Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CHROMIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Evaluation of post-weld heat treatments applied to FeCrAl alloy weldments

The nuclear incident at the Fukushima Daiichi nuclear power plant has created a strong push for accident-tolerant fuel cladding to replace current zirconium-based cladding. A current near-term focus on iron-chromium-aluminum (FeCrAl) alloys. Laser-welded FeCrAl samples (C35MN, C37M, and C35M10 TC) were subjected to three different post-weld heat treatment regimes: 650 °C for 5 h, 850 °C for 1 h, and 850 °C for 5 h. Here, the samples were then analyzed using optical light microscopy, micro-hardness indentation, and scanning electron microscopy coupled with energy-dispersive spectroscopy and electron backscatter diffraction. The base microstructure of C37M and C35M10 TC experienced significant grain coarsening outside the fusion zone due to the applied post-weld heat treatments, whereas Nb-rich precipitation in C35MN limited grain growth compared with the other alloys studied.

36 MATERIALS SCIENCE↗

Process for the Production of Star Tracklng [Tracking] Reticles

A method for the production of reticles, particularly those for use in outer space, wherein the product is a quartz base coated with highly adherent layers of chromium, chromium-silver, and silver vacuum deposited through a mask, and then coated with an electrodeposit of copper from a copper sulfate solution followed by an electrodeposit of black chromium. The masks are produced by coating a beryllium-copper alloy substrate with a positive working photoresist, developing the photoresist according to a pattern to leave a positive mask, plating uncoated areas with gold, removing the photoresist, coating the substrate with a negative working photoresist, developing the negative working photoresist to expose the base metal of the pattern, and chemically etching the unplated side of the pattern to produce the mask. The mask produced is then used in the vacuum deposition of: (1) chromium metal on the surface of a quartz base to obtain a highly adherent quartz-chromium interface; (2) silver on the chromium deposit, during the final stage of chromium deposit, to produce a silver chromium alloy layer; and (3) silver onto the surface of the alloy layer. The coated quartz base is then coated by electroplating utilizing an acid copper deposit followed by a black chromium electrodeposit to produce the product of the present invention.

Smith, Wade O.↗

Ion irradiation effects on Cr-coated zircaloy-4 surface wettability and pool boiling critical heat flux.

The concept of coating the currently used nuclear fuel cladding (zirconium-based alloy, typically Zircaloy-4 or Zirc-4) with an oxidation preventive layer is a progressing Accident tolerant Fuel (ATF) candidate alloys. The coated Zirc-4-based alloys could be a solution to suppress undesirable fast reaction kinetics with high-temperature steam. Zirc-4 has been the most preferred cladding material in pressurized water reactors (PWRs). Chromium (Cr) based alloys as a coating material provides excellent corrosion protection and good strength and wear resistance. In this paper, we present the surface wettability measurements and pool boiling Critical Heat Flux (CHF) for Cr-coated Zirc-4 claddings pre- and post-exposure to an ion irradiation environment. The wettability measurements, including static contact angle (contact angle, θ) and average surface roughness (surface roughness, Ra), are introduced for samples of different coating thicknesses (5–30 μm thick). The coatings fabricated by the cold spray of Cr-Al particles to 10 mm × 10 mm × 1.95 mm Zirc-4 substrates. Post fabrication, a Pilgering (cold rolling) process, was applied to finalize the coating thickness and resulted in a significant reduction in surface roughness of initially fabricated rough surfaces. The process produced three distinguished samples 5-μm unpolished (as machined), 5-μm, and 30-μm polished (cold rolled). The measurements are presented for the three surfaces and bare Zirc-4 as a baseline surface. The contact angle analyses were implemented in theoretical models from the literature to predict pool boiling CHF. Pool boiling experiments were conducted to measure the pool boiling CHF values and compare them to the predicted values. Scanning Electron Microscope (SEM) images and Energy Dispersive X-ray Spectroscopy (EDS) analysis was performed to characterize the surfaces for better understanding and interpreting the results. The SEM images showed localized surface damage due to ion irradiation. No recognized change in the measured surface roughness due to ion irradiation. The contact angles of irradiated Cr-coated surfaces are consistently higher (10°) than pre-irradiated surfaces. Decreasing the Cr-coating layer thickness resulted in lower contact angle pre- and post- ion irradiation. The predicted pool boiling CHF using the Kandlikar model is in good agreement with the experimentally measured CHF values within ±12% for all samples.

36 MATERIALS SCIENCE↗

Study of the effects of gaseous environmental on the hot corrosion of superalloy materials

Studies have been conducted to examine the effect of low concentrations of NaCl(g) on the high temperature oxidation behavior of complex superalloys and potential coating formulations modified by silicon and reactive element (i.e., yttrium and hafnium) additions. Depending on alloy composition, a variety of effects were thermogravimetrically produced. Aluminum free alloys such as MAR-M509 and Hastelloy X with molybdenum and tungsten in solid solution showed accelerated (or breakaway) kinetics similar to that observed for Ni-Cr alloys. For IN-792, an alloy high in chromium and low in aluminum, molybdenum and tungsten present in solid solution does not adversely affect oxidation kinetics in the presence of NaCl(g). On the other hand, nickel-base alloys high in aluminum and molybdenum are catastrophically attacked by NaCl-bearing atmospheres. Silicon additions were, in general, observed to slightly improve the oxidation resistance of Ni, Ni-40Cr and CoCrAlY compositions in NaCl(g)-bearing atmospheres. To the degree that processes responsible for Al2O3 whisker formation deleteriously affect protective scale adherence, the addition of yttrium or hafnium can inhibit such whisker growth.

Smeggil, J. G.↗

Degradation and Failure Phenomena of Accident Tolerant Fuel Concepts: FeCrAl Alloy Cladding

The U.S. Nuclear Regulatory Commission (NRC) is anticipating licensing applications and commercial use of accident tolerant fuel (ATF) in United States commercial nuclear power reactors. Pacific Northwest National Laboratory is providing technical assistance to the NRC related to the newly proposed nuclear fuel and cladding designs. This report focuses specifically on the iron-chromium-aluminum (FeCrAl) alloys being investigated to replace zirconium-based alloys for fuel cladding and provides current state-of-the-industry information on material properties and fuel performance considerations under reactor operating conditions and design basis accident conditions. Currently, Global Nuclear Fuels (GNF) is the only U.S.-based fuel vendor considering FeCrAl cladding as a near-term ATF design. GNF has tested several different FeCrAl alloys including Kanthal APMT, C26M, and MA956; fueled C26M rods and unfueled Kanthal APMT, C26M, and MA956 rods have been inserted in lead test assemblies at Plants Hatch and Clinton. This report will focus on those three alloys specifically, with broader information given regarding in-reactor and ex-reactor testing of FeCrAl alloys. To support the NRC’s readiness efforts, this report will identify and discuss degradation and failure modes of FeCrAl cladding concepts, including fuel performance characteristics that may not be addressed within existing regulatory documents.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Versatile Oxide Films Protect FeCrAl Alloys Under Normal Operation and Accident Conditions in Light Water Power Reactors

The US has currently a fleet of 99 nuclear power light water reactors which generate approximately 20% of the electricity consumed in the country. Near 90% of the reactors are at least 30 years old. There are incentives to make the existing reactors safer by using accident tolerant fuels (ATF). Compared to the standard UO2–zirconium-based system, ATF need to tolerate loss of active cooling in the core for a considerably longer time while maintaining or improving the fuel performance during normal operation conditions. Ferritic iron-chromium-aluminum (FeCrAl) alloys have been identified as an alter-native to replace current zirconium alloys. They contain Fe (base) + 10–22 Cr + 4–6 Al and may contain smaller amounts of other elements such as molybdenum and traces of others. FeCrAl alloys offer outstanding resistance to attack by superheated steam by developing an alumina oxide on the surface in case of a loss of coolant accident like at Fukushima. FeCrAl alloys also perform well under normal operation conditions both in boiling water reactors and pressurized water reactors because they are protected by a thin oxide rich in chromium. Under normal operation condition, the key element is Cr and under accident conditions it is Al.

36 MATERIALS SCIENCE↗

Designing Nuclear Fuels with a Multi-Principal Element Alloying Approach

Previous research has shown that multi-principal element alloys (MPEAs) using chromium, molybdenum, niobium, tantalum, titanium, vanadium, and zirconium can form stable body-centered-cubic (BCC) structures across a large temperature region (25°C to 1000°C). This is the same crystal structure as γ-uranium (U), which has shown desirable thermal and irradiation behavior in previous alloy fuel research. It is hypothesized then that the MPEA alloying approach can be used to produce a stable BCC uranium-bearing alloy and to retain its stability throughout anticipated operating regimes of power-producing reactors. Candidate elements were assessed using Monte Carlo N-Particle (MCNP) analysis to determine uranium densities necessary to make the alloy an economically viable fuel compared to conventional fuel forms. Following neutronic considerations, materials property databases and empirical predictors were used to determine the compositions with a high potential to form a BCC solid solution alloy. The final four alloys were MoNbTaU 2 , MoNbTiU 2 , NbTaTiU 2 , and NbTaVU 2 , which were cast using arc melting of raw elemental foils and chunks. Characterization of the fabricated alloys included scanning electron microscopy, X-ray diffraction, energy dispersive X-ray spectroscopy, and transmission electron microscopy. The results showed a two-phase system with a U-rich matrix phase surrounding the refractory precipitates. The U phase was found to contain varying concentrations of the alloying elements and was a BCC γ-U phase. These results warrant further research to identify ideal compositions for use as an advanced alloy fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhanced Mechanical Properties and Wear Resistance of FeCrAl Alloys at ~ 300°C and Higher Temperatures

Abstract Worldwide, light water reactors (LWRs) have been using zirconium (Zr)-based alloys for the cladding of the uranium dioxide fuel for more than 6 decades. Zr alloys oxidize rapidly in the presence of water and steam at temperatures > 450°C; therefore, they do not respond well to scenarios of loss of coolant accidents. There is a global effort by nuclear materials technologists to find more robust or stronger cladding materials for LWRs. One option is to use an iron-chromium-aluminum (FeCrAl) alloy since they have excellent resistance to high temperature oxidation and superior mechanical properties at LWR operation temperatures. Results show that (1) FeCrAl alloys have better mechanical properties than Zr alloy and are orders of magnitude more resistant to creep at temperatures higher than LWR normal operation conditions. (2) FeCrAl alloys have better resistance to fretting wear than Zr alloys at the normal operation conditions of LWRs.

Materials Science↗

Simple concentration-dependent pair interaction model for large-scale simulations of Fe-Cr alloys

This work is motivated by the need for large-scale simulations to extract physical information on the iron-chromium system that is a binary model alloy for ferritic steels used or proposed in many nuclear applications. From first-principles calculations and the experimental critical temperature we build a new energetic rigid lattice model based on pair interactions with concentration and temperature dependence. Density functional theory calculations in both norm-conserving and projector augmented-wave approaches have been performed. A thorough comparison of these two different ab initio techniques leads to a robust parametrization of the Fe-Cr Hamiltonian. Mean-field approximations and Monte Carlo calculations are then used to account for temperature effects. The predictions of the model are in agreement with the most recent phase diagram at all temperatures and compositions. The solubility of Cr in Fe below 700 K remains in the range of about 6 to 12%. It reproduces the transition between the ordering and demixing tendency and the spinodal decomposition limits are also in agreement with the values given in the literature.

36 MATERIALS SCIENCE↗

Scale formation mechanisms of martensitic steels in high CO{sub 2}/H{sub 2}O-containing gases simulating oxyfuel environments

In oxyfuel power plants, metallic components will be exposed to service environments containing high amounts of CO{sub 2} and water vapour. Therefore, the oxidation behaviour of a number of martensitic 9-12%Cr steels in a model gas mixture containing 70% CO{sub 2}-30% H{sub 2}O was studied in the temperature range 550-700{sup o}C. The results were compared with the behaviour in air, Ar-CO{sub 2} and Ar-H{sub 2}O. It was found that in the CO{sub 2}- and/or H{sub 2}O-rich gases, the mentioned steels tended to form iron-rich oxide scales with significantly higher growth rates than the Cr-rich surface scales formed during air exposure. The iron-rich scales were formed as a result of a decreased flux of chromium in the bulk alloy toward the surface because of enhanced internal oxidation of chromium in the H{sub 2}O-containing gases and carbide formation in the CO{sub 2}-rich gases. Additionally, the presence of water vapour in the exposure atmosphere led to buckling of the outer haematite layer, apparently as a result of compressive oxide growth stresses. The Fe-base oxide scales formed in CO{sub 2}(-H{sub 2}O)-rich gases appeared to be permeable to CO{sub 2} molecules resulting in substantial carburization of the steel.

20 FOSSIL-FUELED POWER PLANTS↗

Development of Computational Capabilities to Predict the Corrosion Wastage of Boiler Tubes in Advanced Combustion Systems

A comprehensive corrosion research project consisting of pilot-scale combustion testing and long-term laboratory corrosion study has been successfully performed. A pilot-scale combustion facility available at Brigham Young University was selected and modified to enable burning of pulverized coals under the operating conditions typical for advanced coal-fired utility boilers. Eight United States (U.S.) coals were selected for this investigation, with the test conditions for all coals set to have the same heat input to the combustor. In addition, the air/fuel stoichiometric ratio was controlled so that staged combustion was established, with the stoichiometric ratio maintained at 0.85 in the burner zone and 1.15 in the burnout zone. The burner zone represented the lower furnace of utility boilers, while the burnout zone mimicked the upper furnace areas adjacent to the superheaters and reheaters. From this staged combustion, approximately 3% excess oxygen was attained in the combustion gas at the furnace outlet. During each of the pilot-scale combustion tests, extensive online measurements of the flue gas compositions were performed. In addition, deposit samples were collected at the same location for chemical analyses. Such extensive gas and deposit analyses enabled detailed characterization of the actual combustion environments existing at the lower furnace walls under reducing conditions and those adjacent to the superheaters and reheaters under oxidizing conditions in advanced U.S. coal-fired utility boilers. The gas and deposit compositions were then carefully simulated in a series of 1000-hour laboratory corrosion tests, in which the corrosion performances of different commercial candidate alloys and weld overlays were evaluated at various temperatures for advanced boiler systems. Results of this laboratory study led to significant improvement in understanding of the corrosion mechanisms operating on the furnace walls as well as superheaters and reheaters in coal-fired boilers resulting from the coexistence of sulfur and chlorine in the fuel. A new corrosion mechanism, i.e., “Active Sulfidation Corrosion Mechanism,” has been proposed to account for the accelerated corrosion wastage observed on the furnace walls of utility boilers burning coals containing sulfur and chlorine. In addition, a second corrosion mechanism, i.e., “Active Sulfide-to-Oxide Corrosion Mechanism,” has been identified to account for the rapid corrosion attack on superheaters and reheaters. Both of the newly discovered corrosion mechanisms involve the formation of iron chloride (FeCl2) vapor from iron sulfide (FeS) and HCl, followed by the decomposition of FeCl2 via self-sustaining cycling reactions. For higher alloys containing sufficient chromium, the attack on superheaters and reheaters is dominated by Hot Corrosion in the presence of a fused salt. Furthermore, two stages of the hot corrosion mechanism have been identified and characterized in detail. The initiation of hot corrosion attack induced by molten sulfate leads to Stage 1 “acidic” fluxing and re-precipitation of the protective scale formed initially on the deposit-covered alloy surfaces. Once the protective scale is penetrated, Stage 2 Hot Corrosion is initiated, which is dominated by “basic” fluxing and re-precipitation of the scale in the fused salt. Based on the extensive corrosion information generated from this project, corrosion modeling was performed using non-linear regression analysis. As a result of the modeling efforts, two predictive equations have been formulated, one for furnace walls and the other for superheaters and reheaters. These first-of-the-kind equations can be used to estimate the corrosion rates of boiler tubes based on coal chemistry, alloy compositions, and boiler operating conditions for advanced boiler systems.

Coal-Environmental Processes↗

A Comparison of Solidification Structures and Submicroscale Cellular Segregation in Rapidly Solidified Stainless Steels Produced via Two-Piston Splat Quenching and Laser Powder Bed Fusion

Fusion-based additive manufacturing techniques leverage rapid solidification (RS) conditions to create parts with complex geometries, unique microscale/nanoscale morphological features, and elemental segregation. Three custom composition stainless steel alloys with varying chromium equivalence to nickel equivalence ratio (Cr eq /Ni eq ) between 1.53 and 1.95 were processed using laser powder bed fusion (LPBF) and/or two-piston splat quenching (SQ) to produce solidification rates estimated between 0.4 and 0.8 m/s. Both scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to collect high-resolution images, electron backscatter diffraction (EBSD) phase identification, and measure cellular segregation. Similar features were observed in both LPBF and SQ samples including phase and microstructure, nanoscale oxide particles, cell size, and segregation behavior. However, dislocation pileup was observed along the cell boundaries only in the LPBF austenite solidified microstructure. Targeted adjustment of the SQ feedstock Cr and Ni concentrations, within the ASTM A240 specification for 316L resulted in no observable impact on the cell size, oxide particle size, or magnitude of segregation. Also, the amount of Ni segregation in the ferrite solidified microstructures did not significantly differ, regardless of Cr/Ni eq or processing technique. Here, SQ is demonstrated as capable of simulating RS rates and microstructures similar to LPBF for use as an alternative screening tool for new RS alloy compositions.

42 ENGINEERING↗

Potential Impact of Cladding Wettability on LWR Transient Progression

The US Department of Energy Office of Nuclear Energy (DOE-NE) Advanced Fuels Campaign (AFC) is working closely with the nuclear industry to develop fuel and cladding candidates with potentially enhanced accident tolerance. This type of fuel is also known as accident tolerant fuel (ATF). Two promising cladding material candidates with potentially enhanced accident tolerance are silicon carbide (SiC) and an iron-chromium-aluminum (FeCrAl) alloy. The FeCrAl alloy features significantly enhanced oxidation resistance versus the Zr-based alloys currently used in state-of-the-art light water reactors (LWRs). Thermal-fluid characteristics are a vital element of a holistic engineering evaluation of ATF concepts. One characteristic related to boiling heat transfer is the critical heat flux (CHF). At CHF, the efficacy of heat transfer rapidly degrades and components can heat up rapidly. CHF is the heat flux at which the departure from nucleate boiling (DNB) occurs in PWRs. DNB is directly relevant to the departure from nuclear boiling ratio (DNBR), which is the ratio between the critical heat flux and the actual heat flux. Surface wettability is an important factor that influences CHF. CHF plays a significant role in determining safety margins during normal operation and also in the progression of potential transient or accident scenarios. Significant changes in CHF properties and boiling heat transfer characteristics will impact the progression of transient and accident events and reactor safety characteristics. Additionally, the behavior of the candidate cladding materials post-CHF impacts reactor safety. A brief description of the relationship between cladding material properties and CHF is provided, followed by an analysis of two hypothetical transient scenarios: a super-prompt reactivity-initiated accident (RIA) and an anticipated transient without scram with instability (ATWS-I). The analysis illustrates the potential impact of cladding material properties on safety margins via direct alteration of calculated CHF values. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗