At least 469 records · Page 26

Exposure of Highly Reflective Far-Ultraviolet Coatings to LEO Environment for TRL Advancement for the Habitable Worlds Observatory

Over the past several years, our team at the NASA Goddard Space Flight Center (GSFC), in collaboration with the Jet Propulsion Laboratory (JPL) and the Naval Research Laboratory (NRL), have developed several new protected Al coating technologies with improved Far-Ultraviolet (FUV) reflectance performance and more robust environmental stability. These include Al protected with lithium-based fluoride (LiF) coatings such as hot deposited LiF (eLiF), XeF 2 -passivated LiF coatings (XeLiF), Li 3 AlF 6 overcoats, AlF 3 (plasma passivated), and XeF 2 passivated MgF 2 coatings (XeMgF 2 ). However, despite these developments, relatively little experimental information exists regarding the long-term stability of these coatings after simultaneous exposure to the Low Earth Orbit (LEO) environment. To evaluate their environmental durability and advance their Technology Readiness Level (TRL), representative samples of these coating technologies, Al+XeLiF, Al+eLiF, Al+Li 3 AlF 6 , Al+AlF 3 , Al+XeMgF 2 , and bare Al as reference samples, were flown onboard the International Space Station (ISS) as part of the Materials International Space Station Experiment 20 (MISSE-20). The MISSE platform is operated by Aegis Aerospace for relatively long-duration (e.g. 6 months) external exposure experiments in a space environment. The coatings were deposited on ULE and Zerodur substrates, and witness samples deposited on the same coatings runs, but on glass slides were left on Earth as control. A subset of the flight samples were fitted with MgF 2 windows to reduce direct exposure to atomic oxygen (AO) and charged particles, and still let through UV and other types of radiation on these samples. After approximately 6 months of exposure in the forward-facing (RAM) direction, the samples were returned to Earth and characterized by performing FUV/NUV/VIS/NIR reflectance measurements to quantify degradation, spectroscopic ellipsometry to evaluate coating thickness and optical constants, atomic force microscopy (AFM) to quantify surface roughness evolution during the flight in the ISS. The MgF 2 protective windows were also analyzed through FUV transmission measurements. Comparison with the witness samples left on the ground and with the flown bare Al samples (with just the naturally occurring Al 2 O 3 layer) provided a quantitative assessment of coating thickness variations, optical performance degradation, and morphological changes induced by prolonged exposure to the LEO environment.

Far Ultraviolet (FUV)↗

Assessing Degradation of Advanced Coatings for Carbon/Carbon Composites

Carbon/carbon (C/C) composites are a well-utilized material system for hot structures to enable hypersonic flight. However, C/C materials are susceptible to attack by environmental degradation mechanisms, notably oxidation, which can limit the durability of components resulting in premature failure. Environmental barrier coatings (EBCs) have been developed to mitigate deleterious oxidation. Coating compositions based on silicon carbide (SiC) offer promise as a protective coating material for C/C composites. Under particular hypersonic flight conditions, a passivating silica scale can form at the surface of the EBC, acting as a barrier that can protect the underlying coating and substrate. However, the transition from passive to active oxidation, which varies with temperature and pressure, causes the formation of gaseous SiO that volatilizes leading to detrimental consumption of the SiC coating. In this work, arc-jet testing of SiC-based coatings developed to protect Advanced C/C-6 (ACC-6) was performed under a range of conditions to replicate varying oxidation conditions. In-situ optical emission spectroscopic measurements of the gas-surface interactions were collected and evaluated to render compositional degradation of the coating and underlying composite during arc-jet testing. Specimens were evaluated before, during and after arc-jet testing using destructive and non-destructive materials characterization methods, including optical and scanning electron microscopy and energy dispersive spectroscopy.

Coatings, Hypersonics, Composites↗

Assessment of Protective Coatings for Metal-Supported Solid Oxide Electrolysis Cells

Green hydrogen is essential to achieving carbon neutrality, and solid oxide electrolysis cells can produce hydrogen using renewable power and waste heat. Insufficient long-term durability of solid oxide electrolysis cells has impeded their commercialization. Here, coatings in the porous stainless steel support of metal-supported solid oxide electrolysis cells (MS-SOECs) are used to dramatically improve their performance and durability. The long-term degradation rate of uncoated MS-SOECs is highly dependent on the current density, with the fastest degradation occurring at the highest current density tested, 0.5 A cm -2 . At this current density, coatings are quite effective. Three protective coatings, Co 3 O 4 deposited by atomic layer deposition (ALD), Co 3 O 4 deposited by electroplating deposition (ED), and CuMn 1.8 O 4 (CMO) deposited by electrophoretic deposition (EPD), are explored to enhance the performance of MS-SOECs with La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 -Sm 0.2 Ce 0.8 O 3 (LSCF-SDC) as the oxygen catalyst and SDC-Ni as the fuel catalyst. The initial average current density at 1.4 V is increased with coatings. It is 0.83 mA cm -2 for the ALD cells, 1.05 mA cm -2 for the ED cells, and 1.13 mA cm -2 for the EPD cells, compared to 0.65 mA cm -2 for the bare cells at 700 °C with 50% H 2 -50% H 2 O. The degradation rate over 1000 h of continuous operation is reduced from 36% to 26%, 27%, and 19% kh -1 with the three coatings, respectively. Furthermore, these improvements are ascribed to reduced Cr poisoning on the oxygen catalyst, which is one of the primary degradation modes for this type of MS-SOEC.

25 ENERGY STORAGE↗

Advanced Thermal Barrier and Environmental Barrier Coating Development at NASA GRC

This presentation summarizes NASA's advanced thermal barrier and environmental barrier coating systems, and the coating performance improvements that has recently been achieved and documented in laboratory simulated rig test conditions. One of the emphases has been placed on the toughness and impact resistance enhancements of the low conductivity, defect cluster thermal barrier coating systems. The advances in the next generation environmental barrier coatings for SiCSiC ceramic matrix composites have also been highlighted, particularly in the design of a new series of oxide-silicate composition systems to be integrated with next generation SiC-SiC turbine engine components for 2700F coating applications. Major technical barriers in developing the thermal and environmental barrier coating systems are also described. The performance and model validations in the rig simulated turbine combustion, heat flux, steam and calcium-magnesium-aluminosilicate (CMAS) environments have helped the current progress in improved temperature capability, environmental stability, and long-term fatigue-environment system durability of the advanced thermal and environmental barrier coating systems.

Thermal Barrier and Environmental Barrier Coatings↗

Thermal Conductivity and Stability of HfO2-Y2O3 and La2Zr2O7 Evaluated for 1650 Deg C Thermal/Environmental Barrier Coating Applications

HfO2-Y2O3 and La2Zr2O7 are candidate thermal and environmental barrier coating (T/EBC) materials for gas turbine ceramic matrix composite (CMC) combustor applications because of their relatively low thermal conductivity and high temperature capability. In this paper, thermal conductivity and high temperature stability of hot-pressed and plasma sprayed specimens with representative partially-stabilized and fully-cubic HfO2-Y2O3 compositions and La2Zr2O7 were evaluated at temperatures up to 1700 C using a steady-state laser heat-flux technique. Sintering behavior of the plasmasprayed coatings was determined by monitoring the thermal conductivity increases during a 20-hour test period at various temperatures. Durability and failure mechanisms of the HfO2-Y2O3 and La2Zr2O7 coatings on mullite/SiC hexoloy or SiC/SiC CMC substrates were investigated at 1650 C under thermal gradient cyclic conditions. Coating design and testing issues for the 1650 C thermal/environmental barrier coating applications are also discussed.

Zhu, Dong-Ming↗

Thermal Conductivity and Water Vapor Stability of Ceramic HfO2-Based Coating Materials

HfO2-Y2O3 and La2Zr2O7 are candidate thermal/environmental barrier coating materials for gas turbine ceramic matrix composite (CMC) combustor liner applications because of their relatively low thermal conductivity and high temperature capability. In this paper, thermal conductivity and high temperature phase stability of plasma-sprayed coatings and/or hot-pressed HfO2-5mol%Y2O3, HfO2-15mol%Y2O3 and La2Zr2O7 were evaluated at temperatures up to 1700 C using a steady-state laser heat-flux technique. Sintering behavior of the plasma-sprayed coatings was determined by monitoring the thermal conductivity increases during a 20-hour test period at various temperatures. Durability and failure mechanisms of the HfO2-Y2O3 and La2Zr2O7 coatings on mullite/SiC Hexoloy or CMC substrates were investigated at 1650 C under thermal gradient cyclic conditions. Coating design and testing issues for the 1650 C thermal/environmental barrier coating applications will also be discussed.

Zhu, Dong-Ming↗

Phase Stability and Thermal Conductivity of Composite Environmental Barrier Coatings on SiC/SiC Ceramic Matrix Composites

Advanced environmental barrier coatings are being developed to protect SiC/SiC ceramic matrix composites in harsh combustion environments. The current coating development emphasis has been placed on the significantly improved cyclic durability and combustion environment stability in high-heat-flux and high velocity gas turbine engine environments. Environmental barrier coating systems based on hafnia (HfO2) and ytterbium silicate, HfO2-Si nano-composite bond coat systems have been processed and their stability and thermal conductivity behavior have been evaluated in simulated turbine environments. The incorporation of Silicon Carbide Nanotubes (SiCNT) into high stability (HfO2) and/or HfO2-silicon composite bond coats, along with ZrO2, HfO2 and rare earth silicate composite top coat systems, showed promise as excellent environmental barriers to protect the SiC/SiC ceramic matrix composites.

Benkel, Samantha↗

Enhancing 300 Degree Celsius Electronic Packaging with Ceramic PCBs and Advanced Interconnection Techniques

Geothermal energy development requires downhole tools that operate reliably at temperatures up to 320 °C. While MWD tools work without thermal protection and logging tools use vacuum flasks for limited high-temperature use, Sandia National Laboratories is developing durable electronics on ceramic PCBs with protective coatings to enable long-term operation of geothermal instruments at sustained temperatures up to 300 °C.

Wright, Andrew Alexander [Sandia National Laborato↗

Monopropellant engine investigation for space shuttle reaction control system. Volume 3: Improvement of metal foam for catalyst retention

The retention of granular catalyst in a metal foam matrix was demonstrated to greatly increase the life capability of hydrazine monopropellant reactors. Since nickel foam used in previous tests was found to become degraded after long-term exposure the cause of degradation was examined and metal foams of improved durability were developed. The most durable foam developed was a rhodium-coated nickel foam. An all-platinum foam was found to be incompatible in a hot ammonia (hydrazine) environment. It is recommended to scale up the manufacturing process for the improved foam to produce samples sufficiently large for space shuttle APU gas generator testing.

Source record↗

Polyimide Film of Increased Tear Strength

High-temperature linear aromatic polyimide with improved resistance to tearing made by new process that incorporates elastomer into polyimide. Linear aromatic condensation polyimides are materials of prime choice for use as films and coatings on advanced spacecraft and aircraft where durability at temperatures in range of 200 to 300 degree C required. Elastomer-containing polyimide film with improved toughness proves useful for applications where resistance to tearing and long-term thermal stability necessary. Desired resistance to tearing achieved by careful control of amount and chemical composition of added elastomer.

St. Clair, A. K.↗

Advanced Oxide Material Systems for 1650 C Thermal/Environmental Barrier Coating Applications

Advanced thermal and environmental barrier coatings (TEBCs) are being developed for low-emission SiC/SiC ceramic matrix composite (CMC) combustor and vane applications to extend the CMC liner and vane temperature capability to 1650 C (3000 F) in oxidizing and water-vapor-containing combustion environments. The advanced 1650 C TEBC system is required to have a better high-temperature stability, lower thermal conductivity, and more resistance to sintering and thermal stress than current coating systems under engine high-heat-flux and severe thermal cycling conditions. In this report, the thermal conductivity and water vapor stability of selected candidate hafnia-, pyrochlore- and magnetoplumbite-based TEBC materials are evaluated. The effects of dopants on the materials properties are also discussed. The test results have been used to downselect the TEBC materials and help demonstrate the feasibility of advanced 1650 C coatings with long-term thermal cycling durability.

Zhu, Dong-Ming↗

Advanced Seal Development for Large Industrial Gas Turbines

Efforts are in progress to develop advanced sealing for large utility industrial gas turbine engines (combustion turbines). Such seals have been under developed for some time for aero gas turbines. It is desired to transition this technology to combustion turbines. Brush seals, film riding face and circumferential seals, and other dynamic and static sealing approaches are being incorporated into gas turbines for aero applications by several engine manufacturers. These seals replace labyrinth or other seals with significantly reduced leakage rates. For utility industrial gas turbines, leakage reduction with advanced sealing can be even greater with the enormous size of the components. Challenges to transitioning technology include: extremely long operating times between overhauls; infrequent but large radial and axial excursions; difficulty in coating larger components; and maintenance, installation, and durability requirements. Advanced sealing is part of the Advanced Turbine Systems (ATS) engine development being done under a cooperative agreement between Westinghouse and the US Department of Energy, Office of Fossil Energy. Seal development focuses on various types of seals in the 501ATS engine both at dynamic and static locations. Each development includes rig testing of candidate designs and subsequent engine validation testing of prototype seals. This presentation gives an update of the ongoing ATS sealing efforts with special emphasis on brush seals.

Chupp, Raymond E.↗

CMC Research at NASA Glenn in 2015: Recent Progress and Plans

As part of NASAs Aeronautical Sciences project, Glenn Research Center has developed advanced fiber and matrix constituents for a 2700F CMC for turbine engine applications. Fiber and matrix development and characterization will be reviewed. Resulting improvements in CMC mechanical properties and durability will be summarized. Plans for 2015 will be described, including development and validation of models predicting effects of the engine environment on durability of SiC/SiC composites with Environmental Barrier Coatings

Propulsion↗

CMC Research at NASA Glenn in 2016: Recent Progress and Plans

As part of NASA's Aeronautical Sciences project, Glenn Research Center has developed advanced fiber and matrix constituents for a 2700 degrees Fahrenheit CMC (Ceramic Matrix Composite) for turbine engine applications. Fiber and matrix development and characterization will be reviewed. Resulting improvements in CMC mechanical properties and durability will be summarized. Plans for 2015 will be described, including development and validation of models predicting effects of the engine environment on durability of SiCSiC composites with Environmental Barrier Coatings (EBCs).

Additive Manufacturing↗

Upper Temperature Limit of Environmental Barrier Coatings Based on Mullite and BSAS

Current state-of-the-art environmental barrier coatings (EBCs) for Si-based ceramics consist of three layers: a silicon bond coat, an intermediate mullite (3Al2O3-2SiO2) or mullite + BSAS (1-xBaO-xSrO-Al2O3-2SiO2) layer, and a BSAS top coat. Areas of concern for long-term durability are environmental durability, chemical compatibility, silica volatility, phase stability, and thermal conductivity. Variants of this family of EBCs were applied to monolithic SiC and melt infiltrated SiC/SiC composites. Reaction between BSAS and silica results in low melting (approx. 1300 C) glasses at T > 1400 C, which can cause the spallation of the EBC. At temperatures greater than 1400 C, the BSAS top coat also degrades by formation of a porous structure, and it suffers significant recession via silica volatilization in water vapor-containing atmospheres. All of these degradation mechanisms can be EBC life-limiting factors. BSAS undergoes a very sluggish phase transformation (hexagonal celsian to monoclinic celsian), the implications of which are not fully understood at this point. There was evidence of rapid sintering at temperatures as low as 1300 C, as inferred from the sharp increase in thermal conductivity.

Lee, Kang N.↗

RECENT ADVANCES IN HIGH TEMPERATURE ELECTROLYSIS AT IDAHO NATIONAL LABORATORY: STACK TESTS

High temperature steam electrolysis is a promising technology for efficient sustainable large-scale hydrogen production. Solid oxide electrolysis cells (SOECs) are able to utilize high temperature heat and electric power from advanced high-temperature nuclear reactors or renewable sources to generate carbon-free hydrogen at large scale. However, long term durability of SOECs needs to be improved significantly before commercialization of this technology. A degradation rate of 1%/khr or lower is proposed as a threshold value for commercialization of this technology. Solid oxide electrolysis stack tests have been conducted at Idaho National Laboratory to demonstrate recent improvements in long-term durability of SOECs. Electrolytesupported and electrode-supported SOEC stacks were provided by Ceramatec Inc., Materials and Systems Research Inc. (MSRI), and Saint Gobain Advanced Materials (St. Gobain), respectively for these tests. Long-term durability tests were generally operated for a duration of 1000 hours or more. Stack tests based on technology developed at Ceramatec and MSRI have shown significant improvement in durability in the electrolysis mode. Long-term degradation rates of 3.2%/khr and 4.6%/khr were observed for MSRI and Ceramatec stacks, respectively. One recent Ceramatec stack even showed negative degradation (performance improvement) over 1900 hours of operation. A three-cell short stack provided by St. Gobain, however, showed rapid degradation in the electrolysis mode. Improvements on electrode materials, interconnect coatings, and electrolyteelectrode interface microstructures contribute to better durability of SOEC stacks.

08 HYDROGEN↗

NASA Glenn/AADC Collaboration Optimized Erosion Coatings for Inlet Guide Vanes

There is a need for lightweight, durable materials and structures to reduce the weight of propulsion systems. Polymer matrix composites (PMC's) are promising materials for aerospace applications because of their high strength-to-weight ratio relative to metals. Unfortunately, they are limited to applications where they are not exposed to hightemperature oxidizing atmospheres and/or particulates from ingested air. This is because oxidation and erosion occur on the surface, leading to weight loss, nodulation, and/or cracking on the surface, and a consequent decline of mechanical properties over time. Although prior research has shown that oxidation can be slowed when metallic or ceramic coatings are applied onto PMC's, there remains a need for erosion-resistant coatings that protect PMC's from high-velocity particulates in the engine flow path. These erosionresistant coatings could extend the life of polymer composites. Polymer composites are heavily damaged without an erosion-resistant coating because they are not as hard as metallic engine structures. The effectiveness and life of the coatings depends on their inherent properties as well as on the interaction between the coating and the PMC. Since polymers, in general, have high thermal expansion coefficients in comparison to metals and ceramics, failure of the coatings often occurs at this interface. The objective of this research is to develop strategies to improve this interface and tailor overlays for erosion resistance. The bondcoat, which was developed at the NASA Glenn Research Center, is composed of zinc blended with polyimides to improve the compatibility between the PMC and the overlay material. Initial coating trials at AADC produced vanes that had poor bonding between the overlay and bondcoats. Subsequently, Glenn successfully demonstrated that high-quality plasma-sprayed erosion coating systems could be applied to these guide vanes. Inlet guide vanes from AE 3007 engines fiber composites were coated using a coating system composed of a bondcoat and a hard topcoat. Optimization of the plasma spray process has led to plans for future erosion testing in gas turbine engine environments.

Sutter, James K.↗

Manufacturing of Low Cost, Durable Membrane Electrode Assemblies Engineered for Rapid Conditioning

Over the past 20 years significant progress in membrane-electrode assembly (MEA) technology development for polymer electrolyte fuel cells (PEMFCs) has resulted in the PEMFC technology approaching a commercial reality for transportation applications. However, there remain two primary technical challenges to be addressed in the MEA. First and foremost is meeting the automotive cost targets: Producing a fuel cell stack cost competitive with today’s internal combustion engine. In addition to the material cost, MEA (and other components) and stack assembly production methods must be amenable for use in low cost, high speed, automotive assembly line. One impediment to this latter goal is that stack components must currently go through a long and tedious conditioning procedure before they produce optimal power. This so-called “break-in” can take many hours, and can involve quite complex voltage, temperature and/or pressure steps. These break-in procedures must be simplified and the time required reduced if fuel cells are to become a viable automotive engine. The second challenge is to achieve the durability targets in real-world automotive duty cycle operations. Significant improvements in cost, break-in time, and durability for the key component of fuel cell stacks, MEAs were achieved in this project. Advanced modeling was used to guide design of the new MEA to maximize performance and durability. A new, innovative process and manufacturing approach utilizing direct in-line coating using scalable, cost-competitive, continuous high volume 3-layer rolled-good manufacturing processes was developed and validated by single cell and short stack testing. In addition, the direct coating methods employed were shown to reduce the cost for sacrificial films. Furthermore, Gore has demonstrated a 10 µm reinforced membrane that is used in the new low-cost process and can meet automotive power density and durability targets. Across a wide range of operating conditions, the direct-coated MEA outperformed the commercial baseline MEA, and did so through a process that delivers MEAs at $92.35/m2 at a volume of 500,000 systems per year, according to Strategic Analysis (SA) estimates.

08 HYDROGEN↗