiency for complex parts production and hence a potential for innovative design as well as cost savings for components in the future. Properties of AM Type 316L have been reported in previous work, showing properties that match wrought properties. The fine grain structure may even lead to better environmental resistance. However, there is a need to confirm the behavior of these innovative materials after exposure to radiation if this innovative technology is to be used in current and future nuclear applications. This paper discusses new efforts being explored via a joint program between GE Hitachi (GEH) and INL (Idaho National laboratory) aimed at developing corresponding un-irradiated and irradiated data for AM materials. This paper will present data for both Type 316L stainless steel, a single-phase alloy, and Ni-base Alloy 718, a precipitation hardened alloy, manufactured using AM. This paper, serving as a progress report, will present the mechanical property and microstructural data for both Type 316L and 718 AM alloys to assess their correspondence to wrought alloy data and establish a baseline for future comparison to irradiated properties. The paper will end by discussing the requirements for using these and other additively manufactured materials in future reactor component applications where irradiated data is not available.
The research objective of this study is to develop an accelerated creep testing (ACT) program for advanced creep resistant alloys for high temperature FE applications. This research produced a new ACT for metallic materials based on Time-Temperature-Stress Superposition (TTSSP). In TTSSP, there exists a fundamental relationship between creep resistance, time, temperature, and stress that can be manipulated to reduce test durations. In our study, the stepped isostress method was employed where step increases of load during creep testing accelerated the time-to-rupture. Well-posed constitutive models including sin-hyperbolic and Wilshire-Cano-Stewart where calibrated using the SSM data and employed to predict the conventional creep response of the material. In our best experiments, <100-hour tests on lnconel 718 at 750 deg C produced over a 64x acceleration of data when compared to conventional data from Japan's National Institute of Materials Science. The ACTs enable the rapid screening of candidate materials, where a small test matrix of short duration tests can be employed to determine the creep resistance (minimum-creep-strain-rate, stress-rupture, and creep deformation) of a material across decades.
Highlights: • DDRX was the primary grain refinement mechanism in friction welding of Alloy 718. • Two models were developed to explain the twin formation mechanism. • Intragranular twins were caused by grain boundary growth incidents. • Intergranular twin boundaries were ascribed to boundary growth stagnation. - Abstract: Quantitative boundary misorientation analysis verified that discontinuous dynamic recrystallization (DDRX) was the primary grain refinement mechanism in friction welding of Alloy 718. Two models were developed to explain the formation mechanism of intragranular twins and intergranular twins, respectively. Intragranular twins were caused by grain boundary growth incidents. After twin initiation, the twin boundary migrated toward the plastic-deformed grain interior to reduce the stored energy. Additionally, intergranular twin boundaries were ascribed to boundary growth stagnation. When boundary growth stagnation occurred, twin boundaries could form and altered the orientation of the boundary migration front, so that boundary migration could progress, leaving a single twin boundary behind.
Highlights: • UFG Alloy 718-5 vol.%Y{sub 2}O{sub 3} alloy is fabricated from alloy machining chips. • The kind of oxide nanoparticles is identified in Nb-rich superalloys. • High thermal stable nanoparticles and UFG microstructure is achieved. • The GB strengthening effects at 25 °C and 650 °C of UFG alloy are calculated. - Abstract: An ultrafine grained (UFG) nickel base superalloy doped with 5 vol.%Y{sub 2}O{sub 3} nanoparticles, Alloy 718-5 vol.%Y{sub 2}O{sub 3}, was fabricated by a powder metallurgy route which combines high energy mechanical milling of Alloy 718 machining chips, spark plasma sintering, hot extrusion and heat treatment, and its microstructure and mechanical properties at room temperature and 650 °C were studied. The study showed that the Y{sub 2}O{sub 3} nanoparticles reacted with Al from the base alloy and transformed to Y{sub 4}Al{sub 2}O{sub 9} nanoparticles (average diameter: 12.5 nm) which were stable during heat treatment at 970 °C (0.78T{sub m}, where T{sub m} is the solidus temperature of the alloy in K). As a result of the high thermal stability of Y{sub 4}Al{sub 2}O{sub 9} nanoparticles and their effective pinning of the grain boundaries, the UFG microstructure (average grain size: 179 nm) of the alloy was stable during heat treatment. Grain boundary and nanoparticle strengthening rendered the heat treated Alloy 718-5 vol.%Y{sub 2}O{sub 3} alloy with a notable room temperature tensile yield strength of 1870 MPa. It was demonstrated that the grain boundary strengthening effect associated with the UFG microstructure was still significant at 650 °C, but clearly decreased from its level at room temperature. The grain boundary strengthening and nanoparticle strengthening effects which are likely to be independent of test temperature sustain a reasonably high tensile yield strength of 800 MPa at 650 °C, despite the absence of γ′ and γ″ precipitates in the UFG microstructure.
Highlights: • In as-deposited condition γ′ and γ″ were found in the interdendritic regions. • JMatPro simulations confirmed accelerated precipitation in interdendritic regions. • Depletion of Niobium was still found in the dendritic core after heat treatment. • The depletion of Niobium were more noticeable when using a high heat input. • γ″ particles were less well-developed in the regions depleted of Niobium. - Abstract: A microstructural study of Laser Metal Powder Deposition (LMPD) of Alloy 718, using a low (40 J/mm) and high (100 J/mm) heat inputs (HIs) was performed. The microstructure was characterized in as-deposited condition as well as after a standard heat-treatment, using optical microscope (OM), scanning electron microscope (SEM) and Transmission Electron Microscope (TEM). Laves, MC-carbides, γ′ and γ″ are observed in the interdendritic areas of both conditions. However, the dendritic core only consists of γ-matrix. The high HI condition shows a slightly larger Primary Dendrite Arm Spacing (PDAS) as compared to the low HI condition. Additionally, the particle size of the Nb-rich constituents in the interdendritic regions (Laves-phase and Niobium carbide) is larger in the high HI sample. After heat-treatment, the Laves phase dissolves and is replaced by δ-phase in the interdendritic regions, while γ′, γ″ and MC-carbide remain in the interdendritic regions. However, the γ″ precipitates seems to be less developed in the dendritic core as compared to the interdendritic regions, especially in the high HI sample. This can be attributed to a heterogeneous distribution of Nb in the microstructure, with a lower Nb content in the dendritic core as compared to close to the interdendritic regions.
The hydrogen embrittlement susceptibility of near-peak-aged UNS N07718 (Alloy 718) was evaluated by performing slow strain rate tests at room temperature in air and substitute ocean water. Tests in substitute ocean water were accomplished in an environmental cell that enabled in situ cathodic charging under an applied potential of −1.1 V versus SCE. Some specimens were cathodically precharged for 4 or 16 weeks at the same potential in a 3.5 wt.% NaCl-distilled water solution at 50 °C. Unprecharged specimens tested in substitute ocean water exhibited only moderate embrittlement with plastic strain to failure decreasing by about 20% compared to unprecharged specimens tested in air. However, precharged specimens exhibited significant embrittlement with plastic strain to failure decreasing by about 70%. Test environment (air or substitute ocean water with in situ charging) and precharge time (4 or 16 weeks) had little effect on the results of the precharged specimens. Fracture surfaces of precharged specimens were typical of hydrogen embrittlement and consisted of an outer brittle ring related to the region in which hydrogen infused during precharging, a finely dimpled transition zone probably related to the region where hydrogen was drawn in by dislocation transport, and a central highly dimpled ductile region. Fracture surfaces of unprecharged specimens tested in substitute ocean water consisted of a finely dimpled outer ring and heavily dimpled central region typical of ductile fracture.
Mechanical testing and microstructural analysis was performed on an Alloy 718 window that was in use at the Los Alamos Neutron Science Center (LANSCE) Isotope Production Facility (IPF) for approximately 5 years. It was replaced as part of the IPF preventive maintenance program. The window was transported to the Wing 9 hot cells at the Chemical and Metallurgical Research (CMR) LANL facility, visually inspected and 3-mm diameter samples were trepanned from the window for mechanical testing and microstructural analysis. Shear punch testing and optical metallography was performed at the CMR hot cells. The 1-mm diameter shear punch disks were cut into smaller samples to further reduce radiation exposure dose rate using Focus Ion Beam (FIB) and microstructure changes were analyzed using a Transmission Electron Microscopy (TEM). Irradiation doses were determined to be ~0.2–0.7 dpa (edge) to 11.3 dpa (peak of beam intensity) using autoradiography and MCNPX calculations. The corresponding irradiation temperatures were calculated to be ~34–120 °C with short excursion to be ~47–220 °C using ANSYS. Mechanical properties and microstructure analysis results with respect to calculated dpa and temperatures show that significant work hardening occurs but useful ductility still remains. The hardening in the lowest dose region (~0.2–0.7 dpa) was the highest and attributed to the formation of γ" precipitates and irradiation defect clusters/bubbles whereas the hardening in the highest dose region (~11.3 dpa) was lower and attributed mainly to irradiation defect clusters and some thermal annealing.
The novel metallurgical joining process for bonding IN718 superalloy was investigated by hot compressive bonding (HCB) process under the deformation temperature range of 1000 °C to 1150 °C and true strains ranging from 0 to 0.5 at a strain rate of 0.001 s{sup −1}. The effect of HCB process parameters on the tensile strength was analyzed. Both the as-deformed and the interfacial microstructures were characterized using the optical microscope, electron backscattered diffraction and transmission electron microscope (TEM) analysis. The results of tensile property revealed that the degree of metallurgical bonding is promoted by increasing deformation temperature and strain. The evolution of the interfacial microstructure showed that the migration of interfacial grain boundary (IGB), which is characterized by discontinuous dynamic recrystallization, is the dominant metallurgical bonding mechanism in the early stages of bonding. TEM analysis indicated that the dislocation density is distributed heterogeneously over both sides of IGB, which is the significant reason for the migration of IGB, during the initial stage of HCB process.
First Online: 21 June 2018 The authors would like to acknowledge the financial support given by the National Key Research and Development Program (Grant Number 2016YFB0300401), National Natural Science Foundation of China (Grant Number U1508215), Key Program of the Chinese Academy of Sciences (Grant Number ZDRW-CN-2017-1), and the National Natural Science Foundation of China (Grant Number 51774265). The authors would also like to thank Bijun Xie and Yifeng Guo for their help in the experimental work.
The laser deposited IN718 alloys were fabricated with laser cladding system under different conditions to estimate the sensitivity of weld metal liquation cracking. The microstructure and the crack characterization of the laser deposited IN718 alloy were investigated, and the effect of metallurgical factors and residual stress on the crack sensitivity was analyzed. The results showed that the continuous dendritic Laves was precipitated and formed a Lave–austenite interface with ambiguous nanohardness distribution. The weld metal liquation cracking was propagated along the laser scanning direction and the buildup direction in the laser deposited IN718 alloy simultaneously, and the Nb-/Mo-riched fine granular clusters were formed in the crack surface. The precipitation amount of the coarse eutectic phases, presented as dendrite or network, was increased in the laser deposited alloy fabricated with IN718/C-Fe-Cr composite powder and slow cooling rate. The total crack length and the maximum crack length were decreased by increasing cooling rate, and the transverse residual stress was increased with increasing buildup layer number. The crack sensitivity of the laser deposited IN718 alloy was increased by the crack initiation provided by the metallurgical defects and the eutectic phases with low melting temperatures, and then, crack propagated along the continuous phase under the transverse residual stress.
In order to simulate foreign object damage (FOD) phenomenon in aircraft high-pressure compressor blades made of a nickel-based super-alloy, Johnson–Cook (J–C) plasticity model was used. For prediction of material’s plastic behavior at temperature of 400 °C (working temperature of the blades) in the range of strain rates associated with the FOD phenomenon (in order of 10{sup 6} s{sup −1}), material parameters of A, B, C, n and m for the J–C plasticity model had to be determined experimentally. Parameters of A, B and n with values of 1108, 699 MPa and 0.5189, respectively, were obtained from quasi-static tensile tests. Moreover, m was determined to be 1.2861, also through quasi-static tensile tests with a strain rate of 1 s{sup −1} at three temperatures of 475, 550 and 625 °C. However, in order to determine C, firstly a steel ball was impacted on the surface of a flat specimen made of a precipitation-hardening alloy, and then, the impact site was 3D scanned to obtain the induced crater profile. Finally, the impact test (ballistic) was simulated using Abaqus, and a C value of 0.0085 was determined by comparing the actual crater profile with the one obtained from the simulation through a trial-and-error approach.
This study presents hot corrosion behavior of the superalloy IN718 in 100 wt.% NaCl (salt S) and in salt mixtures of 60 wt.% Na{sub 2}SO{sub 4} + 40 wt.% V{sub 2}O{sub 5} (SM1) and 75 wt.% Na{sub 2}SO{sub 4} + 15 wt.% NaCl + 10 wt.% V{sub 2}O{sub 5} (SM2), deposited separately by spray gun technique, at elevated temperature of 700 °C. The weight gain per unit area at 700 °C was increased by 49% for salt S, 153% for the dual salt mixture SM1, and only 8% for the triple salt mixture SM2, in comparison with that observed earlier at 600 °C. The marked increase in the severity of corrosion at 700 °C is attributed to formation of the highly damaging compound NaVO{sub 3} that significantly enhances the oxygen activity, in the SM1 coated samples. The effect of surface roughness and dislocation density on corrosion behavior at 700 °C, however, is found to be similar to that at 600 °C. Ultrasonic shot peening, a novel technique of surface modification, is found to enhance the hot corrosion resistance in the salt mixture SM1 at 700 °C appreciably due to extensive grain refinement to nanoscale and formation of highly protective Cr{sub 2}O{sub 3} layer in the surface region.
Highlights: • A simple and efficient recycling procedure of IN718 powder has been defined for the laser cladding process. • Characterization of wasted and cleaned powder and comparison with new IN718 powder pointed out a slight diameter increase. • Microstructure characterization of clad builds showed differences between builds with new and recycled powders. • Clad microstructure and porosity increase remain constant static properties but decrease rupture strain after 3 reuses. • Without special precautions for cladding, the recycled powder can be reused twice without modifying the properties of IN718. - Abstract: The possibility to reuse the metal powder wasted in Laser Material Deposition (LMD) process has been evaluated and a simple procedure developed. LMD uses metal powder which is fed through a nozzle into the focal point of a laser, where it melts the powder and the substrate material. During the process, a high ratio of particles hits against an unmelted area and directly bounces off the deposited area. The efficiency ratio of deposition can drop to 40% depending on the configuration and spot size. This work deals with the design of a procedure to recollect and reuse the wasted powder of a nickel based superalloy IN718. After usage, powder is recollected, undesired fractions are magnetically segregated and aggregates are removed by sieving. The particles are mixed again and ready for reuse. In order to study the effectiveness of the process, no new powder has been added to the recovered fraction, and this procedure has been repeated five times. Experimental tests show that deposited material present similar properties than those obtained with new powder grains. But, after 3 reuses, the porosity content increases consequently and the rupture strain decreases strongly. The implementation of this process allows the improvement of the final efficiency, reducing costs and decreasing the hazardous powder amount.
Here we discuss a gripping capability that was designed, implemented, and tested for in situ neutron diffraction measurements during multiaxial loading and heating on the VULCAN engineering materials diffractometer at the spallation neutron source at Oak Ridge National Laboratory.