At least 469 records · Page 26

In-situ preparation of Fe{sub 2}O{sub 3} hierarchical arrays on stainless steel substrate for high efficient catalysis

Hierarchical array catalysts with micro/nano structures on substrates not only possess high reactivity from large surface area and suitable interface, but intensify mass transfer through shortening the diffusion paths of both reactants and products for high catalytic efficiency. Herein, we first demonstrate fabrication of Fe{sub 2}O{sub 3} hierarchical arrays grown on stainless-steel substrates via in-situ hydrothermal chemical oxidation followed by heat treatment in N{sub 2} atmosphere. As a Fenton-like catalyst, Fe{sub 2}O{sub 3} hierarchical arrays exhibit excellent catalytic activity and life cycle performance for methylene blue (MB) dye degradation in aqueous solution in the presence of H{sub 2}O{sub 2}. The Fe{sub 2}O{sub 3} catalyst with unique hierarchical structures and efficient transport channels, effectively activates H{sub 2}O{sub 2} to generate large quantity of • OH radicals and highly promotes reaction kinetics between MB and • OH radicals. Immobilization of hierarchical array catalysts on stainless-steel can prevent particles agglomeration, facilitate the recovery and reuse of the catalysts, which is expected promising applications in wastewater remediation. - Graphical abstract: The in-situ synthesis of Fe{sub 2}O{sub 3} hierarchical arrays on stainless-steel substrates was reported for the first time, which exhibit excellent catalytic activity performance for methylene blue (MB) dye degradation in aqueous solution in the presence of H{sub 2}O{sub 2}. - Highlights: • Fe{sub 2}O{sub 3} hierarchical arrays was prepared by in-situ hydrothermal chemical oxidation. • F{sup −} ions play an important role in the formation of the Fe{sub 2}O{sub 3} hierarchical arrays. • Fe{sub 2}O{sub 3} hierarchical arrays show high catalytic activity to methylene blue degradation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A transmission electron microscopy study of EBR-II neutron-irradiated austenitic stainless steel 304 and nickel-base alloy X-750

The microstructure of EBR-II neutron-irradiated austenitic stainless steel 304 and nickel-base alloy X-750 was investigated. Both alloys were irradiated at low dose rates (~2 × 10 -8 dpa/s) to a neutron fluence of 6.9 × 10 22 n/cm 2 (E > 0.1 MeV) at 371–389 °C. Different types of defects, including Frank loops, cavities, and γ' precipitates were characterized. The Frank loops in Type 304 stainless steel (SS) are larger in size (~50 nm in diameter) and lower in number density (2.58 × 10 21 m -3 ), compared to most previous higher dose rate neutron irradiation studies. The Frank loops in X-750 have an average size 26.0 nm of and a number density of 9.44 × 10 21 m -3 . In 304 SS and X-750, cavities are of ~20 nm and ~14 nm in diameter, respectively. The swelling of both alloys was found to be insignificant. In 304 SS, Ni and Si were found enriched at the cavity surfaces and Ni,Si-rich precipitates were also found. Multivariate statistical analysis using non-negative matrix factorization reveals that these Ni,Si-rich precipitates contain only ~5.7 at.% Si, differing from the Ni 3 Si γ' precipitates found in several previous studies. In X-750, L1 2 -structured γ' precipitates were found, and multivariate statistical analysis confirmed the 3:1 stoichiometry (Ni 3 (Ti,Al)) of the precipitates and the superlattice reflections confirmed the stability of the crystal structure of these γ' precipitates, indicating higher-than-expected precipitate stability under high-dose neutron irradiation.

36 MATERIALS SCIENCE↗

Detection of secondary phases in duplex stainless steel by magnetic force microscopy and scanning Kelvin probe force microscopy

The secondary phase transformations in a commercial super duplex stainless steel were investigated by micro-chemical analyses and high resolution scanning probe microscopy. Energy dispersive X-ray and electron probe detected ferrite and austenite as well as secondary phases in unetched aged duplex stainless steel type 25Cr-7Ni-3Mo. Volta potential indicated that nitride and sigma appeared more active than ferrite, while secondary austenite and austenite presented a nobler potential. Reversal order in nobility is thought to be attributable to the potential ranking provided by oxide nature diversity as a result of secondary phase surface compositions on steel. After eutectoid transformation, secondary austenite was detected by electron probe microanalysis, whereas atomic force microscopy distinguished this phase from former austenite by image contrast. Magnetic force microscopy revealed a “ghosted” effect on the latter microstructure probably derived from metal memory reminiscence of mechanical polishing at passivity and long range magnetic forces of ferrite phase. - Highlights: • Nobility detection of secondary phases by SKPFM in DSS particles is not a straightforward procedure. • As Volta potential and contrast are not always consistent SKPFM surface oxides is thought played an important role in detection. • AFM distinguished secondary austenite from former austenite by image contrast though SEM required EPMA.

36 MATERIALS SCIENCE↗

Stainless Steel Corrosion Studies Final Report: FY17 End of-Year

Two materials are being considered in applications requiring their contact against stainless steel surfaces. These materials include the solvent methyl ethyl ketone (MEK), and the polymer neoprene (polychloroprene). There is concern that contact of these materials with stainless steel substrates may lead to corrosion. To address these concerns we have undertaken corrosion studies under conditions expected to be more aggressive than in intended applications. These conditions include elevated temperature and humidity, and submersion and suspension in solvent vapors, in an attempt to accelerate any potential deleterious interactions. Corrosion rates below 0.1 mpy have historically been deemed INSIGNIFICANT from a WR Production standpoint; corresponding guidelines for non-production applications are lacking.

36 MATERIALS SCIENCE↗

ZnFe{sub 2}O{sub 4}/TiO{sub 2} nanocomposite films for photocathodic protection of 304 stainless steel under visible light

Highlights: • Hydrothermal method for synthesizing ZnFe{sub 2}O{sub 4} nanoparticles on TiO{sub 2} NTs. • The photoelectrochemical property of TiO{sub 2} could greatly improve by doping ZnFe{sub 2}O{sub 4}. • The ZnFe{sub 2}O{sub 4}/TiO{sub 2} composite films provide a better photocathodic protection for 304SS. - Abstract: ZnFe{sub 2}O{sub 4} sensitized TiO{sub 2} nanotubes were fabricated via anodic oxidation and hydrothermal method. The ZnFe{sub 2}O{sub 4}/TiO{sub 2} composite films with different concentrations were synthesized to explore the optimal photoelectrochemical property compared with pure TiO{sub 2} nanotubes. The morphology and chemical composition of samples were characterized by scanning electron microscopy, energy-dispersive spectrometry, and X-ray diffraction. The performance of protection for 304 stainless steel was investigated by electrochemical tests, such as open circuit potential and photocurrent density. The results indicate that ZnFe{sub 2}O{sub 4}/TiO{sub 2} composite films showed efficient photocathodic protection effect for 304 stainless steel under visible light, and the optimal specimen composite films shifted the corrosion potential of 304 stainless steel to −780 mV.

36 MATERIALS SCIENCE↗

Electrochemical Corrosion Analysis of Stainless Steels in LALM Pyrolysis Bio-Oil with Organic Corrodents

Pyrolysis bio-oils are corrosive to low alloy steels, e.g., 2.25Cr-1Mo, 5Cr-1Mo, and 9Cr-1Mo grades. To identify the alloys with sufficient bio-oil compatibility, several commercial stainless steels were examined in bio-oil using electrochemical impedance spectroscopy to semi quantitatively assess their corrosion resistance. Low-Ash Low-Moisture (LALM) bio-oil, produced from a forest residue feedstock by the National Renewable Energy Laboratory in Golden, CO, was used as a test liquid for electrochemical impedance spectroscopy measurements. Three organic corrodents, formic acid, catechol, and lactobionic acid, were added into LALM bio-oil to produce test liquids with intentionally increased corrosivity. Corrosion reaction resistance, determined from the impedance data, was used to evaluate the corrosion compatibility of each stainless steel in LALM bio-oil and LALM bio-oil + organic corrodent(s). The results from corrosion reaction resistance indicated that the critical Cr content of stainless steels for corrosion resistance would be greater than 14 wt % if Ni and Mo contents are low but can be as low as 12–13 wt % with appreciable amounts of Ni and Mo.

Jun, Jiheon↗

Samarium electrodeposited acetate and oxide thin films on stainless steel substrate characterized by XPS

Characterization of a samarium thin film deposited on a stainless steel substrate using molecular electrodeposition was carried out using a Thermo Scientific K-Alpha X-ray photoelectron spectrometer. We studied two types of samarium electrodeposition samples, one as-deposited and one heated to 700 °C in an air flow. Survey scans include peaks coming from the stainless steel substrate, such as Fe and Cr. An X-ray photoelectron spectroscopy (XPS) survey spectrum, Sm 3d, C 1s, and O 1s narrow scans are shown. It was determined that the heating process decomposed the deposited Sm acetate to Sm 2 O 3 using XPS.

36 MATERIALS SCIENCE↗

Microstructure and deformation mode of a stainless steel rupture disc exposed to sodium-water reaction

This paper deals with microstructural studies carried out on an austenitic stainless steel rupture disc which was exposed to sodium-water reaction. The rupture disc was part of a leak simulator put in a micro leak test section which was used to study the 'self wastage' of steam generator tubes. During micro leak testing, the rupture disc failed exhibiting a linear crack at a much lower pressure of 10 MPa rather than bursting open at the higher designed pressure of 15 MPa. The failed rupture disc revealed different microstructural features on the inner (steam exposed) and outer (sodium exposed) surfaces. Using microstructure as the signature, the temperature experienced by the rupture disc was predicted as {>=} 1273 K. Evidence for the exposure of the rupture disc to highly exothermic sodium-water reaction was obtained in the form of sodium rich debris, microcracks and deformation bands. Detailed transmission electron microscopy revealed the nature of deformation bands as deformation twins which is not a preferred failure mode for austenitic stainless steels.

36 MATERIALS SCIENCE↗

Constitutive Model for the Time-Dependent Mechanical Behavior of 430 Stainless Steel and FeCrAlY Foams in Sulfur-Bearing Environments

The mechanical behavior of 430 stainless steel and pre-oxidized FeCrAlY open-cell foam materials of various densities was evaluated in compression at temperatures between 450 C and 600 C in an environment containing hydrogen sulfide and water vapor. Both materials showed negligible corrosion due to the gaseous atmosphere for up to 168 hours. The monotonic stress-strain response of these materials was found to be dependent on both the strain rate and their density, and the 430 stainless steel foam materials exhibited less stress relaxation than FeCrAlY for similar experimental conditions. Using the results from multiple hardening-relaxation and monotonic tests, an empirical constitutive equation was derived to predict the stress-strain behavior of FeCrAlY foams as a function of temperature and strain rate. These results are discussed in the context of using these materials in a black liquor gasifier to accommodate the chemical expansion of the refractory liner resulting from its reaction with the soda in the black liquor.

Constitutive Model↗

Tribocorrosion Behavior of SAF 2205 Duplex Stainless Steel in Artificial Seawater

Tribocorrosion behaviors of SAF 2205 duplex stainless steel sliding against an Al{sub 2}O{sub 3} counterpart were investigated in artificial seawater. The tribocorrosion mechanisms and synergistic actions between corrosion and wear were analyzed in this work. The results indicated that a higher load was beneficial for the formation of the σ intermetallic phase and strain hardening; thus, the hardness increased first, and then the pure mechanical wear resistance of SAF 2205 was improved by the hardening effect. The wear mechanisms of SAF 2205 were dominated by abrasive wear under lower loads and by abrasive wear and plastic deformation under higher loads. Furthermore, galvanic corrosion was established between the σ intermetallic phase/ferritic/austenitic and passive film (cathode)/fresh surface, which caused corrosion-accelerated wear. Thus, the total damage to SAF 2205 during tribocorrosion in artificial seawater was determined by the mechanical wear and synergetic effects between corrosion and wear. Therefore, improving hardness was an effective way to increase the tribocorrosion properties of metal materials, such as SAF 2205 and 316L.

36 MATERIALS SCIENCE↗

Influence of Heat Treatment on Mercury Cavitation Resistance of Surface Hardened 316LN Stainless Steel

The cavitation-erosion resistance of carburized 316LN stainless steel was significantly degraded but not destroyed by heat treatment in the temperature range 500-800 C. The heat treatments caused rejection of some carbon from the carburized layer into an amorphous film that formed on each specimen surface. Further, the heat treatments encouraged carbide precipitation and reduced hardness within the carburized layer, but the overall change did not reduce surface hardness fully to the level of untreated material. Heat treatments as short as 10 min at 650 C substantially reduced cavitation-erosion resistance in mercury, while heat treatments at 500 and 800 C were found to be somewhat less detrimental. Overall, the results suggest that modest thermal excursions perhaps the result of a weld made at some distance to the carburized material or a brief stress relief treatment will not render the hardened layer completely ineffective but should be avoided to the greatest extent possible.

36 MATERIALS SCIENCE↗

Impact of Dielectronic Recombination on Ionization Dynamics and Spectroscopy of Z-pinch Stainless Steel Plasma

The implosion dynamics of an array of stainless steel (SS) wires on the Z and/or ZR accelerator produces an abundance of radiation from the K- and L-shell ionization stages. As the plasma assembles on axis, a number of time resolved snapshots provide temperature and density profiles and size of the emitting region. The non-LTE populations will be obtained by using detailed atomic models that include all important excitation, ionization, and recombination processes. In particular, we will investigate the effects of dielectronic recombination (DR) which is the most important recombination process for moderate to high Z plasma such as iron at moderate densities. We will analyze the ionization dynamics and generate K- and L-shell spectra using the temperature and density conditions generated in the Z and/or ZR accelerator describing the implosion with a 1-D non-LTE radiation hydrodynamics model.

74 ATOMIC AND MOLECULAR PHYSICS↗

Assessment of Stress Corrosion Cracking Resistance of Activated Tungsten Inert Gas-Welded Duplex Stainless Steel Joints

The stress corrosion cracking behavior of duplex stainless steel (DSS) weld joint largely depends on the ferrite-austenite phase microstructure balance. This phase balance is decided by the welding process used, heat input, welding conditions and the weld metal chemistry. In this investigation, the influence of activated tungsten inert gas (ATIG) and tungsten inert gas (TIG) welding processes on the stress corrosion cracking (SCC) resistance of DSS joints was evaluated and compared. Boiling magnesium chloride (45 wt.%) environment maintained at 155 °C was used. The microstructure and ferrite content of different weld zones are correlated with the outcome of sustained load, SCC test. Irrespective of the welding processes used, SCC resistance of weld joints was inferior to that of the base metal. However, ATIG weld joint exhibited superior resistance to SCC than the TIG weld joint. The crack initiation and final failure were in the weld metal for the ATIG weld joint; they were in the heat-affected zone for the TIG weld joint.

36 MATERIALS SCIENCE↗

Twinning and martensite in a 304 austenitic stainless steel

The microstructure characteristics and deformation behavior of 304L stainless steel during tensile deformation at two different strain rates have been investigated by means of interrupted tensile tests, electron-backscatter-diffraction (EBSD) and transmission electron microscopy (TEM) techniques. The volume fractions of transformed martensite and deformation twins at different stages of the deformation process were measured using X-ray diffraction method and TEM observations. It is found that the volume fraction of martensite monotonically increases with increasing strain but decreases with increasing strain rate. On the other hand, the volume fraction of twins increases with increasing strain for strain level less than 57%. Beyond that, the volume fraction of twins decreases with increasing strain. Careful TEM observations show that stacking faults (SFs) and twins preferentially occur before the nucleation of martensite. Meanwhile, both {var_epsilon}-martensite and {alpha}{prime}-martensite are observed in the deformation microstructures, indicating the co-existence of stress induced- transformation and strain-induced-transformation. We also discussed the effects of twinning and martensite transformation on work-hardening as well as the relationship between stacking faults, twinning and martensite transformation.

36 MATERIALS SCIENCE↗

Influence of Heat Input and Cold Wire Feeding Rate on Pitting Corrosion Resistance of Submerged Arc Welding Duplex Stainless Steel Welds

Welding thermal cycles may severely impair duplex stainless steel (DSS) performance, especially local pitting resistance and toughness. The restricted welding energy between 0.5 and 2.5 kJ mm{sup −1} represents a limiting factor for productivity increase in DSS welding, and the addition of cold wire is an interesting alternative to increase the welding deposition rate without adding extra heat. The aim of this work is to evaluate the influence of the cold wire feeding rate (CW) and heat input (HI) on pitting corrosion behavior of DSS UNS S32304 bead-on-plate welds obtained by submerged arc welding (SAW). Cyclic potentiodynamic polarization was carried out in transverse weld sections using 1 mol L{sup −1} NaCl solution at room temperature. Most pitting corrosion spots were located on the heat-affected zone (HAZ), and the pitting potentials were lower than the base metal due to higher ferrite fractions and the presence of chromium nitrides. Considering the same CW, the HI increasing reduced E{sub pit} for 1.6, 1.9, 2.2 kJ mm{sup −1}, but increased E{sub pit} for 2.7 kJ mm{sup −1}, due to a balance between the HAZ width and the austenite fraction.

36 MATERIALS SCIENCE↗

Effect of deposition rate on microstructure and mechanical properties of 17-4 PH stainless steel fabricated by laser engineered net shaping

Laser engineered net shaping (LENS) is an additive manufacturing technique for fabricating and repairing metallic components. However, the relationships between its process parameters and the resulting mechanical properties of alloys such as 17-4 precipitation-hardening (PH) stainless steel require further investigation to enable reliable application. This study examines the specific effect of LENS deposition rate on the microstructure and mechanical properties of 17-4 PH stainless steel. Specimens were fabricated at two different deposition rates (8.47 and 9.31 mm s−1), subjected to subsequent solution and H900 aging treatment, and then evaluated via tensile testing, hardness measurements, and microscopy. A higher deposition rate results in a finer grain structure but increased porosity, leading to greater ultimate tensile strength (∼1294 MPa) yet lower ductility (strain at failure ∼5.8%) compared to the slower deposition rate (∼1266 MPa, ∼9.0% strain). Hardness follows the same trend as tensile strength. Tensile fracture surfaces for both conditions exhibited a mixed mode of ductile dimples and brittle quasi-cleavage regions, with chromium/silicon oxide particles identified within dimples. Complementary finite element modeling indicates that small void fractions primarily reduce ductility by enhancing localized plasticity, with only a marginal decrease in tensile strength. These integrated experimental and numerical results elucidate the mechanical properties linked to deposition rate, providing insight into tailoring LENS processes to achieve desired properties of 17-4 PH stainless steel.

17-4 PH stainlesssteel↗

Moessbauer spectroscopy study on the corrosion resistance of plasma nitrided ASTM F138 stainless steel in chloride solution

Plasma nitriding of ASTM F138 stainless steel samples has been carried out using dc glow discharge under 80% H{sub 2}-20% N{sub 2} gas mixture, at 673 K, and 2, 4, and 7 h time intervals, in order to investigate the influence of treatment time on the microstructure and the corrosion resistance properties. The samples were characterized by scanning electron microscopy, glancing angle X-ray diffraction and conversion electron Moessbauer spectroscopy, besides electrochemical tests in NaCl aerated solution. A modified layer of about 6 {mu}m was observed for all the nitrided samples, independent of nitriding time. The X-ray diffraction analysis shows broad {gamma}{sub N} phase peaks, signifying a great degree of nitrogen supersaturation. Besides {gamma}{sub N,} the Moessbauer spectroscopy results indicated the occurrence of {gamma}' and {epsilon} phases, as well as some other less important phases. Corrosion measurements demonstrate that the plasma nitriding time affects the corrosion resistance and the best performance is reached at 4 h treatment. It seems that the {epsilon}/{gamma}' fraction ratio plays an important role on the resistance corrosion. Additionally, the Moessbauer spectroscopy was decisive in this study, since it was able to identify and quantify the iron phases that influence the corrosion resistance of plasma nitrided ASTM F138 samples.

36 MATERIALS SCIENCE↗