Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SINTERED MATERIALS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 469 records · Page 26

A Symmetrical, Planar SOFC Design for NASA's High Specific Power Density Requirements

Solid oxide fuel cell (SOFC) systems for aircraft applications require an order of magnitude increase in specific power density (1.0 kW/kg) and long life. While significant research is underway to develop anode supported cells which operate at temperatures in the range of 650-800 C, concerns about Cr-contamination from the metal interconnect may drive the operating temperature down further, to 750 C and lower. Higher temperatures, 900-1000 C, are more favorable for SOFC stacks to achieve specific power densities of 1.0 kW/kg. Since metal interconnects are not practical at these high temperatures and can account for up to 75% of the weight of the stack, NASA is pursuing a design that uses a thin, LaCrO3-based ceramic interconnect that incorporates gas channels into the electrodes. The bi-electrode supported cell (BSC) uses porous YSZ scaffolds, on either side of a 10-20 microns electrolyte. The porous support regions are fabricated with graded porosity using the freeze-tape casting process which can be tailored for fuel and air flow. Removing gas channels from the interconnect simplifies the stack design and allows the ceramic interconnect to be kept thin, on the order of 50 -100 microns. The YSZ electrode scaffolds are infiltrated with active electrode materials following the high temperature sintering step. The NASA-BSC is symmetrical and CTE matched, providing balanced stresses and favorable mechanical properties for vibration and thermal cycling.

Cable, Thomas L.↗

Characterization of Fluorescence Signals in Synthetic Anorthite

In-situ resource utilization (ISRU) is a key capability to enable a long term presence on the Moon and other planetary bodies. For example, efforts have been underway to develop processes to utilize the lunar regolith to produce building materials and extract useful resources. In processes that utilize the regolith directly to produce construction materials, such as in various sintering methods, characterizing the composition of the regolith is important as the composition can affect the optimal process parame-ters. In processes that involve extracting resources such as iron, oxygen, hydrogen, etc., identifying areas with higher abundance of a particular resource will be critical since different regions of the Moon exhibit differing regolith composition. To this end, Ra-man is one technique that can rapidly characterize the mineralogy of rock samples. This technique has al-ready been deployed on Mars to detect various miner-als including olivine, carbonates, phosphates, etc. Besides characterizing the mineralogy, Raman spectra often contain unwanted fluorescence signals that can mask Raman peaks. In some cases, the fluorescence signals are narrow enough to aid in the identification of specific elements in soils. In this work, we explore fluorescence peaks in a synthetic anorthite sample, which are at the same position as Ruby fluorescence peaks attributed to chromium. These fluorescence peaks, as well as similar fluorescence peaks attributed to other elements, could have important implications for ISRU and the mining of critical resources as has been previously described.

Raman Spectroscopy↗

Alternative Processing of High Temperature Hafnium and Zirconium Based Materials

The behavior of refractory hafnium and zirconium based materials are being investigated at NASA Ames as part of ongoing research aimed at developing superior heat resistant materials for aerospace applications. Hafnium and zirconium diboride based materials have shown high temperature capabilities in simulated reentry environments indicating that these materials may successfully operate as reusable oxidation resistant components for leading edge applications. Due to the refractory nature of these materials, processing of fine-grained uniform microstructures poses a number of challenges. To better understand the process-property-microstructure relationship, processing of these materials has been carried out with conventional hot pressing in addition to the novel approach of Spark Plasma Sintering (SPS). The two processing methods are compared and contrasted in an evaluation of the sintering behavior of high temperature diboride based materials and preliminary physical and mechanical properties are presented.

Gasch, Matthew↗

CEFAS Poster for Advanced Manufacturing Workshop 3/26/24

Electric-field assisted sintering (EFAS) is an advanced manufacturing method for the consolidation and processing of ceramic and metal materials. It is a particularly excellent candidate for efficient materials processing as it has greater than 90% energy cost savings and improved CO2 emissions compared to traditional sintering in a furnace. This is due to direct rapid heating of the materials and molds leveraging an electrification phenomenon called Joule heating where electrical current is passed through the sample/mold assemblies causing direct heating. The technique does have limitations though as it is traditionally a batch-process and suffers from scale up difficulties. To overcome this, researchers at Idaho National Laboratory changed the form factor of traditional EFAS instruments to develop and construct a continuous rolling electric-field assisted sintering (CEFAS) device.

36 MATERIALS SCIENCE↗

Flash Sintering of Oxide Ceramics under Microwave Heating

We report on the results of the analysis of the effect of flash sintering, which is observed upon heating compacted powder materials by high-intensity microwave radiation. Ceramic samples of Y{sub 2}O{sub 3}, MgAl{sub 2}O{sub 4}, and Yb: (LaO){sub 2}O{sub 3} were sintered to a density exceeding 98–99% of the theoretical value during 0.5–5 min without isothermal hold. The specific microwave power absorbed volumetrically in the samples was 20–400 W/cm{sup 3}. Based on the analysis of the experimental data (microwave radiation power and heating and cooling rates) and of the microstructure of the obtained materials, we propose a mechanism of flash sintering based on the evolution of the thermal instability and softening (melting) of the grain boundaries. The proposed mechanism also explains the flash sintering effect observed when a dc or a low-frequency ac voltage is applied to the samples. The microwave heating makes it possible to implement flash sintering without using electrodes for supplying energy to the articles being sintered.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis of nanocrystalline yttrium iron garnet by low temperature solid state reaction

In this work, nanocrystalline yttrium iron garnet powders were produced by low temperature solid state reaction. The phase evolution during the procedure was determined from the thermogravimetric and differential thermal analysis, and the x-ray diffraction patterns. The results of transmission electron microscopy indicated that the prepared powders exhibited grain size at the nano-level of 20 {approx} 40 nm. Dense ceramics with a theoretical density of around 98% were obtained from the prepared powders after sintering at 1280 deg. C, a relative low sintering temperature compared with conventional ceramic processes, and the saturation magnetizations of sintered samples were also determined. - Research Highlights: {yields}No sol or gel form during the synthesis processing using nitrates and citric acid as raw materials. {yields}The synthesis method needs a low heating temperature (700 deg. C) compared with conventional solid state reaction. {yields}The product is a single phase with homogeneous size distribution and nano grains (20 {approx} 40 nm) confirmed by TEM. {yields}Dense YIG ceramic can be sintered at a low temperature (1280 deg. C) compared with that in conventional processing.

36 MATERIALS SCIENCE↗

On the Origin of Sinter‐Resistance and Catalyst Accessibility in Raspberry‐Colloid‐Templated Catalyst Design

Abstract Nanoparticle (NP) sintering is a major cause of the deactivation of supported catalysts. Raspberry‐colloid‐templated (RCT) catalysts are an emerging class of materials that show an unprecedented level of sinter‐resistance and exhibit high catalytic activity. Here a comprehensive study of the origin of NP stability and accessibility in RCT catalysts using theoretical modeling, 3D electron microscopy, and epitaxial overgrowth is reported. The approach is showcased for silica‐based RCT catalysts containing dilute Pd‐in‐Au NPs previously used in hydrogenation and oxidation catalysis. Modeling of the contact line of the silica precursor infiltrating into the assembled raspberry colloids suggests that a large part of the particles must be embedded into silica, which is confirmed by quantitative visualization of >200 individual NPs by dual‐axis electron tomography. The RCT catalysts have a unique structure in which all NPs reside at the pore wall but have >50% of their surface embedded in the matrix, giving rise to the strongly enhanced thermal and mechanical stability. Importantly, epitaxial overgrowth of Ag on the supported NPs reveals that not only the NP surface exposed to the pore but the embedded interface as well remained chemically accessible. This mechanistic understanding provides valuable guidance in the design of stable catalytic materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Porosity and mechanical properties of zirconium ceramics

Has been studied a porous ceramics obtained from ultra-fine powders. Porous ceramic ZrO{sub 2}(MgO), ZrO{sub 2}(Y{sub 2}O{sub 3}) powder was prepared by pressing and subsequent sintering of compacts homologous temperatures ranging from 0.63 to 0.56 during the isothermal holding duration of 1 to 5 hours. The porosity of ceramic samples was from 15 to 80%. The structure of the ceramic materials produced from plasma-sprayed ZrO{sub 2} powder was represented as a system of cell and rod structure elements. Cellular structure formed by stacking hollow powder particles can be easily seen at the images of fracture surfaces of obtained ceramics. There were three types of pores in ceramics: large cellular hollow spaces, small interparticle pores which are not filled with powder particles and the smallest pores in the shells of cells. The cells generally did not have regular shapes. The size of the interior of the cells many times exceeded the thickness of the walls which was a single-layer packing of ZrO{sub 2} grains. A distinctive feature of all deformation diagrams obtained in the experiment was their nonlinearity at low deformations which was described by the parabolic law. It was shown that the observed nonlinear elasticity for low deformation on deformation diagrams is due to mechanical instability of the cellular elements in the ceramic carcass.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Optimization of Structurally Enhanced Solder Transient Liquid Phase Bonding

High temperature packaging technologies are a necessity for high temperature capable devices. SAC305 solder has an operational limit of 174°C imposed by creep effects which aligns well with current junction temperature limits of 175°C. Wide band gap semiconductor materials have the potential to reach junction temperatures of up to 800°C that are not currently attainable with significant reliability. Capitalizing on this potential will requires substrates and attachments that can operate well beyond the current 175°C standard. Silver sintering pastes have received widespread interest as a high temperature attachment alternative. However, the process requires high pressure bonding in an inert environment to achieve acceptable bond quality. Transient liquid phase (TLP) sintering is capable of good bond quality without pressure requirements but suffers from low thermal conductivity and only slightly reduced cost compared to silver sintering. SAC305 solder contains the same constituent materials for TLP as available copper-tin TLP sintering paste. By introducing engineered surface structures into the bond, intermetallic formation can be accelerated producing a bond similar to TLP sintering but in an ambient environment and for reduced cost. While this process has been demonstrated, it has not yet been optimized. Currently bonds are formed using a 75 μm stencil on substrate surface structures 24 μm tall, covering 19% of the bonding area. The process takes about 4 hours not including the formation of surface structures. Here, this study will center on the effects of stencil thickness and coating methods. Samples will be analyzed by scanning acoustic microscopy, die shear testing and cross sectional scanning acoustic microscopy.

42 ENGINEERING↗

Compositional inhomogeneity and its effect on the hardness of nanostructured refractory high-entropy alloys

The pronounced compositional inhomogeneity observed in refractory high-entropy alloys (HEAs), as opposed to non-refractory HEAs, has an important influence on their mechanical properties, thereby posing a significant challenge for the development of high-performance refractory HEAs. In this work, by combining transmission electron microscopy imaging, chemical analysis, and nano-hardness tests, we investigate the compositional inhomogeneities in a series of sintered nanostructured HEAs and elucidate their influence on the material's hardness. Further, we reveal that the compositional inhomogeneity of the sintered nanostructured HEAs is temperature- and component- dependent. By correlating the hardness of nanostructured HEAs to the evolving compositional inhomogeneity, our work demonstrates that the compositional inhomogeneity in nanostructured HEAs can be tuned by sintering temperature or alloying towards optimized microstructure and hardness.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Determination of total chlorine and bromine in solid wastes by sintering and inductively coupled plasma-sector field mass spectrometry

A sample preparation method based on sintering, followed by analysis by inductively coupled plasma-sector field mass spectrometry (ICP-SFMS) for the simultaneous determination of chloride and bromide in diverse and mixed solid wastes, has been evaluated. Samples and reference materials of known composition were mixed with a sintering agent containing Na{sub 2}CO{sub 3} and ZnO and placed in an oven at 560 deg. C for 1 h. After cooling, the residues were leached with water prior to a cation-exchange assisted clean-up. Alternatively, a simple microwave-assisted digestion using only nitric acid was applied for comparison. Thereafter the samples were prepared for quantitative analysis by ICP-SFMS. The sintering method was evaluated by analysis of certified reference materials (CRMs) and by comparison with US EPA Method 5050 and ion chromatography with good agreement. Median RSDs for the sintering method were determined to 10% for both chlorine and bromine, and median recovery to 96% and 97%, respectively. Limits of detection (LODs) were 200 mg/kg for chlorine and 20 mg/kg for bromine. It was concluded that the sintering method is suitable for chlorine and bromine determination in several matrices like sewage sludge, plastics, and edible waste, as well as for waste mixtures. The sintering method was also applied for determination of other elements present in anionic forms, such as sulfur, arsenic, selenium and iodine.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Coupling between interfacial charge and mechanical deformation at high temperatures in ceramics. Final report

Basic research, under this project, has led to new fundamental discoveries in the effect of electric field (and temperature) on diffusion kinetics, electroluminescence and electronic conductivity in ceramic materials. For example, yttria stabilized zirconia sinters in just seconds well below 1000°C, while, at the same time, exhibiting a highly non-linear rise in conductivity, and intense electroluminescence. The phenomenon has been shown to occur in nearly all ceramics whether they are ionic or electronic conductors, or insulators. The rise in conductivity leads to Joule heating but in-situ measurements with a platinum standard at APS and Brookhaven (NSLS-II) have shown that the temperatures are much below what would have been needed to sinter in a few seconds. We have explored the hypothesis that huge concentrations of Frenkel pairs of vacancies and interstitials are produced. While these point defects accelerate sintering (by the interstitials being transported to the pores and the vacancies to the grain boundaries), they may also produce electron-hole pairs which can impart high electrical conductivity or recombine to emit photons. Many measurements, including in-situ measurements of lattice expansion are consistent with this hypothesis. However, the energy barrier for generating Frenkels in zirconia for example is much larger than can be expected at temperature and electrical fields in these experiments. Most recent work suggests that short wavelength phonons play a critical role in the genesis of the “flash” phenomenon. For example, the Debye temperature has been shown to be the lower bound for initiating flash. Molecular dynamics simulations have shown that large concentrations of Frenkel pairs can form under the proliferation of “optical” phonons at the edge of the Brillouin zone, that is with a wavelength at or below the lattice parameter. This project has led to the development of new experimental techniques as well as a software hardware interface for process and control and data analysis in real time, with a time scale of less than one second. This approach spells a new paradigm in materials science research. It potential impact on high rate manufacturing is self evident.

36 MATERIALS SCIENCE↗

Development of direct ink write radially graded alumina/zirconia

Functionally graded materials (FGMs) are of interest in multiple fields, yet many materials combinations are limited by coefficient of thermal expansion (CTE) mismatch. Here, a radially graded alumina/yttria-doped zirconia (Al 2 O 3 /8YZ) FGM is used to demonstrate processing strategies to mitigate CTE and sintering behavior differences between these oxides. FGM materials are especially sensitive to ink stability during printing, as all components (in this case, Al 2 O 3 and 8YZ) must be stabilized in the same dispersant or additive solution. Thus, this system is also ideal to demonstrate ink optimization best practices. Materials were characterized throughout processing to correlate the effects of common additives on both the ceramic particle suspensions and final sintered components. Aggregation observed in the initial additive-containing suspensions were present in the sintered component. The differences in sintering onset temperature and shrinkage rate resulted in internal stresses within the sintered component, which ultimately caused mechanical failure of the component under low stress. In conclusion, a processing strategy was recommended to mitigate the sintering behavior mismatch of alumina and 8 wt% yttria-stabilized zirconia.

Lamm, Benjamin W. [Oak Ridge National Laboratory (↗

Processing of Sintered Mo Disks Using Hydrogen Peroxide

Dissolution studies performed on NorthStar and ORNL disks show that an increase in sintering temperature has a negative effect on dissolution rates in 30% hydrogen peroxide. This is due to changes in the microstructure of sintered Mo powder. At higher sintering temperatures, the powder particles coalesce, form diffusion bonds, and grow into larger grains, which reduce the open porosity of the disks. The remaining porosity becomes trapped within the grains, and therefore the dissolution rates are very low. We also observed that different starting materials lead to different dissolution properties, and in some cases, even high sintering temperature at 1600°C does not produce disks with high packing densities. Studies with NorthStar disks showed that increased packing density can be achieved by increased pressing conditions without affecting the dissolution rates if mild sintering conditions are used. Future experiments will focus on producing sintered Mo disks produced from recovered Mo material and on optimizing the sintering process to produce disks with >90% packing density and good dissolution rates.

Dissolution↗

Electrical and optical properties of NdAlO{sub 3} synthesized by an optimized combustion process

Nanocrystals of neodymium aluminate (NdAlO{sub 3}) are synthesized using an optimized single step auto-ignition citrate complex combustion process. The combustion product was characterized by X-ray diffraction, transmission electron microscopy, Fourier transform infrared spectroscopy, Raman spectroscopy and Ultraviolet–visible reflection spectroscopy. The combustion product is single phase and composed of aggregates of nanocrystals of sizes in the range 20–40 nm. The NdAlO{sub 3} crystallized in rhombohedral perovskite structure with lattice parameters a = 5.3223 Å and c = 12.9292 Å. The absorption spectrum of the NdAlO{sub 3} nanocrystals shows characteristic absorption bands of the Nd atom. The polycrystalline fluffy combustion product is sintered to high density (∼ 97%) at ∼ 1450 °C for 4 h and the microstructure was characterized by scanning electron microscopy. The electrical properties of the sintered product were studied using dielectric measurements. The sintered NdAlO{sub 3} has a dielectric constant (ε{sub r}) and a dielectric loss (tan δ) of 21.9 and ∼ 10{sup −3} at 5 MHz, respectively. - Highlights: • NdAlO{sub 3} nanocrystals were synthesized through a citrate combustion process. • The nanocrystals were sintered to ∼ 97% of theoretical density. • The materials were characterized using a number of analytical techniques. • Nanostructured NdAlO{sub 3} showed crystal field splitting of Nd ions. • Dielectric properties of the sintered NdAlO{sub 3} ceramics were studied.

36 MATERIALS SCIENCE↗

Thermochemically evolved nanoplatelets of bismuth selenide with enhanced thermoelectric figure of merit

We firstly present a simple thermochemical method to fabricate high-quality Bi{sub 2}Se{sub 3} nanoplatelets with enhanced figure of merit using elemental bismuth and selenium powders as precursors. The crystal structure of as synthesized products is characterized via X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and high resolution transmission electron microscopy (HRTEM) measurements. Morphological and chemical synthetic parameters are investigated through a series of experiments; thickness and composition of the platelets are well controlled in large scale production. Subsequently spark plasma sintering (SPS) is performed to fabricate n-type nanostructured bulk thermoelectric materials. Raman Spectroscopy of the two selected samples with approximately of 50 and 100 nm thicknesses shows three vibrational modes. The lower thickness sample exhibits the maximum red shift of about 2.17 cm{sup -1} and maximum broadening of about 10 cm{sup -1} by in-plane vibrational mode E{sup 2}{sub g}. The enhanced value of figure of merit ∼0.41 is obtained for pure phase bismuth selenide to the best of our knowledge. We observe metallic conduction behavior while semiconducting behavior for nanostructured bismuth selenide is reported elsewhere which could be due to different synthetic techniques adopted. These results clearly suggest that our adopted synthetic technique has profound effect on the electronic and thermoelectric transport properties of this material.

36 MATERIALS SCIENCE↗

Densification, microstructure and properties of TiB2 ceramics fabricated by spark plasma sintering

Highlights: • Nearly full densification of in-house processed TiB{sub 2} ceramic powders at 1500 °C. • Microstructures revealing the size and shape of TiB{sub 2} grains after SPS. • The effect of sub-micron particles on the densification during SPS. • The effect of sintering pressure on the microstructure. • Microhardness and nano-indentation measurements along with oxidation studies. - Abstract: This study reports the fabrication of high-density TiB{sub 2} ceramics at reduced temperatures (1500 °C) by using field assisted sintering technology/spark plasma sintering (FAST/SPS) technique. In-house processed TiB{sub 2} powders with high purity were employed as starting materials. The effects of SPS conditions on the sintering behavior and microstructure of TiB{sub 2} were investigated. Sub-micron character of TiB{sub 2} particles has a strong influence on the densification during SPS. Microstructural analyses revealed that the high pressure affected both the grain size and the shape of TiB{sub 2} crystallites. Elongated grains with average size of 6 μm were perceived in TiB{sub 2} sample fabricated by SPS at 1500 °C under 60 MPa pressure with a relative density of 96.7%. The microhardness and elastic modulus were measured as 27.4 GPa and 685.2 GPa, respectively. This sample revealed an improved oxidation resistance due to the formation of a thin oxidation layer on the surface when heated up to 1200 °C.

36 MATERIALS SCIENCE↗