Evading strength and ductility trade-off in an inverse nacre structured magnesium matrix nanocomposite

Mimicking nacre structure is an often-used strategy for developing materials which combine high strength and high toughness. Here, a novel strategy, named inverse nacre structure, is proposed where elongated and curled soft constituents are embedded in a matrix of hard constituent to form an ordered brick-and-mortar arrangement. This strategy is demonstrated in a particle reinforced metal matrix composite, using pure Mg as the soft phase and SiC nanoparticle reinforced Mg as the hard phase. In this work, the resulting nanocomposite yields high strength, and especially high tensile elongation which is five times that of the homogeneous counterpart. The superior comprehensive strengthening-toughening effect originates from the tailored inverse nacre structure which enables a stable microcrack-multiplication process by sufficiently promoting strain hardening so as to avoid any significant decrease in post-ultimate tensile strength. This strategy, while demonstrated here for the specific case of particle reinforced Mg, is not restricted to any particular material system but constitutes a generic pathway for the development of high-performance materials for engineering applications.

36 MATERIALS SCIENCE↗

Effect of heavy ion irradiation dose rate and temperature on α' precipitation in high purity Fe-18%Cr alloy

Cr-rich alpha prime precipitates (CrRP) induce hardening and embrittlement of FeCr alloys, but the kinetics of CrRP formation due to particle irradiation are not well understood. In this study, Fe18wt.%Cr alloy in solid solution state and pre-aged to produce relatively coarse CrRP was irradiated with 8 MeV Fe ions. The irradiation conditions involved two midrange doses of 0.37 and 3.7 displacements per atom (dpa), a wide range of dose rates (10 -5 –10 -3 dpa/s) and temperatures (300–450 °C). The distributions of CrRP after irradiation were studied with atom probe tomography (APT). The critical irradiation conditions to suppress CrRP formation were identified as 300 °C and 10-3 dpa/s; CrRP formation occurred readily at lower dose rates or higher temperatures. From 0.37 to 3.7 dpa, CrRP were observed to slightly grow at 350 °C and strongly coarsen at 450 °C. Specimens with pre-existing CrRP evolved into a similar precipitate distribution as detected after ion irradiation on solution annealed specimens at 300–350 °C to 0.37 dpa, indicating that the precipitate microstructure approaches a quasi-equilibrium for doses <1 dpa. Limited shrinking of pre-existing CrRP was observed after irradiation at 450 °C to 0.37 dpa, indicating a higher recovery rate at this temperature. Additionally, the evolution of CrRP is quantitatively explained by employing corrections to the historic Nelson-Hudson-Mazey precipitate stability model, and a radiation modified precipitation mechanism is proposed to account for the competition between radiation enhanced diffusion and ballistic dissolution which results in the modifications on both size and solute concentration of CrRP.

36 MATERIALS SCIENCE↗

High strain rate deformation of aged TRIP Ti-10V-2Fe-3Al (wt.%) examined by in-situ synchrotron X-ray diffraction

Transformation Induced Plasticity (TRIP) is a promising avenue for tailoring the work hardening response of metastable $β$ titanium (Ti) alloys. Here we show that aged TRIP Ti-10V-2Fe-3Al (wt.%) maintains higher elongations and flow stresses as strain rate increases, if phase stability and microstructural characteristics are tuned. Low temperature aging influences the matrix $β$ phase stability by $ω$ phase precipitation, which affords a promising way to impact the TRIP effect and obtain desirable mechanical properties, ranging from high damping capacity to good strength/ductility combinations. Although TRIP is active during quasi-static and dynamic testing up to 2000 s –1 , increasing aging time and/or strain rate reduces the overall propensity for the TRIP effect and extent of transformation, which occurs rapidly just at the onset of yielding. Importantly, TRIP with $ω$ phase precipitation provides interesting alloying, microstructure, and property design strategies for engineering applications like lightweight protective structures, where high strains and the need for energy absorption are encountered.

36 MATERIALS SCIENCE↗

Grain boundary softening from stress assisted helium cavity coalescence in ultrafine-grained tungsten

The formation of helium cavities in coarse-grained materials produces hardening proportional to the number density and size of the cavities and due to the interaction of dislocations with intragranular helium defects. In nanostructured metals containing a high density of interfacial sinks, preferential cavity formation in the grain boundaries instead produces softening that is often attributed to enhanced interfacial plasticity. Here, employing two grades of ultrafine-grained tungsten, we explore this effect using targeted implantation studies to map cavity evolution as a function of the irradiation conditions and quantify its impact on the mechanical response through nanoindentation. Softening is reported at implantation temperatures above the threshold for preferential grain boundary cavity formation but at a sufficiently low fluence prior to the growth of intragranular cavities. Collective changes in the mean cavity size, density, and morphology beneath a residual impression on an implanted surface indicate that cavity coalescence accompanied the reduction in hardness. Complementary atomistic simulations demonstrate that, in tungsten grain structures exhibiting softening, grain boundary bubble coalescence is driven by stress concentrations that further act to localize strain in the grain boundaries through cooperative deformation processes involving local atomic shuffling and sliding, dislocation emission, and even the nucleation of unstable twinning events.

36 MATERIALS SCIENCE↗

Characterizing the flux effect on the irradiation embrittlement of reactor pressure vessel steels using machine learning

In-service exposure to high-energy neutrons embrittles reactor pressure vessel (RPV) steels. An increase in the yield stress (Δσ y ) results in a corresponding increase in the brittle to ductile transition temperature (ΔT c ). Most existing models underpredict ΔT c at higher fluence following accelerated irradiations in test reactors. High fluence, up to 10 20 n/cm 2 in some cases, will be reached over extended RPV vessel operation of 80 years, or more, at low service flux. Embrittlement has been extensively studied in accelerated, higher flux test reaction irradiations. However, the use of test reactor data naturally raises the question of flux effects. Here, this study used a machine learning approach trained on a set of hardening data, covering a wide range of flux, fluence, and steel compositions to determine the interactive effects of both irradiation and material variables on Δσ y . The analysis included machine learning-based cross-plots of the variable dependence of Δσ y for six core steels (i.e., CM6, LC, LD, LG, LH, and LI), with controlled differences in their Cu and Ni contents. A primary objective is to evaluate an effective to actual fluence (Φt e /Φt) ratio, as a function of flux, fluence, and steel composition. This is information critical to properly use intermediate flux-high fluence data in calibrating a low flux-high fluence embrittlement model. The predicted Φt e /Φt is reasonably consistent with estimates previously derived from a physics-based solute recombination trap model.

36 MATERIALS SCIENCE↗

Deformation mechanisms in an additively manufactured dual-phase eutectic high-entropy alloy

Nanostructured metals and alloys often exhibit high strengths but at the expense of reduced ductility. Through harnessing the far-from-equilibrium processing conditions of laser powder-bed fusion (L-PBF) additive manufacturing, we develop a dual-phase nanolamellar structure comprised of FCC/L1 2 and BCC/B2 phases in a Ni 40 Co 20 Fe 10 Cr 10 Al 18 W 2 eutectic high-entropy alloy (EHEA), which exhibits a combination of ultrahigh yield strength (>1.4 GPa) and large tensile ductility (~17%). The deformation mechanisms of the additively manufactured EHEA are studied via in-situ synchrotron X-ray diffraction and high-resolution transmission electron microscopy. The high yield strength mainly results from effective blockage of dislocation motion by the high density of lamellar interfaces. The refined nanolamellar structures and low stacking fault energy (SFE) promote stacking fault (SF)-mediated deformation in FCC/L1 2 nanolamellae. The accumulation of abundant dislocations and SFs at lamellar interfaces can effectively elevate local stresses to promote dislocation multiplication and martensitic transformation in BCC/B2 nanolamellae. The cooperative deformation of the dual phases, assisted by the semi-coherent lamellar interfaces, gives rise to the large ductility of the as-printed EHEA. In addition, here we also demonstrate that post-printing heat treatment allows us to tune the non-equilibrium microstructures and deformation mechanisms. After annealing, the significantly reduced SFE and thicknesses of the FCC nanolamellae facilitate the formation of massive SFs. The dissolution of nano-precipitates in the BCC/B2 nanolamellae reduces spatial confinement and further promotes martensitic transformation to enhance work hardening. Our work provides fundamental insights into the rich variety of deformation mechanisms underlying the exceptional mechanical properties of the additively manufactured dual-phase nanolamellar EHEAs.

36 MATERIALS SCIENCE↗

Unraveling kinking: A plasticity enhancing failure mode in high strength nano metallic laminates

Kinking is an important and plasticity-enhancing deformation/failure mode in numerous mechanically anisotropic materials including high-strength nano metallic laminates (NMLs). However, our current limited understanding of the mechanics of kinking and its dependence on microstructural attributes is insufficient for thoroughly comprehending and eventually being able to control failure behaviors of materials. In this study, we investigate kinking dependencies on microstructural attributes in NMLs via in situ micropillar compression, multiscale microstructure characterization, dislocation dynamic simulations, and crystal plasticity modeling. Additionally, by examining several NML systems (Cu/Fe, Ag/Fe, Al-4Mg/Fe), we demonstrate that the development of internal stresses during loading activates local layer-parallel glide triggering kinking in NMLs. Furthermore, this work reveals the effect of key microstructural features including layer thickness, layer waviness, interface barrier strength, and work hardening capacity on kink band formation in NMLs. More broadly, our efforts represent a generically applicable approach for probing large-strain deformation behavior of complex materials via synergetic modeling and experimental efforts.

36 MATERIALS SCIENCE↗

Dislocation channel broadening–A new mechanism to improve irradiation-assisted stress corrosion cracking resistance of additively manufactured 316 L stainless steel

Additively manufactured (AM) 316 L stainless steel (SS) after hot isostatic pressing (HIP) was found to exhibit superior resistance to irradiation-assisted stress corrosion cracking (IASCC) in high-temperature water, as compared to wrought 316 L SS. The well-accepted IASCC factors of radiation-induced segregation (RIS) and radiation hardening are not accurate descriptions of IASCC susceptibility in this case. A decreased strain localization along grain boundaries, caused by dislocation channel broadening, was confirmed to suppress crack initiation. A unique distribution of irradiation-induced defects in HIP AM 316 L SS eased dislocation cross-slip compared to those in the wrought counterpart, thus increasing the channel width near the grain boundaries. Here for the first time, this study highlights the importance of dislocation channel broadening as a potential mechanism to further improve the IASCC resistance of 316 L SS and provides direct experimental evidence based on commercial-grade materials.

316L stainless steel↗

Ultimate compressive strength and severe plastic deformation of equilibrated single-crystalline copper nanoparticles

Mechanical properties and deformation mechanisms of defect-free copper nanoparticles are investigated by combining experiments with atomistic simulations. The compressive strength of the particles increases with decreasing size and tends to saturate near the theoretical strength in the small-size limit. In this limit, the intrinsic size dependence of the strength is governed by the stochastic nature of dislocation nucleation near the particle surface. The particle deformation process evolves from the initial strain softening to strain hardening as the particle accumulates residual damage. The normalized strength-size relation for Cu is compared with those for Au, Ni, and Pt. The lack of universal behavior among the four FCC metals is discussed. Heavily deformed Cu nanoparticles develop polycrystalline structures and change the lattice orientation from [111] to [110]. The experiments and simulations reveal the twinning mechanism of the lattice rotation leading to the new grain formation.

36 MATERIALS SCIENCE↗

Strong interfaces: the key to high strength in nano metallic laminates

Excellent mechanical properties of nanomaterials are usually attributed to their nanoscale feature size and high-density interfaces. This work explores the effects of intrinsic interface properties on mechanical properties of nano metallic laminates (NMLs). We show that the interface strength significantly affects the mechanical properties of NMLs. Via in situ mechanical testing and characterization, we investigate the deformation behavior and concurrent microstructure evolution in NMLs with four types of dissimilar interfaces. Our results show that the strength and deformation behaviors of NMLs are largely determined by interface strength. Strong interfaces can simultaneously increase the strength, work hardening capability, and deformability of NMLs. In conclusion, this work brings new insight into the design of advanced metallic materials through tuning of interface properties.

36 MATERIALS SCIENCE↗

Tailoring mechanical properties of a multi-principal element alloy through a multi-length-scale approach

In this study, a multi-length-scale strengthening approach was used to tailor the microstructure and the mechanical properties of a NiCoCr-based multi-principal element alloy (MPEA). Grain size refinement, severe lattice distortion, and stacking fault energy (SFE) reduction with Mo addition (up to 10 at.%) enhance yield strength by 85% with only 10% reduction in ductility in as-annealed MPEAs. A pronounced increase in the strain hardening rate was observed with the addition of Mo, which is ascribed to the promotion of complex stacking fault (SF) interaction and intersection, accompanied by Lomer-Cottrell (L-C) and Hirth locks inhibiting dislocation motion and substantial increase in the accumulation of back stress. To push the limit of the yield strength further, the Suzuki segregation phenomenon was manipulated by a careful control of SF density by pre-straining and a subsequent 500 °C heat treatment. The stress-strain responses of the pre-strained and heat treated MPEAs showed an obvious SF density and Mo concentration dependence. Furthermore, the yield strength of the pre-strained Mo-added MPEAs with subsequent heat treatment was increased up to true stress of 2.3 GPa with a corresponding fracture elongation of 12% true strain. SFs formed during pre-straining served as Cr segregation sites during subsequent heat treatment, which substantially varies the local SFE within the SF, presenting a roughened landscape and frustrating the dislocation dynamics.

mechanical properties↗

Thermal Stability and Ion Irradiation Response of Refined Grained V – 4Cr – 4Ti

Since the 1960’s, there has been interest in V-4Cr-4Ti and similar alloys as candidates for low activation structural materials for advanced nuclear reactors. V-4Cr-4Ti was produced using arc melting and subsequently subjected to large strain extrusion machining to produce a multimodal microstructure largely composed of nanocrystalline and ultrafine grain sizes. In-situ thermal stability of the multimodal V-4Cr-4Ti to 800 °C shows the formation of vanadium carbides with negligible grain growth. In-situ dual-beam 16 KeV He+ and 1 MeV Kr2+ ion irradiation performed at 700 °C to a final dose of ~5 displacements per atom show the formation of small He cavities well distributed throughout the system, with preferential clustering at grain boundaries. This work provides insight into how the increased fraction of grain boundaries affect the simultaneous dual beam ion irradiation response of multimodal V – 4 wt.% Cr – 4 wt.% Ti at elevated temperatures. Analysis of the cavities reveal an areal density of 0.024±0.007 cavities/nm2 and swelling of 0.236% after the dual-beam ion irradiation. Nanoindentation shows a ~50% increase in hardening after the ion irradiation at 700 °C.

TEM↗

Ultra-grain refinement creates FCC pure cobalt with high strength and high ductility

Although pure cobalt is generally known to have a hexagonal close-packed (HCP) structure at room temperature, we show that its high-temperature face-centered cubic (FCC) phase can be strongly stabilized through grain refinement, resulting in FCC pure cobalt at room temperature. Ultrafine-grained (UFG) FCC cobalt exhibits a hierarchical microstructure consisting of dense stacking fault (SF) networks in the dominant FCC grains and numerous SFs and thin FCC layers within a few HCP plates. This unique microstructure leads to a high tensile strength exceeding 1 GPa, together with a tensile elongation of over 35%, thereby surpassing the well-known strength–ductility trade-off of pure metals. In-situ synchrotron X-ray diffraction revealed that the UFG FCC cobalt exhibited a markedly enhanced deformation-induced FCC→HCP martensitic transformation, which provided sustained strain hardening through the transformation-induced plasticity (TRIP) effect. Furthermore, ultra-grain refinement dramatically suppressed premature void and crack formation, causing a transition in the fracture mode from brittle to ductile. These findings advance the fundamental understanding of the phase stability and TRIP-assisted deformation in elemental cobalt and offer new guidelines for the microstructure-driven design of high-performance cobalt-based structural alloys.

Metastability↗

Structural integrity of additively manufactured stainless steel with cold sprayed barrier coating under combined cyclic loading

Integration of metal additive manufacturing (AM) and cold spray (CS) technologies provide an unprecedented opportunity to manufacture coated material systems with complex geometrical features. The application of these material systems in functionally critical components requires adequate structural integrity, particularly in the presence of cyclic loading. This article researches the multiaxial fatigue (axial-torsional cyclic loading) behavior of a coated material system consisting of 15Cr-5Ni precipitation-hardening stainless steel (15-5 PH SS) substrate additively manufactured by direct metal laser sintering with a layer of chromium carbide nickel (CrC-Ni) barrier coating deposited by CS. The influence of AM and CS-induced residual stresses on fatigue performance of test specimens was thoroughly studied. Additionally, the effect of surface roughness and processes induced defects were considered to explain the crack growth mechanism. Stresses assessed by synchrotron X-ray diffraction indicated a substantial accumulation of residual stresses, particularly in the outer surface of the as-fabricated 155 PH SS specimens. The state of residual stress was changed notably following the deposition of CrC-Ni coating in the axial, hoop, and radial directions of the fatigue test specimen. Also, CS deposition of CrC-Ni coating caused significant improvement in the surface quality of the additively manufactured components. Fatigue test results indicated, CS deposition of CrC-Ni substantially enhances the fatigue life of the AM-produced 15-5 PH SS substrate in all loading conditions, particularly in the high cycle fatigue regime. The improvement in the fatigue life of the specimens with coating was associated with a reduction in equivalent residual stress at the substrate surface and improvement in the specimens' surface condition (i.e., reduced surface roughness). The fractographic analysis of the specimen indicated the cracks tend to initiate in the surface of both as-fabricated and cold-sprayed specimens. However, the mechanism of crack growth changed notably following the deposition of CrC-Ni coating. The cracks tended to propagate in the planes parallel or with a small deviation from the build layers of the AM-produced specimens. On the other hand, deposition of CrC-Ni coating increased the deviation of crack growth plane from the build layers of the substrate.

36 MATERIALS SCIENCE↗

Residual stresses and microstructure within Allvac 718Plus laser powder bed fusion bars

The residual stresses within Allvac 718Plus bars built using LBPF with different laser powers, speeds and table displacements were measured using diffraction and mechanical methods and modelled with the baseplate attached and then removed. The residual stress profiles within the bars from the top surface down through the bulk were all quite similar, becoming less tensile due to a strain hardening mechanism. Table displacement has the greatest impact on residual stress, decreasing with increasing displacement/powder layer thickness. There was good agreement amongst the modeling and measurements. The microstructures were examined and varied slightly with energy density with higher densities having larger grains and enhanced post solidification diffusion. We found energy density had minimal impact on the residuals stresses within the parameters to produce dense material.

36 MATERIALS SCIENCE↗

Phase transformation dynamics guided alloy development for additive manufacturing

Fusion-based additive manufacturing technologies enable the fabrication of geometrically and compositionally complex parts unachievable by conventional manufacturing methods. However, the non-uniform and far-from-equilibrium heating/cooling conditions pose a significant challenge to consistently obtaining desirable phases in the as-printed parts. Here, in this study, we report a martensite stainless steel development guided by phase transformation dynamics revealed by in-situ high-speed, high-energy, high-resolution X-ray diffraction. This developed stainless steel consistently forms desired fully martensitic structure across a wide range of cooling rates (10 2 –10 7 °C/s), which enables direct printing of parts with fully martensitic structure. The as-printed material exhibits a yield strength of 1157 ± 23 MPa, comparable to its wrought counterpart after precipitation-hardening heat-treatment. The as-printed property is attributed to the fully martensitic structure and the fine precipitates formed during the intrinsic heat treatment in additive manufacturing. The phase transformation dynamics guided alloy development strategy demonstrated here opens the path for developing reliable, high-performance alloys specific for additive manufacturing.

17–4 PH stainless steel↗

Using post-processing heat treatments to elucidate precipitate strengthening of additively manufactured superalloy 718

The poor machinability and extensive work hardening of Ni-based superalloys makes additive manufacturing an attractive option for producing geometrically complex components with distinct microstructures. Although previous studies show recovery of high strength at room temperature, very few studies demonstrate successful properties at elevated temperatures required for industrial applications. Here, the objectives of this study are to present a post-build heat treatment for high strength across a wide temperature range, determine the strength contribution of nanoscale precipitating phases to the overall mechanical properties of superalloy 718, and from these, provide a comprehensive microstructure-property relationship for wrought and AM 718 to guide efforts to simulate the properties of AM components. Laser powder bed fusion–produced superalloy 718 was characterized at multiple length scales using scanning electron microscopy and transmission electron microscopy in the as-built condition and with multiple heat treatments designed to form combinations of γ', γ", and δ precipitates. Uniaxial tensile tests performed from room temperature to 600 °C on subsize specimens determined the yield strength, elastic modulus, ultimate tensile strength, fracture stress, and uniform elongation. Precipitates in this work proved to be weak barriers to dislocation motion through a dispersed barrier model, but they provided strength to the alloy through their consistent high density. The relative contribution to the yield strength from γ" remained consistent between 48% and 57% of the total strength up to 600 °C, the primary influence on the high temperature strength of superalloy 718. The strength factors for γ" and δ precipitates were found to trend inversely with tensile test temperature and may be attributable to the differences in precipitate coherency. A post-build heat treatment is recommended to maintain high strength at elevated temperatures. A quantitative microstructure-property relationship, dependent on precipitate size, density, and morphology, was derived and can estimate the yield strength across a wide temperature range applicable to the operational regimes for superalloy 718.

36 MATERIALS SCIENCE↗