Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Corrosion Protection”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 469 records · Page 26

Surface effects of corrosive media on hardness, friction, and wear of materials

Hardness, friction, and wear experiments were conducted with magnesium oxide exposed to various corrosive media and also with elemental iron and nickel exposed to water and NaOH. Chlorides such as MgCl2 and sodium containing films were formed on cleaved magnesium oxide surfaces. The MgCl2 films softened the magnesium oxide surfaces and caused high friction and great deformation. Hardness was strongly influenced by the pH value of the HCl-containing solution. The lower the pH, the lower the microhardness. Neither the pH value of nor the immersion time in NaOH containing, NaCl containing, and HNO3 containing solutions influenced the microhardness of magnesium oxide. NaOH formed a protective and low friction film on iron surfaces. The coefficient of friction and the wear for iron were low at concentrations of NaOH higher than 0.01 N. An increase in NaOH concentration resulted in a decrease in the concentration of ferric oxide on the iron surface. It took less NaOH to form a protective, low friction film on nickel than on iron.

Miyoshi, K.↗

Role of EIS in Materials and Coatings Selection for NASA's Launch Facilities

Corrosion studies began at NASA's John F. Kennedy Space Center (KSC) in 1966, during the Gemini/Apollo Programs, with the evaluation of long-term anti-corrosion coatings for carbon steel structures. NASAIKSC's Atmospheric Exposure Test Site was established at that time on the beach near the launch pad. In the years that followed, numerous studies at the site have identified materials, coatings, and maintenance procedures for launch hardware and equipment exposed to the highly corrosive environment at the launch pad. The atmosphere at the launch pad is highly corrosive due to the proximity of the Atlantic Ocean, high heat from rocket exhaust, and since the introduction of the Space Shuttle, the acidic combustion products of the Solid Rocket Boosters (SRBs). Currently, NASAIKSC maintains about $2 billion worth of unique equipment and facilities, not including the orbiters, each valued at about $1.8 billion. Among the items: two launch complexes, two crawler transporters, three mobile launch platforms, and specialized testing equipment. Atmospheric exposure provides very valuable data but it takes a long time and relies on human visual inspection. NASA Technical Standard for Protective Coatings requires 18 months of good performance at the Atmospheric Exposure Test Site for preliminary approval and continued good performance for 5 years for final approval of a coating system. The use of electrochemical impedance spectroscopy (EIS) was introduced at KSC in 1989 as a supplement to the traditional dc electrochemical techniques and atmospheric exposure studies. This paper presents and overview of several projects in which EIS was used in order to select materials and coatings to be used at NASA's launch facilities [1-2].

Calle, Luz Marina↗

Study of the effects of gaseous environments on sulfidation attack of superalloys

Studies were conducted to examine the effect of the gaseous corrodents NaCl, HCl, and NaOH on the high temperature oxidation and Na2SO4-induced corrosion behavior of the alumina former NiAl, the chromia former Ni-25 wt.% Cr, elemental Cr, and the superalloy B-1900. Experiments were conducted at 900 and 1050 C in air in the presence and absence of the gaseous corrodents. Effects involving both reaction rates and microstructural changes in oxide morphology were observed due to the presence of these corrodents at levels anticipated to be present in operating industrial and marine gas turbines. The effect of gaseous NaCl, HCl, and possibly NaOH on NiAl in simple oxidation was to remove aluminum from below the protective alumina layer and to simultaneously weaken the adherence of the protective alumina oxide scale to the substrate. The aluminum removed from below the oxide scale was redeposited on its surface as alpha-Al2O3 whiskers. With respect to the chromia formers, gaseous NaCl and HCl promoted breakaway oxidation kinetics and changes in the microstructures of the oxide scales.

Smeggil, J. G.↗

Lightning Protection and Structural Bonding for the B2 Test Stand

With the privatization of the space industry, NASA has entered a new era. To explore deeper parts of the solar system, NASA is developing a new spacecraft, the Space Launch System (SLS), capable of reaching these destinations, such as an asteroid or Mars. However, the test stand that is capable of testing the stage has been unused for many years. In addition to the updating/repair of the stand, more steel is being added to fully support the SLS. With all these modifications, the lightning protection system must be brought up to code to assure the protection of all personnel and assets. Structural bonding is a part of the lightning protection system. The focus of this project was to assure proper structural bonding. To begin, all relevant technical standards and the construction specifications were reviewed. This included both the specifications for the lightning protection and for general construction. The drawings were reviewed as well. From the drawings, bolted structural joints were reviewed to determine whether bonding was necessary. Several bolted joints were determined to need bonding according to the notes in the drawings. This exceeds the industry standards. The bolted joints are an electrically continuous joint. During tests, the stand experiences heavy vibration that may weaken the continuity of the bolted joint. Therefore, the secondary bonding is implemented to ensure that the structural joint has low resistance. If the structural joint has a high resistance because of corrosion, a potential gradient can occur that can cause a side flash. Damage, injury, or death can occur from a side flash so they are to be prevented. A list of the identified structural joints was compiled and sent to the contractor to be bonded. That covers the scope of this project.

Kinard, Brandon↗

New generation of plasma-sprayed mullite coatings on silicon carbide

Mullite is promising as a protective coating for silicon-based ceramics in aggressive high-temperature environments. Conventionally plasma-sprayed mullite on SiC tends to crack and debond on thermal cycling. It is shown that this behavior is due to the presence of amorphous mullite in the conventionally sprayed mullite. Heating the SiC substrate during the plasma spraying eliminated the amorphous phase and produced coatings with dramatically improved properties. The new coating exhibits excellent adherence and crack resistance under thermal cycling between room temperature and 1000 to 1400 C. Preliminary tests showed good resistance to Na2CO3-induced hot corrosion.

Lee, Kang N.↗

Mach 0.3 Burner Rig Facility at the NASA Glenn Materials Research Laboratory

This Technical Memorandum presents the current capabilities of the state-of-the-art Mach 0.3 Burner Rig Facility. It is used for materials research including oxidation, corrosion, erosion and impact. Consisting of seven computer controlled jet-fueled combustors in individual test cells, these relatively small rigs burn just 2 to 3 gal of jet fuel per hour. The rigs are used as an efficient means of subjecting potential aircraft engine/airframe advanced materials to the high temperatures, high velocities and thermal cycling closely approximating actual operating environments. Materials of various geometries and compositions can be evaluated at temperatures from 700 to 2400 F. Tests are conducted not only on bare superalloys and ceramics, but also to study the behavior and durability of protective coatings applied to those materials.

Fox, Dennis S.↗

Electroluminescence Imaging: A Quantitative Characterization Technique to Measure Dust Occlusion of Solar Cells

Electroluminescence (EL) imaging is a qualitative characterization technique that is typically used to identify cracks, corrosion, and other defects in solar cells. It consists of imaging a cell under forward bias, where the solar cell emits photons due to radiative electron-hole pair recombination. Over the past few years, our team has expanded this into a quantitative technique with the help of image processing. We have primarily used this method to investigate lunar dust occlusion of solar cells and arrays. Lunar dust accumulation on solar cells is a major concern because it directly limits light accessible to the cell, decreasing power output. Many teams are working to develop dust mitigation technology to protect these arrays on the surface of the Moon, but thoroughly characterizing their efficacy is important to ensure their success prior to launch. Here, we present EL as a quantitative characterization technique to observe dust coverage on solar cells that, when coupled with IV performance measurements, can offer unique insights into how dust coverage impacts power output. Quantitative electroluminescence imaging works by running EL images through an image processing script that first grayscales the image then plots a histogram of the brightness of each pixel. On its own, it does not offer much insight into a solar cell’s performance. However, when comparing images to a baseline pristine, undamaged, or uncoated solar cell, it can quickly provide information about the impacts of surface contaminants or damage to the cell. Here, we present a case study where quantitative EL is used to measure the efficacy of dust mitigation technology for flexible solar arrays and discuss the lessons learned about dust mitigation, testing with lunar simulant, and this characterization technique.

photovoltaics↗

Oxidation-resistance Mechanism and Other Properties of Molybdenum Disilicide

The outstanding oxidation resistance of molybdenum disilicide at 2400 F and above was found to depend on the formation of a protective siliceous coating which a-cristobalie has been identified. Molybdenum disilicide is not inherently resistant to oxidation and in powdered form burns at low temperatures.Melting and casting experiments have demonstrated the decomposition of the material at the melting point. The room-temperature modulus of elasticity has been determined and electric-resistivity data are given to 2000 F.

MATERIALS, PROPERTIES-CORROSION RESISTANCE↗

Asbestos Free Insulation Development for the Space Shuttle Solid Propellant Rocket Motor (RSRM)

Asbestos has been used for many years as an ablation inhibitor in insulating materials. It has been a constituent of the AS/NBR insulation used to protect the steel case of the RSRM (Reusable Solid Rocket Motor) since its inception. This paper discusses the development of a potential replacement RSRM insulation design, several of the numerous design issues that were worked and processing problems that were resolved. The earlier design demonstration on FSM-5 (Flight Support Motor) of the selected 7% and 11% Kevlar(registered) filled EPDM (KF/EPDM) candidate materials was expanded. Full-scale process simulation articles were built and FSM-8 was manufactured using multiple Asbestos Free (AF) components and materials. Two major problems had to be overcome in developing the AF design. First, bondline corrosion, which occurred in the double-cured region of the aft dome, had to be eliminated. Second, KF/EPDM creates high levels of electrostatic energy (ESE), which does not readily dissipate from the insulation surface. An uncontrolled electrostatic discharge (ESD) of this surface energy during many phases of production could create serious safety hazards. Numerous processing changes were implemented and a conductive paint was developed to prevent exposed external insulation surfaces from generating ESE/ESD. Additionally, special internal instrumentation was incorporated into FSM-8 to record real-time internal motor environment data. These data included inhibitor insulation erosion rates and internal thermal environments. The FSM-8 static test was successfully conducted in February 2000 and much valuable data were obtained to characterize the AF insulation design.

Allred, Larry D.↗

Robust Low Cost Liquid Rocket Combustion Chamber by Advanced Vacuum Plasma Process

Next-generation, regeneratively cooled rocket engines require materials that can meet high temperatures while resisting the corrosive oxidation-reduction reaction of combustion known as blanching, the main cause of engine failure. A project was initiated at NASA-Marshal Space Flight Center (MSFC) to combine three existing technologies to build and demonstrate an advanced liquid rocket engine combustion chamber that would provide a 100 mission life. Technology developed in microgravity research to build cartridges for space furnaces was utilized to vacuum plasma spray (VPS) a functional gradient coating on the hot wall of the combustion liner as one continuous operation, eliminating any bondline between the coating and the liner. The coating was NiCrAlY, developed previously as durable protective coatings on space shuttle high pressure fuel turbopump (HPFTP) turbine blades. A thermal model showed that 0.03 in. NiCrAlY applied to the hot wall of the combustion liner would reduce the hot wall temperature 200 F, a 20% reduction, for longer life. Cu-8Cr-4Nb alloy, which was developed by NASA-Glenn Research Center (GRC), and which possesses excellent high temperature strength, creep resistance, and low cycle fatigue behavior combined with exceptional thermal stability, was utilized as the liner material in place of NARloy-Z. The Cu-8Cr-4Nb material exhibits better mechanical properties at 650 C (1200 F) than NARloy-Z does at 538 C (1000 F). VPS formed Cu-8Cr-4Nb combustion chamber liners with a protective NiCrAlY functional gradient coating have been hot fire tested, successfully demonstrating a durable coating for the first time. Hot fire tests along with tensile and low cycle fatigue properties of the VPS formed combustion chamber liners and witness panel specimens are discussed.

Holmes, Richard↗

Fabrication of Lightweight Radiation Shielding Composite Materials by Field Assisted Sintering Technique (FAST)

Advances in radiation shielding technologies are needed to protect humans and electronic components from all threats of space radiation over long durations. In this paper, we report on the use of the innovative and novel fabrication technology known as Field Assisted Sintering Technology (FAST) to fabricate lightweight material with enhanced radiation shielding strength to safeguard humans and electronics suitable for next generation space exploration missions. The base materials we investigated were aluminum (Al), the current standard material for space hardware, and Ultra-High Molecular Weight Polyethylene (UHMWPE), which has high hydrogen content and resistance to nuclear reaction from neutrons, making it a good shielding material for both gamma radiation and particles. UHMWPE also has high resistance to corrosive chemicals, extremely low moisture sensitivity, very low coefficient of friction, and high resistance to abrasion. We reinforced the base materials by adding high density (ie, high atomic weight) metallic material into the composite. These filler materials included: boron carbide (B4C), tungsten (W), tungsten carbide (WC) and gadolinium (Gd).

Prasad, Narasimha↗

Thermal and Environmental Barrier Coatings for Advanced Propulsion Engine Systems

Ceramic thermal and environmental barrier coatings (TEBCs) are used in gas turbine engines to protect engine hot-section components in the harsh combustion environments, and extend component lifetimes. For future high performance engines, the development of advanced ceramic barrier coating systems will allow these coatings to be used to simultaneously increase engine operating temperature and reduce cooling requirements, thereby leading to significant improvements in engine power density and efficiency. In order to meet future engine performance and reliability requirements, the coating systems must be designed with increased high temperature stability, lower thermal conductivity, and improved thermal stress and erosion resistance. In this paper, ceramic coating design and testing considerations will be described for high temperature and high-heat-flux engine applications in hot corrosion and oxidation, erosion, and combustion water vapor environments. Further coating performance and life improvements will be expected by utilizing advanced coating architecture design, composition optimization, and improved processing techniques, in conjunction with modeling and design tools.

Zhu, Dong-Ming↗

Anti-Corrosion Coating

NASA-Goddard developed a zinc-rich coating with a special binder that exhibits longer life and booths with the air purifiers. superior adhesion characteristics-so that only a single coat is required. Unlike conventional coatings, . the NASA compound is easy to mix and it requires no straining before application; its materials also cost less. Thus the new coating offers cost advantages in materials, labor hours per application, and fewer applications over a given time span. The NASA coating is now undergoing test on a number of coastal area structures. In a cooperative effort with the Philadelphia Mayor's Science and Technology Council, the coating has been applied to sample sections of the Frankford Elevated System's steel support structure. On the West Coast, it is being tested on facilities of the Pillar Point Satellite Tracking Station, Pillar Point, Cat. and on segments of the Golden Gate Bridge. It is also undergoing evaluation as an undercoating to protect road equipment against de-icing salts; the coating was applied to the underside of a truck and its performance is being recorded periodically by the Vermont Department of Highways. NASA has issued patent licenses to two paint companies and the coating is expected to be commercially available this year.

Source record↗

NASA Tech Briefs, July 2003

Topics covered include: Real-Time, High-Frequency QRS Electrocardiograph; Software for Improved Extraction of Data From Tape Storage; Radio System for Locating Emergency Workers; Software for Displaying High-Frequency Test Data; Capacitor-Chain Successive-Approximation ADC; Simpler Alternative to an Optimum FQPSK-B Viterbi Receiver; Multilayer Patch Antenna Surrounded by a Metallic Wall; Software To Secure Distributed Propulsion Simulations; Explicit Pore Pressure Material Model in Carbon-Cloth Phenolic; Meshed-Pumpkin Super-Pressure Balloon Design; Corrosion Inhibitors as Penetrant Dyes for Radiography; Transparent Metal-Salt-Filled Polymeric Radiation Shields; Lightweight Energy Absorbers for Blast Containers; Brush-Wheel Samplers for Planetary Exploration; Dry Process for Making Polyimide/ Carbon-and-Boron-Fiber Tape; Relatively Inexpensive Rapid Prototyping of Small Parts; Magnetic Field Would Reduce Electron Backstreaming in Ion Thrusters; Alternative Electrochemical Systems for Ozonation of Water; Interferometer for Measuring Displacement to Within 20 pm; UV-Enhanced IR Raman System for Identifying Biohazards; Prognostics Methodology for Complex Systems; Algorithms for Haptic Rendering of 3D Objects; Modeling and Control of Aerothermoelastic Effects; Processing Digital Imagery to Enhance Perceptions of Realism; Analysis of Designs of Space Laboratories; Shields for Enhanced Protection Against High-Speed Debris; Study of Dislocation-Ordered In(x)Ga(1-x)As/GaAs Quantum Dots; and Tilt-Sensitivity Analysis for Space Telescopes.

Source record↗

Digital temperature and velocity control of mach 0.3 atmospheric pressure durability testing burner rigs in long time, unattended cyclic testing

Hardware and software were developed to implement the hybrid digital control of two Jet A-1 fueled Mach 0.3 burners from startup to completion of a preset number of hot corrosion flame durability cycle tests of materials at 1652 F. This was accomplished by use of a basic language programmable microcomputer and data aquisition and control unit connected together by the IEEE-488 Bus. The absolute specimen temperature was controlled to + or - 3 F by use of digital adjustment of the fuel flow using a P-I-D (Proportional-Integral-Derivative) control algorithm. The specimen temperature was within + or - 2 F of the set point more than 90 percent of the time. Pressure control was achieved by digital adjustment of the combustion air flow using a proportional control algorithm. The burner pressure was controlled at 1.0 + or - 0.02 psig. Logic schemes were incorporated into the system to protect the test specimen from abnormal test conditions in the event of a hardware of software malfunction.

Deadmore, D. L.↗

The 2004 NASA Aerospace Battery Workshop

Topics covered include: Super NiCd(TradeMark) Energy Storage for Gravity Probe-B Relativity Mission; Hubble Space Telescope 2004 Battery Update; The Development of Hermetically Sealed Aerospace Nickel-Metal Hydride Cell; Serial Charging Test on High Capacity Li-Ion Cells for the Orbiter Advanced Hydraulic Power System; Cell Equalization of Lithium-Ion Cells; The Long-Term Performance of Small-Cell Batteries Without Cell-Balancing Electronics; Identification and Treatment of Lithium Battery Cell Imbalance under Flight Conditions; Battery Control Boards for Li-Ion Batteries on Mars Exploration Rovers; Cell Over Voltage Protection and Balancing Circuit of the Lithium-Ion Battery; Lithium-Ion Battery Electronics for Aerospace Applications; Lithium-Ion Cell Charge Control Unit; Lithium Ion Battery Cell Bypass Circuit Test Results at the U.S. Naval Research Laboratory; High Capacity Battery Cell By-Pass Switches: High Current Pulse Testing of Lithium-Ion; Battery By-Pass Switches to Verify Their Ability to Withstand Short-Circuits; Incorporation of Physics-Based, Spatially-Resolved Battery Models into System Simulations; A Monte Carlo Model for Li-Ion Battery Life Projections; Thermal Behavior of Large Lithium-Ion Cells; Thermal Imaging of Aerospace Battery Cells; High Rate Designed 50 Ah Li-Ion Cell for LEO Applications; Evaluation of Corrosion Behavior in Aerospace Lithium-Ion Cells; Performance of AEA 80 Ah Battery Under GEO Profile; LEO Li-Ion Battery Testing; A Review of the Feasibility Investigation of Commercial Laminated Lithium-Ion Polymer Cells for Space Applications; Lithium-Ion Verification Test Program; Panasonic Small Cell Testing for AHPS; Lithium-Ion Small Cell Battery Shorting Study; Low-Earth-Orbit and Geosynchronous-Earth-Orbit Testing of 80 Ah Batteries under Real-Time Profiles; Update on Development of Lithium-Ion Cells for Space Applications at JAXA; Foreign Comparative Technology: Launch Vehicle Battery Cell Testing; 20V, 40 Ah Lithium Ion Polymer Battery for the Spacesuit; Low Temperature Life-Cycle Testing of a Lithium-Ion Battery for Low-Earth-Orbiting Spacecraft; and Evaluation of the Effects of DoD and Charge Rate on a LEO Optimized 50 Ah Li-Ion Aerospace Cell.

Source record↗

Study of the effects of gaseous environmental on the hot corrosion of superalloy materials

Studies have been conducted to examine the effect of low concentrations of NaCl(g) on the high temperature oxidation behavior of complex superalloys and potential coating formulations modified by silicon and reactive element (i.e., yttrium and hafnium) additions. Depending on alloy composition, a variety of effects were thermogravimetrically produced. Aluminum free alloys such as MAR-M509 and Hastelloy X with molybdenum and tungsten in solid solution showed accelerated (or breakaway) kinetics similar to that observed for Ni-Cr alloys. For IN-792, an alloy high in chromium and low in aluminum, molybdenum and tungsten present in solid solution does not adversely affect oxidation kinetics in the presence of NaCl(g). On the other hand, nickel-base alloys high in aluminum and molybdenum are catastrophically attacked by NaCl-bearing atmospheres. Silicon additions were, in general, observed to slightly improve the oxidation resistance of Ni, Ni-40Cr and CoCrAlY compositions in NaCl(g)-bearing atmospheres. To the degree that processes responsible for Al2O3 whisker formation deleteriously affect protective scale adherence, the addition of yttrium or hafnium can inhibit such whisker growth.

Smeggil, J. G.↗

Kinetic Monte Carlo Simulations of Oxygen Diffusion in Environmental Barrier Coating Materials

Ceramic Matrix Composite (CMC) materials are of interest for use in next-generation turbine engine components, offering a number of significant advantages, including reduced weight and high operating temperatures. However, in the hot environment in which such components operate, the presence of water vapor can lead to corrosion and recession, limiting the useful life of the components. Such degradation can be reduced through the use of Environmental Barrier Coatings (EBCs) that limit the amount of oxygen and water vapor reaching the component. Candidate EBC materials include Yttrium and Ytterbium silicates. In this work we present results of kinetic Monte Carlo (kMC) simulations of oxygen diffusion, via the vacancy mechanism, in Yttrium and Ytterbium disilicates, along with a brief discussion of interstitial diffusion. An EBC system typically includes a bond coat located between the EBC and the component surface. Bond coat materials are generally chosen for properties other than low oxygen diffusivity, but low oxygen diffusivity is nevertheless a desirable characteristic, as the bond coat could provide some additional component protection, particularly in the case where cracks in the coating system provide a direct path from the environment to the bond coat interface. We have therefore performed similar kMC simulations of oxygen diffusion in this material.

Good, Brian S.↗