Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “HOT PRESSING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Processing and thermal properties of an Mo5Si3C SiC ceramic

Composite ceramics containing w25 vol% of the Mo Si C ternary compound and SiC (referred to as MS) were reaction hot pressed up to 96% relative density. The electrical resistivity of the composite processed at 2150 C decreased fromw4.60 U cm at room temperature to 4.15 U cm at 700 C. Thermal conductivity of the MS ceramics processed at 2150 C was above 100 W/m K at room temperature, decreasing to between 62 and 68 W/m K at 500 C. Using the Eucken model for thermal conductivity, the interconnected SiC phase in the MS materials was calculated to have a room temperature thermal conductivity between 160 and 170 W/m K. As compared to a baseline SiC composition, the continuous SiC in the MS materials had an average increase in thermal conductivity of w50% over the temperature range of room temperature to 500 C. This increase in thermal conductivity was attributed to the accommodation of impurities that would typically be present in SiC grains and grain boundaries (e.g., N and O) into the ternary phase.

Buchheit, Andrew A↗

The microstructure and mechanical properties of Al-containing 9Cr ODS ferritic alloy

In this study, a 9Cr oxide-dispersion strengthened (ODS) alloy with additional corrosion resistant element Al was fabricated by mechanical alloying (MA) and hot pressing (HP) to explore the impact of Al on the microstructure and mechanical property of a 9Cr ODS alloy. It is found that the Al completely dissolved into the FeeCr matrix after milling for 30 h. The minor phases in the Al-containing 9Cr ODS ferritic alloy were investigated by a high-energy X-ray, and were identified to be orthorhombic-YAlO3 (YAP), bcc-Y3Al5O12 (YAG), monoclinic-Al2Y4O9 (YAM), and hexagonal-YAlO3 (YAH). These phases were further confirmed by selected area diffraction pattern (SADP), energy dispersive spectroscopy (EDS), and high resolution transmission electron microscopy (HRTEM). In addition, their volume fractions were also calculated from the integrated intensities. According to the analysis of the particles and their formation sequences, the larger particles (greater than 100 nm) are identified as mainly YAG and Al2O3 particles, while the particles with small size (less than 30 nm) are likely primarily YAM, YAH, and YAP particles. The yielding strength (YS) and ultimate tensile strength (UTS) at RT are 563 MPa and 744 MPa, respectively, while the YS and UTS at 700 C are 245 MPa and 276 MPa, respectively. Although the addition Al in ODS alloys decreases the strength at RT, the values at high temperature are similar to those obtained for 9Cr ODS alloys strengthened by fine YeTieO particles.

Microstructure↗

Enhanced Thermoelectric Properties of Cu 2 ZnSnSe 4 with Ga-doping

Gallium doped Cu 2 ZnSnSe 4 quaternary chalcogenides with and without excess Cu were synthesized by elemental reaction and densified using hot pressing in order to investigate their high temperature thermoelectric properties. The resistivity, , and Seebeck coefficient, S, for these materials decrease with increased Ga-doping while both mobility and effective mass increase with Ga doping. The power factor (S 2 /ρ) therefore increases with Ga-doping. The highest thermoelectric figure of merit (ZT = 0.39 at 700 K) was obtained for the composition that had the lowest thermal conductivity. Our results suggest an approach to achieving optimized thermoelectric properties and are part of the continuing effort to explore different quaternary chalcogenide compositions and structure types, as this class of materials continues to be of interest for thermoelectrics applications.

36 MATERIALS SCIENCE↗

Fabrication, microstructure and mechanical properties of W-NiTi composites

Here, new two-phase tungsten-based composites containing 88 wt% tungsten powders and 12 wt% nearly equiatomic NiTi alloy deforming by martensite variant detwinning were fabricated by infiltration and hot pressing in this study. The change of Ti/Ni ratio in NiTi mater alloy and the effect of addition of Nb element on the microstructure, martensitic transformation and mechanical properties of W-NiTi composites were investigated by comparison of W-Ni 50 Ti 50 , W-Ni 44 Ti 56 , W-Ni 42 Ti 58 and W-Ni 42 Ti 53 Nb 5 composites. The results showed that brittle Ni 3 Ti formed in the W-Ni 50 Ti 50 and W-Ni 44 Ti 56 composites and brittle Ti 2 Ni formed in the W-Ni 42 Ti 58 composites while no brittle intermetallics formed in the W-Ni 42 Ti 53 Nb 5 composite. The W-Ni 42 Ti 53 Nb 5 composite exhibited the sharpest martensitic transformation with the largest transformation enthalpy among the four different composites. The W-Ni 42 Ti 53 Nb 5 composite exhibited a double-yielding phenomenon under compression with an ultimate compressive strength of 3820 MPa and a deformation of 50.4%. In-situ synchrotron high-energy Xray diffraction measurements revealed the first yielding was caused by the martensite reorientation of the NiTi matrix and the second was due to the commencement of massive plastic deformation of the reoriented martensite and is also attributed to the microscopic internal fracturing of the W particles.

36 MATERIALS SCIENCE↗

Characterization of fusion welded ceramics in the SiC-ZrB 2 -ZrC system

Various SiC-ZrB 2 -ZrC ceramics were joined by fusion welding to determine the maximum silicon carbide content that could be joined. Commercial powders were hot pressed, machined, and preheated to 1450 °C before joining with a tungsten inert gas welding torch at 160–200 A. Resulting welds were cross-sectioned and analyzed to determine which compositions were weldable and to characterize microstructural evolution in welded samples. As compositions approached the ternary eutectic, the welds had smaller SiC grains and exhibited better weldability. Penetration depth of welds was controlled by a combination of current input and welding speed. Here, the ternary eutectic in the system was found at 36.9 ± 1.3 vol% SiC, 42.7 ± 1.5 vol% ZrB 2 , and 20.4 ± 1.9 vol% ZrC and its melting temperature was 2330 ± 23 °C. A ternary phase diagram for the SiC-ZrB 2 -ZrC was constructed and proposed via microstructural analysis of arc melted pellets on binary joins between each binary eutectic and the ternary eutectic in the system.

36 MATERIALS SCIENCE↗

Review of additive manufacturing and densification techniques for the net- and near net-shaping of geometrically complex silicon nitride components

Silicon nitride (Si 3 N 4 ) is an advantageous material due its unique combination of mechanical, thermal, chemical, and electrical properties both at ambient and elevated temperatures. Because of these properties there are a wide range of applications for Si 3 N 4 components. Applications include heat exchangers, environmental barrier coatings, osteointegration scaffolds, radomes, and integrated circuitry. Furthermore, such applications often require geometric complexity for efficient and/or effective operation. However, traditional ceramics processing methods such as hot-pressing or die extrusion are typically limited to simple axis-symmetric shapes. With the advent of additive manufacturing, there has been significant advancement into the forming of geometrically complex Si 3 N 4 components. This review documents additive manufacturing advancements that have demonstrated, or are capable of, fabricating Si 3 N 4 components with complex geometry.

36 MATERIALS SCIENCE↗

Mechanical properties of fusion welded ceramics in the $\mathrm{SiC-ZrB}$ 2 and $\mathrm{SiC-ZrB}$ 2 -$\mathrm{ZrC}$ systems

Mechanical properties of welded SiC-ZrB 2 and SiC-ZrB 2 -ZrC ceramics were measured up to 1700 °C. Commercial powders were hot pressed, machined into coupons, and preheated to 1600 °C before joining the ceramics using either tungsten inert gas welding or plasma arc welding. Toughness of the parent materials was 3–4 MPa*m 1/2 which decreased after welding to 2–2.5 MPa*m 1/2 . Strength of the SiC-ZrB 2 -ZrC parent material was ~700 MPa at 25 °C, ~300 MPa at 1700 °C, and retained 40–60% of this strength once welded. Strength of the SiC-ZrB2 parent material was ~600 MPa at 25 °C and 1700 °C and retained 20–30% of this strength once welded. Griffith analysis indicated that the strength in the parent materials was controlled by the size of SiC clusters while strength of welds was controlled by the size of pores in fusion zones. Therefore, removal of pores in produced fusion zones should be investigated to improve strength of future ceramic welds.

36 MATERIALS SCIENCE↗

Fusion welding of refractory metals and ZrB 2 -SiC-ZrC ceramics

Molybdenum and a molybdenum alloy were fusion welded to ZrB2-based ceramics to determine if the electrical and thermal properties of the metals and ceramics affected their weldability. Commercial ceramic powders were hot pressed, machined into coupons, and preheated to 1600 °C before joining the ceramics to commercial metals using plasma arc welding. Weldability varied as indicated by the range of porosity observed within the fusion zones. Measured thermal and electrical properties appeared to have little to no effect on the weldability of metal-ceramic welds despite the large range of values measured across each property. Differences in melting temperatures between metal and ceramic coupons did affect weldability by changing the weld penetration depth into ceramic coupons. Finally, future studies on metal-ceramic welds are suggested to investigate the effect that work function, melt viscosity, wetting, or other properties have on weldability.

36 MATERIALS SCIENCE↗

Magnetic property and microstructure of single crystalline Nd2Fe14B ultrafine particles ball milled from HDDR powders

In this work we report the microstructure and magnetic property of single crystalline Nd2Fe14B ultrafine particles ball milled from HDDR Nd-Fe-B alloys. The average size of the particles is 283 nm, and TEM observation reveals that these particles are single crystalline. The coercivity of these particles is 6.0 kOe, which is much higher than that of the particles ball milled from sintered and hot pressed Nd-Fe-B magnets. Micromagnetic analysis shows that the coercivity degradation is caused by surface damage during ball milling. (C) 2013 Elsevier B.V. All rights reserved.

Li, WF↗

Ion irradiation study of lithium silicates for fusion blanket applications

Here, this study reports on the microstructural and compositional evolutions, deuterium release and lithium loss behavior in lithium silicates. Pellets of biphasic Li 4 SiO 4 and Li 2 SiO 3 were fabricated using hot pressing of powders. Sequential irradiation with Si + , He + and D + ions was performed up to 773 K to emulate one-year 6 Li burnup in 6 Li 4 SiO 4 inside the SlimCS DEMO. Crystalline Li 4 SiO 4 phase was not observed in the irradiated depth region of all the samples in this study. In spite of full amorphization in the near-surface region, Li 2 SiO 3 irradiated to a high dose at 773 K remained crystalline in the damage peak region, suggesting that Li 2 SiO 3 is more irradiation resistant to amorphization than Li 4 SiO 4 . Radiolysis may be primarily responsible for silicate decomposition and amorphization. Data from this study also show that D release from the pellet is very efficient during ion irradiation at 773 K, which is accompanied with a significant Li loss. Thermal annealing for 10 min at 773 K for the room-temperature irradiated pellet leads to a nearly complete D release without an observable Li loss. A concept of Ni coating on tritium breeder materials is discussed with supporting data to minimize Li loss without a significant impact on tritium diffusion and release.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Characterizing the Li–Li 7 La 3 Zr 2 O 12 interface stability and kinetics as a function of temperature and current density

The stability and kinetics of the Li–Li 7 La 3 Zr 2 O 12 (LLZO) interface were characterized as a function of temperature and current density. Polycrystalline LLZO was densified using a rapid hot-pressing technique achieving 97 ± 1% relative density, and <10% grain boundary resistance; effectively consisting of an ensemble of single LLZO crystals. It was determined that by heating to 175 °C, the room temperature Li-LLZO interface resistance decreases dramatically from 5822 (as-assembled) to 514 Ω cm 2 ; a > 10-fold decrease. In characterizing the maximum sustainable current density (or critical current density – CCD) of the Li-LLZO interface, several signs of degradation were observed. In DC cycling tests, significant deviation from Ohmic behavior was observed. In post-cycling tests, regions of metallic Li were observed; propagating parallel to the ionic current. For the cells cycled at 30, 70, 100, 130 and 160 °C, the CCD was determined to be 50, 200, 800, 3500, and 20000 μA cm –2 , respectively. As a result, the relationships and phenomena observed in this work can be used to better understand the Li-LLZO interface stability, enabling the use of batteries employing Li metal anodes.

36 MATERIALS SCIENCE↗

Facile and scalable fabrication of polymer-ceramic composite electrolyte with high ceramic loadings

Solid state electrolytes are a promising alternative to flammable liquid electrolytes for high-energy lithium battery applications. In this work polymer-ceramic composite electrolyte membrane with high ceramic loading (greater than 60 vol%) is fabricated using a model polymer electrolyte poly(ethylene oxide) + lithium trifluoromethane sulfonate and a lithium-conducting ceramic powder. The effects of processing methods, choice of plasticizer and varying composition on ionic conductivity of the composite electrolyte are thoroughly investigated. The physical, structural and thermal properties of the composites are exhaustively characterized. We demonstrate that aqueous spray coating followed by hot pressing is a scalable and inexpensive technique to obtain composite membranes that are amazingly dense and uniform. The ionic conductivity of composites fabricated using this protocol is at least one order of magnitude higher than those made by dry milling and solution casting. The introduction of tetraethylene glycol dimethyl ether further increases the ionic conductivity. The composite electrolyte's interfacial compatibility with metallic lithium and good cyclability is verified by constructing lithium symmetrical cells. As a result, a remarkable Li + transference number of 0.79 is discovered for the composite electrolyte.

36 MATERIALS SCIENCE↗

Determination of Ce 3+ , Co 2+ , Mn 2+ and Fe 2+ diffusion coefficients in Nafion® membrane

Concentration gradient diffusion coefficients for Ce 3+ , Co 2+ , Mn 2+ and Fe 2+ cations are determined in Nafion®211 membranes over a wide range of environmental conditions. Measurements are made using finite-width cation-rich bands introduced to NR211 via a hot-pressing procedure. A robust method of accurate diffusion coefficient determination of the finite-width deposits is developed using a Fick's second law of diffusion solution for one-dimensional systems. The transition metal dications are found to have nearly identical NR211 diffusion coefficients under water saturated conditions over the 22–80 °C range. The powerful chemical mitigant, Ce 3+ , is about one-half as diffusive as the dications under identical conditions. Derived diffusion coefficients for Ce 3+ and Co 2+ are found to be independent of initial cation concentration over the range of 12.5–70 mol% exchange level. The diffusion behavior of Ce 3+ in 80 °C liquid water and saturated water vapor is identical. The diffusion coefficients of Ce 3+ are shown to have a strong dependence on membrane hydration level varying by a factor of more than 30 over the range of 95 to 40% RH. Finally, the implications of these new diffusion findings are applied to a discussion of potential guidelines for the development of highly durable fuel cell systems, which employ mobile metal cations as lifetime-extending redox stabilizers.

08 HYDROGEN↗

Structure and high-temperature thermoelectric properties of SrAl{sub 2}Si{sub 2}

Single crystals of SrAl{sub 2}Si{sub 2} were synthesized by reaction of the elements in an aluminum flux at 1000 deg. C. SrAl{sub 2}Si{sub 2} is isostructural to CaAl{sub 2}Si{sub 2} and crystallizes in the hexagonal space group P-3m1 (90 K, a=4.1834 (2), c=7.4104 (2) A, Z=1, R1=0.0156, wR2=0.0308). Thermal analysis shows that the compound melts at {approx}1020 deg. C. Low-temperature resistivity on single crystals along the c-axis shows metallic behavior with room temperature resistivity value of {approx}7.5 m{omega} cm. High-temperature Seebeck, resistivity, and thermal conductivity measurements were made on hot-pressed pellets. The Seebeck coefficient shows negative values in entire temperature range decreasing from {approx}-78 {mu}V K{sup -1} at room temperature to -34 {mu}V K{sup -1} at 1173 K. Seebeck coefficients are negative indicating n-type behavior; however, the temperature dependence is consistent with contribution from minority p-type carriers as well. The lattice contribution to the thermal conductivity is higher than for clathrate structures containing Al and Si, approximately 50 mW cm{sup -1} K, and contributes to the overall low zT for this compound. - Abstract: Single crystals of SrAl{sub 2}Si{sub 2} have been prepared via an Al flux reaction and are of the CaAl{sub 2}Si{sub 2} structure type. The melting point is approximately 1020deg. C. Low temperature resistivity curve is similar to that observed for single crystals of CaAl{sub 2}Si{sub 2} High temperature Seebeck coefficient is negative, indicating n-type carriers. Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of Rh on the thermoelectric performance of the p-type Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} half-Heusler alloys

We show that Rh substitution at the Co site in Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} (0<=x<=1) half-Heusler alloys strongly reduces the thermal conductivity with a simultaneous, significant improvement of the power factor of the materials. Thermoelectric properties of hot-pressed pellets of several compositions with various Rh concentrations were investigated in the temperature range from 300 to 775 K. The Rh 'free' composition shows n-type conduction, while Rh substitution at the Co site drives the system to p-type semiconducting behavior. The lattice thermal conductivity of Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} alloys rapidly decreased with increasing Rh concentration and lattice thermal conductivity as low as 3.7 W/m*K was obtained at 300 K for Zr{sub 0.5}Hf{sub 0.5}RhSb{sub 0.99}Sn{sub 0.01}. The drastic reduction of the lattice thermal conductivity is attributed to mass fluctuation induced by the Rh substitution at the Co site, as well as enhanced phonon scattering at grain boundaries due to the small grain size of the synthesized materials. - Graphical abstract: Significant reduction of the lattice thermal conductivity with increasing Rh concentration in the p-type Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} half-Heusler materials prepared by solid state reaction at 1173 K.

36 MATERIALS SCIENCE↗

Crystal structure, characterization and thermoelectric properties of the type-I clathrate Ba{sub 8-y}Sr{sub y}Al{sub 14}Si{sub 32} (0.6{<=}y{<=}1.3) prepared by aluminum flux

The title compound was prepared as single crystals using an aluminum flux technique. Single crystal and powder X-ray diffraction indicate that this composition crystallizes in the clathrate type-I structure, space group Pm3-bar n. Electron microprobe characterization indicates the composition to be Ba{sub 8-y}Sr{sub y}Al{sub 14.2(2)}Si{sub 31.8(2)} (0.77<y<1.3). Single-crystal X-ray diffraction data (90 and 12 K) were refined with the Al content fixed at the microprobe value (12 K data: R{sub 1}=0.0233, wR{sub 2}=0.0441) on a crystal of compositions Ba. The Sr atom preferentially occupies the 2a position; mixed Al/Si occupancy was found on all framework sites. These refinements are consistent with a fully occupied framework and nearly fully occupied cation guest sites as found by microprobe analysis. Temperature dependent electrical resistivity and thermal conductivity have been measured from room temperature to 1200 K on a hot-pressed pellet. Electrical resistivity reveals metallic behavior. The negative Seebeck coefficient indicates transport processes dominated by electrons as carriers. Thermal conductivity is between 22 and 25 mW/cm K. The sample shows n-type conductivity with a maximum figure of merit, zT of 0.3 at 1200 K. A single parabolic band model predicts a five-fold increase in zT at 800 K if carrier concentration is lowered. -- Graphical abstract: The inorganic type-I clathrate phase with nominal composition Ba{sub 7}Sr{sub 1}Al{sub 14}Si{sub 32} has been prepared by Al flux. Single crystal diffraction at 90 and 12 K reveal that the framework is fully occupied with the cation sites nearly fully occupied. The lattice thermal conductivity is low thereby suggesting further optimization of the carrier concentration will lead to a high zT. Display Omitted Highlights: {yields} Ba{sub 7}Sr{sub 1}Al{sub 14}Si{sub 32} is a light element phase ideal for thermoelectric power generation. {yields} Ba{sub 7}Sr{sub 1}Al{sub 14}Si{sub 32} is a high melting point cubic structure ideal for efficient power generation. {yields} The framework is fully occupied with the cation sites nearly fully occupied. {yields} Further optimization of the carrier concentration is expected to lead to a high zT.

36 MATERIALS SCIENCE↗

Thermoelectric and microstructural properties of Pb{sub 0.9-x}Sn{sub 0.1}Ge{sub x}Te compounds prepared by spinodal decomposition

Three samples of Pb{sub 0.9-x}Sn{sub 0.1}Ge{sub x}Te with x=0.25, 0.35, 0.6 were prepared by heating the mixtures above the melting point of the constituent elements followed by quenching in water. The x=0.6 sample is close to the center of the immiscibility region, while the x=0.25 and 0.35 samples are in the Pb rich region inside the spinodal miscibility gap. Microstructural investigations using Powder X-ray Diffraction, Scanning Electron Microscopy and Energy Dispersive X-ray Spectroscopy revealed both GeTe-rich and PbTe-rich phases. The samples were uniaxially hot pressed and the thermoelectric properties were characterized in the temperature range 2-400 K using a commercial apparatus and from 300 to 650 K with a custom designed setup. The best sample (x=0.6) reached zT{approx}0.6 at 650 K, while the x=0.25 and 0.35 samples showed thermal instability at elevated temperatures. -- Graphical abstract: Spinodal decomposition in the GeTe-SnTe-PbTe system demonstrated by SEM and EXS images. Display Omitted Highlights: {yields} Investigation of Pb-rich part of the spinodal miscibility gap in PbTe-SnTe-GeTe. {yields} zT=0.6 at 650 K reproduced for Pb{sub 0.3}Sn{sub 0.1}Ge{sub 0.6}Te. {yields} Pb-rich phases shown to be thermally instable. {yields} Thermoelectric property characterization at low and high temperature. {yields} Microstructural investigations using PXRD, SEM, EDX and PSM.

36 MATERIALS SCIENCE↗

Thermoelectric properties and nonstoichiometry of GaGeTe

Polycrystalline samples of composition Ga{sub 1+x}Ge{sub 1-x}Te (x=-0.03 Division-Sign 0.07) and GaGeTe{sub 1-y} (y=-0.02 Division-Sign 0.02) were synthesized from elements of 5 N purity using a solid state reaction. The products of synthesis were identified by X-ray diffraction; phase purity and microstructure were examined by EDX/SEM. Samples for measurement of transport properties were prepared using hot-pressing. They were characterized by measurement of electrical conductivity, the Hall coefficient, and the Seebeck coefficient over a temperature range 80-480 K and of thermal conductivity over a temperature range 300-580 K. All samples show p-type conductivity. We discuss the influence of stoichiometry on the phase purity of the samples and on free carrier concentration. The investigation of thermoelectric properties shows that the power factor of these samples is low compared to state-of-the-art materials at room temperature but increases distinctly with temperature. - Graphical abstract: Structure and preparation of GaGeTe. Electrical conductivity {sigma}, the Hall coefficient R{sub H}, the Seebeck coefficient S and thermal conductivity {kappa} as a function of temperature for the Ga{sub 1.01}Ge{sub 0.99}Te{sub 0.99} sample. Highlights: Black-Right-Pointing-Pointer We explore thermoelectric and transport properties of Ga{sub 1+x}Ge{sub 1-x}Te and GaGeTe{sub 1-y}. Black-Right-Pointing-Pointer GaGeTe is p-type degenerate semiconductor; the hole concentration increase with x and y. Black-Right-Pointing-Pointer Maximum power factor {sigma}S{sup 2}=3.6 Multiplication-Sign 10{sup -4} Wm{sup -1} K{sup -2} at 475 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗