At least 469 records · Page 26

The Active Oxidation of Silicon Carbide

The high temperature oxidation of silicon carbide occurs in two very different modes. Passive oxidation forms a protective oxide film which limits further attack of the SiC: SiC(s) + 3/2 O2(g) = SiO2(s) + CO(g) Active oxidation forms a volatile oxide and may lead to extensive attack of the SiC: SiC(s) + O2(g) = SiO(g) + CO(g) Generally passive oxidation occurs at higher oxidant pressures and active oxidation occurs at lower oxidant pressures and elevated temperatures. Active oxidation is a concern for reentry, where the flight trajectory involves the latter conditions. Thus the transition points and rates of active oxidation are a major concern. Passive/active transitions have been studied by a number of investigators. An examination of the literature indicates many questions remain regarding the effect of impurity, the hysteresis of the transition (i.e. the difference between active-to-passive and passive-toactive), and the effect of total pressure. In this study we systematically investigate each of these effects. Experiments were done in both an alumina furnace tube and a quartz furnace tube. It is known that alumina tubes release impurities such as sodium and increase the kinetics in the passive region [1]. We have observed that the active-to-passive transition occurs at a lower oxygen pressure when the experiment is conducted in alumina tubes and the resultant passive silica scale contains sodium. Thus the tests in this study are conducted in quartz tubes. The hysteresis of the transition has been discussed in the detail in the original theoretical treatise of this problem for pure silicon by Wagner [2], yet there is little mention of it in subsequent literature. Essentially Wagner points out that the active-to-passive transition is governed by the criterion for a stable Si/SiO2 equilibria and the passive-to-active transition is governed by the decomposition of the SiO2 film. A series of experiments were conducted for active-to-passive and passive-to-active transitions by increasing and decreasing oxygen pressure, respectively. For pure silicon a dramatic difference was found; whereas for SiC the difference was not as great. This may be due to the oxidation of the carbon in SiC which may break down the scale [3]. The third area is the effect of total pressure. In the literature, low oxygen potentials are achieved via either low total pressure or low oxygen pressure in an O2/Ar mixture. Both types of experiments are done in this study and the differences are discussed with regard to the presence or absence of a boundary layer.

Jacobson, Nathan S.↗

Synthesis and optical properties of antimony oxide glasses doped with holmium trioxide

Holmium doped lithium-antimony-lead borate glasses having 1 mol% AgNO{sub 3} with composition 50B{sub 2}O{sub 3}-20PbO-25Sb{sub 2}O{sub 3}-5Li{sub 2}O have been prepared using single step melt quenching technique. The XRD spectrum confirms amorphous nature of glasses. The optical absorbance studies were carried out on these glasses. The optical direct band gap energies were found to be in the range of 3.10 eV to 3.31 eV and indirect band gap energies were found to be in the range of 2.28 eV to 3.00 eV. The refractive indexes have been calculated by using Lorentz-Lorenz formula and the calculated values in the range of 2.31 to 2.37.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Oxidation of low cobalt alloys

Four high temperature alloys: U-700, Mar M-247, Waspaloy and PM/HIP U-700 were modified with various cobalt levels ranging from 0 percent to their nominal commercial levels. The alloys were then tested in cyclic oxidation in static air at temperatures ranging from 1000 to 1150 C at times from 500 to 100 1 hour cycles. Specific weight change with time and X-ray diffraction analyses of the oxidized samples were used to evaluate the alloys. The alloys tend to be either Al2O3/aluminate spinel or Cr2O3/chromite spinel formers depending on the Cr/Al ratio in the alloy. Waspaloy with a ratio of 15:1 is a strong Cr2O3 former while this U-700 with a ratio of 3.33:1 tends to form mostly Cr2O3 while Mar M-247 with a ratio of 1.53:1 is a strong Al2O3 former. The best cyclic oxidation resistance is associated with the Al2O3 formers. The cobalt levels appear to have little effect on the oxidation resistance of the Al2O3/aluminate spinel formers while any tendency to form Cr2O3 is accelerated with increased cobalt levels and leads to increased oxidation attack.

Barrett, C. A.↗

Composition dependent spectroscopic properties of Nd{sup 3+} doped sodium lead borate glasses

Nd{sup 3+} doped oxide glasses of the type xNa{sub 2}O–30 PbO–(69.5-x) B{sub 2}O{sub 3}–0.5Nd{sub 2}O{sub 3} were prepared and investigated for physical and spectroscopic properties. Optical absorption spectra and Judd-Ofelt theory has been used to determine the oscillator strengths and the intensity parameters Ω{sub λ} (λ=2, 4, 6). The radiative transition probability (A), radiative lifetime (τ{sub R}) and branching ratio (β{sub R}) for the fluorescent levels of Nd{sup 3+} in the prepared glasses have been determined. The lasing efficiency of the prepared glasses has been characterized by the spectroscopic quality factor (Ω{sub 4} / Ω{sub 6}), the value of which is in the range 0.2-1.5, typical for Nd{sup 3+} in different laser hosts. The radiative transition probability of the potential lasing transition {sup 4}F{sub 3/2} → {sup 4}I{sub 11/2} of Nd{sup 3+} ions is found to increase with increase in content of Na{sub 2}O.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Analysis of iron-chromium-aluminum samples exposed to accident conditions followed by quench in the QUENCH-19 experiment

The QUENCH-19 experiment was a first-of-its-kind full-bundle test simulating accident conditions followed by water quench on accident-tolerant fuel (ATF) cladding. Here, a type of FeCrAl(Y) alloy, B136Y3, was developed at Oak Ridge National Laboratory and tested at the Karlsruhe Institute of Technology using Kanthal APM corner rods, a shroud, and Kanthal AF spacer grids. Testing conditions were similar to those in QUENCH-15—which tested ZIRLO cladding behavior—so that B136Y3 and ZIRLO cladding could be compared. QUENCH-19 consisted of an initial pre-oxidation heating followed by a transient. Then, a maximum power hold, which was not present in QUENCH-15, was executed to extend the heating period for the FeCrAl(Y) rods. Finally, a rapid water quench was executed that was similar to emergency core coolant system (ECCS) actuation. Compared with the ZIRLO rods in QUENCH-15, the bundle in QUENCH-19 released significantly less H 2 (9.2 g vs. 47.6 g) and achieved a much lower maximum temperature (1455°C vs. 1880°C). Furthermore, no breakaway oxidation was observed in QUENCH-19. Metallographic mounts revealed that despite the symmetry of the setup, at elevations near the maximum temperature, cladding and thermocouples were heavily damaged, substantial melting and oxidation occurred, and the cladding underwent chemical interaction with the thermocouple sheaths. Additionally, the ZrO 2 spacers detrimentally interacted with the cladding, leading to mixed oxide debris and the full destruction of some rods. Additional failure was found in certain cooler rods that may have risen due to the high thermal expansion coefficient of FeCrAl alloys. This paper presents an analysis of this work, which suggests that FeCrAl cladding can chemically survive anticipated loss-of-coolant accident events followed by rapid ECCS quench if the correct geometry and core design are present.

36 MATERIALS SCIENCE↗

Understanding the Deactivation of Ag–ZrO 2 /SiO 2 Catalysts for the Single-step Conversion of Ethanol to Butenes

Ag–ZrO 2 /SBA-16 has recently been found to be efficient for catalyzing the single-step conversion of ethanol to butene (1- and 2-butene mixtures) in the presence of H 2 . The reaction proceeds via a cascading sequence of reactions over mixed metal and Lewis sites, with the catalyst composition tuned to selectively favor butene formation. However, the catalyst slowly deactivates when evaluated over long reaction times. Here, we evaluated the lifetime of the Ag–ZrO 2 /SBA-16 catalyst system for ethanol-to-butene conversion at 325 °C for up to 800 hours on stream. Several characterization techniques were used to elucidate the mechanism(s) by which catalyst deactivation occurs. Coke deposition, Ag particle sintering, and Ag 0 -to-Ag + oxidation state change were identified to be the major causes of catalyst deactivation. Coke deposits cover primarily Lewis acid sites which are responsible for aldol condensation, Meerwein-Ponndorf-Verley (MPV) reduction, and dehydration reactions. Ag particle sintering and Ag oxidation state change leads to a reduction in the number of metallic Ag sites responsible for the dehydrogenation/hydrogenation steps. The fresh catalyst likely experiences hydrothermal sintering in the early stage of reaction and permanently loses some active Lewis acid sites before reaching a new structural steady state. The deactivation of Lewis acid sites leads to a decrease in overall ethanol conversion, whereas the deactivation of the metallic Ag sites decreases the butene selectivity. For catalyst regeneration, oxidative calcination (at 500 °C) followed by reduction (at 325 °C) successfully removes all the coke species on the catalyst surface and restores the metallic Ag particles of the 4Ag–4ZrO 2 /SBA-16 catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Macroscopic and microscopic behaviors of Mn(II) (ad)sorption to goethite with the effects of dissolved carbonates under anoxic conditions

Manganese and its compounds have been extensively researched because of their far-reaching roles in a wide range of biogeochemical processes in natural systems. The (ad)sorption behavior of Mn(II), however, is poorly understood despite its important role as the primary reaction step for surface-catalyzed Mn(II) oxidation that is the principal abiotic process forming various Mn (oxyhydr)oxides in nature. Here, we systematically examined Mn(II) (ad)sorption to one of the most common natural sorbents, goethite, in oxygen- and carbonate-free systems. Traditional sorption edge and isotherm experiments were conducted by varying sorbate-to-sorbent ratio (0.027–15 μmol∙m -2 ) and solution pH (pH 5.0–9.0). The effects of dissolved carbonates on Mn(II) sorption were also assessed in a range of naturally prevalent concentrations (0.5–10 mM NaHCO 3 ). The Mn(II) uptake on goethite followed a typical Langmuir isotherm in the absence of dissolved carbonates, with increasing maximum adsorption capacities (Γ max ) from 0.19 at pH 6.5 to 3.4 μmol∙m -2 at pH 9.0. The presence of dissolved carbonates raised the extent of Mn(II) adsorption, which appeared to be directly correspondent to that of the adsorption of dissolved carbonates. Extended X-ray absorption fine structure (EXAFS) analysis indicated that Mn(II) predominantly formed inner-sphere binuclear bidentate surface complexes. Mn(II) uptake became deviated from the Langmuir model and showed a clear indication of surface precipitation when the Mn(II) sorption density (Γ) exceeded a threshold value in a given solution composition. This secondary Mn(II) phase was identified as rhodochrosite using X-ray diffraction (XRD) and transmission electron microscope (TEM). Furthermore, it would be plausible that a minor fraction of adsorbed Mn(II) coexisted with the secondary rhodochrosite according to a linear combination fitting (LCF) of the X-ray absorption near edge structure (XANES) spectra of Mn reference and samples. These systematic investigations of the macroscopic and microscopic behaviors of Mn(II) (ad)sorption to goethite provide a critical avenue for disentangling surface-catalytic Mn(II) oxidation processes, which ultimately lead to the formation of diverse Mn (oxyhydr)oxides in the environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Enhancing nitrogen fixation efficiency in glow-like discharge by reducing cathode-fall voltage

In plasma nitrogen fixation devices, discharge electrodes are crucial yet susceptible to oxidation and corrosion due to plasma’s high temperatures and oxygen content, which could alter discharge modes. This research evaluates the impact of different electrode materials, including iron, chromium, nickel, copper, and 304 stainless steel, on nitrogen fixation efficiency in glow-like discharges driven by high-voltage DC power. Notably, iron and 304 stainless steel cathodes undergo a mode transition at increased currents, evident from plasma color shifts and significant voltage reductions. Fourier transform infrared spectroscopy analyses reveal that such mode changes minimally affect nitrogen oxide production rates, leading to a notable decrease in energy consumption for nitrogen fixation by up to 40%. OES and SEM-EDS measurements suggest that iron oxide, with its higher secondary electron emission, replaces metal as the cathode material, facilitating mode transitions and maintaining discharge current at lower voltages. Further, this voltage change is largely attributed to the cathode voltage drop, highlighting the minimal role of the cathode fall region in NO x synthesis. These findings underscore the potential for improving plasma nitrogen fixation energy efficiency by choosing suitable cathode materials to lower the cathode-fall voltage.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Kinetics and mechanism of corrosion of SiC by molten salts

Corrosion of sintered alpha-SiC under thin films of Na2CO3/CO2, Na2SO4/O2, and Na2SO4/SO3 was investigated at 1000 C. Chemical analysis was used to follow silicate and silica evolution as a function of time. This information coupled with morphology observations leads to a detailed corrosion mechanism. In all cases the corrosion reactions occur primarily in the first few hours. In the Na2CO3/CO2 case, rapid oxidation and dissolution lead to a thick layer of silicate melt in about 0.25 h. After this, silica forms a protective layer on the carbide. In the Na2SO4/O2 case, a similar mechanism occurs. In the Na2SO4/SO3 case, a porous nonprotective layer of SiO2 grows directly on the carbide, and a silicate melt forms above this. In addition, SiO2 and regenerated Na2SO4 form at the melt/gas interface due to reaction of silicate with SO3 and SO2 + O2. The reaction slows when the lower silica layer becomes nonporous.

Jacobson, N. S.↗

A More Reduced Mantle Source for Enriched Shergottites; Insights from the Olivine-Phyric Shergottite Lar 06319

A detailed petrographic study of melt inclusions and Cr-Fe-Ti oxides of LAR 06319 leads to two main conclusions: 1) this enriched oxidized olivine- phyric shergottite represents nearly continuous crystallization of a basaltic shergottite melt, 2) the melt became more oxidized during differentiation. The first crystallized mineral assemblages record the oxygen fugacity which is closest to that of the melt s mantle source, and which is lower than generally attributed to the enriched shergottite group.

Peslier, A. H.↗

Rock-Salt Growth-Induced (003) Cracking in a Layered Positive Electrode for Li-Ion Batteries

For the first time, the (003) cracking is observed and determined to be the major cracking mechanism for the primary particles of Ni-rich layered dioxides as the positive electrode for Li-ion batteries. Using transmission electron microscopy techniques, here we show that the propagation and fracturing of platelet-like rock-salt phase along the (003) plane of the layered oxide are the leading cause for the cracking of primary particles. The fracturing of the rock-salt platelet is induced by the stress discontinuity between the parent layered oxide and the rock-salt phase. The high nickel content is considered to be the key factor for the formation of the rock-salt platelet and thus the (003) cracking. The (003)-type cracking can be a major factor for the structural degradation and associated capacity fade of the layered positive electrode.

Environmental Molecular Sciences Laboratory↗

Improvement of plasmonic enhancement of quantum dot emission via an intermediate silicon-aluminum oxide interface

We studied the emission of quantum dots in the presence of plasmon-metal oxide substrates, which consist of arrays of metallic nanorods embedded in amorphous silicon coated with a nanometer-thin layer of aluminum oxide on the top. We showed that the combined effects of plasmons and the silicon-aluminum oxide interface can lead to significant enhancement of the quantum efficiency of quantum dots. Our results show that such an interface can significantly enhance plasmonic effects of the nanorods via quantum dot-induced exciton-plasmon coupling, leading to partial polarization of the quantum dots' emission.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Solvent-free bottom-up patterning of zeolitic imidazolate frameworks

Patterning metal-organic frameworks (MOFs) at submicrometer scale is a crucial yet challenging task for their integration in miniaturized devices. Here we report an electron beam (e-beam) assisted, bottom-up approach for patterning of two MOFs, zeolitic imidazolate frameworks (ZIF), ZIF-8 and ZIF-67. A mild pretreatment of metal oxide precursors with linker vapor leads to the sensitization of the oxide surface to e-beam irradiation, effectively inhibiting subsequent conversion of the oxide to ZIFs in irradiated areas, while ZIF growth in non-irradiated areas is not affected. Well-resolved patterns with features down to the scale of 100 nm can be achieved. This developer-free, all-vapor phase technique will facilitate the incorporation of MOFs in micro- and nanofabrication processes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Study of the oxidation effects on isothermal solidification based high temperature stable Pt/In/Au and Pt/In/Ag thick film interconnections on LTCC substrate

The objective of the presented paper is to determine the oxidized phase compositions of indium lead-free solders during solidification at 190 ° C under room environment with the help of X-ray diffraction (XRD) and Energy dispersive spectroscopy (EDX). Many lead-free solders alloys available oxidizes and have poor wetting properties. The oxidation of pure indium solder foil, Au, Pt, and Ag alloys were identified and investigated, in the process of isothermal solidification based solder joints construction at room environment and humidity. Both EDX and XRD characterization techniques were performed to trace out the amount of oxide levels and variety of oxide formations at solder interface respectively. The paper also aims to report the isothermal solidification technique to provide interconnections to pads on Low temperature co-fired ceramic (LTCC) substrate. It also elaborates advantages of isothermal solidification over the other methods of interconnection. Scanning electron microscope (SEM) used to identify the oxidized spots on the surface of Pt, Ag substrates and In solder. The identified oxides were reported.

36 MATERIALS SCIENCE↗

Effect of pH on Structural Changes in Perch Hemoglobin that Can Alter Redox Stability and Heme Affinity

pH can be manipulated to alter the oxidative stability of fish-based foods during storage. X-ray diffraction was used to investigate the ability of reduced pH to cause structural changes in fish hemoglobins that lead to enhanced oxidative degradation. Decreasing pH from 8.0 to 6.3 and 5.7 created a large channel for solvent entry into the heme crevice of perch hemoglobin beta chains. The proton-induced opening of this channel occurred between site CD3 and the heme-6-propionate. Solvent entry into the heme crevice can enhance metHb formation and hemin loss, processes that accelerate lipid oxidation. Reduced pH also decreased the distance between Ile at E11 in one of the alpha chains and the ligand above the heme iron atom. This sterically displaces O{sub 2} and protonated O{sub 2} which increases metHb formation. These studies demonstrate that pH reduction causes structural changes in perch hemoglobin which increase oxidative degradation of the heme pigment.

59 BASIC BIOLOGICAL SCIENCES↗

Electro–Oxidation of Nitroxide Radicals: Adsorption–Mediated Charge Transfer Probed Using SERS and Potentiometry

Organic compounds containing nitroxide radicals such as 4–hydroxy–2,2,6,6–tetramethylpiperidine–1–oxyl (4–hydroxy–TEMPO) are redox–active and are of interest for potential applications in redox flow batteries. The mechanisms governing charge–transfer reactions of such compounds are not well understood. Specifically, the anodic charge transfer coefficient (αa) corresponding to the electro–oxidation of 4–hydroxy–TEMPO in an aqueous medium is ~0.9, i.e., αa deviates considerably from the expected value (0.5) for a symmetric single–step one–electron transfer redox reaction. In a previous publication (J. Electrochem. Soc., 2020, 167, 143505), we have proposed a reaction mechanism to explain such asymmetric behavior by invoking adsorption–desorption processes. In the proposed mechanism, reversible oxidation of 4–hydroxy–TEMPO leads to the adsorption of the oxidation product, which then undergoes slow rate–limiting desorption from the electrode surface. In the present contribution, supporting evidence is provided for this mechanism. In situ surface–enhanced Raman spectroscopy combined with density functional theory simulations are employed to confirm the presence of surface–adsorbed species at a Au electrode during electro–oxidation of 4–hydroxy–TEMPO. Furthermore, we employ chronopotentiometry to track the gradual re–equilibration of the electrode–electrolyte interface following the electro–oxidation of 4–hydroxy–TEMPO. Analysis of the chronopotentiometry data further suggests the presence of adsorbed species, which were previously proposed and are now confirmed by direct spectroscopic evidence.

25 ENERGY STORAGE↗

Biospheric-atmospheric coupling on the early Earth

Theoretical calculations performed with a one-dimensional photochemical model have been performed to assess the biospheric-atmospheric transfer of gases. Ozone reached levels to shield the Earth from biologically lethal solar ultraviolet radiation (220-300 nm) when atmospheric oxygen reached about 1/10 of its present atmospheric level. In the present atmosphere, about 90 percent of atmospheric nitrous oxide is destroyed via solar photolysis in the stratosphere with about 10 percent destroyed via reaction with excited oxygen atoms. The reaction between nitrous oxide and excited oxygen atoms leads to the production of nitric oxide in the stratosphere, which is responsible for about 70 percent of the global destruction of oxygen in the stratosphere. In the oxygen/ozone deficient atmosphere, solar photolysis destroyed about 100 percent of the atmospheric nitrous oxide, relegating the production of nitric oxide via reaction with excited oxygen to zero. Our laboratory and field measurements indicate that atmospheric oxygen promotes the biogenic production of N2O and NO via denitrification and the biogenic production of methane by methanogenesis.

Levine, J. S.↗