Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 469 records · Page 26

Alternative PWHT to Improve High-Temperature Mechanical Properties of Advanced 9Cr Steel Welds

Creep-resistant 9Cr steels are extremely important in thermal power generation industry due to their marked resistance to creep and corrosion. The weldability of these alloys is critical since they are used in welded construction equipment. The required mechanical properties are achieved after post-weld heat treatment. This study examined the effect of different post-weld heat treatments on microstructure and mechanical properties of creep strength-enhanced 9Cr steel welding deposits. It was obtained with an experimental flux-cored arc welding wire used under protective gas (Ar-20% CO{sub 2}). The heat treatments used were: (1) tempering (760 °C × 2 h), (2) solubilizing (1050 °C × 1 h) + tempering (760 °C × 2 h) and (3) solubilizing (1150 °C × 1 h) + first tempering (660 °C × 3 h) + second tempering (660 °C × 3 h). All-weld metal chemical composition was analyzed, and hot tensile tests were carried out at different temperatures. Charpy-V impact tests and Vickers microhardness measurements were also performed. Microstructures were studied using x-ray diffraction and optical and scanning electron microscopy. In all cases, a martensitic matrix with intergranular and intra-granular precipitates was detected. In the as-welded condition, δ-ferrite was also found. Microhardness dropped, and the impact energy increased with post-weld heat treatments. The highest hot tensile strength result was achieved with samples submitted to austenization at 1150 °C and double tempering at 660 °C.

36 MATERIALS SCIENCE↗

Cooling Environment Effect on the Microstructure and Mechanical Properties of Friction Stir-Welded Joints

The heat input in friction stir welding (FSW) influences the localized properties in welded joint. The external cooling during FSW reduces the localized heating and post-weld cooling time by extracting heat comparatively at a faster rate. In the present study, we have investigated the effect of different cooling environments on the performance of friction stir-welded (FSWed) AA5052 strain-hardenable aluminum alloy. Welding was performed under three different cooling environments such as natural air, water and liquid nitrogen in order to understand their effects on grain structure, metallurgical changes and mechanical properties of the joints. It has been noted that the width of weld nugget zone, thermo-mechanically affected zone and heat-affected zone has been decreased with the respective change in cooling environments. Welding speed could also influence the width of different zones in weldment alike the cooling environments. Finer grain size has been noticed with water cooling against the liquid nitrogen cooling. Comparatively, water was observed to be more favorable cooling environment against liquid nitrogen because of its better weld quality (97%) compared with base metal. The favorable mechanical properties resulting from the different weldment regions for different cooling environments have been elaborated in the present study.

36 MATERIALS SCIENCE↗

Effect of Rotational Speed on Microstructure and Mechanical Properties in Submerged Friction Stir Welding of ME20M Magnesium Alloy

Submerged friction stir welding of magnesium alloys has not been well investigated to date. ME20M is an important lightweight magnesium (Mg) alloy with enhanced yield strength and heat resistance that merits further research. In this paper, submerged friction stir welding of the ME20M Mg alloy was carried out using different parameters for the underwater cooling. Defect-free weld joints were produced, and the macrostructure, microstructure, tensile properties, and hardness were investigated. The results show that by increasing the rotational speed, the grain size of the weld nugget increased, the tensile strength of the joint decreased, and the microhardness of the different weld zones decreased. The finest obtained grain size was about 3.5 µm in the weld nugget at a rotational speed of 1100 rpm. The highest tensile strength achieved was 183.2 MPa, which was ~ 76.32% of the base metal. The highest and lowest hardness values of the weld joint were obtained at rotational speeds of 1100 and 1600 rpm, respectively, in the weld nugget and heat-affected zones.

36 MATERIALS SCIENCE↗

Hydrogen-assisted fracture resistance of pipeline welds in gaseous hydrogen

Fracture resistance of pipeline welds from a range of strength grades and welding techniques was measured in air and 21 MPa hydrogen gas, including electric resistance weld of X52, friction stir weld of X100 and gas metal arc welds (GMAW) of X52, X65 and X100. Welds exhibited a decrease in fracture resistance in hydrogen compared to complementary tests in air. A general trend was observed that fracture resistance in 21 MPa hydrogen gas decreased with increasing yield strength. To accommodate material constraints, two different fracture coupon geometries were used in this study, which were shown to yield similar fracture resistance values in air and 21 MPa hydrogen gas; values using different coupons resulted in less than 15% difference. In addition, fracture coupons were removed from controlled locations in select welds to examine the potential influence of orientation and residual stress. The two orientations examined in the X100 GMAW exhibited negligible differences in fracture resistance in air and, similarly, negligible differences in hydrogen. Residual stress exhibited a modest influence on fracture resistance; however, a consistent trend was not observed between tests in air and hydrogen, suggesting further studies are necessary to better understand the influence of residual stress. A comparison of welds and base metals tested in hydrogen gas showed similar susceptibility to hydrogen-assisted fracture. The overall dominant factor in determining the susceptibility to fracture resistance in hydrogen is the yield strength.

08 HYDROGEN↗

Force measurement-based discontinuity detection during friction stir welding

Here, the objective of this work is to develop a method for detecting the creation of discontinuities ( i.e. , voids, volume defects) during friction stir welding. Friction stir welding is inherently cost effective, however, the need for significant weld inspection can make the process cost prohibitive. A new approach to weld inspection is required in which an in situ characterization of weld quality can be obtained, reducing the need for postprocess inspection. To this end, friction stir welds with subsurface voids and without voids were created. The subsurface voids were generated by reducing the friction stir tool rotation frequency and increasing the tool traverse speed in order to create “colder” welds. Process forces were measured during welding, and the void sizes were measured postprocess by computerized tomography ( i.e. , 3D X-ray imaging). Two parameters, based on frequency domain content and time-domain average of the force signals, were found to be correlated with void size. Criteria for subsurface void detection and size prediction were developed and shown to be in good agreement with experimental observations. Furthermore, with the proper choice of data acquisition system and frequency analyzer the occurrence of subsurface voids can be detected in real time.

47 OTHER INSTRUMENTATION↗

Room temperature mechanical properties of electron beam welded zircaloy-4 sheet

Room temperature mechanical properties of electron beam welded and plain Zircaloy-4 sheet (1.6mm thick) have been measured and compared. Various welding parameters were utilized to join sheet material. Electron beam welded specimens and as-received sheet specimens show comparable mechanical properties. Zr-4 sheet displays anisotropy; tensile properties measured for transverse display higher elastic modulus, yield strength, reduction of area and slightly lower ductility than for the longitudinal (rolling direction). Higher welding power increases the alloy’s hardness, elastic modulus and yield strength, with a corresponding decrease in tensile strength and ductility. The hardness measured at weld is comparable to the parent metal hardness. Hardness at heat-affected-zone is slightly higher. Electron microscopic examination shows distinct microstructure morphology and grain size at the weld zone, HAZ and parent metal. A correlation between welding parameters, mechanical properties and microstructural features was established for electron beam welded Zircaloy-4 sheet material.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

A comparative research on bobbin tool and conventional friction stir welding of Al-Mg-Si alloy plates

Highlights: • 6061-T4 Al plates were successfully welded by both BT-FSW and C-FSW processes. • A wide welding parameter window was achieved with bobbin tool. • BT-FSW joints showed good strength similar to that of C-FSW joints. • Proving that an Isothermal Dissolution Layer Theory also apply to BT-FSW - Abstract: In our work, Al-Mg-Si (6061Al -T4) plates of 6 mm thickness were subjected to bobbin tool friction stir welding (BT-FSW) and conventional friction stir welding (C-FSW) for comparison. How the welding process affects the microstructure and mechanical properties was investigated at various rotation rates and welding speeds. The results showed that butt FSW joints with high quality could be produced at the selected parameters. The joint strength rose with enhanced welding speed and was nearly independent of the rotation rate in both the welding processes. The strength of the joints produced with BT-FSW reached the same level as that of the C-FSW. The maximum joint strength of 229 MPa was 93% of the base material (BM), which is superior to the reported results of 60–80% for the T4 condition. The fracture position of most of the joints was in the heat-affected zone (HAZ), which is the lowest hardness zone.

36 MATERIALS SCIENCE↗

Effect of niobium interlayer in dissimilar friction stir welding of aluminum to titanium

Highlights: • In the present study, FSW of Al to Ti with Nb interlayer has been characterized. • Fragmentation and distribution of Nb and Ti have been correlated with properties. • Ternary mixing and chemical reaction reduced the brittleness of the joint. • Al in the weld nugget showed a gradient in microstructural features. • The weld with Nb interlayer exhibited higher ductility. - Abstract: The most important issue associated with dissimilar welding is the formation of detrimental intermetallics and consequent reduction in mechanical properties of the weld. It was expected that addition of an interlayer would modify the pattern of the intermetallic formation. The present investigation deals with Friction Stir Welding of aluminum (Al) to titanium (Ti) in presence of niobium (Nb) interlayer. X-ray Computed Tomography results highlighted that fine particles of both Ti and Nb are homogeneously distributed. Large Ti particles are substantially fragmented whereas large Nb particles remain as flakes. Microstructural features of the nugget zone indicated a complex mixing of materials. Jointing had been perceived through elemental diffusion at the interfaces of Al/Ti and Ti/Nb. However, Nb restricted the reaction between Al and Ti, and acted as an efficient interlayer to retard the formation of brittle Al{sub 3}Ti intermetallic phase. Mechanisms of microstructural evolution in Al side of the weld have been identified as Dynamic Recovery, Dynamic Recrystallization and particle stimulated nucleation. Significant improvement in the tensile ductility had been observed due to the presence of finer particles. The presence of Nb in the weld nugget influences the microstructural evolution and tensile properties of the weld by reducing the formation of intermetallics.

36 MATERIALS SCIENCE↗

Nondestructive evaluation of resistance spot-welded Al-steel joints

With increasing demand for better fuel economy for automobiles, multimaterial solutions are increasingly being utilized in the automotive industry for reducing weight in the vehicle body structure. This poses challenges in terms of joining dissimilar metals, especially those with vastly different properties such as aluminum to steel joining. General Motors has developed a new resistance spot-welding technique for dissimilar materials using a multi-ring domed (MRD) electrode and multiple solidification weld schedules to address this challenge. Originally developed for aluminum to aluminum resistance spot welding, this technology is being enabled as the mainstream aluminum joining solution to leverage existing infrastructure and workforce competency in resistance spot welding. With the recent expansion of MRD technology to aluminum to steel resistance spot welding, there is an ever-greater need to experimentally verify the quality of each aluminum to steel resistance spot-weld application with limited time and resources. Nondestructive evaluation (NDE) would allow the transfer of resistance spot-welding technology to dissimilar aluminum to steel joints. This article describes the current state of the art of aluminum to steel resistance spot welding and the challenges in developing a robust NDE process for this technology.

36 MATERIALS SCIENCE↗

Developing a dissimilar metal foil-to-substrate resistance welding process.

Materials changes occurring upon redesign caused redevelopment of the multiple spot resistance weld procedure employed to join a 23 micrometer thick foil of 15-7PH to a thick substrate and (at a separate location) a second, smaller thermal mass substrate. Both substrates were 304L. To avoid foil wrinkling, minimal heat input was used. The foil/thick substrate weld was solid-state, though the foil/small substrate weld was not. Metallographic evidence indicated occasional separation of the solid-state weld, hence a fusion weld was desired at both locations. In the redesign, a Co-Cr-Fe-Ni alloy was substituted for the foil, and a Ni-Cr-Mo alloy was evaluated for the small substrate. Both materials are substantially more resistive than their predecessors. This study reports development of weld schedules to accommodate the changes, yet achieve the fusion weld goal. Thermal analysis was employed to understand the effects caused by the various weld schedule parameters, and guide their optimization.

36 MATERIALS SCIENCE↗

The Effect of Weld Residual Stress on Life of Used Nuclear Fuel Dry Storage Canisters

With the elimination of Yucca Mountain as the long-term storage facility for spent nuclear fuel in the United States, a number of other storage options are being explored. Currently, used fuel is stored in dry-storage cask systems constructed of steel and concrete. It is likely that used fuel will continue to be stored at existing open-air storage sites for up to 100 years. This raises the possibility that the storage casks will be exposed to a salt-containing environment for the duration of their time in interim storage. Austenitic stainless steels, which are used to construct the canisters, are susceptible to stress corrosion cracking (SCC) in chloride-containing environments if a continuous aqueous film can be maintained on the surface and the material is under stress. Because steel sensitization in the canister welds is typically avoided by avoiding post-weld heat treatments, high residual stresses are present in the welds. While the environment history will play a key role in establishing the chemical conditions for cracking, weld residual stresses will have a strong influence on both crack initiation and propagation. It is often assumed for modeling purposes that weld residual stresses are tensile, high and constant through the weld. However, due to the strong dependence of crack growth rate on stress, this assumption may be overly conservative. In particular, the residual stresses become negative (compressive) at certain points in the weld. The ultimate goal of this research project is to develop a probabilistic model with quantified uncertainties for SCC failure in the dry storage casks. In this paper, the results of a study of the residual stresses, and their postulated effects on SCC behavior, in actual canister welds are presented. Progress on the development of the model is reported.

36 MATERIALS SCIENCE↗

STRESS CORROSION CRACK GROWTH RESPONSE FOR ALLOY 152/52 DISSIMILAR METAL WELDS IN PWR PRIMARY WATER

As part of ongoing research into primary water stress corrosion cracking (PWSCC) susceptibility of alloy 690 and its welds, SCC tests have been conducted on alloy 152/52 dissimilar metal (DM) welds with cracks positioned with the goal to assess weld dilution and fusion line effects on SCC susceptibility. No increased crack growth rate was found when evaluating a 20% Cr dilution zone in alloy 152M joined to carbon steel (CS) that had not undergone a post-weld heat treatment (PWHT). However, high SCC crack growth rates were observed when the crack reached the fusion line of that material where it propagated both on the fusion line and in the heat affected zone (HAZ) of the carbon steel. Crack surface and crack profile examinations of the specimen revealed that cracking in the weld region was transgranular (TG) with weld grain boundaries not aligned with the geometric crack growth plane of the specimen. The application of a typical pressure vessel PWHT on a second set of alloy 152/52 – carbon steel DM weld specimens was found to eliminate the high SCC susceptibility in the fusion line and carbon steel HAZ regions. PWSCC tests were also performed on alloy 152-304SS DM weld specimens. Constant K crack growth rates did not exceed 5x10-9 mm/s in this material with post-test examinations revealing cracking primarily on the fusion line and slightly into the 304SS HAZ.

alloy 152↗

The Effect of Ar and N 2 Shielding Gas on Laser Weld Porosity in Steel, Stainless Steel, and Nickel

Complete, or near complete, elimination of porosity in 304L stainless steel keyhole laser welds was observed when using N2 instead of Ar shielding gas. Partial penetration autogeneous welds made at intermediate power levels of 2-4 kW using a CW fiber laser at travel speeds of 8-11 mm/s where porosity often occurs when using inert shielding gas. To investigate this effect further, laser welds were made in N 2 and Ar gas on three additional metals (A36 steel, 21-6-9 stainless steel, and pure nickel) that have varying properties and degrees of reactivity and solubilities with the shielding gasses. Optical metallography, x-ray radiography, and x-ray computed tomography were used to characterize the porosity levels in the welds. Results show that high levels of porosity occurred in nickel, regardless of shielding gas type, while low levels or no porosity was observed in 21-6-9 for either shielding gas. However, A36 and 304L exhibited porosity in all of the welds made with Ar, and very low or no porosity when made with N2. Computed tomography was used to quantify the porosity in selected welds, showing that the pore sizes are distributed in a monotonically decreasing trend that can be described by a two parameter Weibull relationship (β=0.5429, α=0.0366). Based on the results, it is believed that the reactivity of N 2 with alloying elements, and/or its solubility in the liquid weld pool, play a significant role in reducing the amount of retained porosity in unstable keyhole welds as they solidify and cool to room temperature.

Steel↗

Investigation into Interface Lifting Within FSW Lap Welds

Friction stir welding (FSW) is rapidly penetrating the welding market in many materials and applications, particularly in aluminum alloys for transportation applications. As this expansion outside the research laboratory continues, fitness for service issues will arise, and process control and NDE methods will become important determinants of continued growth. The present paper describes research into FSW weld nugget flaw detection within aluminum alloy lap welds. We present results for two types of FSW tool designs: a smooth pin tool and a threaded pin tool. We show that under certain process parameters (as monitored during welding with a rotating dynamometer that measures x, y, z, and torque forces) and tooling designs, FSW lap welds allow significant nonbonded interface lifting of the lap joint, while forming a metallurgical bond only within the pin region of the weld nugget. These lifted joints are often held very tightly together even though unbonded, and might be expected to pass cursory NDE while representing a substantial compromise in joint mechanical properties. The phenomenon is investigated here via radiographic and ultrasonic NDE techniques, with a copper foil marking insert (as described elsewhere) and by the tensile testing of joints. As one would expect, these results show that tool design and process parameters significantly affect plactic flow and this lifted interface. NDE and mechanical strength ramifications of this defect are discussed.

36 MATERIALS SCIENCE↗

Investigation of Structure and Crack Formation in Welded Joints of Single Crystal Ni-Base Alloys

Conditions of initiation of hot cracks in welding of single crystal heat-resistant alloys with a 56% content of the γ’-phase were studied. Conditions for providing a polycrystalline structure in HAZ and part of the weld metal were artificially created in one region of a welded joint with the single crystal structure. Welding of the single crystal alloy was performed by the electron beam method in vacuum. Cracks in a low-temperature ductility dip range (ductility dip cracking) were found to form in HAZ and weld of a welded joint with the polycrystalline structure. The nature of cracking of the single crystal weld is related to formation of low-melting point eutectoid interlayers, as well as to exhausting of the safety factor for ductility. In conclusion, cracks in the single crystal weld along the strain grain boundaries are formed by a similar mechanism.

36 MATERIALS SCIENCE↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Joint strength in high speed friction stir spot welded DP 980 steel

High speed friction stir spot welding was applied to 1.2 mm thick DP 980 steel sheets under different welding conditions, using PCBN tools. The range of vertical feed rates used during welding was 2.5 mm – 102 mm per minute, while the range of spindle speeds was 2500 – 6000 rpm. Extended testing was carried out for five different sets of welding conditions, until tool failure. These welding conditions resulted in vertical welding loads of 3.6 – 8.2 kN and lap shear tension failure loads of 8.9 – 11.1 kN. PCBN tools were shown, in the best case, to provide lap shear tension fracture loads at or above 9 kN for 900 spot welds, after which tool failure caused a rapid drop in joint strength. Joint strength was shown to be strongly correlated to bond area, which was measured from weld cross sections. Failure modes of the tested joints were a function of bond area and softening that occurred in the heat-affected zone.

DP980↗

Stress relaxation cracking susceptibility evaluation in 347H stainless steel welds

Abstract Stress relaxation cracking (SRC) has been reported as a dominant failure mechanism for 347H stainless steel welds at elevated service temperatures, occurring in either the heat-affected zone (HAZ) or fusion zone (FZ). In this study, SRC susceptibility of physically simulated HAZ and cross-welded E347-347H stainless steel welds was studied using a four-step accelerated SRC test with a thermomechanical physical simulator. The stress and temperature range studied represents weld-induced residual stress at 150–600 MPa and post-weld heat treatment temperatures between 800 and 1050 °C. For all temperature conditions, the cross-welded samples failed at a lower critical stress threshold than the simulated HAZ. A finite element model of a 50.8-mm-thick single-V groove weld was used to generate the residual stress maps induced by a 40-pass welding procedure, which in combination with the experimental threshold stress map predicted potential SRC failure locations. Postmortem microstructural evaluations were performed to identify contributing characteristics to SRC. It was found that HAZ samples exhibited a combination of creep void development, secondary cracks with intergranular fracture near grain boundary carbides, and eutectic phases. FZ samples showed brittle fracture with cracks propagating along straight, non-tortuous interdendritic grain boundaries.

42 ENGINEERING↗