Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Bed”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 469 records · Page 26

Island scanning pattern optimization for residual deformation mitigation in laser powder bed fusion via sequential inherent strain method and sensitivity analysis

Laser powder bed fusion (L-PBF) has emerged as one of the mainstream additive manufacturing approaches for fabricating metal parts with complex geometries and intricate internal structures. However, large deformation associated with rapid heating and cooling can lead to build failure and requires post-processing which may increase manufacturing cost and prolong the production period. Here in this work, an island scanning pattern design method is proposed to optimize the scanning direction of each island in order to reduce part deformation after cutting off the build platform. The objective of this optimization is to minimize the upward bending of the part after sectioning, which allows the part deformation to satisfy the tolerance requirement or reduce the post heat treatment time. Inherent strain method is employed in the sequential finite element analysis consisting of layer-by-layer activations and sectioning for fast residual distortion prediction. Full sequential sensitivity analysis for the formulated optimization is provided to update the island scanning directions. To show the feasibility and effectiveness of the proposed method, the scanning patterns of a block structure and a connecting rod were designed and parts were fabricated using an open architecture L-PBF machine. The fabrication experiments demonstrated that the residual deformation of both parts fabricated by optimized scanning pattern can be reduced by over 50% compared to the initial scanning patterns, which demonstrate the effectiveness of the proposed method.

36 MATERIALS SCIENCE↗

Predicting defects in laser powder bed fusion using in-situ thermal imaging data and machine learning

Variation in the local thermal history during the Laser Powder Bed Fusion (LPBF) process in Additive Manufacturing (AM) can cause micropore defects, which add to the uncertainty of the mechanical properties (e.g., fatigue life, tensile strength) of the built materials. In-situ sensing has been proposed for monitoring the AM process to minimize defects, but successful minimization requires establishing a quantitative relationship between the sensing data and the porosity, which is particularly challenging with a large number of variables (e.g., laser speed, power, scan path, powder property). Physics-based modeling can simulate such an in-situ sensing-porosity relationship, but it is computationally costly. In this work, we develop Machine Learning (ML) models that can use in-situ thermographic data to predict the micropore of LPBF stainless steel materials. This work considers two identified key features from the thermal histories: the time above the apparent melting threshold ($\tau$) and the maximum radiance ( T max ). These features are computed, stored for each voxel in the built material, and then used as inputs. The binary state of each voxel, either defective or normal, is the output. Different ML models are trained and tested for the binary classification task. In addition to using the thermal features of each voxel to predict its own state, the thermal features of neighboring voxels are also included as inputs. This is shown to improve the prediction accuracy, which is consistent with thermal transport physics around each voxel contributing to its final state. Among the models trained, the F1 scores on test sets reach above 0.96 for Random Forests. Feature importance analysis based on the ML models shows that T max is more important to the voxel state than $\tau$ . The analysis also finds that the thermal history of the voxels above the present voxel is more influential than those beneath it. Our study significantly extends the capability of using in-situ thermographic data to predict porosity in LPBF materials. Finally, since ML models are fast, they may play integral roles in the optimization and control of such AM technologies.

36 MATERIALS SCIENCE↗

Fatigue performance of laser powder bed fusion hydride-dehydride Ti-6Al-4V powder

We report hydride-dehydride (HDH) Ti-6Al-4V alloy with particle size distribution of 50–120 µm is laser powder bed fusion (L-PBF) processed using optimum processing parameters and a near-fully dense structure with a density of 99.9 % is achieved. Microstructural observations and phase analyses indicate formation of columnar β grains with acicular α/α' phases in as-built condition. The roughness of the as-fabricated samples is significant with an average roughness of R a = 15.71 ± 3.96 µm and a root mean square roughness of R rms = 108.4 ± 24.9 µm, however, both values are reduced to R a = 0.19 ± 0.04 µm and R rms = 4.9 ± 0.6 µm after mechanical grinding. Mechanical tests are carried out on as-fabricated specimens followed by stress relief treatment. All samples are tested to failure in fatigue, under fully-reversed tension-compression conditions of R = –1. The as-built samples failed from the surface with crack initiation mainly at micro-notches, whereas after mechanically grinding, crack initiation changed to subsurface defects such as pores. Minimizing surface roughness by mechanically grinding eliminates surface micro-notches which improves fatigue strength in the high cycle fatigue region. Fatigue notch factor calculations showed that the effect of surface roughness was significantly lower when HDH powder is used compared to standard spherical powder. X-ray diffraction analysis revealed an in-plane compressive stress, micro-strain and grain refinement on the surface of the mechanically ground samples. Fractography observations (macroscale) revealed a fully brittle fracture in the first stage of crack growth with a transition to a dominantly ductile fracture in the third stage of crack growth. On the other hand, at the micro scale, even the brittle fracture regions showed evidence of ductile fracture within the α' martensite laths.

36 MATERIALS SCIENCE↗

Simultaneous optimization of hatching orientations and lattice density distribution for residual warpage reduction in laser powder bed fusion considering layerwise residual stress stacking

The reduction in the residual warpage generated via fabrication is an emerging issue in metals’ laser powder bed fusion additive manufacturing (AM). One solution from a design for additive manufacturing (DfAM) perspective is to arrange a hatching strategy that utilizes the asymmetry of the residual stress generated from a molten pool. Another approach is to arrange the geometry of the parts, such as forming an inner lattice structure to arrange the effective stiffness. In this study, the simultaneous optimization of the laser hatching orientation and lattice density distribution was conducted to minimize the residual warpage in lattice infill structures and confirm their synergetic effect. The mutual effect of each layer was highlighted when considering the mechanical background of the optimal results because an imbalance in the residual stress caused the warpage of the AM parts between the layers. The proposed methodology was validated via experimental verification using a quasi-2D plate, 3D bracket, and 3D connecting-rod design problems. The residual warpage in the quasi-2D study, measured as the edge’s vertical deformation, was reduced from 23.4% to 39.4% compared with the benchmark design. In the 3D studies, the warpage reductions ranged from 13.1% to 20.7%.

36 MATERIALS SCIENCE↗

Observation of spatter-induced stochastic lack-of-fusion in laser powder bed fusion using in situ process monitoring

Material produced via additive manufacturing (AM) continues to exhibit variable mechanical properties despite apparent optimization of processing parameters, inhibiting qualification efforts and limiting use in critical applications. Stochastic lack-of-fusion flaws may help explain this variability, but the origin of these seemingly random defects has to this point remained unclear. In this work, we show that spatter particles, material ejected from the laser melt pool, are directly responsible for generating stochastic lack-of-fusion in laser-based powder bed fusion components through the application of spatial statistics. Herein a statistically significant, causal relationship between spatter particles and stochastic lack-of-fusion is established, and the spatial and morphological relationships between spatter and internal flaws are investigated. The occurrence of spatter-induced lack-of-fusion in relation to the inert gas flow and laser trajectory direction is also investigated, and recommendations for mitigating the occurrence of spatter are evaluated.

36 MATERIALS SCIENCE↗

Ultrafine-grained Fe-TiB 2 high-modulus nanocomposite steel with high strength and isotropic mechanical properties by laser powder bed fusion

Fe-TiB 2 metal matrix composite, also called high-modulus steels (HMSs), are of great interest for applications in fuel-efficient transportation infrastructure, aerospace, and wear industries due to their high specific stiffness and yield strength. However, conventional cast Fe-TiB 2 HMSs often contain coarse and sharp-edged TiB 2 particles which easily trigger premature cracking during loading. Here, we synthesized a Fe-TiB 2 nanocomposite HMS via laser powder bed fusion (LPBF) additive manufacturing of mixed micro-sized powders of Fe, Ti, and Fe 2 B. We investigated the microstructure formation and mechanical behavior of the Fe-TiB 2 HMS. We found that in situ chemical reaction of Ti and Fe 2 B enables the formation of TiB 2 particles at nanoscale during rapid solidification of LPBF. These nanoscale TiB 2 particles can serve as heterogeneous nucleation sites and promote the formation of ultrafine and equiaxed α-Fe grains with random crystallographic textures, which differ from many other additively manufactured (AM) metal alloys characteristic of strong crystallographic textures. As such, isotropic mechanical properties were achieved in the AM Fe-TiB 2 nanocomposite HMS with a high elastic modulus of ~ 240 GPa, an exceptional yield strength of ~ 1450 MPa, and a large plasticity of ~ 20% under compression. Quantitative analysis reveals that the high yield strength primarily originates from strengthening contributions of the ultrafine grains with an average grain size of ~450 nm, the nanoscale TiB 2 reinforcing particles of 20–180 nm, and a high density of printing-induced dislocations of the order of 10 15 m –2 . In situ synchrotron high-energy X-ray diffraction unveils the load partitioning from the softer α-Fe matrix to the stiffer and stronger TiB 2 nanoparticles, contributing to the sustained strain hardening during compression. Our work not only provides a general pathway for achieving high-performance metal matrix nanocomposites by in situ chemical reaction and precipitation of ceramic nanoparticles during additive manufacturing, but also offers mechanistic insights into the deformation mechanism of nanoparticle-reinforced HMS composites.

36 MATERIALS SCIENCE↗

An assessment of the utility of multirate time integration for the modeling of laser powder bed fusion

Finite element simulation of the laser powder bed fusion process is made challenging by the inherently multiscale nature of the process. When using the typical global time stepping techniques, slowly-evolving regions of the domain receive the same numerical treatment as the regions with the highest temperature rates. The current work details the implementation and evaluation of an implicit multirate method which is able to advance different regions of the domain with distinct time steps, depending on their current solution rate. Previous work indicates that this representation of the temporal scales of the problem can lead to significant reductions in wall clock run time, and it is shown herein that multirate time integration, when used with a uniform process-scale mesh, can result in speedups of approximately 19, 42, and 87 times, for domains with edge lengths of approximately 1 mm, 2 mm, and 5 mm, respectively. When used in conjunction with $\ h$-refinement (limited to two levels of refinement), the resulting speedups (taken relative to the uniform mesh) are around 28, 85, and 665 times. The method is demonstrated to converge as indicated by the literature, and its use with an AM-Bench domain is demonstrated.

42 ENGINEERING↗

Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion

In this study, an Al-6Ce-3Ni-0.7Fe (wt%) alloy was fabricated via laser powder-bed fusion and its microstructure, thermal stability, tensile properties, and creep properties are investigated for two rapid-solidification rates with different eutectic spacings. For both faster- and slower-cooled states, the as-fabricated alloy mostly shows elongated grains with very fine eutectic networks (~40 nm lamellar width) comprising a high-volume fraction (~18 %) of intermetallic phases. Faster-cooled samples, however, display a less continuous eutectic network with finer spacing (~100 nm), leading to higher Orowan strengthening and therefore superior microhardness and yield stress up to ~350 °C. Upon aging (300 - 450 °C), micron-size Al 9 (Ni,Fe) 2 needle-like precipitates form within grains, and the Al 11 Ce 3 eutectic network spheroidizes, while retaining a submicron width and spacing, resulting in 33–37 % drop in microhardness after 144 h aging at 400 °C. Limited tensile ductility (~6 %) and creep ductility (~1-2 %) are measured for both faster- and slower-cooled alloys due to an inhomogeneous microstructure, where cavitation preferentially initiates at melt-pool boundaries, precipitate-free zones, and/or denuded zones, eventually leading to local fracture. Denuded zones, induced by stress, form due to diffusional flow with stress-dependent orientations, and are identified as microstructurally weak regions leading to strain localization. The present alloy does not show a significant difference in 300 °C creep resistance between: (i) tensile and compressive loading, (ii) faster- and slower-cooled samples, and (iii) continuous and spheroidized eutectics. Creep resistance at 300 °C is comparable to that of a Ce-richer Al-10.5Ce-3.1Ni-1.2Mn (wt%) alloy, despite the formation of denuded zones and needle-like Al 9 (Ni,Fe) 2 precipitates.

36 MATERIALS SCIENCE↗

Grain structure and texture selection regimes in metal powder bed fusion

Additive manufacturing (AM) offers opportunities to produce complex part geometries not possible with conventional processing and in some cases even improve part performance. However, adoption has been slowed by difficulties assessing microstructure variability and there is no straightforward approach to relate processing to grain structure characteristics. In this study, datasets from AdditiveFOAM heat transport simulations of laser powder bed fusion (LPBF) are used to drive ExaCA simulations of grain structure. The GPU utilization of ExaCA and an algorithmic update for modeling melt pool overlap region solidification enabled rapid and parallel simulation across a wider range of process conditions than previously explored with cellular automata-based solidification models. A texture selection angle $θ_s$ is defined based on melt pool overlap geometry, and the range of $θ_s$ over which a commonly observed texture transition occurs in characterized AM builds was well-reproduced by ExaCA simulations over a wide range of melt pool shape, hatch spacing, and layer height. ExaCA simulations with 90 degree rotation of the scan direction on every other layer reproduced a number of trends from the AM literature including grain refinement, the dominance of layers with larger melt pools on the final grain structure, and the weakening or strengthening of texture depending on odd and even layer melt pool overlap geometry. EBSD data from a benchmark AM part is used to validate the simulated mechanism of a layer rotation-induced texture strengthening effect. Importantly, these results expand the understanding of the mechanisms for texture selection in alloys with cubic crystal symmetry and offer an approach to easily evaluate processing conditions. With this new understanding, these modeling tools will enable anticipation of previously unexpected variations in grain structure and target specific microstructures and properties.

36 MATERIALS SCIENCE↗

Part-scale microstructure prediction for laser powder bed fusion Ti-6Al-4V using a hybrid mechanistic and machine learning model

Laser powder bed fusion (LPBF) Ti-6Al-4V is widely studied for use in structural applications in aerospace and medical industries, but mechanical anisotropy and microstructural inhomogeneity prohibits its wider adoption. Although successful microstructure prediction models have been developed, a remaining challenge is their limited integration across length/time scales and validation by experimental studies. Here, this work proposes a physics-augmented machine learning surrogate model to unite predictions of LPBF temperature, β phase morphology and texture, and α/α’ formation into a single framework that is calibrated and validated with experiments. First, a phase field (PF) model of the martensitic β→α’ transformation is developed and calibrated using data from in-situ synchrotron cyclic heating/cooling studies quantifying the variation of α phase fraction with time. In parallel, an established finite difference-Monte Carlo (FDMC) model predicts the part-scale temperature profile and β grain formation during solidification. A dataset is developed using LPBF cyclic temperature descriptors from the FDMC model as inputs and corresponding α/α’ phase fraction and width from the PF model as outputs. Five machine learning (ML) regression models are tested and optimized, having mean absolute error in testing ≤ 4 %, and the k-nearest neighbors (KNN) model is selected as the best performing. The KNN model is called at the nodal level during post-processing of the FDMC model to replace and downscale the response of the PF model. The combined agility and accuracy of the hybrid FDMC-ML model enables part-scale microstructure predictions that can be further used for property predictions to accelerate AM process optimization.

36 MATERIALS SCIENCE↗

Effect of Zr and Sc additions on coarsening- and creep resistance of AlSi10Mg fabricated by laser powder bed fusion

Microstructure and creep properties are studied in a eutectic AlSi10Mg alloy modified with Zr and Sc additions (Al-9.8Si-0.32Mg-0.70Zr-0.23Sc, wt%) manufactured through laser powder-bed fusion (L-PBF). Three types of Zr/Sc-bearing powders - elemental, master-alloy, and pre-alloyed - are employed in the fabrication process, with the pre-alloyed powders providing the highest incorporation of Zr and Sc in the Al matrix. Here, the as-printed alloy exhibits a fine cellular Al-Si eutectic structure which fragments and coarsens into micron-sized Si particles during aging at 300 ºC, leading to a steady drop in alloy microhardness between 0.1 and 1000 h. Coarsening of the eutectic Si phase during aging is not measurably affected by Zr and Sc in solid solution, which precipitate during aging and increases strength, compensating weakening from Si coarsening between 1 and 200 h at 300 ºC. Atom-probe analysis in the peak-aged condition (96 h/300 °C) confirms the presence of Al 3 (Sc,Zr) secondary nano-precipitates with an average radius of 1.0 nm and some Si solubility. Micron-sized grains are present throughout the alloy, with ultra-fine-grained regions at the melt pool boundaries, neither of which coarsen during long-term aging at 300 ºC. Under creep conditions at 300 °C, the Zr/Sc-bearing alloy with Al 3 (Sc,Zr) nano-precipitates exhibits power-law behavior, with a high apparent stress exponent (n a = 9) and a high threshold stress (σ th = 43 MPa), exhibiting nearly double the strength of a Zr/Sc-free AlSi10Mg control alloy (σ th = 22 MPa).

36 MATERIALS SCIENCE↗

Ink-based laser powder bed fusion of barium titanate

Barium titanate (BTO) is a lead-free functional ceramic that is widely used in sensors, transducers, and actuators. The increasing demand for complex geometries and quick design iterations motivates the use of additive manufacturing techniques. Laser powder bed fusion (L-PBF) additive manufacturing technique enables the net-shape or near-net-shape fabrication of metals and alloys. Ceramic L-PBF remains challenging due to their high melting temperature. Here, to address this challenge, a nanoparticle ink feedstock was incorporated into the L-PBF process to allow low power melting of BTO. Key print parameters (i.e. laser power, scanning speed, and hatching spacing) were optimized to fabricate millimeter-scale BTO parts. The printed BTO samples possessed an inhomogeneous equiaxed-columnar-cellular microstructure. Semiconducting current-voltage behavior was observed in as-printed samples, which was attributed to the creation of oxygen vacancies. The piezoelectric d 33 coefficient was measured to be 4.6 pC/N.

Dielectrics↗

Which way does the dendrite grow? Competition among epitaxy, preferred growth direction, and thermal gradients in powder bed fusion additive manufacturing

The as-processed microstructure of metal alloy parts manufactured through laser powder bed fusion (LPBF) is heavily derived from the cellular dendritic solidification. The growth direction of dendrites within the melt pool is determined through competition among epitaxial growth, preferred growth directions, and maximum thermal gradients. However, the dominant factor and the specific role of each in developing melt pool microstructures remain unknown. Here, in this study, we performed single laser track scans on an SS316L single crystal substrate and combined experimental characterization of microstructure and crystal orientations with Computational Fluid Dynamics simulations of thermal gradients to evaluate the role of each factor in determining dendritic growth direction and evolution. Our results reveal that epitaxial growth dominates microstructure development by preferentially growing along a single 〈100〉 variant of the single crystal substrate adjacent to the melt pool boundary. Under LPBF’s highly curved and rapidly evolving thermal field, this preferential dendrite variant selection and its continued growth from the melt pool boundary to the centerline are governed by the local temperature gradient magnitude at the solid-liquid interface, rather than by the instantaneous maximum temperature gradient direction alone. Using these findings, we successfully predict changes in the dendrite growth direction with changing laser scan direction on a single crystal substrate, and show that the geometric melt pool centerline can deviate from the microstructural centerline because asymmetric local temperature gradient magnitudes transiently limit growth, resulting in different dendrite travel distances on each side of the melt pool.

36 MATERIALS SCIENCE↗

Transformations of Ti-5Al-5V-5Cr-3Mo powder due to reuse in laser powder bed fusion: A surface analytical approach

Reactive Ti-5Al-5 V-5Cr-3Mo (Ti5553) alloy feedstock powder is used in laser powder-bed fusion (LPBF). Due to the large quantity of powder necessary for LPBF, powder is reused numerous times under oxidizing environments. Transformations to the powder’s native surface oxide may impact the LPBF process and lead to deviations from expected behavior of printed parts. In this work, we present a multimodal characterization of new and reused powder by combining X-ray photoelectron spectroscopy (XPS), time-of-flight secondary ion mass spectrometry (ToF-SIMS), and transmission electron microscopy (TEM) of focused ion beam (FIB)-prepared cross sections of individual powder particles to understand how the surface oxide composition changes, grows, and becomes hydroxylated and hydrated due to reuse. We show that the native oxide film of Ti5553 powder is a hydroxylated mixed oxide composed of TiO 2 and Al 2 O 3 that grows from 5.6 +/- 0.7 nm to 8.3 +/- 1.1 nm due to reuse. Al oxide regions of the surface oxide become more hydroxylated during reuse in comparison to Ti oxide regions. This indicates that an outer oxide of pure TiO 2 may enhance recyclability of Ti5553 powder while the presence of Al oxides may decrease recyclability. Further characterization of surface transformations due to recyclability may eliminate unnecessary variation in LPBF.

36 MATERIALS SCIENCE↗

Oxide dispersion strengthened 304 L stainless steel produced by ink jetting and laser powder bed fusion

This paper discusses the fundamentals of a novel hybrid method to synthesize oxide dispersion strengthened (ODS) 304 L stainless steel (SS) alloy using a modified laser powder bed fusion (LPBF) machine. Previously, ODS metal matrix composites have been produced by LPBF via ball-milling, which is expensive to scale. Here, we selectively dope yttria nanoparticles into a SS matrix by jetting a precursor chemistry onto the SS substrate prior to laser conversion and consolidation. Here, the new alloy shows good room temperature mechanical properties. Microstructures are studied using electron microscopy, energy dispersive spectroscopy and electron backscatter diffraction.

36 MATERIALS SCIENCE↗

Investigation of Reactivities of Bimetallic Cu-Fe Oxygen Carriers with Coal in High Temperature In-situ Gasification Chemical-Looping Combustion (iG-CLC) and Chemical-Looping with Oxygen Uncoupling (CLOU) Using a Fixed Bed Reactor

This study investigated reduction reactivities and CO2 conversion efficiency of synthesized Fe-Cu-Si OCs for both in-situ gasification CLC (iG-CLC) and Chemical-Looping with Oxygen Uncoupling (CLOU) at high temperatures (950 to 1100°C) with varying ratios of OC to coal char (φ) using a fixed bed reactor-quadrupole mass spectrometer system.

Wang, Ping↗

Brazing characteristics, microstructure, and wettability of laser powder bed fusion additive manufactured GRCop-84 compared to CuCrZr and OFC, and brazing to titanium-zirconium-molybdenum alloy limiters

Laser Powder Bed Fusion (L-PBF) of Glenn Research Copper 84 (GRCop-84), a Cr 2 Nb (8 at. % Cr, 4 at. % Nb) precipitation hardened alloy, produces a fully dense, high conductivity alloy with a yield strength of 500 MPa and ultimate tensile strength (UTS) of 740 MPa with 20% elongation; superior to other competing copper alloys. Braze wetting characteristics of GRCop-84 with Ag-Cu-X, and Au-Cu brazes were similar to CuCrZr, but less than oxygen free copper. No difference in wetting was observed between infill and surface contour areas in L-PBF GRCop-84. Wet sanding to 240 grit (R a =0.24 µm) was considered the optimal surface condition. Silver diffusing through GRCop-84 depleted Cr 2 Nb precipitates from the copper grain and deposited agglomerations of coarsened precipitates within silver-rich regions of intergranular diffusion once a density threshold was reached. Microstructure modification was minimized with 50Au-50Cu braze implying that silver caused precipitate coarsening and agglomeration, and not high temperature exposure. Coarsened precipitates were observed on the surface within braze pools implying a contribution to braze wetting. Palcusil-25, Ticusil, CuSil-ABA, and 50Au-50Cu brazes were suitable for brazing to unplated Titanium-Zirconium-Molybdenum (TZM), while sulfamate nickel plating to allows wetting with CuSil or other non-active brazes. Additionally, vacuum brazing techniques were developed to join a 1 mm thick layer of TZM to the front of additive manufactured GRCop-84 waveguides considering the brazing characteristics of both GRCop-84, TZM, and internal stress from the difference in coefficient in thermal expansion.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Size effect characteristics and influences on fatigue behavior of laser powder bed fusion of thin wall GRCop-42 copper alloy

Size effects, influencing a material's strength, elongation, fatigue limit, and longevity, depend on the operative and dominant deformation and failure mechanisms. This study explores the size effects in additive manufactured (AM) GRCop-42 (Cu-4at%Cr-2at%Nb) thin wall structures fabricated via laser-powder bed fusion (L-PBF) and their impact on fatigue life. The influence of internal defects and surface topography on the fatigue life of specimens in both as-built and hot isostatic pressed (HIP) conditions across different thicknesses is investigated. Where micro-computed tomography (μCT) was used to quantify the internal porosity of as-built, pristine HIP'd, and fatigued HIP'd specimens, and laser microscopy was employed to quantify the surface topography of specimens prior to fatigue. Additionally, quasi-static tests were used to establish baseline mechanical properties (i.e. yield strength (YS), ultimate tensile strength (UTS), and elongation) to frame fatigue testing conditions. Results indicate a significant enhancement in fatigue life for HIP'd specimens for both thicknesses, with internal defects depicting a greater impact than surface topography. Furthermore, fractographic analysis suggests that thicker specimens exhibit higher resistance to crack propagation during fatigue testing in the absence of substantial porosity. Thus, the size effects observed on the fatigue life of L-PBF GRCop-42 appears to be dominated by internal defects.

36 MATERIALS SCIENCE↗